968 resultados para elasticity modulus


Relevância:

40.00% 40.00%

Publicador:

Resumo:

Currently, the standards that deal with the determination of the properties of rigidity and strength for structural round timber elements do not take in consideration in their calculations and mathematical models the influence of the existing irregularities in the geometry of these elements. This study has as objective to determine the effective value of the modulus of longitudinal elasticity for structural round timber pieces of the Eucalyptus citriodora genus by a technique of optimization allied to the Inverse Analysis Method, to the Finite Element Method and the Least Square Method.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Round timber has great use in civil construction, performing the function of beams, columns, foundations, poles for power distribution among others, with the advantage of not being processed, such as lumber. The structural design of round timber requires determining the elastic properties, mainly the modulus of elasticity. The Brazilian standards responsible for the stiffness and strength determination of round timber are in effect for over twenty years with no technical review. Round timber, for generally present an axis with non-zero curvature according to the position of the element in the bending test, may exhibit different values of modulus of elasticity. This study aims to analyze the position effect of Eucalyptus grandis round timber on the flexural modulus of elasticity. The three-point bending test was evaluated in two different positions based on the longitudinal rotation of the round timber element. The results revealed that at least two different positions of the round timber element are desired to obtain significant modulus of elasticity.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This study aims to present an alternative calculation methodology based on the Least Squares Method for determining the modulus of elasticity in bending wooden beams of structural dimensions. The equations developed require knowledge of three or five points measured in displacements along the piece, allowing greater reliability on the response variable, using the statistical bending test at three points and non-destructively, resulting from imposition of measures from small displacements L/300 and L/200, the largest being stipulated by the Brazilian norm NBR 7190:1997. The woods tested were Angico, Cumaru, Garapa and Jatoba. Besides obtaining the modulus of elasticity through the alternative methodology proposed, these were also obtained employing the Brazilian norm NBR 7190:1997, adapted to the condition of non-destructive testing (small displacements) and for pieces of structural dimensions. The results of the modulus of elasticity of the four species of wood according to both calculation approaches used proved to be equivalent, implying the good approximation provided by the methodology of calculation adapted from the Brazilian norm.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A madeira roliça possui grande emprego nas construções civis, desempenhando a função de vigas, colunas, fundações, postes para distribuição de energia elétrica, entre outras, apresentando a vantagem de não ser processada, como é o caso da madeira serrada. O projeto envolvendo elementos roliços requer, além de outras variáveis estruturais, o conhecimento do módulo de elasticidade. No Brasil, os documentos normativos que tratam da determinação das propriedades de rigidez e resistência para peças roliças de madeira estão em vigência há mais de vinte anos sem revisão técnica. A madeira roliça, por geralmente possuir eixo com curvatura não nula, pode apresentar, segundo a posição da peça no ensaio de flexão, valores diferentes do módulo de elasticidade. Este trabalho tem como objetivo analisara influência da posição de peças roliças de madeira de Eucalyptus grandis na determinação do módulo de elasticidade na flexão. O ensaio de flexão utilizado é o de três pontos, sendo cada peça avaliada em duas posições distintas, definidas mediante o giro da seção transversal em torno do eixo. Os resultados encontrados indicam a necessidade do ensaio de flexão em, pelo menos, duas posições distintas da peça.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Brazilian Standard ABNT NBR7190:1997 for timber structures design, adopts a first degree equation to describe the influence of wood moisture content. Periodically, when necessary, the referred standard is revised in order to analyze inconsistencies and to adopt considerations according new realities verified. So, the present paper aims to examine the adequacy of its equation which corrects to 12% of moisture the values of rigidity properties obtained on experimental tests. To quantify the moisture influence on modulus of elasticity, it was applied tests of compression parallel to the grain for six specimens of different strength classes, considering nominal moisture of 12; 20; 25; 30%. As results, modulus of elasticity in the moisture range 25-30% showed statistically equivalents, and was obtained a first degree equation to correlate the studied variables which leads to statically equivalent estimations when compared with results by ABNT NBR7190:1997 equation. However, it was indicated to maintain the current expression for the next text of the referred document review, without prejudice to statistical significance of the estimates.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Periodically, when necessary, standard documents are revised in order to analyze inconsistencies and to include considerations according new realities verified. In this sense, aiming to quantify the wood moisture content influence on modulus of elasticity, it was applied tension tests parallel to the grain for six specimens of different strength classes of wood, considering nominal moisture of 12, 20, 25, and 30% in Brazil. The present paper examine the adequacy of the current Brazilian standard ABNT NBR7190:1997, in review, about the adoption of a first degree equation to describe the influence of wood moisture content for timber structures design. It was obtained a new first degree equation which leads to statically equivalent estimations when compared with results by ABNT NBR7190:1997 equation. However, as recommendations it could be maintain the current expression for the next text of the referred document review, without prejudice to statistical significance of the estimates.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

1024x768 This research aimed to investigate possible differences in values of longitudinal modulus of elasticity for wood species usually employed for structural purposes, as Castanheira (Bertholletia excelsa), Cambará (Erisma uncinatum), Cumaru (Dipteryx odorata), Jatobá (Hymenaea stilbocarpa), Garapa (Apuleia leiocarpa) and Peroba Rosa (Aspidosperma polyneuron), obtained from compression and tension parallel to grain, and static bending tests. Recommendations of the Brazilian standard ABNT NBR 7190:1997, Annex B, were followed. Statistical analysis results for the cited properties, had equivalent averages for the six wood species analyzed. This confirms that any of the three tests can be used to obtain the longitudinal elastic modulus and which could avoid the necessity of evaluating stiffness values for wood by more than one kind of mechanical test. Normal 0 21 false false false PT-BR X-NONE X-NONE /* Style Definitions */ table.MsoNormalTable {mso-style-name:"Tabela normal"; mso-tstyle-rowband-size:0; mso-tstyle-colband-size:0; mso-style-noshow:yes; mso-style-priority:99; mso-style-qformat:yes; mso-style-parent:""; mso-padding-alt:0cm 5.4pt 0cm 5.4pt; mso-para-margin:0cm; mso-para-margin-bottom:.0001pt; mso-pagination:widow-orphan; font-size:11.0pt; font-family:"Calibri","sans-serif"; mso-ascii-font-family:Calibri; mso-ascii-theme-font:minor-latin; mso-fareast-font-family:"Times New Roman"; mso-fareast-theme-font:minor-fareast; mso-hansi-font-family:Calibri; mso-hansi-theme-font:minor-latin; mso-bidi-font-family:"Times New Roman"; mso-bidi-theme-font:minor-bidi;}

Relevância:

40.00% 40.00%

Publicador:

Resumo:

There are several techniques to characterize the elastic modulus of wood and those currently using the natural frequencies of vibration stand out as they are non-destructive techniques, producing results that can be repeated and compared over time. This study reports on the effectiveness of the testing methods based on the natural frequencies of vibration versus static bending to obtain the elastic properties of reforested structural wood components usually employed in civil construction. The following components were evaluated: 24 beams of Eucalyptus sp. with nominal dimensions (40 x 60 x 2.000 mm) and 14 beams of Pinus oocarpa with nominal dimensions (45 x 90 x 2.300 mm) both without treatment; 30 boards with nominal dimensions (40 x 240 x 2.010 mm) and 30 boards with nominal dimensions (40 x 240 x 3.050 mm), both of Pinus oocarpa and with chromate copper arsenate (CCA) preservative treatment. The results obtained in thiswork show good correlation when compared to the results obtained by the static bending mechanical method, especially when applying the natural frequency of longitudinal vibration. The use of longitudinal frequency was reliable and practical, therefore recommended for determining the modulus of elasticity of wood structural elements. It was also found that no specific support is needed for the specimens using the longitudinal frequency, as well as no previous calibrations, reducing the execution time and enabling to test many samples.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

OBJECTIVE To investigate how the modulus of elasticity of resin composites influences marginal quality in restorations submitted to thermocyclic and mechanical loading. METHODS Charisma, Filtek Supreme XTE and Grandio were selected as they were found to possess different moduli of elasticity but quite similar polymerization contraction. MOD cavities (n=30) were prepared in extracted premolars, restored and then subjected to thermocyclic and mechanical loading. Marginal quality of the restorations before and after loading was analyzed on epoxy replicas under a scanning electron microscope. The percentage of gap-free margins and occurrence of paramarginal fractures were registered. Modulus of elasticity and polymerization contraction were analyzed with parametric and margins with nonparametric ANOVA and post hoc Tukey HSD or Wilcoxon rank-sum tests, respectively. The number of paramarginal fractures was analyzed with exact Fisher tests (α=0.05). RESULTS Grandio demonstrated significantly more gap-free enamel margins than Charisma and Filtek Supreme XTE, before and after loading (p<0.01), whereas there was no difference between Charisma and Filtek Supreme XTE (p>0.05). No significant effect of resin composite (p=0.81) on the quality of dentine margins was observed, before or after loading. Deterioration of all margins was evident after loading (p<0.0001). More paramarginal enamel fractures were observed after loading in teeth restored with Grandio when compared to Charisma (p=0.008). CONCLUSIONS The resin composite with the highest modulus of elasticity resulted in the highest number of gap-free enamel margins but with an increased incidence of paramarginal enamel fractures. CLINICAL SIGNIFICANCE The results from this study suggest that the marginal quality of restorations can be improved by the selection of a resin composite with modulus of elasticity close to that of dentine, although an increase in paramarginal enamel fractures can result as a consequence.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This study includes an analysis of the applicability of current models used for estimating the mechanical properties of conventional concrete to self-compacting concrete. The mechanical properties evaluated are: modulus of elasticity, tensile strength, and modulus of rupture. An extensive database which included the dosifications and the mechanical properties of 627 mixtures from 138 different references, was used. The models considered are: ACI, EC-2, NZS 3101:2006 (New Zealand code) and the CSA A23.3-04 (Canadian code). The precision in estimating the modulus of elasticity and tensile strength is acceptable for all models; however, all models are less precise in estimating the modulus of rupture.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Central to the biological function of microtubules is their ability to modify their length which occurs by addition and removal of subunits at the ends of the polymer, both in vivo and in vitro. This dynamic behavior is strongly influenced by temperature. Here, we show that the lateral interaction between tubulin subunits forming microtubule is strongly temperature dependent. Microtubules deposited on prefabricated substrates were deformed in an atomic force microscope during imaging, in two different experimental geometries. Microtubules were modeled as anisotropic, with the Young's modulus corresponding to the resistance of protofilaments to stretching and the shear modulus describing the weak interaction between the protofilaments. Measurements involving radial compression of microtubules deposited on flat mica confirm that microtubule elasticity depends on the temperature. Bending measurements performed on microtubules deposited on lithographically fabricated substrates show that this temperature dependence is due to changing shear modulus, implying that the lateral interaction between the protofilaments is strongly determined by the temperature. These measurements are in good agreement with previously reported measurements of the disassembly rate of microtubules, demonstrating that the mechanical and dynamic properties of microtubules are closely related.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The vascular properties of large vessels in the obese have not been adequately studied. We used cardiovascular magnetic resonance imaging to quantify the cross-sectional area and elastic properties of the ascending thoracic and abdominal aorta in 21 clinically healthy obese young adult men and 25 men who were age-matched lean controls. Obese subjects had greater maximal cross-sectional area of the ascending thoracic aorta (984 +/- 252 vs 786 +/- 109 mm(2), p <0.01) and of the abdominal aorta (415 +/- 71 vs 374 +/- 51 mm(2), p <0.05). When indexed for height the differences persisted, but when indexed for body surface area, a significant difference between groups was found only for the maximal abdominal aortic cross-sectional area. The obese subjects also had decreased abdominal aortic elasticity, characterized by 24% lower compliance (0.0017 +/- 0.0004 vs 0.0021 +/- 0.0005 mm(2)/kPa/mm, p <0.01), 22% higher stiffness index beta (6.0 +/- 1.5 vs 4.9 +/- 0.7, p <0.005), and 41% greater pressure-strain elastic modulus (72 +/- 25 vs 51 +/- 9, p <0.005). At the ascending thoracic aorta, only the pressure-strain elastic modulus was different between obese and lean subjects (85 +/- 42 vs 65 +/- 26 kPa, respectively; p <0.05), corresponding to a 31% difference-but arterial compliance and stiffness index were not significantly different between groups. In clinically healthy young adult obese men, obesity is associated with increased cross-sectional aortic area and decreased aortic elasticity.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We have investigated the dynamic mechanical behavior of two cross-linked polymer networks with very different topologies: one made of backbones randomly linked along their length; the other with fixed-length strands uniformly cross-linked at their ends. The samples were analyzed using oscillatory shear, at very small strains corresponding to the linear regime. This was carried out at a range of frequencies, and at temperatures ranging from the glass plateau, through the glass transition, and well into the rubbery region. Through the glass transition, the data obeyed the time-temperature superposition principle, and could be analyzed using WLF treatment. At higher temperatures, in the rubbery region, the storage modulus was found to deviate from this, taking a value that is independent of frequency. This value increased linearly with temperature, as expected for the entropic rubber elasticity, but with a substantial negative offset inconsistent with straightforward enthalpic effects. Conversely, the loss modulus continued to follow time-temperature superposition, decreasing with increasing temperature, and showing a power-law dependence on frequency.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium alloys have several advantages over ferrous and non-ferrous metallic materials, such as high strengthto-weight ratio and excellent corrosion resistance. A blended elemental titanium powder metallurgy process has been developed to offer low cost commercial products. The process employs hydride-dehydride (HDH) powders as raw material. In this work, results of the Ti-35Nb alloy sintering are presented. This alloy due to its lower modulus of elasticity and high biocompatibility is a promising candidate for aerospace and medical use. Samples were produced by mixing of initial metallic powders followed by uniaxial and cold isostatic pressing with subsequent densification by isochronal sintering between 900 up to 1600 °C, in vacuum. Sintering behavior was studied by means of microscopy and density. Sintered samples were characterized for phase composition, microstructure and microhardness by X-ray diffraction, scanning electron microscopy and Vickers indentation, respectively. Samples sintered at high temperatures display a fine plate-like alpha structure and intergranular beta. A few remaining pores are still found and density above 90% for specimens sintered in temperatures over 1500 °C is reached.