Resumo:
Relationships of several reproductve traits and milk yield were studied in 716 Gyr cows at Sant'Ana da Serra farm, Mococa, State of São Paulo, a humid tropical climate region. Mean age at first calving was 49.8 +/- 0.4 months, with a coeficient of cariation (C. V.) of 20.8%. Only year of parturition significantly affected age at first calving (P < 0.01). Heritability, estimated from paternal half-sib correlations, was 0.91 +/- 0.20, a value considered unrealistically high. Overall mean gestation length was 287.7 +/- 0.5 days (C. V. = 3.3%) for 419 observations, with month and year of parturition having significant effects. Heritability estimate was 0.30 +/- 0.14. Overall mean dry period for 1.276 observations was 238 +/- 3 days (C. V. = 48%); repeatability estimate was 0.19 +/- 0.06. Estimated annual genetic trend for dry period was -0.6 days, phenotypic trend was 11.5 days, and environmental trend, 12.1 days. Month and year of parturition and cow age had no significant effect on dry period. Highest milk yield was obtained at fourth lactation. The gross correlation between milk yield and gestation period was 0.11, and between previous dry period and subsequent milk yield, 0.16. Normal gestations of 285 to 290 days were associated with higher milk yields. Milk yield increased as dry period advanced from 30 to 390 days, and declined as dry period continued beyond 390 days. Delays in first mating and a more extensive dry period decreased reproductive efficiency in the herd studied.
Study of the dielectric and ferroelectric properties of chemically processed BaxSr1-xTiO3 thin films
Resumo:
Polycrystalline BaxSr1-xTiO3 (x = 0.4 and 0.8) thin films with a perovskite structure were prepared by the polymeric precursor method on a platinum-coated silicon substrate. High-quality thin films with uniform composition and thickness were successfully produced by dip-coating and spin-coating techniques. The resulting thin films prepared by dip and spin-coating showed a well-developed dense polycrystalline structure with uniform grain size distribution. The metal-BST-metal structure of the thin films displays good dielectric and ferroelectric properties. The ferroelectric nature to BaxSr1-xTiO3 (x = 0.8) thin film, indicated by butterfly-shaped C-V curves and confirmed by the hysteresis curve, showed 2P(r) = 5.0 muC/cm(2) and E-c = 20 kV/cm. The capacitance-frequency curve reveals that the dielectric constant may reach a value of up to 794 at 1 kHz. on the other hand, the BaxSr1-xTiO3 (x = 0.4) thin films had paraelectric nature and dielectric constant and the dissipation factor at a frequency of 100 kHz were 680 and 0.01, respectively, for film annealed at 700 degreesC. In addition, an examination of the film's I-V curve at room temperature revealed the presence of two conduction regions in the BaxSr1-xTiO3 (x = 0.4 and 0.8) thin films, showing ohmic-like behavior at low voltage and a Schottky-emission or Poole-Frenkel mechanism at high voltage. (C) 2001 Elsevier B.V. B.V. All rights reserved.
Resumo:
Recent studies have shown the existence of two important inhibitory mechanisms for the control of NaCl and water intake: one mechanism involves serotonin in the lateral parabrachial nucleus (LPBN) and the other depends on alpha(2)-adrenergic/imidazoline receptors probably in the forebrain areas. In the present study we investigated if alpha(2)-adrenergic/imidazoline and serotonergic inhibitory mechanisms interact to control NaCl and water intake. Male Holtzman rats with cannulas implanted simultaneously into the lateral ventricle (LV) and bilaterally into the LPBN were used. The ingestion of 0.3 M NaCl and water was induced by treatment with the diuretic furosemide (10 mg/kg of body weight)+the angiotensin converting enzyme inhibitor captopril (5 mg/kg) injected subcutaneously 1 h before the access of rats to water and 0.3 M NaCl. Intracerebroventricular (i.c.v.) injection of the alpha(1)-adrenergic/imidazoline agonist clonidine (20 nmol/l RI) almost abolished water (1.6 +/- 1.2, vs. vehicle: 7.5 +/- 2.2 ml/2 h) and 0.3 M NaCl intake (0.5 +/- 0.3, vs. vehicle: 2.2 0.8 ml/2 h). Similar effects were produced by bilateral injections of the 5HT(2a/2b) serotonergic agonist 2,5-dimetoxy-4-iodoamphetamine (DOI, 5 mug/0.2 mul each site) into the LPBN on water (3.6 +/- 0.9 ml/2 h) and 0.3 M NaCl intake (0.4 +/- 0.2 m1/2 h). Injection of the (alpha(2)-adrenergic/imidazoline antagonist idazoxan (320 nmol) i.c.v. completely blocked the effects of clonidine on water (8.4 +/- 1.5 ml/2 h) and NaCl intake (4.0 +/- 1.2 ml/2 h), but did not change the effects of LPBN injections of DOI on water (4.2 +/- 1.0 ml/2 h) and NaCl intake (0.7 +/- 0.2 ml/2 h). Bilateral injections of methysergide (4 mug/0.2 mul each site) into the LPBN increased 0.3 M NaCl intake (6.4 +/- 1.9 ml/2 h), not water intake. The inhibitory effect of i.c.v. clonidine on water and 0.3 M NaCl was still present after injections of methysergide into the LPBN (1.5 +/- 0.8 and 1.7 +/- 1.4 ml/2 h, respectively). The results show that the inhibitory effects of the activation of a,-adrenergic/imidazoline receptors in the forebrain are still present after blockade of the LPBN serotonergic mechanisms and vice versa for the activation of serotonergic mechanisms of the LPBN. Therefore, each system may act independently to inhibit NaCl and water intake. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
The effect in rats of an anteroventral third ventricle (AV3V) electrolytic lesion on salivary secretion induced by intraperitoneal (i.p.) or intracerebroventricular (i.c.v.) injection of a cholinergic agonist (pilocarpine) was investigated. Sham- or AV3V-lesioned rats anesthetized with urethane and with a stainless steel cannula implanted into the lateral ventricle (LV) were used. The amount of salivary secretion was studied over a seven-minute period after i.c.v. or i.p. injection of pilocarpine. In sham-operated rats, i.p. injection of pilocarpine (1 mg/kg b.w.) (after 6 h, 2, 7, and 15 days) produced salivary secretion (486 +/- 21, 778 +/- 85, 630 +/- 50, and 560 +/- 55 mg/7 min, respectively). This effect was reduced 6 h, 2, and 7 days after an AV3V lesion (142 +/- 22, 113 +/- 32, and 290 +/- 62 mg/7 min, respectively), but not 15 days after an AV3V lesion (516 +/- 19 mg/7 min). I.c.v. injection of pilocarpine (120 mug in 1 muL), in sham-operated rats after 6 h, 2, 7, and 15 days also produced salivary secretion (443 +/- 20, 417 +/- 81, 496 +/- 14, and 427 +/- 47 mg/7 min, respectively). The effects of i.c.v. pilocarpine were also reduced 6 h, 2, and 7 days after an AV3V lesion (143 +/- 19, 273 +/- 14, and 322 +/- 17 mg/7 min, respectively), but not after 15 days (450 +/- 28 mg/7 min). The results demonstrate that the central nervous system, and particularly the AV3V region, is important for the effect of pilocarpine on salivary secretion in rats. Moreover, they suggest that activation of central pathways may play an important part in the salivary secretion to peripheral pilocarpine in rats.
Resumo:
The alpha(2)-adrenergic agonist clonidine and the neuropeptide oxytocin, inhibit sodium intake when injected intracerebroventricularly (i.c.v.). The present work investigates whether (1) vasopressin also inhibits sodium intake when injected i.c.v., and (2) the effect of oxytocin and of vasopressin on sodium intake is affected by i.c.v. injection of idazoxan, an alpha(2)-adrenergic antagonist. Clonidine (30 nmol), oxytocin (40, 80 nmol) and vasopressin (40, 80 nmol) were injected i.c.v. 20 min prior to a 1.5% NaCl appetite test, in rats depleted of sodium for 24 h by a combination of a single s.c. injection of furosemide (10 mg/rat) and removal of ambient sodium. Every dose of clonidine, oxytocin and vasopressin inhibited the 1.5% NaCl intake. Seizures were observed with the higher dose of vasopressin, but not with either dose of oxytocin. The effect of i.c.v. injection of clonidine (30 nmol), oxytocin (80 nmol) or vasopressin (40 nmol) was partially inhibited by prior i.c.v. injection of idazoxan (160, 320 nmol). The results suggest that the inhibition of 1.5% NaCl intake induced by i.c.v. injection of neuropeptides in sodium-depleted rats depends, in part, on the activation of central alpha(2)-adrenoceptors. (C) 1997 Elsevier B.V. B.V. All rights reserved.
Resumo:
Tin dioxide (SnO2) thin film photoconductivity spectra were measured for a large temperature range using a deuterium source, the intensity of photocurrent spectra in the range 200-400 nm is temperature dependent, and the photocurrent increases in the ultraviolet even for illumination with photon energies much higher than the bandgap transition. This behavior is related to recombination of photogenerated electron-hole pairs with oxygen adsorbed at grain boundaries, which is consistent with nanoscopic crystallite size of sol-gel deposited films. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Protein is one of the limiting factors in animal production, and the knowledge of protein requirements by livestock is crucial for the success of a commercial animal raising enterprise. Thirty-four castrated lambs, 17 of them F1 Ideal x lie de France wool lambs and the remaining ones were Santa Ines hair lambs, with homogeneous initial BW, were used in the experiment. Five animals from each genotype were slaughtered in the beginning of the experimental period and used as reference. Diets (D) were composed of concentrate mix (C) and Cynodon sp. c.v. Tifton 85 hay (R), combined in three different ratios: D1 =60CAOR; D2=40C:60R and D3=20C:80R. Animals of each group of three lambs, that showed simultaneously an initial BW of 20 +/- 0.14 kg at the beginning of the dietary regimen, were slaughtered when one of them reached 35 kg, what always happened to be the one fed with D1. Net requirements for BW gain in wool lamb, fleece-free, ranged from 101 to 110 g of protein/kg BW, and for hair lamb ranged from 1 10 to 118 g of protein/kg BW. Net protein requirements for wool production ranged from 634 to 642 g/kg of produced wool. Hair lambs presented a 7.8-9.5% higher estimated net protein requirements than wool lambs, according to BW and daily weight gain (DG). Total net protein requirements for Santa Ines and wool lambs, with 30 kg of initial B W and an approximate 200 g mean DG, were 48.5 and 45.4 g/day, respectively. Metabolizable protein requirements for Santa Ines and wool lambs, with 20 kg of initial BW and an approximate 200 g mean DG were 59.4 g and 76.5 -/day, respectively. Net protein requirements for wool production was 64g/100g of produced wool. Thus, under the conditions of this experiment, it is concluded that hair lambs showed a higher concentration of protein in the body, more efficient use of the ingested protein and a consequent additional BW gain when fed isoproteic diets as compared to F1 Ideal x Ile de France wool lambs. (c) 2006 Elsevier B.V All rights reserved.
Resumo:
The objective of this work was to evaluate the total endogenous N losses, and protein and energy net requirements for maintenance in growing lambs. Thirty-four castrated lambs, 17 F1 Ideal X Ile de France wool and 17 Santa Inas hair lambs, averaging 20 +/- 0.14 kg BW, were used in the experiment. Five animals from each genotype were slaughtered at the beginning of the experiment and taken as controls. Diets (D) were composed of concentrate mix (C) and Cynodon sp. c.v. Tifton 85 hay (R), combined in three different ratios: D1 = 60C:40R; D2 = 40C:60R and D3 = 20C:80R. Animals of each group of three lambs, that showed BW of 20 kg at the beginning of the dietary regimen, were slaughtered when one of them reached 35 kg, what always happened to be the one fed with D1. Total endogenous N losses estimated for wool lambs were 250 mg N/kg BW0.75. For hair lambs, total endogenous N losses reached 324 mg N/kg BW0.75 . Hair lambs showed higher (P < 0.01) (29.9%) net requirements of protein for maintenance than wool lambs. In contrast, net energy (NE) requirement for maintenance was similar (P > 0.05) for both genotypes (74.27 kcal/kg BW0.75 per day), the average of the antilog of the two intercept values obtained from the estimated regression equations of heat production for zero metabolizable energy (ME) consumption. Further studies should be done to check if this trend is also true for metabolizable energy and protein in animals exhibiting BW gains in tropical region. (C) 2003 Elsevier B.V. B.V. All rights reserved.
Resumo:
Photoconductivity of SnO2 sol-gel films is excited, at low temperature, by using a 266 nm line-fourth harmonic-of a Nd:YAG laser. This line has above bandgap energy and promotes generation of electron-hole pairs, which recombines with oxygen adsorbed at grain boundary. The conductivity increases up to 40 times. After removing the illumination on an undoped SnO2 film, the conductivity remains unchanged, as long as the temperature is kept constant. Adsorbed oxygen ions recombine with photogenerated holes and are continuously evacuated from the system, leaving a net concentration of free electrons into the material, responsible for the increase in the conductivity. For Er doped SnO2, the excitation of conductivity by the laser line has similar behavior, however after removing illumination, the conductivity decreases with exponential-like decay. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
Pb1- xCaxTiO3 thin films with x = 0.24 composition were prepared by the polymeric precursor method on Pt/Ti/SiO2/Si substrates. The surface morphology and crystal structure, and the ferroelectric and dielectric properties of the films were investigated. X-ray diffraction patterns of the films revealed their polycrystalline nature. Scanning electron microscopy (SEM) and atomic force microscopy (AFM) analyses showed the surface of these thin films to be smooth, dense and crack-free with low surface roughness. The multilayer Pb1-xCaxTO3 thin films were granular in structure with a grain size of approximately 60-70 nm. The dielectric constant and dissipation factor were, respectively, 174 and 0.04 at a 1 kHz frequency. The 600-nm thick film showed a current density leakage in the order of 10(-7) A/cm(2) in an electric field of about 51 kV/cm. The C-V characteristics of perovskite thin films showed normal ferroelectric behavior. The remanent polarization and coercive field for the deposited films were 15 muC/cm(2) and 150 kV/cm, respectively. (C) 2001 Kluwer Academic Publishers.
Resumo:
Electro-optical properties of sol-gel derived 2 mol% antimony or niobium doped tin dioxide films have been measured. The electron density has been calculated considering all the relevant scattering mechanisms and experimental conductivity data measured in the range -197 to 25 degrees C. The results support the hypothesis that both ionised impurity scattering and grain boundary scattering have comparable effects in the resistivity of coatings, for free electron density congruent to 5 x 10(18) cm(-3). We have measured variation of photoconductivity excitation with wavelength using xenon and deuterium lamp as light sources. Results show that the main band in the photoconductivity spectrum is dependent on the spectral light source emission, the excitation peak reaching 5 eV (deuterium lamp). This band is due to the recombination process involving oxygen species and photogenerated electron-hole pairs. (C) 1999 Elsevier B.V. B.V. All rights reserved.