949 resultados para Metal ceramic restorations


Relevância:

90.00% 90.00%

Publicador:

Resumo:

Pós-graduação em Química - IQ

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Purpose: To evaluate the microtensile bond strength (MTBS) of ceramic cemented to dentin varying the resin cement and ceramic shades.Materials and Methods: Two VITA VM7 ceramic shades (Base Dentine 0M1 and Base Dentine 5M3) were used. A spectrophotometer was used to determine the percentage translucency of ceramic (thickness: 2.5 mm). For the MTBS test, 80 molar dentin surfaces were etched and an adhesive was applied. Forty blocks (7.2 x 7.2 x 2.5 mm) of each ceramic shade were produced and the ceramic surface was etched (10% hydrofluoric acid) for 60 s, followed by the application of silane and resin cement (A3 yellow and transparent). The blocks were cemented to dentin using either A3 or transparent cement. Specimens were photoactivated for 20 s or 40 s, stored in distilled water (37 degrees C/24 h), and sectioned. Eight experimental groups were obtained (n = 10). Specimens were tested for MTSB using a universal testing machine. Data were statistically analyzed using ANOVA and Tukey's post-hoc tests (alpha <= 0.05).Results: The percentage translucency of 0M1 and 5M3 ceramics were 10.06 (+/- 0.25)% and 1.34 (+/- 0.02)%, respectively. The lowest MTBS was observed for the ceramic shade 5M3. For the 0M1 ceramic, the A3 yellow cement that was photocured for 20 s exhibited the lowest MTBS, while the transparent cement that was photocured for 40 s presented the highest MTBS.Conclusions: For the 2.5-mm-thick 5M3 ceramic restorations, the MTBS of ceramic cemented to dentin significantly increased. The dual-curing cement Variolink II photocured for 40 s is not recommended for cementing the Base Dentine 5M3 feldspathic ceramic to dentin.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The continuing advances in technology, dental materials and equipment have contributed significantly to improve the level of esthetic dentistry today. Among these innovations, development of pure ceramic restorations has evolved to give different alternatives. Dental ceramics have presented a rapidly technological changing to improve mechanical and optical properties. Currently there are several systems of metal free ceramics with excellent mechanical and optical properties, for making crowns and plurals. These modern systems are presented with various compositions and different preparation techniques, making these more versatile. Within this perspective, the dental market offers a huge range of new indirect and metal-free materials for prostheses, providing new options, plus also new questions to decide among the available alternatives. The aim of this review is take a view of the different ceramic systems in terms of its composition and different techniques of production.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Introduction: Based on the importance of the integrity of the metal/ceramic interface, the purpose of this work was to evaluate the shear bond strength of the metal-ceramic union of two Co-Cr alloys (Wirobond C, Bego; Remanium 2000, Dentaurum) combined with Omega 900 ceramic (Vita Zahnfabrik). Material and Method: Eleven cylindrical matrixes were made for each alloy, and the metallic portion was obtained with the lost wax casting technique with standardized waxing of 4mm of height and of 4mm of diameter. The ceramic was applied according to the manufacturer's recommendations with the aid of a teflon matrix that allowed its dimension to be standardized in the same size as the metallic portion. The specimens were submitted to the shear bond test in an universal testing machine (EMIC), with the aid of a device developed for such intention, and constant speed of 0.5mm/min. Results and Conclusions: The mean resistance was 48.387MPa for Wirobond C alloy, with standard deviation of 17.718, and 55.956MPa for Remanium 2000, with standard deviation of 17.198. No statistically significant difference was observed between the shear strength of the two metal-ceramic alloys.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The purpose of this study was to warn the dental community about a possible problem in function with partial implant-supported prostheses used for long periods. The misalignment between natural teeth and the implant-supported prosthesis on teeth 11 and 12, observed in a 14-year clinical follow-up, illustrates the fact. The metal-ceramic crowns were placed in 1995 after a rigorous occlusal adjustment. Evaluations were made at 4, 6, 9, and 14 years, when it was noticed that the restorations were positioned palatally and extruded in comparison with the natural teeth. After 9 years, a greater discrepancy was noticed, with anterior occlusion and esthetic changes. The possible causes have been discussed: occlusal problems, parafunctional habits, and natural movement. The first 2 options were discarded after clinical analysis and diagnosis. Therefore, the natural movement probably deriving from an interaction of mechanical and genetic factors might have been the cause. The implants do not have periodontal ligaments but rather ankylosis, so they do not suffer those movements. This case emphasizes the need to inform patients that implants can last more than 10 years in function, but this is not the case with restorations, which lose function and esthetics and must be replaced.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objectives: The purpose of this study was to evaluate the influence of thermal and mechanical cycling and veneering technique on the shear bond strength of Y-TZP (yttrium oxide partially stabilized tetragonal zirconia polycrystal) core–veneer interfaces. Materials and methods: Cylindrical Y-TZP specimens were veneered either by layering (n = 20) or by pressing technique (n = 20). A metal ceramic group (CoCr) was used as control (n = 20). Ten specimens for each group were thermal and mechanical cycled and then all samples were subjected to shear bond strength in a universal testing machine with a 0.5 mm/min crosshead speed. Mean shear bond strength (MPa) was analysed with a 2-way analysis of variance and Tukey’s test ( p < 0.05). Failure mode was determined using stereomicroscopy and scanning electron microscopy (SEM). Results: Thermal and mechanical cycling had no influence on the shear bond strength for all groups. The CoCr group presented the highest bond strength value ( p < 0.05) (34.72 7.05 MPa). There was no significant difference between Y-TZP veneered by layering (22.46 2.08 MPa) or pressing (23.58 2.1 MPa) technique. Failure modes were predominantly adhesive for CoCr group, and cohesive within veneer for Y-TZP groups. Conclusions: Thermal and mechanical cycling, as well as the veneering technique does not affect Y-TZP core–veneer bond strength. Clinical significance: Different methods of veneering Y-TZP restorations would not influence the clinical performance of the core/veneer interfaces.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

OBJECTIVES: This study evaluated the initial and the artificially aged push-out bond strength between ceramic and dentin produced by one of five resin cements. METHODS: Two-hundred direct ceramic restorations (IPS Empress CAD) were luted to standardized Class I cavities in extracted human molars using one of four self-adhesive cements (SpeedCEM, RelyX Unicem Aplicap, SmartCem2 and iCEM) or a reference etch-and-rinse resin cement (Syntac/Variolink II) (n=40/cement). Push-out bond strength (PBS) was measured (1) after 24h water storage (non-aged group; n=20/cement) or (2) after artificial ageing with 5000 thermal cycles followed by 6 months humid storage (aged group; n=20/cement). Nonparametrical ANOVA and pairwise Wilcoxon rank-sum tests with Bonferroni-Holm adjustment were applied for statistical analysis. The significance level was set at alpha=0.05. In addition, failure mode and fracture pattern were analyzed by stereomicroscope and scanning electron microscopy. RESULTS: Whereas no statistically significant effect of storage condition was found (p=0.441), there was a significant effect of resin cement (p<0.0001): RelyX Unicem showed significantly higher PBS than the other cements. Syntac/Variolink II showed significantly higher PBS than SmartCEM2 (p<0.001). No significant differences were found between SpeedCEM, SmartCem2, and iCEM. The predominant failure mode was adhesive failure of cements at the dentin interface except for RelyX Unicem which in most cases showed cohesive failure in ceramic. SIGNIFICANCE: The resin cements showed marked differences in push-out bond strength when used for luting ceramic restorations to dentin. Variolink II with the etch-and-rinse adhesive Syntac did not perform better than three of the four self-adhesive resin cements tested.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

AIM: To assess survival rates and complications of root-filled teeth restored with or without post-and-core systems over a mean observation period of >or=4 years. METHODOLOGY: A total of 325 single- and multirooted teeth in 183 subjects treated in a private practice were root filled and restored with either a cast post-and-core or with a prefabricated titanium post and composite core. Root-filled teeth without post-retained restorations served as controls. The restored teeth served as abutments for single unit metal-ceramic or composite crowns or fixed bridges. Teeth supporting cantilever bridges, overdentures or telescopic crowns were excluded. RESULTS: Seventeen teeth in 17 subjects were lost to follow-up (17/325: 5.2%). The mean observation period was 5.2 +/- 1.8 (SD) years for restorations with titanium posts, 6.2 +/- 2.0 (SD) years for cast post-and-cores and 4.4 +/- 1.7 (SD) years for teeth without posts. Overall, 54% of build-ups included the incorporation of a titanium post and 26.5% the cementation of a cast post-and-core. The remaining 19.5% of the teeth were restored without intraradicular retention. The adjusted 5-year tooth survival rate amounted to 92.5% for teeth restored with titanium posts, to 97.1% for teeth restored with cast post-and-cores and to 94.3% for teeth without post restorations, respectively. The most frequent complications included root fracture (6.2%), recurrent caries (1.9%), post-treatment periradicular disease (1.6%) and loss of retention (1.3%). CONCLUSION: Provided that high-quality root canal treatment and restorative protocols are implemented, high survival and low complication rates of single- and multirooted root-filled teeth used as abutments for fixed restorations can be expected after a mean observation period of >or=4 years.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

STATEMENT OF PROBLEM The increasing demand by patients for esthetic and metal-free restorations has driven the development of ceramic restorations with good esthetic and mechanical stability. Recent clinical studies have investigated the use of zirconium dioxide as a core material for complete crowns and computer-aided-design/computer-aided-manufacturing fabricated restorations. PURPOSE The aim of this systematic review was to evaluate the clinical survival rates of porcelain-fused-to-zirconia (PFZ) single crowns on anterior and posterior teeth and to compare them with metal ceramic (MC) crowns. MATERIAL AND METHODS A systematic search was conducted with PubMed and manual research to identify literature written in English that refers to in vivo studies published from January 1, 1950 through July 1, 2011. Clinical trials that evaluated PFZ and MC single crowns on natural teeth were selected for further analysis. Titles and/or abstracts of articles identified through the electronic searches were reviewed and evaluated for appropriateness. In addition, a hand search of relevant dental journals was peformed, and reference lists of culled articles were screened to identify publications. RESULTS The search resulted in a total of 488 initial matches. Nineteen studies with a total of 3621 crowns met the inclusion criteria. The survival rates of PFZ crowns (total 300) ranged from 92.7% to 100% for a follow-up time of 24 to 39 months, whereas those of MC crowns (total 3321) ranged from 70% to 100% for a follow-up time of 12 to 298 months. Studies that reported long-term results were found only for the MC crown group. CONCLUSIONS The scientific clinical data available to compare PFZ and MC crowns are limited. The survival rates may well be influenced by the selection and appropriate use of the veneering ceramic, and, therefore, additional prospective long-term clinical trials are necessary to draw reliable conclusions.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

STATEMENT OF PROBLEM: Long-term fluoride application on the teeth of patients receiving radiation therapy for head and neck tumors results in excessive staining and roughening of ceramic restorations. PURPOSE: The purpose of this in vitro study was to compare the staining effects of 2 fluoride treatments on ceramic disks by simulating 1 year of clinical exposure at 10 minutes per day. In addition, 2 different surface preparations were tested. MATERIAL AND METHODS: Eighty ceramic disks (IPS Empress), 20 x 2 mm, were fabricated. Half of the disks were glazed, and the remaining disks were polished. All disks were brushed for 3 minutes with a soft-bristle power toothbrush and mild dentifrice (baseline) and were immersed in 1 of the 2 fluoride products (0.4% SnF(2), Gel-Kam Gel, or 1.1% NaF, Prevident 5000) for 10 days (n=20). Means and standard deviations of color change (Delta E), surface roughness (Ra, um), and surface gloss (GU) of the ceramic material were measured with a reflection spectrophotometer, a profilometer, and a gloss meter, respectively, at baseline and after fluoride treatment. Two- and 3-way ANOVA (alpha=.05), with surface preparation (polished vs. glazed) and fluoride treatment (0.4% SnF(2) or 1.1% NaF) as independent variables and condition (baseline vs. after fluoride treatment) as a repeated measure, was used to analyze the data. Fisher's PLSD intervals (alpha=.05) were calculated for comparisons among the means. RESULTS: The polished specimens had significantly higher Delta E values, significantly higher surface gloss values, and significantly lower surface roughness values than the glazed specimens before fluoride treatment (P<.001). After both fluoride treatments, ceramic disks exhibited significantly higher surface roughness values when polished and significantly lower surface gloss values when glazed or polished (P<.001). The glazed specimens presented significantly higher surface roughness (P<.001) and lower surface gloss values (P<.001) when treated with 0.4% SnF(2) as compared to NaF. For the polished specimens, there was no significant difference in surface roughness and surface gloss values between the 2 fluoride treatments. CONCLUSIONS: Use of 0.4% SnF(2) and 1.1% NaF gels, in vitro, caused significant color change in the polished IPS Empress ceramic disks. Polishing of the ceramic surface before immersion in either fluoride agent caused the ceramic tested to be more resistant to etching by the 2 solutions tested. The NaF caused less deterioration of the porcelain surface and was less stain inducing than SnF(2).

Relevância:

90.00% 90.00%

Publicador:

Resumo:

BACKGROUND Endodontic treatment involves removal of the dental pulp and its replacement by a root canal filling. Restoration of root filled teeth can be challenging due to structural differences between vital and non-vital root-filled teeth. Direct restoration involves placement of a restorative material e.g. amalgam or composite, directly into the tooth. Indirect restorations consist of cast metal or ceramic (porcelain) crowns. The choice of restoration depends on the amount of remaining tooth, and may influence durability and cost. The decision to use a post and core in addition to the crown is clinician driven. The comparative clinical performance of crowns or conventional fillings used to restore root-filled teeth is unknown. This review updates the original, which was published in 2012. OBJECTIVES To assess the effects of restoration of endodontically treated teeth (with or without post and core) by crowns versus conventional filling materials. SEARCH METHODS We searched the following databases: the Cochrane Oral Health Group's Trials Register, CENTRAL, MEDLINE via OVID, EMBASE via OVID, CINAHL via EBSCO, LILACS via BIREME. We also searched the reference lists of articles and ongoing trials registries.There were no restrictions regarding language or date of publication. The search is up-to-date as of 26 March 2015. SELECTION CRITERIA Randomised controlled trials (RCTs) or quasi-randomised controlled trials in participants with permanent teeth that have undergone endodontic treatment. Single full coverage crowns compared with any type of filling materials for direct restoration or indirect partial restorations (e.g. inlays and onlays). Comparisons considered the type of post and core used (cast or prefabricated post), if any. DATA COLLECTION AND ANALYSIS Two review authors independently extracted data from the included trial and assessed its risk of bias. We carried out data analysis using the 'treatment as allocated' patient population, expressing estimates of intervention effect for dichotomous data as risk ratios, with 95% confidence intervals (CI). MAIN RESULTS We included one trial, which was judged to be at high risk of performance, detection and attrition bias. The 117 participants with a root-filled, premolar tooth restored with a carbon fibre post, were randomised to either a full coverage metal-ceramic crown or direct adhesive composite restoration. None experienced a catastrophic failure (i.e. when the restoration cannot be repaired), although only 104 teeth were included in the final, three-year assessment. There was no clear difference between the crown and composite group and the composite only group for non-catastrophic failures of the restoration (1/54 versus 3/53; RR 0.33; 95% CI 0.04 to 3.05) or failures of the post (2/54 versus 1/53; RR 1.96; 95% CI 0.18 to 21.01) at three years. The quality of the evidence for these outcomes is very low. There was no evidence available for any of our secondary outcomes: patient satisfaction and quality of life, incidence or recurrence of caries, periodontal health status, and costs. AUTHORS' CONCLUSIONS There is insufficient evidence to assess the effects of crowns compared to conventional fillings for the restoration of root-filled teeth. Until more evidence becomes available, clinicians should continue to base decisions about how to restore root-filled teeth on their own clinical experience, whilst taking into consideration the individual circumstances and preferences of their patients.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Materiais compósitos restauradores representam um dos mais bem sucedidos biomateriais na pesquisa moderna, na substituição do tecido biológico em aparência e função. Nesta linha, a porcelana feldspática tem sido largamente usada em odontologia devido suas interessantes qualidades como estabilidade de cor, propriedades estéticas, elevada durabilidade mecânica, biocompatibilidade, baixa condutividade térmica e elevada resistência ao desgaste. Entretanto, este material é frágil e pode falhar em ambiente oral devido ao micro-vazamento, baixa resistência à tração, descolagem ou fratura. Assim, para melhorar as propriedades mecânicas da porcelana, a zircônia parcialmente estabilizada com Ítria (Y-TZP) pode ser uma boa alternativa para fortalecer e produzir infraestruturas totalmente cerâmicas (coroas e próteses parciais fixas). Portanto, este estudo tem por objetivo avaliar as propriedades mecânicas e características microestruturais da porcelana reforçada com zircônia (3Y-TZP) em diferentes conteúdos e as variáveis que afetam as propriedades mecânicas destes materiais. O estudo de caracterização revelou que a zircônia comercial apresenta melhores resultados quando comparada com a zircônia sintetizada pelo CPM. Assim, os estudos seguintes utilizaram a zircônia comercial para todos os testes requeridos. As partículas de zircônia apresentam elevadas propriedades mecânicas quando comparadas a zircônia aglomerada. Os diferentes conteúdos revelam que as propriedades mecânicas dos compósitos aumentam com o aumento do conteúdo volumétrico até 30% vol.% (198,5Mpa), ou seja, maior resistência à flexão quando comparada com os outros compósitos. Do mesmo modo, a resistência ao desgaste para os compósitos com (30%, vol.% de zircônia) apresenta valores superiores quando comparado aos demais compósitos. Na adesão cerâmico-cerâmico a porcelana exibe elevada adesão para a superfície de zircônia porosa quando comparada a superfície rugosa. Os furos superficiais (PZ) e aplicação de compósitos com camada intermediária (RZI) na zircônia causam separadamente uma melhoria da resistência ao cisalhamento da zircônia-porcelana quando comparados as amostras convencionais de zircônia-porcelana (RZ), embora não sejam estatisticamente significativas (p>0.05). A presença de uma camada intermediaria produz um aumento significativo na força de ligação (~55%) em relação as amostras convencionais (RZ). Portanto, a correta a correta configuração e tratamento superficial podem produzir subestruturas com qualidade e força de ligação adequadas aos requisitos odontológicos.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Purpose: Chipping within veneering porcelain has resulted in high clinical failure rates for implant-supported zirconia (yttria-tetragonal zirconia polycrystals [Y-TZP]) bridges. This study evaluated the reliability and failure modes of mouth-motion step-stress fatigued implant-supported Y-TZP versus palladium-silver alloy (PdAg) three-unit bridges. Materials and Methods: Implant-abutment replicas were embedded in polymethylmethacrylate resin. Y-TZP and PdAg frameworks, of similar design (n = 21 each), were fabricated, veneered, cemented (n = 3 each), and Hertzian contact-tested to obtain ultimate failure load. In each framework group, 18 specimens were distributed across three step-stress profiles and mouth-motion cyclically loaded according to the profile on the lingual slope of the buccal cusp of the pontic. Results: PdAg failures included competing flexural cracking at abutment and/or connector area and chipping, whereas Y-TZP presented predominantly cohesive failure within veneering porcelain. Including all failure modes, the reliability (two-sided at 90% confidence intervals) for a ""mission"" of 50,000 and 100,000 cycles at 300 N load was determined (Alta Pro, Reliasoft, Tucson, AZ, USA). No difference in reliability was observed between groups for a mission of 50,000. Reliability remained unchanged for a mission of 100,000 for PdAg, but significantly decreased for Y-TZP. Conclusions: Higher reliability was found for PdAg for a mission of 100,000 cycles at 300 N. Failure modes differed between materials.