64 resultados para Compositos polimericos


Relevância:

10.00% 10.00%

Publicador:

Resumo:

The objective of this research is the fabrication of a composite reinforced with dyed sisal fiber and polyester matrix for application in the fields such as, fashion, clothing, interior textiles; fashion accessories are some of the examples. For the fabrication of the composite, the sisal fibers were subjected to processes such as: chemical treatment with sodium hydroxide (NaOH) in the removal of impurities; bleaching for removing the yellowish color of the natural fiber and dyeing with direct dyes to confer the colors blue, green and orange. The search for new technologies ecologically correct has become a major concern in recent decades. Studies show that composite polymer reinforced by natural fibers is suitable for a large number of applications, and its use is advantageous in terms of economic and ecological. The dyed fibers were cut to a length of 30 mm, is used in the confection of webs. For this purpose, a web preparer by immersion, developed in the Laboratory of Chemical Textile of UFRN. The composite sheets measuring 300 x 300 x3 mm were molded by compression, with unsaturated orthophthalic polyester as matrix, and the samples in sizes 150 x 25 x 3 mm were cut with the aid of a laser machine, to be subjected to traction and flexion. The mechanical properties of traction and flexion in three points were performed in the Laboratory of metal and mechanical tests of Materials Engineering of UFRN. The resulting samples from the tests were evaluated in scanning electron microscope (SEM) at CTGas RN. On the basis of the analysis of the results from the mechanical tests, it was observed that the composite had good mechanical behavior, both in traction as in flexion. Furthermore, it was observed that in the water absorption test, the samples had a different percentage among themselves, this occurred due to the variation of density found in the fibre webs. The images of the SEM showed the failures from the manufacturing process and the adhesion of fibre/matrix. When the samples were prepared with the dyed fibers to be applied in fashion, the results were positive, and it can be concluded that the main objective of this work was achieved

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pós-graduação em Ciência e Tecnologia de Materiais - FC

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present invention comprises composites with multifunctional characteristics, being capable of substituting glass, with significant advantages, with particular emphasis on flexibility, for a variety of applications such as, for example, display screens and others. Among other aspects, the product that constitutes the object of the invention is particularly characterized by rendering bacterial cellulose transparent, in addition to being flexible, biocompatible and able to replace glass in 100% of possible applications. Among other aspects, the development of the composites according to the present invention allows an effective increase in optical transmission, enabling an optical transmission of more than 90%, such transparency being necessary, equally, for the development of medical devices, for example.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Compósitos de polímeros de polietileno linear de baixa densidade (LLDPE) possuem baixo desempenho mecânico devido principalmente à sua fraca interação, intermolecular, entre a cadeia polimérica e a carga. Uma maneira de minimizar esse baixo desempenho mecânico se faz com a mudança da estrutura química da poliolefina com a inserção de um grupo polar a sua cadeia, ou seja, faz-se a funcionalização das poliolefinas. O sistema de funcionalização adotado foi o processamento reativo, no qual foi utilizado para este sistema de processamento o misturador de dupla rosca acoplado a um reâmetro de torque. Neste trabalho, os grupos polares inseridos à cadeia dos polímeros de LLDPE\'s de copolímeros 1-buteno e 1-octeno (LLDPE-but e LLDPE-oct) foram o anidrido maléico (AM) e o anidrido tetrahidroftálico (ATF). Para a confecção dos compósitos foram utilizadas as cargas de microesferas de sílica modificada, no qual foi inserido compostos silanados em sua superfície (3-aminopropilsilano - APS - e trimetoxiclorosilano TMCISi) para estudo de interação com as poliolefinas funcionalizadas. Neste trabalho foram realizados ensaios de caracterização térmica, vibracional além de análises de torque do polímero fundido, análises do grau de reticulação e ensaios mecânicos de tração por elongação. Na caracterização térmica foram utilizadas as técnicas: termogravimetria (TG) e calorimetria exploratória diferencial (DSC). Na caracterização vibracional utilizou-se a espectroscopia fotoacústica no infravermelho (PAS-IR) e a espectroscopia de espalhamento Raman. Pela técnica PAS-IR foi possível comprovar a inserção dos anidridos à cadeia das poliolefinas assim como foi possível verificar a interação entre o polímero funcionalizado e a carga. Pelas técnicas térmicas de DSC e TG foi possível verificar mudanças das propriedades do compósito frente aos polímeros originais ou funcionalizados. Os ensaios mecânicos comprovaram que os compósitos de polímeros funcionalizados possuem maior elongação e tensão à ruptura comparada aos compósitos dos LLDPE\'s não funcionalizados