934 resultados para Crepe rubber
Resumo:
Solar radiation is an important factor for plant growth, being its availability to understory crops strongly modified by trees in an Agroforestry System (AFS). Coffee trees (Coffea arabica - cv. Obatã IAC 1669-20) were planted at a 3.4 x 0.9 m spacing inside and aside rows of monocrops of 12 year-old rubber trees (Hevea spp.), in Piracicaba-SP, Brazil (22º42'30" S, 47º38'00" W - altitude: 546m). One-year-old coffee plants exposed to 25; 30; 35; 40; 45; 80; 90; 95 and 100% of the total solar radiation were evaluated according to its biophysical parameters of solar radiation interception and capture. The Goudriaan (1977) adapted by Bernardes et al. (1998) model for radiation attenuation fit well to the measured data. Coffee plants tolerate a decrease in solar radiation availability to 50% without undergoing a reduction on growth and LAI, which was approximately 2m².m-2 under this condition. Further reductions on the availability of solar radiation caused a reduction in LAI (1.5m².m-2), thus poor land cover and solar radiation interception, resulting in growth reduction.
Resumo:
Water uptake and use by plants are essentially energy processes that can be largely modified by percentage of soil cover, plant type; foliage area and its distribution; phenological stage and several environmental factors. Coffee trees (Coffea arabica - cv. Obatã IAC 1669-20) in Agrforestry System (AFS) spaced 3.4x0.9m apart, were planted inside and along rows of 12- year-old rubber trees (Hevea spp.) in Piracicaba-SP, Brazil (22 42'30" S, 47 38'00" W - altitude: 546m). Sap flow of one-year-old coffee plants exposed to 35; 45; 80; 95 and 100% of total solar radiation was estimated by the heat balance technique (Dynamax Inc.). Coffee plants under shade showed greater water loss per unit of incident irradiance. On the other hand, plants in monocrop (full sun) had the least water loss per unit of incident irradiance. For the evaluated positions average water use was (gH2O.m-2Leaf area.MJ-1): 64.71; 67.75; 25.89; 33.54; 27.11 in Dec./2002 and 97.14; 72.50; 40.70; 32.78; 26.13 in Feb./2003. This fact may be attributed to the higher stomata sensitivity of the coffee plants under more illuminated conditions, thus plants under full sun presented the highest water use efficiency. Express transpiration by leaf mass can be a means to access plant adaptation to the various environments, which is inaccessible when the approach is made by leaf area.
Resumo:
OBJECTIVE: to verify the effectiveness of the rubber elastic band in the treatment of large wounds of the body wall of rabbits by means of traction of its edges. METHODS: we studied 30 New Zealand rabbits, divided into three groups (n=10): Group 1- healing by secondary intention; Group 2- removal and eutopic repositioning of skin as full thickness skin graft; Group 3- Approximation of wound edges with elastic rubber band. In all animals, we removed a segment of the back skin and subcutaneous tissue down to the fascia, in accordance with an acrylic mold of 8cm long by 12cm wide. All animals were observed for 21 days. RESULTS: two animals of groups 1 and 2 had wound abscess. In Group 2, there was partial or total graft loss in 90% of animals. The complete closure of the wounds was observed in four animals of Group 1, six of Group 2 and eight of Group 3. There was no difference between the scar resistance values of groups 2 and 3, which were higher than those in Group 1. The scars of the three groups were characterized by the presence of mature connective tissue mixed with blood vessels and inflammatory infiltration, predominantly polymorphonuclear. CONCLUSION: the tensile strength of the wound edges with rubber elastic band is as efficient as the skin graft to treat rabbits' large body wounds.
Resumo:
The ideal therapy for early stages of hemorrhoids is always debated. Some are more effective but are more painful, others are less painful but their efficacy is also lower. Thus, comfort or efficacy is a major concern. In the present randomized study, a comparison is made between infrared coagulation and rubber band ligation in terms of effectiveness and discomfort. One hundred patients with second degree bleeding piles were randomized prospectively to either rubber band ligation (N = 54) or infrared coagulation (N = 46). Parameters measured included postoperative discomfort and pain, time to return to work, relief in incidence of bleeding, and recurrence rate. The mean age was 38 years (range 19-68 years). The mean duration of disease was 17.5 months (range 12 to 34 months). The number of male patients was double that of females. Postoperative pain during the first week was more intense in the band ligation group (2-5 vs 0-3 on a visual analogue scale). Post-defecation pain was more intense with band ligation and so was rectal tenesmus (P = 0.0059). The patients in the infrared coagulation group resumed their duties earlier (2 vs 4 days, P = 0.03), but also had a higher recurrence or failure rate (P = 0.03). Thus, we conclude that band ligation, although more effective in controlling symptoms and obliterating hemorrhoids, is associated with more pain and discomfort to the patient. As infrared coagulation can be conveniently repeated in case of recurrence, it could be considered to be a suitable alternative office procedure for the treatment of early stage hemorrhoids.
Resumo:
Mémoire numérisé par la Division de la gestion de documents et des archives de l'Université de Montréal
Resumo:
The research work has been in the area of compounding and characterization of rubbers for use in under water electro acoustic transducers. The study also covers specific material system such as encapsulation materials, baffle material, seal material, etc. Life prediction techniques of under water rubbers in general have been established with reference to more than one functional property. Ranges of passive materials, besides the active sensing material go into the construction of underwater electro acoustic transducers. Reliability of the transducer is critically dependent on these passive materials. Rubbers are a major class of passive materials. The present work concentrates on these materials. Conventional rubbers are inadequate to meet many of the stringent function specific requirements. There exists a large gap of information in the rubber technology of underwater rubbers, particularly relating to underwater electro acoustic transducers. This study is towards filling up the gaps of information in this crucial area. Water intake into rubber is considered as the single most important issue for the long-term performance of rubbers, especially Neoprene. In this study, the cause and effects of a range of parameters affecting the water absorption by diffusion and permeation have been investigated.
Resumo:
The present work is to impart radiopacity in various natural polymers like chitosan, natural rubber and derivatives of chitosan and to characterize it. This thesis collated the radiopaque properties of these radiopaque polymers and various technological applications in the medical field. The applications of radiopaque polymers leads to an exploitation of radiopaque properties like X-ray visibility, optical density, effective atomic number, attenuation coefficient of biopolymers like chitosan, chitosan formate, chitosan acetate, carboxy methyl chitosan and natural rubber. The radiopaqe properties of these materials highly depend upon the size, shape, amount of radiopacifier and crystallinity of the radiopaque material. Radiopaque chitosan microspheres were prepared by cross linking with glutaraldehyde followed by the encapsulation of barium sulpahte. The effect of different emulsion systems on the morphology of chitosan microspheres were studied. The study concentrates radiopaque natural rubber for shielding applications. It reveals that to improve the particle size, morphology and crystalline phase of the zinc oxide particles, a novel method for the preparation of zinc oxide is adopted. A detailed radiopacity study was done in natural rubber containing 100phr precipitated zinc oxide prepared from different zinc salts. One of the significant findings of this investigation is that NR vulcanizates containing precipitated zinc oxide (from zinc acetate) shows higher attenuation coefficient. These interesting findings reveal the applications of these natural radiopaque systems in various fields like surgical tools, medical tubings, catheters, radiation shielding,etc.
Resumo:
In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.
Resumo:
In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.
Resumo:
Prevulcanized natural rubber latex was prepared by the heating of the latex compound at 55°C for different periods of time (2, 4, 6, 8, and 10 h). The changes in the colloidal stability and physical properties were evaluated during the course of prevulcanization. The prevulcanized latex compounds were stored for 300 days, and the properties were monitored at different storage intervals (0, 20, 40, 60, 120, 180, 240, and 300 days). During prevulcanization, the mechanical stability time increased, and the viscosity remained almost constant. The tensile strength increased during storage for a period of 20 days. The degree of crosslinking, modulus, elongation at break, and chloroform number were varied with the time of storage.
Resumo:
A novel method of blending natural rubber with polyvinylchloride in the latex stage was developed, Dioctyl phthalate (DOP) and Amine terminated natural rubber (ATNR) were used as plasticisers, for improving the mechanical properties of these blends. Properties of the latex stage blends were compared with those of dry blends. Latex stage blends showed superior mechanical properties compared to the blends prepared in the dry state. The ageing resistance, oil resistance and processability were found to be improved by latex stage blending.
Resumo:
Natural rubber/isora fibre composites were cured at various temperatures. The solvent swelling characteristics of natural rubber composites containing both untreated and alkali treated fibres were investigated in aromatic and aliphatic solvents like toluene, and n-hexane. The diffusion experiments were conducted by the sorption gravimetric method. The restrictions on elastomer swelling exerted by isora fibre as well as the anisotropy of swelling of the composite have been confirmed by this study. Composite cured at 100°C shows the lowest percentage swelling. The uptake of aromatic solvent is higher than that of aliphatic solvent for the composites cured at all temperatures. The effect of fibre loading on the swelling behaviour of the composite was also investigated in oils like petrol, diesel, lubricating oil etc. The % swelling index and swelling coefficient of the composite were found to decrease with increase in fibre loading. This is due to the increased hindrance exerted by the fibres at higher fibre loadings and also due to the good fibre-rubber interactions. Maximum uptake of solvent was observed with petrol followed by diesel and then lubricating oil. The presence of bonding agent in the composites restrict the swelling considerably due to the strong interfacial adhesion. At a fixed fibre loading, the alkali treated fibre composite showed lower percentage swelling compared to the untreated one.
Resumo:
A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent.
Resumo:
Polymers exhibit low electron density and they are radiolucent. Polymers can be made radiopaque by different techniques. We report a method for the preparation of radiopaque material from natural rubber (NR). NR in its latex form was iodinated. Iodinated natural rubber (INR) was characterized by using UV, thermo gravimetric analysis (TGA), and X-ray images. INR was compounded at high and low temperatures and its physical properties were measured. The low temperature cured samples show good radiopacity and conductivity. The optical density of low temperature cured samples was measured.
Resumo:
The mechanism of devulcanization of sulfur-vulcanized natural rubber with aromatic disulfides and aliphatic amines has been studied using 23-dimethyl-2-butene (C5H1,) as a low-molecular weight model compound. First C6H12 was vulcanized with a mixture of sulfur, zinc stearate and N-cyclohexyl-2-benzothiazylsulfenamide (CBS) as accelerator at 140 °C, resulting in a mixture of addition products (C(,H 1 i-S,-C5H 1 i ). The compounds were isolated and identified by High Performance Liquid Chromatography (HPLC) with respect to their various sulfur ranks. In it second stage, the vulcanized products were devulcanized using the agents mentioned above at 200 °C. The kinetics and chemistry of the breakdown of the sulfur-hridges were monitored. Both devulcanization agents decompose sulfidic vulcanization products with sulfur ranks equal or higher than 3 quite effectively and with comparable speed. Di phenyldisulfide as devulcanization agent gives rise to a high amount of mono- and disulfidic compounds formed during the devulcanization, hexadecylamine, as devulcanization agent, prevents these lower sulfur ranks from being formed.