A transmission electron microscopy study has been carried out on the domain structures of SrBi2Nb2O9 (SBN) ferroelectric ceramics which belong to the Aurivillius family of bismuth layered perovskite oxides. SBN is a potential candidate for Ferroelectric Random access memory (FeRAM) applications. The 90° ferroelectric domains and antiphase boundaries (APBs) were identified with dark field imaging techniques using different superlattice reflections which arise as a consequence of octahedral rotations and cationic shifts. The 90° domain walls are irregular in shape without any faceting. The antiphase boundaries are less dense compared to that of SrBi2Ta2O9(SBT). The electron microscopy observations are correlated with the polarization fatigue nature of the ceramic where the domain structures possibly play a key role in the fatigue- free behavior of the Aurivillius family of ferroelectric oxides.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Suivant la pression partielle d'oxygène, la zircone peut être conducteur ionique ou électronique. Mise au point de méthodes de mesures de f.é.m. permettant de s'affranchir des sources d'erreur introduites par ces propriétés.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

K0.5La0.5Bi2Nb2O9, a relaxor, was synthesized and the structural studies confirmed it to be an n = 2 member of the Aurivillius oxides. The ½{h00} and ½{hk0} types of superlattice reflections in the electron diffraction patterns reflected the presence of ordered polar regions. A broad dielectric peak with frequency dependent dielectric maximum temperature was observed. The dielectric relaxation obeyed the Vogel-Fulcher relation wherein Ea = 0.04 eV, Tf = 428 K,and ωo = 1010 Hz. The diffuseness parameter γ = 2.003 established the relaxor nature and it was attributed to the A-site cationic disorder. The piezoelectric d31 coefficient was 0.5 pC/N at 300 K and 2 pC/N at 480 K.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A ferroelectriclike hysteresis loop was obtained at room temperature for CaCu3Ti4O12 (CCTO) ceramic. The remnant polarization and coercive field for 1100 °C/5 h sintered CaCu3Ti4O12 ceramics were 0.063 μC/cm2 and 195 V/cm, respectively. Remnant polarization increased while the coercive field decreased with increase in sintering temperature/duration, implying that these were microstructural dependent. The observation of the hysteresis loop for CCTO ceramic was corroborated by its pyroelectric behavior, and the pyroelectric current at room temperature was −0.0028 nA. These findings were attributed to the presence of mixed-valent Ti ions, apart from off center displacement of Ti ions in TiO6 octahedra.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Barium lanthanum bismuth niobate Ba1−(3/2)xLaxBi2Nb2O9 (x = 0, 0.05, 0.1, and 0.15) powders have been prepared via solid state reaction route. The monophasic layered perovskite nature of each composition of these was confirmed by x-ray diffraction studies. A continuous decrease in the lattice parameter c of parent BaBi2Nb2O9 with increase in La3+ doping level was noteworthy. A decrease in dielectric constant maximum (εm), a shift in dielectric anomaly to lower temperatures (from 488 to 382 K), and an increase in the diffuseness (γ) (from 1.58 to 1.84) of dielectric anomaly were encountered on increasing x from 0 to 0.15. Vogel-Fulcher analyses showed a decrease in freezing temperature (Tf) (from 157 to 40 K) and an increase in the activation energy (0.53 to 1.12 eV) for frequency dispersion with increase in La3+ content. A downward shift in the peak position of the pyroelectric coefficient with increasing La3+ doping level was observed. The observed changes in the above physical properties were attributed to the increase in A-site chemical heterogeneity as a result of aliovalent La3+ doping on Ba2+ sites and associated A-site vacancy formation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Phase-singular solids of the composition, (Mg1−(x+y) Cax Lay)(Ti1−yAly)O3 (x = 0 to 0.88; y = 0.05 to 0.35) having the cubic perovskite-type structure were prepared by the substitution of La3+ and Al3+ in equivalent quantities which brought about complete miscibility between MgTiO3 and CaTiO3. These ceramics showed relative permittivities of 16.5 to 50 (at 6 GHz) with increasing Ca content, high Q values of 10 000 to 30 000 and retained near-zero temperature coefficients in permittivity at optimum y values. Their dielectric characteristics are better accountable in terms of the positional disorder rather than the tolerance factor of perovskite structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

CaxCu3Ti4O12 (x=0.90, 0.97, 1.0, 1.1 and 1.15) polycrystalline powders with variation in calcium content were prepared via the oxalate precursor route. The structural, morphological and dielectric properties of the ceramics fabricated using these powders were studied using X-ray diffraction, scanning electron microscope along with energy dispersive X-ray analysis, transmission electron microscopy, electron spin resonance (ESR) spectroscopy and impedance analyzer. The X-ray diffraction patterns obtained for the x = 0.97, 1.0 and 1.1 powdered ceramics could be indexed to a body-centered cubic perovskite related structure associated with the space group Im3. The ESR studies confirmed the absence of oxygen vacancies in the ceramics that were prepared using the oxalate precursor route. The dielectric properties of these suggest that the calcium deficient sample (x = 0.97) has a reduced dielectric loss while retaining the high dielectric constant which is of significant industrial relevance. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The SrNaBi2Nb3O12 (SNBN) powder was prepared via the conventional solid-state reaction method. X-ray structural studies confirmed the phase to be a three-layered member of the Aurivillius family of oxides. The SNBN ceramics exhibited the typical characteristics of relaxor ferroelectrics, associated with broad and dispersive dielectric maxima. The variation of temperature of dielectric maxima (T-m) with frequency obeyed the Vogel-Fulcher relationship. Relaxor behavior was believed to be arising from the cationic disorder at A-site. Pinched ferroelectric hysteresis loops were observed well above T-m.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polycrystalline powders of Ba1-xCaxBi4Ti4O15 (where x = 0, 0.25, 0.50, 0.75 and 1) were prepared via the conventional solid-state reaction route. X-ray diffraction (XRD) and Raman scattering techniques have been employed to probe into the structural changes on changing x. XRD analyses confirmed the formation of monophasic bismuth layered structure of all the above compositions with an increase in orthorhombic distortion with increase in x. Raman spectra revealed a redshift in A(1g) peak and an increase in the B-2g/B-3g splitting with increasing Ca content. The average grain size was found to increase with increasing x. The temperature of the maximum dielectric constant (T-m) increased linearly with increasing Ca-content whereas the diffuseness of the phase transition was found to decrease with the end member CaBi4Ti4O15 showing a frequency independent sharp phase transition around 1048 K. Ca doping resulted in a decrease in the remnant polarization and an increase in the coercive field. Ba0.75Ca0.25Bi4Ti4O15 ceramics showed an enhanced piezoelectric coefficient d(33) of 15 pC N-1 at room temperature. Low values of dielectric losses and tunability of temperature coefficient of dielectric constant (tau(epsilon)) in the present solid-solution suggest that these compounds can be of potential use in microwave dielectrics at high temperatures. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of this paper is to discuss the results of the ballistic testing of spark plasma sintered TiB2-Ti based functionally graded materials (FGMs) with an aim to assess their performance in defeating small-calibre armor piercing projectiles. We studied the efficacy of FGM design and compared its ballistic properties with those of TiB2-based composites as well as other competing ceramic armors. The ballistic properties are critically analyzed in terms of depth of penetration, ballistic efficiency, fractographs of fractured surfaces as well as quantification of the shattered ceramic fragments. It was found that all the investigated ceramic compositions exhibit ballistic efficiency (eta) of 5.1 -5.9. We also found that by increasing the thickness of FGM from 5 mm to 7.8 mm, the ballistic property of the composite degraded. Also, the strength of the ceramic compositions studied is sufficient to completely fracture the nose of the pointed projectile used. Analysis of the ceramic fragments (2 mu m-10 mm) showed that harder the ceramic, coarser were the fragments formed. On comparing the results with available armor systems, it has been concluded that TiB2 based composites can show better ballistic properties, except B4C. SEM analysis of the fragments obtained after testing with FGM showed formation of cleavage steps as well as presence of intergranular cracks, indicating that the FGM fractured by mixed mode of failure. It can be concluded that the FGM developed has lower ballistic properties compared to its monolith TiB2-20 wt.% Ti.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nonlinear dielectric response of BaBi4Ti4O15 ceramics synthesized via the conventional solid-state reaction route has been monitored over a wide range of electric field strengths (E-0 = 0.5 - 5 kV/cm). Dielectric permittivity was found to increase linearly within the range of applied field. Rayleigh relations were employed to interpret the nonlinear dielectric response and the contribution of irreversible domain wall motion to the macroscopic permittivity was separated. The values of room temperature Rayleigh dielectric coefficient (alpha) and relative initial permittivity (epsilon'(init)) were found to be 2.28 +/- 0.02 cm/kV and 146.10 +/- 0.07, respectively. A reasonable agreement between the simulated and measured polarization-electric field (P-E) hysteresis loops was observed at an applied electric field of 5 kV/cm.