894 resultados para VINYLIC POLYMERIZATION
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Plasmas generated in de discharges in aromatic compounds have been used for several years in polymerization processes. The chemical kinetics developed in such a plasma environment are extremely complicated. Therefore it is extremely important to set up optical and electrical diagnostics in order to establish the kinetics of the film growth, In this work we studied de plasmas generated ill low-pressure atmospheres of benzene for different values of gas pressure and power coupled to the discharge. The pressure range varied from 0.2 to 1.0 mbar for electric power running from 4 to 25 W, the main chemical species observed within the discharge were CH, H and C. It was observed that the CH relative concentration increases continuously with the power in the range investigated. The electron temperature varied from 0.5 to 2.0 eV with the increase of the power, for a fixed value of gas pressure. The relative dielectric constant of the plasma polymerized benzene was kept around 4.8 from 100 Hz to 10 kHz, presenting a resonance near 25 kHz. This electric behaviour of the film was the same fur different conditions of polymeric film deposition, (C) 1997 Elsevier B.V. S.A.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Modern industry has frequently employed ethylene glycol ethers as monomers in plasma polymerization process to produce different types of coatings. In this work we used a stainless steel plasma reactor to grow thin polymeric films from low pressure RF excited plasma of diethylene glycol dimethyl ether. Plasmas were generated at 5W RF power in the range of 16 Pa to 60 Pa. The molecular structure of plasma polymerized films and their optical properties were analyzed by Fourier Transform Infrared Spectroscopy (FTIR) and UltravioletVisible Spectroscopy, respectively. The IR spectra show C-H stretching at 3000-2900 cm(-1), C=O stretching at 1730-1650 cm(-1), C-H bending at 1440-1380 cm(-1), C-O and C-O-C stretching at 1200-1000 cm(-1). The refraction index was around 1.5 and the optical gap calculated from absorption coefficient presented value near 3.8 eV. Water contact angle of the films ranged from 40 degrees to 35 degrees with corresponding surface energy from 66 to 73x10(-7) J. Because of its favorable optical and hydrophilic characteristics these films can be used in ophthalmic industries as glass lenses coatings.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
In this work biodiesel was gotten through the transesterification reaction using the oil of castor as source of triglycerides and using the methylic route for obtaining of esters. For the characterization of biodiesel and its mixtures with mineral diesel oil, physical chemical parameters and several analytical techniques had been used, as well as: gas chromatography (GC), nuclear magnetic resonance of proton (1H NMR), infrared spectroscopy (IR) and thermal analysis. The chromatography confirmed the complete reaction of esters in biodiesel presenting a 97,08% conversion. The 1H - NMR presented singlet in 3,6 ppm corresponding to the hydrogen of the group ester RCOO CH3. The infrared presented a strong band in 1741 cm-1 referring to stretching C=O of ester and an average band in 1175 cm-1 referring C O deformation. With the data of thermal analysis it was possible to observe the thermal and oxidative stability of the samples changing the atmospheres of synthetic air and nitrogen, where stages of the thermal decomposition had been verified and had been attributed to the volatilization and/or decomposition of the triacylglycerides. The thermal degradation of the samples was carried through 150 and 210°C during 1, 12, 24 and 48 hours and was observed change in the thermogravimetric profile, therefore an increase in the number of stages of the thermal decomposition also occurred indicating characteristic intermediate composites of polymerization, being this confirmed through the rheological study that presented brusque increase of viscosity. The kinetic study showed that the activation energy has the following order: biodiesel > mineral diesel oil > mixtures biodiesel/diesel
Resumo:
Latices based on acrylic acid and ethyl methacrylate, crosslinked with 1,6‐propoxylate‐hexanodiol diacrylate were synthesized via emulsion polymerization with different monomeric compositions. The resultant latices were thickened with different NaOH/(acrylic acid) molar ratios and were characterized by titrimetry, zeta potential measurements, turbidimetry, and capillary viscometry. Intrinsic viscosity was determined for an uncrosslinked copolymer, using toluene as solvent. All the latices were coagulated with NaCl and washed with water at 60°C analyzed by FTIR spectrophotometry, in order to characterize functional groups from the copolymer and crosslinking agent.
Resumo:
Latexes based on acrylic acid, acrylamide, ethyl methacrylate, and ethyl acrylate were synthesized via emulsion polymerization with different monomer compositions. The resultant latices were thickened with different molar ratios of NaOH to acrylic acid and were analyzed in terms of acid‐basis titrimetry, turbidimetry, rheology, and tensiometry. Titrimetry, turbidimetry, and rheometry were used to analyze factors such as carboxyl group availability and particle solubilization, tensiometry monitoring the influence of carboxyl neutralization on polymer‐surfactant interactions. For the acrylic acid content used in this work (20 wt%), the results indicated that as carboxyl groups distribution became more homogeneous, the process of latex thickening became more effective
Resumo:
The present work aims the preparation of filmes of strontium-doped lanthanum manganite (perovskita) yttria-stabilized zirconia (LSM-SDC) films deposited on substrate of YSZ by means of spin coating technique having as principal objective their application to solid oxide fuel cells of intermediate temperature. La0,8Sr0,2MnO3 and Ce0,8Sm0,2O1,9 were obtained by modified Pechini method by use of gelatin which act as polymerization agent. The powders obtained were characterized by Xray fluorescence, X ray diffraction, electronic scanning microscopy and the superficial area by BET method. The results obtained by X-ray fluorescence showed that the route adopted for obtention of powders was effective in the obtention of the compositions with close values to the stoichiometrics. Ethyl cellulose was used as pore-forming agent and mixed with the LSM-SDC powders in weight proportions of 1:24, 2:23 and 1:9. The films were sintered at 1150 °C for 4 h and characterized by X-ray diffraction and scanning electron microscopy technique (SEM) and atomic force. The phases quantification of the precursory powders and of the obtained films was carried through Rietveld method. According with the analysis of SEM, as the content of ethyl cellulose was increased, the pore distribution in films become more uniform and the pore size reduced. The methodology used for the obtention of the films was very efficient, considering a material was obtained with characteristics that were proper to the application as electrolyte/cathode system to solid oxide fuel cells
Resumo:
Electrically conductive poly(vinylidene fluoride)(PVDF) - polyaniline blends of different composition were synthesized by chemical polymerization of aniline in a mixture of PVDF and dimethylformamide (DMF) and studied by electrical conductivity measurement, UV-Vis-NIR and FTIR spectroscopy. The samples were obtained as flexible films by pressing the powder at 180 degrees C for 5 min. The electrical conductivity showed a great dependence on the syntheses parameters. The higher value of the electrical conductivity was obtained for the oxidant/aniline molar ratio equal to 1 and p-toluenesulfonic acid-TSA/aniline ratio between 3 and 6. UV-Vis-NIR and FTIR spectra of the blend are similar to the doped PANI, indicating that the PANI is responsible for the high electrical conductivity of the blend. The electrical conductivity of blend proved to be stable as a function of temperature decreasing about one order at temperature of 100 degrees C. The route used to obtain the polymer blend showed to be a suitable alternative in order to obtain PVDF/PANI-TSA blends with high electrical conductivity. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Non-isothermal dielectric analysis (DEA) and differential scanning calorimetry (DSC) techniques were used to study the epoxy nanocomposites prepared by reacting 1,3,5,7,9,11,13,15-octa[dimethylsiloxypropylglycidylether] pentaciclo [9.5.1.1(3,9).1(5,15).1(7,13)] octasilsesquioxane (ODPG) with methylenedianiline (MDA). Loss factor (epsilon) and activation energy were calculated by DEA. The relationships between the loss factor, the activation energy, the structure of the network, and the mechanical properties were investigated. Activation energies determined by DEA and DSC, heat of polymerization, fracture toughness and tensile modulus show the same profile for mechanical properties with respect to ODPG content.
Resumo:
Compósitos de borracha natural (Hevea brasiliensis)-BN/polianilina - PANI, com diferentes composições foram obtidos através da polimerização por emulsão do monômero anilina na presença da BN e do ácido dodecilbenzeno sulfônico (DBSA). Filmes finos e homogêneos foram obtidos por prensagem a quente. Os compósitos foram caracterizados por condutividade elétrica, FTIR, UV-vis-NIR, DSC e difração de raios X. Compósito com condutividade elétrica cerca de 14 ordens de grandeza maior que a BN foi obtido. Este alto valor de condutividade é atribuído à formação da PANI no estado dopado no compósito, que foi verificado através das técnicas de UV-vis-NIR e FTIR. Os resultados obtidos com a técnica de DSC e difratometria de raios X indicaram que os polímeros são imiscíveis e que a presença da borracha não altera significantemente a fase cristalina da PANI-DBSA no compósito.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
A partially hydrolyzed polyacrylamide (HPAM) is a copolymer composed of acrylamide and sodium acrylate. Due to its wide range of applications there are different methods for its quantification and characterization in solution systems. Evaluation of C* is important to describe the transition from dilute to semi-dilute, behavior, when the solution will have its characteristic viscosity at concentrations above C*. This dissertation describes the determination of the critical concentration of overlap C* by potentiometry of partially hydrolyzed polyacrylamide - HPAM under acidic conditions. Based on the law of mass action and the proper treatment of the constant of aggregate formation, polymer molecular weight, degree of polymerization and hydrolysis were calculated. The inflection point was determined by the intersection of the resulting equation and mathematical development, statistically satisfy the experimental points relating the number of moles of monomers (n), equilibrium constant of formation of the entanglements (K*), pH, C* and acidity constant of the polymer (Ka). The viscometric parameters of C* showed a percentage difference compared to potentiometers. The results for the determination of C*, and degree of copolymerization molar mass proved to be a simple alternative for the characterization of polymers with protonated monomers and water soluble