948 resultados para wear resistance


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrical resistance is measured in two binary liquid systems CS2 + CH3NO2 and n-C7H16 + CH3OH in the critical region as a function of frequency from 10 Hz to 100 kHz. The critical exponent b ≈ 0.35 in the singularity of dR/dT α (T - Tc)−b near Tc has no appreciable dependence upon the frequency. Thus any contribution from dielectric dispersion to the critical resistivity is not appreciable. The universal behaviour of the dR/dT anomaly does not seem to be followed in binary liquid systems.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Several methods for improving the strength of metallic materials are available and correlations between strength and various microstructural features have been established. The purpose of this paper is to review parallel developments favouring improved fracture resistance. Resistance to fracture in monotonie loading, cyclic loading and when fracture is environment-aided have been considered in steels, aluminium alloys and anisotropic materials. Finally, the question of optimising alloy behaviour is discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Marked ball grinding tests were carried out in the laboratory with a lead-zinc sulphide ore under different experimental conditions using high carbon low alloy steel (cast and forged) and high chrome cast iron balls. Relative ball wear as a function of grinding period and milling conditions was evaluated for the different types of ball materials. The role of corrosion and abrasion-erosion in the wear of grinding media is brought out. Methods to minimise ball wear through control of mill atmosphere and addition of reagents are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three distinct mechanisms — sliding, bonding and bearing — for the mobilisation of interfacial friction have been identified. In the light of these mechanisms, the effect of variation in reinforcement parameters, such as extensibility, flexibility and hardness on mobilisation of interfacial friction, and the mechanisms themselves has been examined. The influence of boundary effects of apparatus on the interfacial friction has been discussed and a method of estimating the same in a pull-out box has been proposed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The higher levels of cytochrone P-450 dependent enzyme activities reported earlier are traced to higher levels of cytochrome P-450 (CYPIIB1/B2 like) messenger RNA in the chloroquine resistant than the sensitive strains. The messenger RNA is also induced by phenobarbitone in the sensitive strain. Pretreatment with phenobarbitone affords partial protection to chloroquine toxicity in the sensitive strain and this is not due to a differential accumulation of the drug.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper describes the electrical contact resistance (ECR) measurements made on thin gold plated (gold plating of <= 0.5 mu m with a Ni underlayer of similar to 2 mu m) oxygen free high conductivity (OFHC) Cu contacts in vacuum environment. ECR in gold plated OFHC Cu contacts is found to be slightly higher than that in bare OFHC Cu contacts. Even though gold is a softer material than copper, the relatively high ECR values observed in gold plated contacts are mainly due to the higher hardness and electrical resistivity of the underlying Ni layer. It is well known that ECR is directly related to plating factor, which increases with increasing coating thickness when the electrical resistivity of coating material is more than that of substrate. Surprisingly, in the present case it is found that the ECR decreases with increasing gold layer thickness on OFHC Cu substrate (gold has higher electrical resistivity than OFHC Cu). It is analytically demonstrated from the topography and microhardness measurements results that this peculiar behavior is associated with thin gold platings, where the changes in surface roughness and microhardness with increasing layer thickness overshadow the effect of plating factor on ECR.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Erosion characteristics of high chromium (Cr, 16-19%) alloy cast iron with 5% and 10% manganese (Mn) prepared in metal and sand moulds through induction melting are investigated using jet erosion test setup in both as-cast and heat-treated conditions. The samples were characterised for hardness and microstructural properties. A new and novel non-destructive evaluation technique namely positron lifetime spectroscopy has also been used for the first time to characterise the microstructure of the material in terms of defects and their concentration. We found that the hardness decreases irrespective of the sample condition when the mould type is changed from metal to sand, On the other hand, the erosion volume loss shows an increasing trend. Since the macroscopic properties have a bearing on the microstructure, good credence is obtained from the microstructural features as seen from light and scanning electron micrographs. Faster cooling in the metal mould yielded fine carbide precipitation on the surface. The defect size and their concentration derived from positron method are higher for sand mould compared to metal mould. Lower erosion loss corresponds to smaller size defects in metal mould are the results of quicker heat transfer in the metal mould compared to the sand mould. Heat treatment effects are clearly seen as the reduced concentration of defects and spherodisation of carbides points to this. The erosion loss with respect to the defects size and concentration correlate very well.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Root and butt rot is the most harmful fungal disease affecting Norway spruce in southern Finland. In approximately 90 % of cases the causal agent is Heterobasidion parviporum. Root and butt rot infections have not been reported in Finnish peatlands. However, the increase in logging operations in peatlands means there is a risk that the fungus will eventually spread to these areas. The aim of this study was to find out the impact of growing site on the resistance of Norway spruce to Heterobasidion parviporum infections. This was investigated by artificially inoculating H. parviporum to spruce trees in pristine mire, drained peatland and mineral soil and comparing the defence reactions. Additionally, the effect of genotype on resistance was studied by comparing the responses of spruce clones representing different geographic origins. The roots and stems of the trees to be sampled were wounded and inoculated with wood dowels pre-colonised by H. parviporum hyphae. The resulting necrosis around the point of inoculation was observed. It was presumed that increased length of necrosis indicates high susceptibility of the tree to the disease. The relationship between growth rate and host resistance was also studied. The results indicated that growing site does not have a statistically significant effect on host resistance. The average length of necrosis around the point of inoculation was 35 mm in pristine mire, 37 mm in drained peatland and 40 mm in mineral soil. It was observed that growth rate does not affect resistance, but that the genotype of the tree does have an effect. The most resistant spruce clone was the one with Russian origin. The results suggest that the spruce stands in peatlands are not more resistant to root and butt rot infections than those in mineral soil. These findings should be taken into consideration when logging peatland forests.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polytetrafluoroethylene (PTFE) is an important engineering material. When rubbed or slid against a hard surface, PTFE exhibits a low coefficient of friction but a high rate of wear. These unique properties of the polymer have encouraged many mechanistic and physical examinations of the processes involved in the friction and wear of this polymer. A section of such work carried out over the past 30 years is reviewed here. When rubbed against a hard surface, the PTFE chain undergoes scission, creating active groups which chemically react with the counterface. This results in strong adhesion and a coherent transfer film. Further interaction between the bulk polymer and the transfer film gives rise to anisotropic deformation of the unit cell, which results in closeness of adjacent chains and easy shear between chains. Sliding brings about growth in as well as reorientation of crystallites situated in a very thin subsurface region of the bulk polymer. Such structural rearrangement facilitates the joining of adjacent aligned crystallites to form films and ribbons which emerge as debris.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The type of abrasion that the grinding medium experiences inside a ball mill is classified as high stress or grinding abrasion, because the stress levels at the surface of the medium exceed the yield stress of the metal when hard abrasives are crushed. During dry grinding of ores the medium undergoes not only abrasion but also erosion and impact. As all three mechanisms of wear occur simultaneously, it is difficult to follow the individual components of wear. However, it is possible to show that the overall kinetics of wear follows a simple power law of the type w = at(b), where w is the weight loss of the grinding medium for a specified grinding time t and a and b are constants. Experimental data, obtained from dry grinding of quartz for a wide range of times using AISI 52100 steel balls having various microstructures in a laboratory scale batch mill, are fitted to the proposed equation and the wear rate w is calculated from the first derivative of the equation. The mean particle sizes of the quartz charge DBAR corresponding to 50 and 80% retained size are determined by mechanical sieving of the ground product after a grinding time t and thus the relationship between wear rate and particle size of the abrasive is established. It is found that w increases rapidly with DBAR up to some critical size and then increases at a much lower rate.