881 resultados para High mechanical strength


Relevância:

40.00% 40.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This work is about the 21st century reinforced concrete analysis under the point of view of its constituent materials. First of all it is described the theoretical approach of the bending elements calculated based on the Norms BAEL 91 standarts. After that, numerical load-displacement are presented from reinforced concrete beams and plates validated by experimental data. The numerical modellings has been carried on in the program CASTEM 2000. In this program a elastoplastic model of Drucker-Prager defines the rupture surface of the concrete in non associative plasticity. The crack is smeared on the Gauss points of the finite elements with formation criterion starting from the definition of the rupture surface in the branch traction-traction of the Rankine model. The reinforcements were modeled in a discrete approach with perfect bond. Finally, a comparative analysis is made between the numerical results and calculated criteria showing the future of high performance reinforced concrete in this beginning of 21st century.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: To evaluate the effects of mechanical ventilation (MV) of high-oxygen concentration in pulmonary dysfunction in adult and elderly rats. Methods: Twenty-eight adult (A) and elderly (E), male rats were ventilated for 1 hour (G-AV1 and G-EV1) or for 3 hours (G-AV3 and G-EV3). A and E groups received a tidal volume of 7 mL/kg, a positive end-expiratory pressure of 5 cm H2O, respiratory rate of 70 cycles per minute, and an inspiratory fraction of oxygen of 1. We evaluated total protein content and malondialdehyde in bronchoalveolar lavages (BAL) and performed lung histomorphometrical analyses. Results: In G-EV1 animals, total protein in BAL was higher (33.0 +/- 1.9 mu g/mL) compared with G-AV1 (23.0 +/- 2.0 mu g/mL). Upon 180 minutes of MV, malondialdehyde levels increased in elderly (G-EV3) compared with adult (G-AV3) groups. Malondialdehyde and total proteins in BAL after 3 hours of MV were higher in elderly group than in adults. In G-EV3 group we observed alveolar septa dilatation and significative increase in neutrofiles number in relation to adult group at 60 and 180 minutes on MV. Conclusion: A higher fraction of inspired oxygen in short courses of mechanical ventilation ameliorates the parameters studied in elderly lungs.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Statement of problem. Denture bases may become increasingly weaker as a result of thermal stress and flexural cyclic loading. Information regarding this potential problem and its relationship to the denture base reline is limited.Purpose. This study evaluated the influence of thermal and mechanical stresses on the strength of intact and relined denture bases.Material and methods. Twenty-eight microwave-polymerized (Acron MC) intact denture bases were prepared in the shape of a 3-mm-thick maxillary denture. Additionally, fifty-six 2-mm-thick denture bases were relined with 1 mm of autopolymerizing resin (Tokuyama Rebase Fast II or New Truliner) (n = 28). Intact and relined specimens were divided into 4 groups (n = 7) as follows: without stress (control); a mechanical stress at 0.8 Hz for 10,000 cycles; 5000 thermal cycles between 5 degrees C and 55 degrees C; or a combination thermo-mechanical stress. The specimens were vertically loaded in compression with a rounded rod at 5 mm/min until failure, using a universal testing machine. Data on maximum fracture load (N), deflection at fracture (%), and fracture energy (N-mm) were analyzed by 2-way analysis of variance and Student-Newman-Keuls tests (alpha = .05).Results. The strength of the denture bases relined with New Truliner was not significantly affected by any of the experimental conditions, but comparing the control groups, New Truliner exhibited the lowest maximum fracture load values. The maximum fracture load of intact denture bases (P = .002) and those relined with Tokuyama Rebase Fast II (P = .01) showed a significant decrease after thermal stress. Additionally, cyclic loading significantly decreased the maximum fracture load (P < .001), deflection at fracture (P = .025), and fracture energy (P < .001) of intact denture bases and those relined with Tokuyama Rebase (P values of .002, .039, and .001, respectively).Conclusion. Thermal and mechanical stresses exert deleterious effects on the strength of intact and/or relined denture bases, which vary according to the relining material used.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Studies has been reported a significant incidence of chipping of the feldspathic porcelain veneer in zirconia-based restorations. The purpose of this study was to compare the three-point flexural strength (MPa), Weibull parameters, Vickers hardness (VHN) and Vickers indentation fracture toughness (MPa/mm(1/2)) in feldspatic porcelains for metal and for zirconia frameworks. Bar specimens were made with the porcelains e.MaxCeram (EM) and VitaVM9 (V9) for zirconia core, and Duceragold (DG) and VitaVMK95 (VK) for metal core (n = 15). Kruskal-Wallis and Dun test were used for statistical analysis. There was no significant difference (p=0.31) among the porcelains in the flexural strength (Median = 73.2; 74.6; 74.5; 74.4). Weibull calculation presented highest reliability for VK (10.8) followed by em (7.1), V9 (5.7) and DG (5.6). Vickers hardness test showed that em (536.3), V9 (579.9) and VK (522.1) had no difference and DG (489.6) had the lowest value (p<.001). The highest fracture toughness was to VK (1.77), DG (1.58) had an intermediate value while V9 (1.33) and em (1.18) had the lowest values (p<.001). Despite of the suitable flexural strength, reliability and high hardness, the porcelains used to zirconia-based fixed dental prostheses showed lower fracture toughness values.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Objectives: To evaluate the hypothesis that a process of hydrofluoric acid precipitate neutralization and fatigue load cycling performed on human premolars restored with ceramic inlays had an influence on microtensile bond strength results (MTBS). Methods: MOD inlay preparations were performed in 40 premolars (with their roots embedded in acrylic resin). Forty ceramic restorations were prepared using glass-ceramic (IPS Empress). The inner surfaces of all the restorations were etched with 10% hydrofluoric acid for 60 seconds, rinsed with water and dried. The specimens were divided into two groups (N=20): 1-without neutralization; 2-with neutralization. All the restorations were silanized and adhesively cemented (self-curing and self-etching luting composite system, Multilink). Ten premolars from each group were submitted to mechanical cycling (1,400,000 cycles, 50N, 37 degrees C). After cycling, the samples were sectioned to produce non-trimmed beam specimens (vestibular dentin-restoration-lingual dentin set), which were submitted to microtensile testing. Results: Bond strength was significantly affected by the surface treatment (p<0.0001) (no neutralization > neutralization) and mechanical cycling (p<0.0001) (control > cycling) (2-way ANOVA and Tukey test, alpha=.05). Conclusion: Hydrofluoric acid precipitate neutralization appears to significantly damage the resin bond to glass-ceramic and should not be recommended. The clinical simulation of the specimens, by using mechanical cycling, is important when evaluating the ceramic-dentin bond.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This study evaluated the effects of mechanical and thermal cycling on the flexural strength (ISO 9693) of three brands of ceramics fused to commercially pure titanium (cpTi). Metallic frameworks of 25 x 3 x 0.5 mm dimensions (N = 84) were cast in cpTi, followed by 150-mu m aluminum oxide airborne particle abrasion at a designated area of the frameworks (8 x 3 mm). Bonder and opaque ceramic were applied on the frameworks, and then the corresponding ceramic (Triceram, Super Porcelain Ti-22, Vita Titankeramik) was fired onto them (thickness: 1 mm). Half of the specimens from each ceramic-metal combination were randomly tested without aging (only water storage at 37 degrees C for 24 hours), while the other half were mechanically loaded (20,000 cycles under 10 N load, immersion in distilled water at 37 degrees C) and thermocycled (3,000 cycles, between 5-55 degrees C, dwell time of 13 seconds). After the flexural strength test, failure types were noted. Mechanical and thermal cycling decreased the mean flexural strength values significantly (p<0.05) for all the three ceramic-cpTi combinations tested when compared to the control group. In all the three groups, failure type was exclusively adhesive at the opaque ceramic-cpTi interfacial zone with no presence of ceramic on the substrate surface except for a visible oxide layer.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

De forma geral, os cursos de física clássica oferecidos nas universidades carecem de exemplos de aplicações nas áreas de química e biologia, o que por vezes desmotivam os alunos de graduação destas áreas a estudarem os conceitos físicos desenvolvidos em sala de aula. Neste texto, a analogia entre os osciladores elétrico e mecânico é explorada visando possívies aplicações em química e biologia, mostrando-se de grande valia devido ao seu uso em técnicas de medição de variação de massa com alta precisão, tanto de forma direta como indireta. Estas técnicas são conhecidas como técnicas eletrogravimétricas e são de especial importância em aplicações que envolvem biossensores. Desta forma, o texto explora o estudo da analogia eletromecânica de forma interdisciplinar envolvendo as áreas de física, química e biologia. Baseado nessa analogia é proposto um experimento que permite a sua aplicação em diferentes níveis conceituais dessas disciplinas, tanto em abordagem básica como mais profunda.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Argilas de interesse da indústria de cerâmica estrutural foram caracterizadas. Algumas propriedades físicas de diversas massas cerâmicas, preparadas a partir de material coletado em depósitos artificiais, também foram analisadas. Todas as massas investigadas exibem alta concentração de componentes finos (< 2 mim) e considerável grau de plasticidade, o que é compatível com a presença de elevado teor de argilominerais. Corpos de prova cerâmicos foram preparados por prensagem a seco e queimados em temperaturas ao redor de 855 °C. Os parâmetros resistência mecânica à flexão, retração linear, absorção de água, cor aparente e perda de peso foram medidos. Como resultado, as aplicações industriais destas matérias primas foram analisadas e revistas, bem como novas aplicações foram propostas.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The mechanical and thermo-oxidative degradation of high density polyethylene (HDPE) was measured in a twin-screw extruder using various processing conditions. Two types of HDPE, Phillips and Ziegler-Natta, having different levels of terminal vinyl unsaturation were analysed. Mild screw profiles, having mainly conveying elements, have short mean residence times then profiles with kneading discs and left hand elements. Carbonyl and traps-vinylene group concentrations increased, whereas vinyl group concentration decreased with number of extrusions. Higher temperature profiles intensified these effects. The thermo-mechanical degradation mechanism begins with chain scission in the longer chains due to their higher probability of entanglements. These macroradicals then react with the vinyl terminal unsaturations of other chains producing chain branching. Shorter chains are more mobile, not suffering scission but instead are used for grafting the macroradicals, increasing the molecular weight. Increase in the levels of extrusion temperature, shear and vinyl end groups content facilitates the thermo-mechanical degradation reducing the amount of both, longer chains via chain scission and shorter chains via chain branching, narrowing the polydispersity. Phillips HDPE produces a higher level of chain branching than does the Ziegler-Natta type. (C) 2004 Elsevier Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Bending fatigue tests were carried out to clarify the effects of heat treatment parameters: temperature and time after cadmium electroplating on a high strength steel, to avoid hydrogen embrittlement. Temperatures heat of 190 degrees C, 230 degrees C, 250 degrees C and 300 degrees C at 3, 8 and 24 hours together with the base material electroplated, with and without heat treatment, resulted in 14 conditions studied with respect to fatigue behaviour. Statistical data analysis was performed to identify the best combination temperature/time regarding fatigue strength of the ABNT 4340 steel and the results obtained revealed that the fatigue strength depend on temperature/time conditions.