948 resultados para Wear resistance


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Bi3+ ions substituting at Ba-sites in a limited concentration range with another donor dopant occupying the Ti-sites in polycrystalline BaTiO3 enhanced the positive temperature coefficient of resistance (PTCR) by over seven orders of magnitude. These ceramics did not require normal post sinter annealing or a change to an oxygen atmosphere during annealing. These ceramics had low porosities coupled with better stabilities to large applied electric fields and chemically reducing atmospheres. Bi3+ ions limited the grain growth to less than 8 mum in size, they enhanced the concentration of acceptor-type trap centres at the grain-boundary-layer regions and maintained complete tetragonality at low grain sizes in BaTiO3 ceramics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present paper deals with the study of microstructure and wear characteristics of TiB2 reinforced aluminium metal matrix composites (MMCs). Matrix alloys with 5, 10 and 15% of TiB2 were made using stir casting technique. Effect of sliding velocity on the wear behaviour and tribo-chemistry of the worn surfaces of both matrix and composites sliding against a EN24 steel disc has been investigated under dry conditions. A pin-on-disc wear testing machine was used to find the wear rate, in which EN24 steel disc was used as the counter face, loads of 10-60N in steps of 10N and speeds of 100, 200, 300, 400 and 500 rpm were employed. The results showed that the wear rate was increased with an increase in load and sliding speed for both the materials. However, a lower wear rate was obtained for MMCs when compared to the matrix alloys. The wear transition from slight to severe was presented at the critical applied loads. The transition loads for the MMCs were much higher than that of the matrix alloy. The transition loads were increased with increase in TiB2 and the same was decreased with the increase of sliding speeds. The SEM and EDS analyses were undertaken to demonstrate the effect of TiB2 particles on the wear mechanism for each conditions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Wear of high carbon low alloy (HCLA) cast steel balls during the grinding of a chalcopyrite ore was evaluated under different experimental conditions. The role of oxygen in enhancing ball wear during wet finding is brought out. The influence of pH on ball wear was also examined from the view point of acid production during grinding and reactivity of sulphides. Contributions from corrosion and abrasion towards ball wear are quantified in terms of ball wear rates as a function of time, particle size and gaseous atmosphere in the mill.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A previous study on the tribological performance of a compression-moulded aramid fibre-phenolic resin composite, containing 30% continuous fibre, showed that this composite provides a reasonable combination of the friction coefficient and wear rate to be used as a friction component, such as a brake shoe. In the present work, the effect of sliding speed on the friction and wear behaviour of this composite has been investigated. The sliding experiments were conducted in a speed range of 0.1-6 m s(-1) at two normal pressure levels of 1.0 and 4.9 MPa. The coefficient of friction was found to be stable over a wide range of sliding speeds and normal pressures. The wear of the composite was found to be insensitive to changes in the speed in the higher speed range. The results have been supplemented with scanning electron micrographs to help understand possible friction and wear mechanisms.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sliding tests were conducted, in air, of YTZP ceramic pins against steel discs at an applied pressure of 15.5 MPa over a speed range of 0.3 to 4.0 ms(-1). Pin wear was not detectable until 2.0 m s(-1), after which a finite but small wear rate was observed at 3.0 m s(-1), accompanied by a red glow at the contacting surface. A transition in wear behaviour and friction (mu) occurred at 4.0 ms(-1), increasing the former by over two orders of magnitude. Both mu and wear behaviour changed with time at 4.0 m s(-1). During initial periods mu was high and wear rate increased steadily with time accompanied by ceramic transfer onto the disc, which increased with time. When disc coverage exceeds a certain threshold value, mu decreased rapidly and the wear rate stabilized at a very high value. Metal transfer was not observed at any speed. High surface temperatures brought about significant adhesion between TZP and steel and this together with enhanced plastic deformation brought about a transition in wear behaviour.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High?quality Ag?doped YBa2Cu3O7?? thin films have been grown by laser ablation on R?plane ?1102? sapphire without any buffer layer. Thin films have been found to be highly c?axis oriented with Tc=90 K, transition width ?T?1 K, and transport Jc=1.2×106 A?cm?2 at 77 K in self?field conditions. The microwave surface resistance of these films measured on patterned microstrip resonators has been found to be 530 ?? at 10 GHz at 77 K which is the lowest reported on unbuffered sapphire. Improved in?plane epitaxy and reduced reaction rate between the substrate and the film caused due to Ag in the film are believed to be responsible for this greatly improved microwave surface resistance. © 1995 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present investigation, Al 2024-15vol.%Al2O3 particulate (average size, 18 mu m) composites were fabricated using the liquid metallurgy route. The wear and friction characteristics of Al alloy 2024 and Al 2024-15vol.%Al2O3p, composite in the as-extruded and peak-aged conditions were studied using a pin-on-disc machine (with a steel disc as the counterface material). The worn surfaces, subsurfaces and the debris were analysed in a scanning electron microscope.The performance of the composite in the as-extruded condition is slightly inferior to that of the unreinforced alloy. However, in the T6 condition, although the wear rates of two materials are initially comparable, the unreinforced alloy seizes while the composite does not within the tested range employed. In the as-extruded condition, the presence of Al2O3 particles is not particularly beneficial as they fracture and result in extensive localized cracking and removal of material from the surface. In the peak-aged condition, however, while the unreinforced alloy exhibits severe plastic deformation and undergoes seizure, there is no significant change in the mechanism in the case of the composite. Except in the case of the peak-aged unreinforced alloy, worn surfaces of all other materials show the presence of an iron-rich layer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Donor-doped n-BaTiO3 polycrystalline ceramics show a strong negative temperature coefficient of resistivity below the orthorhombic-rhombohedral phase transition point, from 10(2-3) Omega cm af 190 K to 10(10-13) Omega cm at less than or similar to 50 K, with thermal coefficient of resistance alpha = 20-23% K-1. Stable thermal sensors for low-temperature applications are realized therefrom. The negative temperature coefficient of resistivity region can be modified by substituting isovalent ions in the lattice. Highly nonlinear current-voltage (I-V) curves are observed at low temperatures, with a voltage maximum followed by the negative differential resistance. The I-V curves are sensitive to dissipation so that cryogenic sensors can be fabricated for liquid level control, flow rate monitoring, radiation detection or in-rush voltage limitation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The tol-pal genes are essential for maintaining the outer membrane integrity and detergent resistance in various Gram-negative bacteria, including Salmonella. The role of TolA has been well established for the bile resistance of Salmonella enterica subsp. enterica serovar Typhimurium. We compared the bile resistance pattern between the S. enterica serovars Typhi and Typhimurium and observed that Typhi is more resistant to bile-mediated damage. A closer look revealed a significant difference in the TolA sequence between the two serovars which contributes to the differential detergent resistance. The tolA knockout of both the serovars behaves completely differently in terms of membrane organization and morphology. The role of the Pal proteins and difference in LPS organization between the two serovars were verified and were found to have no direct connection with the altered bile resistance. In normal Luria broth (LB), S. Typhi Delta tolA is filamentous while S. Typhimurium Delta tolA grows as single cells, similar to the wildtype. In low osmolarity LB, however, S. Typhimurium Delta tolA started chaining and S. Typhi Delta tolA showed no growth. Further investigation revealed that the chaining phenomenon observed was the result of failure of the outer membrane to separate in the dividing cells. Taken together, the results substantiate the evolution of a shorter TolA in S. Typhi to counteract high bile concentrations, at the cost of lower osmotic tolerance.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The sliding-wear behavior of Al2O3-SiC-Al composites prepared by melt oxidation against a steel counterface has been recorded in a pin-on-disk machine. At high speeds and pressures (10 m/s, 20 MPa), friction and wear appear to be principally controlled by the in-situ formation of an interfacial film that consists of a layer of Fe3O4. The formation of this him is examined as a function of sliding speed, lubrication, and composite microstructure. A model is proposed in which high surface temperatures cause the preferential extrusion of aluminum from the composite onto the pin/disk interface. This promotes the adhesive pickup of iron and its oxidation to form a stable tribologically beneficial layer of Fe3O4.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Donor-doped n-(Ba,Pb)TiO3 polycrystalline ceramics exhibit distinctly two-step positive temperature coefficient of resistance (PTCR) characteristics when formulated with suitable combinations of B2O3 and Al2O3 as grain boundary modifiers by heterogeneous addition. B2O3 or Al2O3 when added singularly resulted in either steep or broad PTCR jumps respectively across the phase transition. The two-step PTCR is attributed to the activation of the acceptor states, created through B2O3 and Al2O3, for various temperature regimes above the Curie point (T-c). The changing pattern of trap states is evident from the presence of Ti4+-O--Al3+ type hole centres in the grain boundary layer regions, identified in the electron paramagnetic resonance (EPR) spectra. That charge redistribution occurs among the inter-band gap defect states on crossing the Curie temperature is substantiated by the temperature coefficient in the EPR results. Capacitance-voltage results clearly show that there is an increase in the density of trap states with the addition of B2O3 and Al2O3. The spread in energy values of these trap states is evident from the large change in barrier height (phi similar or equal to 0.25-0.6 eV) between 500 and 650 K.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

OFHC copper pins with 10 ppm oxygen were slid against alumina at a load of 50 N and sliding speeds of 0.1 ms(-1) to 4.0 ms(-1) The wear characteristics of copper were related to the strain rate response of copper under uniaxial compression between strain rates of 0.1 s(-1) and 100 s(-1) and temperatures in the range of 298 K to 673 K. It is seen that copper undergoes flow banding at strain rates of 1 s(-1) up to a temperature of 523 K, which is the major instability in the region tested. These flow bands are regions of crack nucleation. The strain rates and temperatures existing in the subsurface of copper slid against alumina are estimated and superimposed on the strain rate response map of copper. The superposition shows that the subsurface of copper slid at low velocities is likely to exhibit flow band instability induced cracking. It is suggested that this is the,reason for the observed high wear rate at low velocities. The subsurface deformation with increasing velocity becomes more homogeneous. This reduces the wear rate. At velocities >2 ms(-1) there is homogenous flow and extrusion of thin (10 mu m) bands of material out of the trailing edge. This results in the gradual increase of wear rate with increasing velocity above 2.0 ms(-1).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Al2O3-SiC-(Al,Si) cermets are fabricated using the melt oxidation route. The tribological properties of the composites are tested under adhesive sliding and two body abrasion conditions. Under adhesive conditions, the network of residual aluminium in the matrix plays a role in the formation of a thin tribofilm on the interface while in abrasion the hardness of the composite plays a prominent tribological role. The work suggests that microstructural control can make this low temperature composite competitive with the conventional high temperature monolithic ceramics. (C) 1999 Published by Elsevier Science S.A. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ASTM D2303 standard provides a method for evaluating the tracking and erosion resistance of polymeric insulators under ac voltages. In this paper, the above method has been extended for evaluating the performance of the insulators under dc stresses. Tests were conducted on polymeric silicone rubber (SR) insulators under positive and negative dc stresses. Micron sized Alumina trihydrate (uATH) and nano sized Alumina (nALU) were used as fillers in SR matrix to improve the resistance to tracking and erosion. Results suggest that SR composites perform better under negative dc than under positive dc voltages. Eroded mass and leakage current data support the above result. Samples with low concentration of nano alumina fillers performed on par with the samples with large loadings of uATH.