Although already to exist alternative technique and economically viable for destination of used tires, quantitative data on properties of constructive elements that use the rubber waste as aggregate still are restricted. In the present work, the waste proceeding from industry of retreading as material for manufacture of composite destined to the production of constructive elements was considered. Mechanical and thermal properties of mortar had been analyzed Portland cement with addition of waste without treatment, in the ratios of 10%, 20% and 30% in mass in relation to the mass of the cement, substituting the aggregate in the trace in mortar 1:5 mass cement and sand. The size of the used residue varied between 0,30mm and 4,8mm (passing in the bolter 4,8mm and being restrained in the one of 0,30mm), being it in the formats fibers and granular. The influences of the size and the percentage of residue added to the mortar (in substitution to the aggregate) in the thermal and mechanical properties had been considered. Assays of body-of-test in thestates had been become fullfilled cool (consistency index) and hardened (absorption of water for capillarity, strength the compression, traction and strength flexural). The work is centralized in the problem of the relation thermal performance /strength mechanics of used constructive systems in regions of low latitudes (Been of the Piauí), characterized for raised indices of solar radiation.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Population growth experienced in major cities, allied to society s need of infra-structure, especially ones related to habitational demands, increases the consumption of construction materials. As a consequence, consumption of natural resources itself. Thus, due to this process, concrete is one of the most produced materials in civil construction. This is also due to the great diversity of its application, easiness in its execution and adequate mechanical performance, as well as low production costs. Following the same tendencies in construction development, the ceramic industry has intensified the production of porcelain ceramic tiles and floors. These are achieved by a fine finishing and receive polishing at the end of the fabrication process. This work researched the use of porcelain residues in polishing for the production of concrete. All of which; due to economical and environmental issues. This process aims to prove adequate destiny for this type of residue, due to environmental issues, incorporating it to the concrete itself; all of which provides economy in consumption of the materials that constitute concrete. Thus, the main characteristics of concrete were investigated through the inclusion of different concentration of the porcelain residue as additional trait element. The residue rates incorporated to the trait varied from 10% to 50% in relation to the cement mass, in the traits with plastic additives and without plastic additives. It is observed that the inclusion of porcelain residue produced a meaningful alteration in the consistency of fresh concrete. This residue has a fine granulometry and it considerably absorbed the water used in the concrete spreading, influencing the way this material is dealt with. Thus, the value of cement striking decreases with the increase of residues present in trait. The maximal incorporation of the residue was of 50%, massively, for the same factor water/initial cement. The use of residues in concrete results in an 40% increase in the compression resistance. It is also proportional to residue concentration of porcelain in the trait. The microstructure was also favored once porosity and concrete absorption decreases with the use of this residue. The parameters demonstrate the quality and durability of the concrete produced with this residue. The use of porcelain residue in concrete composition has not produced meaningful thermal behavior changes. Thermal conductivity, heat capacity and thermal diffusivity have been maintained basically constant

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The northeastern region of Brazil has a large number of wells producing oil using a method of secondary recovery steam injection, since the oil produced in this region is essentially viscous. This recovery method puts the cement / coating on thermal cycling, due to the difference in coefficient of thermal expansion between cement and metal coating causes the appearance of cracks at this interface, allowing the passage of the annular fluid, which is associated with serious risk socioeconomic and environmental. In view of these cracks, a correction operation is required, resulting in more costs and temporary halt of production of the well. Alternatively, the oil industry has developed technology for adding new materials in cement pastes, oil well, providing high ductility and low density in order to withstand the thermo-mechanical loads generated by the injection of water vapor. In this context, vermiculite, a clay mineral found in abundance in Brazil has been applied in its expanded form in the construction industry for the manufacture of lightweight concrete with excellent insulation and noise due to its high melting point and the presence of air in their layers lamellar. Therefore, the vermiculite is used for the purpose of providing low-density cement paste and withstand high temperatures caused by steam injection. Thus, the present study compared the default folder containing cement and water with the folders with 6%, 8% and 10% vermiculite micron conducting tests of free water, rheology and compressive strength where it obtained the concentration of 8 % with the best results. Subsequently, the selected concentration, was compared with the results recommended by the API standard tests of filtered and stability. And finally, analyzed the results from tests of specific gravity and time of thickening. Before the study we were able to make a folder with a low density that can be used in cementing oil well in order to withstand the thermo-mechanical loads generated by steam injection

Relevância:

10.00% 10.00%

Publicador:

Resumo:

One of the major current challenges for oilwell companies is the extraction of oil from evaporitic zones, also known as pre-salt basins. Deep reservoirs are found under thick salt layers formed from the evaporation of sea water. Salt layers seal the flow of oil from underneath rock formations, which store hydrocarbons and increase the probability of success in oil and gas exploration. Oilwells are cemented using Portland-based slurries to promote mechanical stability and zonal isolation. For pre-salt oilwells, NaCl must be added to saturate the cement slurries, however, the presence of salt in the composition of slurries affects their overall behavior. Therefore, the objective of the present study was to evaluate the effect of the addition of 5 to 25% NaCl on selected properties of Portland-based slurries. A series of tests were carried out to assess the rheological behavior, thickening time, free water and ultrassonic compressive strength. In addition, the slurries were also characterized by thermal analysis, X ray diffraction and scanning electron microscopy. The results showed that the addition of NaCl affected the thickening time of the slurries. NaCl contents up to 10% shortened the thickening time of the slurries. On the other hand, concentrations in excess of 20% not only extended the thickening time, but also reduced the strength of hardened slurries. The addition of NaCl resulted in the formation of a different crystalline phase called Friedel´s salt, where free chlorine is bonded to tricalcium aluminate

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Portland-polymers composites are promising candidates to be used as cementing material in Northeastern oil wells of Brazil containing heavy oils submitted to steam injection. In this way, it is necessary to evaluate its degradation in the commonly acidizind agents. In addition, to identify how aggressive are the different hostile environments it is an important contribution on the decision of the acidic systems to be used in. It was investigated the performance of the Portland-polymer composites using powdered polyurethane, aqueous polyurethane, rubber tire residues and a biopolymer, those were reinforced with polished carbon steel SAE 1045 to make the electrochemical measurements. HCl 15,0 %, HCl 6,0 % + HF 1,5 % (soft mud acid), HCl 12,0 % + HF 3,0 % (regular mud acid) and HAc 10 % + HF 1,5 % were used as degrading environment and electrolytes. The more aggressive acid solution to the plain Portland hardened cement paste was the regular mud acid, that showed loss of weight around 23.0 %, followed by the soft mud acid, the showed 11.0 %, 15.0 % HCl with 7,0 % and, at last the 10.0 % HAc plus HF 1.5 % with just 1.0 %. The powdered polyurethane-composite and the aqueous polyurethane one showed larger durability, with reduction around 87.0 % on the loss of weight in regular mud acid. The acid attack is superficial and it occurs as an action layer, where the degraded layer is responsible for the decrease on the kinetic of the degrading process. This behavior can be seen mainly on the Portland- aqueous polyurethane composite, because the degraded layer is impregnated with chemically modified polymer. The fact of the acid attack does not have influence on the compressive strength or fratography of the samples, in a general way, confirms that theory. The mechanism of the efficiency of the Portland-polymers composites subjected to acid attack is due to decreased porosity and permeability related with the plain Portland paste, minor quantity of Ca+2, element preferentially leached to the acidic solution, wave effect and to substitute part of the degrading bulk for the polymeric one. The electrolyte HAc 10 % + HF 1,5 % was the least aggressive one to the external corrosion of the casing, showing open circuit potentials around +250 mV compared to -130 mV to the simulated pore solution to the first 24 hours immersion. This behavior has been performed for two months at least. Similar corrosion rates were showed between both of the electrolytes, around 0.01 μA.cm-2. Total impedance values, insipient arcs and big polarization resistance capacitive arcs on the Nyquist plots, indicating passivity process, confirm its efficiency. In this way, Portlandpolymers composites are possible solutions to be succeed applied to oilwell cementing concomitant submitted to steam injection and acidizing operation and the HAc 10,0 % + HF 1,5 % is the less aggressive solution to the external corrosion of the casing

Relevância:

10.00% 10.00%

Publicador:

Resumo:

As unidades estratigráficas que resultaram da evolução do rio Tejo em Portugal, aqui analisadas em pormenor entre Vila Velha de Ródão e Chamusca, possuem distintas características sedimentares e indústrias líticas: uma unidade culminante do enchimento sedimentar (o ancestral Tejo, antes do início da etapa de incisão fluvial) - SLD13 (+142 a 262 m acima do leito actual; com provável idade 3,6 a 1,8 Ma), sem indústrias identificadas; terraço T1 (+76 a 180 m; ca. 1000? a 900 ka), sem indústrias; terraço T2 (+57 a 150 m; idade estimada em ca. 600 ka), sem indústrias; terraço T3 (+36 a 113 m; ca. 460 a 360? ka), sem indústrias; terraço T4 (+26 a 55 m; ca. 335 a 155 ka), Paleolítico Inferior (Acheulense) em níveis da base e intermédios mas Paleolítico Médio inicial em níveis do topo; terraço T5 (+5 a 34 m; 135 a 73 ka), Paleolítico Médio (com talhe Mustierense, Levallois); terraço T6 (+3 a 14 m; 62 a 32 ka), Paleolítico Médio final (Mustierense final); Areias da Carregueira (areias eólicas) e coluviões (+3 a ca. 100 m; 32 a 12 ka), Paleolítico Superior a Epipaleolítico; enchimento da planície aluvial (+0 a 8 m; ca. 12 ka a actual), Mesolítico e indústrias mais recentes. As diferenças na elevação (a.r.b.) das escadarias de terraços resultam de soerguimento diferencial, devido a falhas ativas. Numa dada escadaria datada, a projeção da elevação da superfície de cada terraço (a.r.b.) versus a sua idade permitiu estimar a idade do topo do terraço T2 (ca. 600 ka) e a provável idade do início da etapa de incisão (ca. 1,8 Ma). Obteve-se a duração da fase de agradação dos terraços baixos e médios: T6 – 30 ka; T5 – 62 ka; T4 – ca. 180 ka; T3 – ca. 100? ka. Conclui-se que durante o Plistocénico médio e final, as fases de incisão e alargamento do vale foram curtas (ca. 11-25 ka) e ocorreram durante períodos de nível do mar muito baixo, alternando com mais longas fases de inundação e agradação do vale durante níveis do mar mais altos. Estas oscilações eustáticas de causa climática estão sobrepostas a um contexto de soerguimento de longo termo, controlando o desenvolvimento das escadarias. Calculou-se que para os últimos ca. 155 ka as taxas de incisão de curto-termo apresentam valores (0,09 a 0,41 m/ka), aproximadamente, duplos dos calculados para o intervalo ca. 155 a 900 ka (0,04 a 0,28 m/ka). Este aumento na taxa de incisão deve estar relacionado com um aumento na taxa de soerguimento por intensificação da compressão devido à convergência entre as placas Africana e Eurasiática. Abstract: The terrace staircases of the Lower Tagus River (Ródão to Chamusca) – characterization and interpretation of the sedimentary, tectonic, climatic and Palaeolithic data The stratigraphic units that record the evolution of the Tagus River in Portugal (study area between Vila Velha de Ródão and Chamusca villages) have different sedimentary characteristics and lithic industries: a culminant sedimentary unit (the ancestral Tagus, before the drainage network entrenchment) – SLD13 (+142 to 262 m above river bed – a.r.b.; with probable age 3.6 to 1.8 Ma), without artefacts; T1 terrace (+76 to 180 m; ca. 1000? to 900 ka), without artefacts; T2 terrace (+57 to 150 m; top deposits with a probable age ca. 600 ka), without artefacts; T3 terrace (+36 to 113 m; ca. 460 to 360? ka), without artefacts; T4 terrace (+26 to 55 m; ca. 335 a 155 ka), Lower Paleolithic (Acheulian) at basal and middle levels but early Middle Paleolithic at top levels; T5 terrace (+5 to 34 m; 135 to 73 ka), Middle Paleolithic (Mousterian; Levallois technique); T6 terrace (+3 to 14 m; 62 to 32 ka), late Middle Paleolithic (late Mousterian); Carregueira Sands (aeolian sands) and colluvium (+3 a ca. 100 m; 32 to 12 ka), Upper Paleolithic to Epipaleolithic; alluvial plain (+0 to 8 m; ca. 12 ka to present), Mesolithic and more recent industries. The differences in elevation (a.r.b.) of the several terrace staircases results from differential uplift due to active faults. The age interval for each aggradation phase of T3 to T6 terraces was obtained: T3 – ca. 100? ka; T4 – ca. 180 ka; T5 – 62 ka; T6 – 30 ka. The intervals of river down-cutting and widening of the valley floor were short (ca. 11-25 ka) and coincided with periods of very low sea-level. The plotting of the elevation (a.r.b.) versus the age of each terrace surface allows to estimate the age of the T2 terrace (ca. 600 ka) and the probable age of the beginning of the incision stage (ca. 1.8 Ma). So, the high amplitude sea-level changes that characterized the Middle and Late Pleistocene strongly determined the episodic down-cutting phases of the river during the low stands sea levels that alternated with the flooding and aggradation phases of the incised valley during highstand sea levels. These climate related eustatic oscillations are superimposed onto a long term uplift pattern, controlling the river terrace staircase development. During the last ca. 155 ka, the short-term incision rates (0.09 a 0.41 m/ka) were twice the values determined for the interval 155 to 900 ka (0.04 to 0.28 m/ka). This increase in incision rate should be related with an increase in uplift rate resulting from an intensification of compression due to the convergence between African - Eurasian plates.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present work is to study the characteristics and technological properties of soil-cement bricks made from binary and ternary mixtures of Portland cement, sand, water, with or without addition of gravel from the drilling of oil wells, which could be used by industry, aiming to improve its performance and reduce cost by using the residue and, consequently, increasing its useful life. The soil-cement bricks are one of the alternatives to masonry construction. These elements, after a short curing period, provide compressive strength similar to that of solid bricks and ceramic blocks, and the higher the resistance the higher the amount of cement used. We used the soil from the city of São José do Mipibu / RN, the banks of the River Baldun, cement CPIIZ-32 and residue of drill cuttings from oil wells drilling onshore wells in the town of Mossley, RN, provided Petrobras. To determine the optimum mix, we studied the inclusion of different residues (100%, 80%, 70%, 60% and 50%) where 15 bodies were made of the test piece. The assessment was made of bricks made from simple compression tests, mass loss by immersion and water absorption. The experimental results proved the efficiency and high utilization of the waste from the drilling of oil wells, making the brick-cement-soil residue with a higher strength and lower water absorption. The best result in terms of mechanical strength and water absorption for the ternary mixture was 10% soil, 14% cement and 80% residue. In terms of binary mixtures, we obtained the best result for the mix-cement residue, which was 14% cement incorporated in the residue

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Current environmental concerns include the excessive consumption and inefficient use of non-renewable natural resources. The construction industry is considered one of the largest consumers of natural raw materials, significantly contributing to the environmental degradation of the planet. The use of calcareous quarry (RPPC) and porcelain tile polishing residues (RPP) as partial replacements of the cement in mortars is an interesting alternative to minimize the exploration of considerably large amounts of natural resources. The present study aimed at investigating the properties of fresh and hardened mortars produced using residues to replace cement. The residues used were fully characterized to determine their specific mass, unitary mass, particle size distribution and morphology, and composition. The performance of the mortars was compared to that of reference compositions, prepared without residues. A total of 18 compositions were prepared, 16 using residues and 2 reference ones. The mortars were prepared using Portland CP II F 32 cement, CH I hydrated lime, river sand and tap water. The compositions of the mortars were 1:1:6 and 1:0.5:4.5 (vol%), and water to cement ratios of 1.87 and 1.45 were used, respectively. The mortars in the fresh state were evaluated by consistency index, water retention, density of mass and incorporated air content tests. In their hardened state, the mortars were evaluated by apparent mass density, modulus of elasticity, flexural tensile strength, compressive strength and water absorption by capillarity. The mortars were also analyzed by scanning electron microscopy, energy dispersive spectroscopy, X-ray diffraction and fluorescence. Finally, they were classified according to NBR 13281 standards. The mortars prepared using residues partially replacing the cement exhibited lower modulus of elasticity compared to the reference compositions, thus improving the performance in their intended use. On the downside, the water absorption by capillarity was affected by the presence of residues and both the tensile and compressive strength were reduced. However, from the overall standpoint, the replacement of cement by calcareous quarry or porcelain tile polishing residues did not result in significant changes in the properties of the mortars. Therefore, compositions containing these residues can be used in the construction industry

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The corrosive phenomenon on reinforced concrete structures is one of the most founded pathologies on the coastal area. With the objective to prevent the process development, or even, retard its beginning, it was studied the application of inorganic covering over concrete surfaces, after its cure, as well as, evaluate the efficiency of the covering applied on the concrete in reducing its porosity of concrete preventing the entrance of aggressive agents to preserve the integrity of the existing armor inside it, comparing the result obtained with the body-of-proof reference, that didn´t receive covering protection. On the concrete production it was used Portland Cement CP II 32, coarse aggregate, fine aggregate and water from the local distributive. Two types of covering were used, one resin based of silicon and solvent and other white cement based, selected sands and acrylic resin. The concrete mixture adopted was 1:1,5:2,5 (cement, fine aggregate, coarse aggregate) and 0.50 water/cement ratio. With the concrete on fresh state was made the experiment test to determinate the workability. On the hardened state was made the concrete resistance experiment, absorption of water and electrochemical experiments, through polarization curves. Also was held optical microscopy and Scanning Electron Microscopy experiments to analyze the layer of the covering applied to the concrete surface and the interface between the concrete and the layer. The obtained results shows that the covering applied to the concrete surface didn´t affect the resistance towards compression. On the absorption of water occurred a diminution of the percentage absorbed, improving the concrete development by making it more impermeable towards the entrance of aggressive agents. The electrochemical experiment results confirmed the water absorption results; the body-of-proof covered presented larger protection towards the development of corrosives process and retarded the evolution of the corrosive phenomenon

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Novel cementing materials formulations containing flexible polymeric admixtures have been studied aiming at improving the mechanical behavior of oil well cement slurries submitted to steam injection. However, research activities in this sector are still under development. The steam injected directly into the well causes casing dilation, which after a reduction in temperature, tends to return to its original dimensions, resulting in crack formation and hydraulic isolation loss of the well, which will result in shortening of well life. In this scenario, the objective of the present study was to evaluate the mechanical behavior of Portland-based slurries containing SBR latex, applied in oil well cementing of wells submitted to steam injection. Were formulated slurries with densities of 1.797 g/cm3 (15.0 lb/Gal) and 1.869 g/cm3 (15.6 lb/Gal), containing admixtures with a latex concentration of 0; 66.88; 133.76; 200.64 and 267.52 L/m3 (0, 0.5, 1.0, 1.5 and 2.0 gpc). Tests including rheology, fluid loss control, thickening time, API compressive strength and splitting tensile strength, beyond steam injection simulation. Microstrutural characteristics of the slurries were also performed (XRD, TG, FTIR and SEM). The results showed that increasing the polymer concentration increased in the rheological properties and fluid loss, and a decrease in the elasticity modulus of the cement slurries. The results obtained showed that the slurries can be applied in cementing operations of oil wells submitted to steam injection.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This work addresses the production of lightweight concrete building elements, such as plates, prefabricated slabs for pre-molded and panels of fencing, presenting a singular concrete: the Lightweight Concrete, with special properties such low density and good strength, by means of the joint use of industrial waste of thermosetting unsaturated polyesters and biodegradable foaming agent, named Polymeric Lightweight Concrete. This study covered various features of the materials used in the composition of the Polymeric Lightweight Concrete, using a planning of factorial design 23, aiming at studying of the strength, production, dosage processes, characterization of mechanical properties and microstructural analysis of the transition zone between the light artificial aggregate and the matrix of cement. The results of the mechanical strength tests were analyzed using a computational statistics tool (Statistica software) to understand the behavior and obtain the ideal quantity of each material used in the formula of the Polymeric Lightweight Concrete. The definition of the ideal formula has the purpose of obtaining a material with the lowest possible dry density and resistance to compression in accordance with NBR 12.646/92 (≥ 2.5 MPa after 28 days). In the microstructural characterization by scanning electron microscopy it was observed an influence of the materials in the process of cement hydration, showing good interaction between the wrinkled face of the residue of unsaturated polyesters thermosetting and putty and, consequently, the final strength. The attaining of an ideal formula, given the Brazilian standards, the experimental results obtained in the characterization and comparison of these results with conventional materials, confirmed that the developed Polymeric Lightweight Concrete is suitable for the production of building elements that are advantageous for construction

Relevância:

10.00% 10.00%

Publicador:

Resumo:

O trabalho foca-se no estudo biomecânico de próteses do joelho. Através de modelos computacionais pretendeu-se obter o melhor desempenho da prótese, variando as geometrias e os materiais. Os modelos foram submetidos à compressão com carga assimétrica para avaliação do comportamento da prótese e zonas de maior desgaste ósseo.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Oil wells subjected to cyclic steam injection present important challenges for the development of well cementing systems, mainly due to tensile stresses caused by thermal gradients during its useful life. Cement sheath failures in wells using conventional high compressive strength systems lead to the use of cement systems that are more flexible and/or ductile, with emphasis on Portland cement systems with latex addition. Recent research efforts have presented geopolymeric systems as alternatives. These cementing systems are based on alkaline activation of amorphous aluminosilicates such as metakaolin or fly ash and display advantageous properties such as high compressive strength, fast setting and thermal stability. Basic geopolymeric formulations can be found in the literature, which meet basic oil industry specifications such as rheology, compressive strength and thickening time. In this work, new geopolymeric formulations were developed, based on metakaolin, potassium silicate, potassium hydroxide, silica fume and mineral fiber, using the state of the art in chemical composition, mixture modeling and additivation to optimize the most relevant properties for oil well cementing. Starting from molar ratios considered ideal in the literature (SiO2/Al2O3 = 3.8 e K2O/Al2O3 = 1.0), a study of dry mixtures was performed,based on the compressive packing model, resulting in an optimal volume of 6% for the added solid material. This material (silica fume and mineral fiber) works both as an additional silica source (in the case of silica fume) and as mechanical reinforcement, especially in the case of mineral fiber, which incremented the tensile strength. The first triaxial mechanical study of this class of materials was performed. For comparison, a mechanical study of conventional latex-based cementing systems was also carried out. Regardless of differences in the failure mode (brittle for geopolymers, ductile for latex-based systems), the superior uniaxial compressive strength (37 MPa for the geopolymeric slurry P5 versus 18 MPa for the conventional slurry P2), similar triaxial behavior (friction angle 21° for P5 and P2) and lower stifness (in the elastic region 5.1 GPa for P5 versus 6.8 GPa for P2) of the geopolymeric systems allowed them to withstand a similar amount of mechanical energy (155 kJ/m3 for P5 versus 208 kJ/m3 for P2), noting that geopolymers work in the elastic regime, without the microcracking present in the case of latex-based systems. Therefore, the geopolymers studied on this work must be designed for application in the elastic region to avoid brittle failure. Finally, the tensile strength of geopolymers is originally poor (1.3 MPa for the geopolymeric slurry P3) due to its brittle structure. However, after additivation with mineral fiber, the tensile strength became equivalent to that of latex-based systems (2.3 MPa for P5 and 2.1 MPa for P2). The technical viability of conventional and proposed formulations was evaluated for the whole well life, including stresses due to cyclic steam injection. This analysis was performed using finite element-based simulation software. It was verified that conventional slurries are viable up to 204ºF (400ºC) and geopolymeric slurries are viable above 500ºF (260ºC)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A artroplastia é a solução para diversos problemas que destabilizam a articulação do joelho. Os profissionais de saúde tem ao seu dispor várias próteses, variando essencialmente a geometria e o material. O trabalho foca-se no estudo biomecânico de próteses do joelho. Através de um modelo aproximado pretendeu-se obter o melhor desempenho de uma prótese, variando geometrias e materiais. O modelo biomecânico foi submetido a um carregamento à compressão permitindo avaliar as zonas de maior desgaste ósseo.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This dissertation presents a hybrid ceramic block the use of which reside in the buildings executed with walls. Initially, we conducted a survey on the requirements and / or norms prevailing in Brazil about structural ceramic blocks, making use of the experiences in other countries. This work seeks new materials and / or products in order to maintain or increase the compressive strength of the ceramic blocks, without neglecting the other properties. Then was collected materials (clay and crushed powder) and an approach on the characterization, through fluorescence, Mineralogy, vitrification curve and characterization of these materials used in the manufacture of the blocks by Ray Diffraction "X" and SEM. Subsequently it was made, numbered and measured dimensions of about 150 bodies of the test piece (hybrid ceramic blocks in small sizes) with varying percentages of 0%, 5%, 10% and 15% substitution of crushed clay powder. After sintering of the bodies of the test piece at temperatures of 900oC, 1000oC 1100oC and with a heating rate of 5oC/minuto and level of 1 hour, the samples were submitted to the tests (compressive strength and water absorption) and calculated their retractions, which were subsequently carried out the analysis of the results according to the criteria and parameters required by Brazilian legislation and standards in force