885 resultados para piezoelectric ceramic element
Resumo:
This work describes the development of an analytical procedure for on-line tin determination using thermospray flame furnace atomic absorption spectrometry (TS-FF-AAS). Two tubes were evaluated as atomization cells: a metallic tube (Ni-Cr, principal components composition: 73.95% Ni and 16.05% Cr) and a ceramic tube (99.8% Al2O3). The use of air as the carrier was made by employing a Rheodyne valve to inject the samples, allowing an analytical frequency of 90 h(-1) and avoiding sample dispersion. The carrier flow rate (air), sample volume injected, and acid concentration (HCl) were evaluated for the optimization of the TS-FF-AAS system. The sensitivity for 50 mL of analytical solution with TS-FF-AAS was 2 and 5 times higher (to metallic and ceramic tube, respectively) than using an acetylene-nitrous oxide flame with pneumatic aspiration (requiring a sample volume of approximately 20 times higher.
Resumo:
Composites, made of lead zirconate titanate (PZT) ceramic powder and castor oil-based polyurethane (PU), were prepared in the film form. The films were obtained in the thickness range 100-300 mum using up to 50/50 vol.% of ceramic. Another composite (PZT/C/PU) was obtained by adding a small amount (1.0 vol.%) of graphite (C) to the PZT/PU composite. By increasing the conductivity of PU-containing graphite, polarization of PZT could be carried out with better efficiency. A comparison of piezo- and pyroelectric activities and spatial distribution of polarization between graphite doped and undoped composites reveal the advantages of using semiconductor filler. These composites were used as sensors to detect acoustic emission (AE). The detection was made using two simulated sources of AE, i.e., ball bearing drop and pencil lead break. PZT/C/PU composite was able to detect both flexural and extensional components of wave vibration. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
The electrical properties of the grain boundary region of electroceramic sensor temperature based on inverse spinel Zn7Sb2O12 were investigated at high temperature. The zinc antimoniate was synthesized by a chemical route based on the modified Pechini method. The electric properties of Zn7Sb2O12 were investigated by impedance spectroscopy in the frequency range from 5 Hz to 13 MHz and from 250 up to 600 degreesC. The grain boundary conductivity follows the Arrhenius law, with two linear branches of different slopes. These branches exhibit activation energies with very similar values; the low-temperature (less than or equal to350 degreesC) and high-temperature (greater than or equal to400 degreesC) regions are equal to 1.15 and 1.16 eV, respectively. Dissimilar behavior is observed on the relaxation time (tau) curve as a function of temperature, where a single slope is identified. The negative temperature coefficient parameters and nature of the polarization phenomenon of the grain boundary are discussed. (C) 2003 American Institute of Physics.
Resumo:
Statement of problem. The success of metal-ceramic restorations is influenced by the compatibility between base metal alloys and porcelains. Although porcelain manufacturers recommend their own metal systems as the most compatible for fabricating metal-ceramic prostheses, a number of alloys have been used.Purpose. This study evaluated the shear bond strength between a porcelain system and 4 alternative alloys.Material and methods. Two Ni-Cr alloys: 4 ALL and Wiron 99, and 2 Co-Cr alloys: IPS d.SIGN 20 and Argeloy NP were selected for this study. The porcelain (IPS d.Sign porcelain system) portion of the cylindrical inetal-ceramic specimens was 4 mm thick and 4 mm high; the metal portion was machined to 4 x 4 mm, with a base that was 5 nun thick and 1 mm high. Forty-four specimens were prepared (n=11). Ten specimens from each group were subjected to a shear load oil a universal testing machine using a 1 min/min crosshead speed. One specimen from each group was observed with a scanning electron microscope. Stress at failure (MPa) was determined. The data were analyzed with a 1-way analysis of variance (alpha=.05).Results. The groups, all including IPS d.Sign porcelain, presented the following mean bond strengths (+/-SD) in MPa: 4 ALL, 54.0 +/- 20.0; Wiron, 63.0 +/- 13.5; IPS d.SIGN 20, 71.7 +/- 19.2; Argeloy NP, 55.2 +/- 13.5. No significant differences were found among the shear bond strength values for the metal-ceramic specimens tested.Conclusion. None of the base metal alloys studied demonstrated superior bond strength to the porcelain tested.
Resumo:
In this study the Minos element was analyzed in 26 species of the repleta group and seven species of the saltans group of the genus Drosophila. The PCR and Southern blot analysis showed a wide occurrence of the Minos transposable element among species of the repleta and the saltans groups and also a low number of insertions in both genomes. Three different analyses, nucleotide divergence, historical associations, and comparisons between substitution rates (d(N) and d(S)) of Minos and Adh host gene sequences, suggest the occurrence of horizontal transfer between repleta and saltans species. These data reinforce and extend the Arca and Savakis [Genetica 108 (2000) 263] results and suggest five events of horizontal transfer to explain the present Minos distribution: between D. saltans and the ancestor of the mulleri and the mojavensis clusters; between D. hydei and the ancestor of the mulleri and the mojavensis clusters; between D. mojavensis and D. aldrichi; between D. buzzatii and D. serido; and between D. spenceri and D. emarginata. An alternative explanation would be that repeated events of horizontal transfer involving D. hydei, which is a cosmopolitan species that diverged from the others repleta species as long as 14 Mya, could have spread Minos within the repleta group and to D. saltans. The data presented in this article support a model in which distribution of Minos transposon among Drosophila species is determined by horizontal transmission balanced by vertical inactivation and extinction. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
The mechanisms of material removal and the interactions among scratches performed in ceramic materials were investigated using acoustic emission signals, and scanning electron microscopy, in scratching experiments. Several testing conditions were used to produce different types of removing mechanism on a glass as well as on a polycrystalline alumina sample composed by heterogeneous grain size. It is known that the material removing process on a polycrystalline ceramic involves intergranular microfracture and grain dislodgement, unlike the chipping produced by the extension of lateral cracks in non-granular materials, such as glass. Distinct settings for velocities, loads, and two types of diamond indenter were tested. The material removal was carried out by three different methods of scratching: single passes, repeated overlapping passes, and parallel scratches. As a general result, there was a clear relationship between the acoustic emission signals and the damage intensity occurred in the material removal. More specifically, there were differences in the acoustic emission signal levels in the scratches made on the alumina and on the glass owing to the material removal mechanisms associated with the structure of these materials. A gradual increase in the acoustic emission levels was observed when the number of repeated passes was increased as a result of the damage accumulation process followed by severe material removal. It was also noticed that the acoustic emission signals were capable of reflecting the interactions between two parallel scratches.
Resumo:
This paper presents a finite element numerical solution of free convection in a cavity with side walls maintained at constant but different temperatures. The predictions from the model and the method of solution were validated by comparison with the 'bench mark' solution and Vahl Davis' results and good agreement was found. The present model was used to obtain additional results over a wide range of Rayleigh number (10(3)-10(6)) and L/H ratios varying from 0.1 to 1.0. The predicted stream function patterns, temperature and velocity profiles as well as the mean Nusselt number were presented and discussed. (C) 2000 Elsevier B.V. Ltd. All rights reserved.
Resumo:
An experimental and theoretical study of the ferroelectric and piezoelectric behavior of PZT doped with barium is presented. Ab initio perturbed ion calculations was carried out. The properties, such as remnant polarization, coercive field and the coupling factor of the PZT at constant sintering temperature was compared with the Zr4+/Ti4+ ions dislocation energy and the lattice interaction energy. An agreement between the experimental and theoretical results, with a decrease of the interaction energy and an inversion of the energy stability from tetragonal to rhombohedral phase was observed. (C) 1999 Kluwer Academic Publishers.
Resumo:
The dielectric permittivity of Na0.80K0.20NbO3 ceramic was investigated by impedance spectroscopy. The dielectric characterization was performed from room temperature to 800 degreesC, in the frequency range 5 Hz-13 MHz. The bulk permittivity was derived by the variation of the imaginary part of the impedance as a function of reciprocal angular frequency. The permittivity values as a function of temperature showed two maxima. The first maximum is very similar at 200degreesC and the second one positioned at around 400degreesC, which was associated to Curie's temperature. The evolution of the complex permittivity as a function of frequency and temperature was investigated. At low frequency dispersion was investigated in terms of dielectric loss. The Na0.80K0.20NbO3 showed a dissipation factor between 5 and 40 over a frequency range from 1 to 10(2) kHz. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
In this paper a piezoelectric composite membranes were developed for charge generator to promoter bone regeneration on defects sites. Is known that the osteogenesis process is induced by interactions between biological mechanisms and electrical phenomena. The membranes were prepared by mixing Barium Titanate (BT) powders and PVDF-TrFE (PVDF:TrFE = 60:40 mol%) on dimethylformamide medium. This precursor solution was dried and crystallized at 100degreesC for 12 hours. Composites membranes were obtained by following methods: solvent casting (SC), spincoating (SP), solvent extraction by water addition (WS) and hot pressing (HP).The microstructural analysis performed by SEM showed connectivity type 3-0 and 3-1 with high homogeneity for samples of ceramic volume fraction major than 0.50. Powder agglomerates within the polymer matrix was evidenced were observed for composites with the BT volume fraction major than 40%. The composite of ceramic fraction of 0.55 presented the best values of remanent polarization (similar to33 muC/cm(2)), but the flexibility of these composites with the larger ceramic fraction was significantly affected.For in vivo evaluation PVDF-TrFE/BT 90/10 membranes with 3cm larger were longitudinally implanted under tibiae of male rabbit. After 21 days the animals were sacrificed. By histological analyses were observed neo formed bone with a high mitotic activity. In the interface bone-membrane was evidenced a pronounced callus formation. These results encourage further applications of these membranes in bone-repair process.