985 resultados para FLUORESCENCE-SPECTRA
Resumo:
Carbon nanomaterials (CNMs), such as exfoliated graphene (EG), long-chain functionalized EG, single-walled carbon nanotubes (SWNTs), and fullerene (C-60), have been investigated for their interaction with two structurally different gelators based on all-trans tri-p-phenylenevinylene bis-aldoxime (1) and n-lauroyl-L-alanine (2) both in solution and in supramolecular organogels. Gelation occurs in toluene through hydrogen bonding and van der Waals interactions for 1 and 2 in addition to pp stacking specifically in the case of 1. These nanocomposites provide a thorough understanding in terms of molecular-level interactions of dimensionally different CNMs with structurally different gelators. The presence of densely wrapped CNMs encapsulated fibrous network in the resulting composites is evident from various spectroscopic and microscopic studies, indicating the presence of supramolecular interactions. Concentration- and temperature-dependent UV/Vis and fluorescence spectra show that CNMs promote aggregation of the gelator molecules, leading to hypochromism and quenching of the fluorescence intensity. Thermotropic mesophases of 1 are altered by the inclusion of a small amount of CNMs. The gelCNM composites show increased electrical conductivity compared with that of the native organogel. Rheological studies of the composites demonstrate the formation of rigid and viscoelastic solidlike assembly due to reinforced aggregation of the gelators on CNMs. Synergistic behavior is observed in case of the composite gel of 1, containing a mixture of EG and SWNT, when compared with other mixtures of CNMs in all combinations with EG. This affords new nanocomposites with interesting optical, thermal, electrical, and mechanical properties.
Resumo:
We report micromodification of Eu element distribution in a silicate glass with femtosecond laser irradiation. Elemental analysis shows that the content of Eu decreased at the focal point and increased in a ring-shaped region around the focal point, which indicates migration of Eu ions has been induced by the femtosecond laser irradiation. Confocal fluorescence spectra demonstrate that the fluorescence intensity of Eu3+ ions increased by 20% in the laser-induced, Eu-enriched, ring-shaped region compared with that for nonirradiated glass. The mechanism for the laser induced change in fluorescence properties of Eu3+ has been investigated. (C) 2009 Optical Society of America
Resumo:
Fluorescence spectra of Nd: YVO4 under excitation of a continuous wave (CW) diode laser and a femtosecond laser at 800nm were investigated. It was found that Nd: YVO4 shows different upconversion and downconversion luminescencent behaviors when excited by the diode laser and the femtosecond laser. The dependence of the upconversion luminescence intensity on the pump power of the femtosecond laser was discussed. The populations of the upper energy levels for upconversion and downconversion luminescence were calculated based on the Bloch equations. The calculations agree well with the experimental results. (c) 2007 Optical Society of America.
Resumo:
Levofloxacino é uma fluorquinolona sintética de 3 geração. É eficaz contra uma variedade de infecções, incluindo o trato respiratório superior e inferior, trato urinário, obstétrico, ginecológico, e infecções dermatológicas. Com o objetivo de quantificar o levofloxacino em medicamentos e amostras de pacientes saudáveis e ter a resolução de seu espectro, foram realizados estudos preliminares em medicamento utilizando espectrofluorescência molecular com concentrações na faixa de 28,8 108 ng/mL e cromatografia líquida de alta eficiência (HPLC) na faixa de concentração de 2,9 10,8 g/mL; e também quantificação em urina de paciente em tratamento com o medicamento, usando os dois métodos citados. Após isso, foram feitos estudos conclusivos utilizando espectrofluorescência molecular e os métodos univariado e PLS para determinação de levofloxacino na faixa de concentração de 0 250 ng/mL e PARAFAC combinado com o método da adição de padrão, para quantificação de levofloxacino em urina de paciente saudável, na faixa de concentração de 0 150 ng/mL, com diluição da amostra em três níveis (100 x, 500 x e 1000x). O método de ordem zero se mostrou mais eficiente na determinação de levofloxacino em medicamento que o de primeira ordem, seus desvios padrão foram 2,0% e 7,9%, respectivamente. Já o PARAFAC com o método de adição de padrão apresentou melhores resultados com a urina, pois possibilitou a quantificação do antibiótico em uma amostra complexa, de forma mais precisa e exata com o aumento da diluição da urina, sem necessidade de tratamento prévio.
Resumo:
A produção de porfirinas por Corynebacterium diphtheriae é um objeto de estudo antigo, porém pouco explorado em Química e Ciências Médicas. O presente trabalho teve como objetivos comparar a influência de diferentes meios de cultura na produção de porfirinas por Corynebacterium diphtheriae, determinar a influencia da concentração do ferro na produção de porfirina, comparar quantitativamente a produção de porfirinas por diferentes amostras de bacilo diftérico e caracterizar químicamente os tipos de porfirinas produzidas. As técnicas utilizadas para isso foram a espectroscopia de absorção UV-visível e de fluorescência. O meio de cultura descrito por Mueller (1939), para a produção de toxina, se mostrou mais eficiente que o meio B de king, utilizado no diagnóstico laboratorial da difteria. A concentração de ferro no cultivo de Corynebacterium diphtheriae influencia a produção de porfirina. Altas concentrações de ferro inibem a produção de porfirina. A concentração de ferro onde a produção de porfirinas é máxima é de 0,20g/mL. Dentre as 11 amostras de bacilo diftérico estudadas, a amostra HC03, fermentadora de sacarose e toxinogênica, isolada de um caso de endocardite, foi a maior produtora de porfirina. A amostra ATCC de Corynebacterium ulcerans, não fermentadora de sacarose e toxinogênica, foi a amostra que produziu menos porfirina. Todas as 11 amostras apresentaram o mesmo perfil de espectro de fluorescência, sugerindo que a porfirina produzida seja a mesma nas amostras pesquisadas. As análises feitas para a caracterização do tipo de porfirina produzida levam a crer que esta seja uma coproporfirina. Os espectros de absorção e fluorescência não permitem porém determinar o(s) isômero(s) presente(s).
Resumo:
研究了两种新型芴类衍生物9,9-二(2-乙基已基)-2,7-二咔唑-9H-芴(简记为DCZF)和9,9-二(2-乙基已基)-2,7-二(2-(4-甲氧基)苯-2,1-乙烯基)芴(简记为BMOSF)在N,N-二甲基甲酰胺(DMF)中的线性吸收和单光子荧光行为,并用脉冲宽度为38ps,重复频率为10Hz的1064 nm Nd:YAG脉冲激光研究了两种化合物的三光子吸收性质.结果表明:两种新材料的最大线性吸收峰分别位于330和380nm,吸收区域覆盖了270-420nm波段.两种化合物的荧光带位于蓝-紫区,中心
Resumo:
制备了四种不同铒离子掺杂浓度的碲酸盐玻璃,通过测定吸收光谱计算了吸收谱线的振子强度,根据Judd-Ofelt理论计算了不同浓度下Er^3+离子发光光谱的强度参数Ω(i=2,4,6),计算了自发辐射电偶和磁偶跃迁概率、辐射寿命、荧光分支比等参数,讨论了Er^3+离子浓度变化对以上这些参数的影响。测试了Er^3+:^4I13/2→^4I15/2跃迁对应的荧光光谱和Er^3+:^4I13/2能级荧光寿命。最后应用McCumber理论计算了玻璃中Er^3+:^4I13/2→^4I15/2跃迁对应的受激发射截面大小
Resumo:
Er3+/Yb3+ cocloped fluorophosphate glasses were prepared and their thermal stabilities, Raman spectra, absorption spectra, and fluorescence spectra were measured. It is found that proper content of NaF or PbF2 is helpful for the increase of stability against crystallization. The variation of AI(PO3)3 or NaF content in the composition affects not the maximum phonon energy but the phonon density. The introduction of PbF2 decreases the phonon energy slightly. Intense green and red upconversion luminescence was observed for the fluorophosphate glass with low phosphate content. A glass matrix for upconversion luminescence requiring neither expensive raw material nor special atmospheric conditioned preparation is provided. Infrared luminescence around 1530 nm was researched. Fluorophosphate glasses with bandwidth properties and stimulated-emission cross sections better than tellurite, germanate and silicate glasses are obtained. Through the introduction of NaF, the bandwidth properties are decreased. Through the introduction of PbF2 the gain properties are increased. On the whole, it is difficult to obtain a material with the best gain properties and bandwidth properties simultaneously. There should be a compromise between them according to the demand. (C) 2006 Elsevier B.V. All rights reserved.
Resumo:
Nd-doped and Nd-Al-codoped high silica glasses were obtained by sintering porous glass impregnated with Nd3+ and Al3+ ions. The absorption, fluorescence spectra and fluorescence lifetime of Nd-doped and Nd-Al-codoped high silica glasses were measured. The intensity parameters Omega(1), ( t = 2, 4, 6), fluorescence lifetime, radiative quantum efficiency and stimulated emission cross section were calculated by Judd-Ofelt theory. The effect of aluminum codoping on the fluorescence and structural properties of Nd-doped silica glass has been discussed. By comparing the spectroscopic properties with other Nd-doped oxide glasses and commercial silicate glasses, this Nd-doped high silica glass is likely to be a promising laser material for use in high power and high repetition rate lasers.
Resumo:
Series of tellurite glasses were prepared by traditional melting method, the glass composition were changed and the different effects of glass modifier oxides(alkali metals and alkaline earth metal oxides) and glass intermediate (Y
Resumo:
Er3+-doped halide modified tellurite glasses were synthesized by conventional melting and quenching method. The Judd-Ofelt analysis was performed on the absorption spectra and the transition probabilities, excited state lifetimes, and the branching ratios were calculated and discussed. The intense infrared and visible fluorescence spectra under 980 nm excitation were obtained. Strong upconversion signal was observed at pumping power as low as 30 mW in the glasses with halide ions. The upconversion mechanisms and power dependent intensities were discussed, which showed two-photon process are involved for the green and red emissions. The decay times of the emitting states and the corresponding quantum efficiency were determined and explained. (C) 2004 American Institute of Physics.
Resumo:
(100 - x)TeO2 - xNb(2)O(5) (x=5-20) mobic tellurite glasses doped with 0.5 mol.% Er2O3 were synthesized, and their thermal, mechanical, and spectroscopic properties were measured and compared to the properties of the typical 75TeO(2)-20ZnO-5Na(2)O (TZN) tellurite glass. The refractive index (n(d)), density (p), and glass transition temperature (T-g) of bulk glasses increase with the Nb2O5 content. The Vickers microhardness (H-v) of bulk glass in niobic tellurite glasses also increases with the Nb2O5 content. The values (2.5-3.2 GPa) of H, in the niobic tellurite glasses are 47-88% larger than that (1.7 GPa) in TZN glass. The effect of Nb2O5 content on absorption spectra, the Judd-Ofelt parameters Omega(t) (t = 2, 4, 6), fluorescence spectra and the lifetimes of Er3+ :I-13/2 level were also investigated, and the stimulated emission crosssection was calculated from McCumber theory. With increasing Nb2O5 content in the glass composition, the Omega(t) (t = 2, 4, 6) parameters, fluorescence full width at half maximum (FWHM) Of I-13/2 of Er3+ increase, while the I-4(13/2) lifetimes of Er3+ decreases. Compared with TZN glass, the gain bandwidth properties of Er3+-doped TeO2-Nb2O5 glass is much larger than in tellurite glass based TeO2-ZnO-Na2O system, bismush-based glass, germanate, and silicate glasses, which indicates that TeO2-Nb2O5 glasses are better choice as a practical available host material for broadband Er3+-doped amplifier. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
TiO2/ormosil films doped with laser dyes have been prepared by the sol-gel method. Spectroscopic properties of the entrapped dyes are studied by the absorption and emission techniques. The results indicate that the absorption and fluorescence spectra of kiton red depend strongly on the properties of the ormosil matrices. The heat-treatment of the kiton red-doped film obviously leads to the increasing fluorescence intensity and the largest fluorescence intensity is obtained after heat-treatment of 150 degrees C for 2 h. However, the fluorescence intensity of the rhodamine 6G-doped film decreases with the increase of the heat-treatment temperature. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A series of five different concentration erbium-doped tellurite glasses with various hydroxl groups were prepared. Infrared spectra of glasses were measured. In order to estimate the exact content of OH- groups in samples, various absorption coefficients of the OH- vibration band were analyzed under the different oxygen bubbling times. The absorption spectra of the glasses were measured, and the Judd-Ofelt intensity parameters Omega(i) of samples with the different erbium ions concentration and OH- contents were calculated on the basis of the Judd-Ofelt theory. The peak stimulated emission cross-section of (I13/2 ->I15/2)-I-4-I-4 transition of the samples was finally calculated by using the McCumber theory. The fluorescence spectra of Er3+:I-4(13/2)->I-4(15/2) transition and the lifetime of Er3+:I-4(13/2) level of the samples were measured. The effects of OH- groups on the spectroscopic properties of Er3+ doped samples with the different concentrations were discussed. The results showed that the OH- groups had great influences on the Er3+ lifetime and the fluorescence peak intensity. The OH- group is a main influence factor of fluorescence quenching when the doping concentration of Er2O3 is smaller than 1.0 mol%, but higher after this concentration, the energy transfer of Er3+ ions turns into the main function of the fluorescence quenching. And basically, there is no influence on the other spectroscopic properties (FWHM, absorption spectra, peak stimulated emission cross section, etc.).
Resumo:
测试了不同掺杂浓度和样品厚度下掺铒磷酸盐和碲酸盐玻璃的吸收光谱、荧光光谱和荧光寿命,计算了Er^3+离子在1.53μm处的吸收截面(σa)、发射截面(σe)、自发辐射跃迁概率(Arad)、辐射跃迁寿命(τrad)、以及辐射跃迁量子效率(η)等光谱参数.讨论了荧光俘获效应对掺铒磷酸盐和碲酸盐玻璃光谱性质及光谱参数的影响.结果表明即使在铒离子低掺杂浓度(0.1mol%Er2O3)下,荧光俘获效应也普遍存在于掺铒玻璃材料中,使得荧光寿命(τt)和荧光半高宽(FWHM)随样品的厚度和铒离子掺杂浓度增加而增大,导致