939 resultados para Crack-bridging
Resumo:
CD40L is one of the key molecules bridging the activation of specific T cells and the maturation of professional and nonprofessional antigen-presenting cells including B cells. CD4(+) T cells have been regarded as the major T-cell subset that expresses CD40L upon cognate activation; however, we demonstrate here that a putative CD8(+) helper T-cell subset expressing CD40L is induced in human and murine CD8(+) T cells in vitro and in mice immunized with antigen-pulsed dendritic cells. IL-12 and STAT4-mediated signaling was the major instructive cytokine signal boosting the ability of CD8(+) T cells to express CD40L both in vitro and in vivo. Additionally, TCR signaling strength modulated CD40L expression in CD8(+) T cells after primary differentiation in vitro as well as in vivo. The induction of CD40L in CD8(+) T cells regulated by IL-12 and TCR signaling may enable CD8(+) T cells to respond autonomously of CD4(+) T cells. Thus, we propose that under proinflammatory conditions, a self-sustaining positive feedback loop could facilitate the efficient priming of T cells stimulated by high affinity peptide displaying APCs.
Resumo:
The three miles of fibrous concrete resurfacing in Greene County, Iowa were placed in September and early October, 1973. It was recognized in advance that cracking and other performance characteristics of the fibrous concrete sections and of the control sections would be major factors in the evaluation of the project. A low level aerial survey was made of the old pavement. During construction of the resurfacing, the aerial survey was checked to insure that cracks in the old pavement were referenced to the 100 ft. station marks placed in the resurfacing. Crack surveys have been conducted on dates indicated below. Additional cracks found at each subsequent survey are shown in a color matching the date notation. April, 1974 November, 1974 October, 1975 October, 1976
Resumo:
The three miles of fibrous concrete resurfacing in Greene County, Iowa were placed in September and early October, 1973. It was recognized in advance that cracking and other performance characteristics of the fibrous concrete sections and of the control sections would be major factors in the evaluation of the project. A low level aerial survey was made of the old pavement. During construction of the resurfacing, the aerial survey was checked to insure that cracks in the old pavement were referenced to the 100 ft. station marks placed in the resurfacing. Crack surveys have been conducted on dates indicated below. Additional cracks found at each subsequent survey are shown in a color matching the date notation. April, 1974 November, 1974 October, 1975 October, 1976 October, 1977
Resumo:
The three miles of fibrous concrete resurfacing in Greene County, Iowa were placed in September and early October, 1973. It was recognized in advance that cracking and other performance characteristics of the fibrous concrete sections and of the central sections would be major factors in the evaluation of the project. A low level aerial survey was made of the old pavement. During construction of the resurfacing, the aerial survey was checked to insure that cracks in the old pavement were referenced to the 100 ft. station marks placed in the resurfacing. The crack survey recorded herein was made in March and April, 1974. Those cracks in the resurfacing that are reflections of cracks in the underlying slab are identified by /\ marks. Observations (not detailed crack surveys) made in June, 1974 indicate that further cracking of the resurfacing has occurred since this report was prepared. In particular, there appears to be same additional longitudinal cracking over the widening joints.
Resumo:
The crack and seat (C & S) method of rehabilitating concrete pavements has been proposed to reduce the incidence of reflective cracking in asphalt overlays. These cracked pieces help reduce the thermal effects on lateral joint movement while the seating of slab pieces reduces vertical movement. This 1986 project demonstrated that a 0.6 m x 0.9 m (2 ft x 3 ft) cracking pattern was optimal to retard reflective cracking in an asphalt overlay. The best performance among three C & S test sections was section 4 with a 0.6 m x 0.9 m (2 ft x 3 ft) cracking pattern and 7.6 cm (3 in) overlay. Structural ratings determined from the Road Rater™ indicated little difference between each C & S section with varying AC thicknesses and crack spacings. Although reflection cracking is reduced in the early years after construction, the effectiveness of the C & S method diminishes over time.
Resumo:
Roughly 242 million used tires are generated annually in the United States. Many of these tires end up being landfilled or stockpiled. The stockpiles are unsightly, unsanitary, and also collect water which creates the perfect breeding ground for mosquitoes, some of which carry disease. In an effort to reduce the number of used tire stockpiles the federal government mandated the use of recycled rubber in federally funded, state implemented department of transportation (DOT) projects. This mandate required the use of recycled rubber in 5% of the asphalt cement concrete (ACC) tonnage used in federally funded projects in 1994, increasing that amount by 5% each year until 20% was reached, and remaining at 20% thereafter. The mandate was removed as part of the appropriations process in 1994, after the projects in this research had been completed. This report covers five separate projects that were constructed by the Iowa Department Of Transportation (DOT) in 1991 and 1992. These projects had all had some form of rubber incorporated into their construction and were evaluated for 5 years. The conclusion of the study is that the pavements with tire rubber added performed essentially the same as conventional ACC pavement. An exception was the use of rubber chips in a surface lift. This performed better at crack control and worse with friction values than conventional ACC. The cost of the pavement with rubber additive was significantly higher. As a result, the benefits do not outweigh the costs of using this recycled rubber process in pavements in Iowa.
Resumo:
This final report for Phase 1 of the research on epoxy-coated, prestressing strands in precast prestressed concrete (PC) panels has been published in two volumes. Volume 1--Technical Report contains the problem description, literature review, and survey results; descriptions of the test specimens, experimental tests, and analytical models; discussions of the analytical and experimental results; summary, conclusions, and recommendations; list of references; and acknowledgments. Volume 2--Supplemental Report contains additional information in the form of appendix material for Volume 1 on the questionnaires, strand forces, geometry of the specimens, concrete crack patterns that formed in the strand transfer length and strand development length specimens, concrete strains in the strand transfer length specimens, and load-point deflections and strand-slip measurements for the strand development length specimens. Appendix A contains the questionnaires that were sent to the design agencies and precast concrete producers. A summary of the results to the questions on the surveys are given as the number of respondents who provided the same answers and as paraphrased comments from the respondents. Appendix B contains graphs of strand force versus time, strand force versus temperature, and strand force versus strand cutting sequence for the concrete castings. Appendix C contains figures that show the location of each specimen in the prestress bed, the geometrical configurations for the strand transfer length (T-type) specimens and strand development length (D-type) specimens, and the concrete cracks that developed in some of the T-type specimens when they were prestressed. Appendix D contains figures that show the concrete cracks that developed in the D-type specimens during the strand development length tests. For each of these tests, the sequence of the failure for the specimen is specified. Appendix E contains graphs of concrete strain versus distance from the end of the T-type specimens that were instrumented with internal embedment strain gages. Appendix F contains graphs of load versus load-point deflection and load versus strand-slip for the strand development length tests of the D-type specimens.
Resumo:
An ACC overlay is most often the rehabilitative effort used to maintain the serviceability of either an ACC or PCC pavement. The major problem in durability of this ACC overlay comes from reflective cracking. These cracks usually open, allowing water to enter the unsealed crack and strip the ACC in the overlay. The stripping of the ACC allows accelerated deterioration at the crack. Two engineering fabrics were evaluated in this project in order to determine their effectiveness in reducing reflective cracking. These two materials are: • PavePrep, Contech Construction Products Inc. • ProGuard, Phillips Fiber Corporation The data indicated a statistically significant decrease in reflective crack formation in the ProGuard fabric sections compared to control. There was little evidence of a similar effect from the PavePrep fabric sections compared to control. However, the rate of cracking (the rate of formation of new cracks) for both fabrics and control tended to be similar after three years. The benefits of using these fabrics (possible delay of some crack formation by two years) on this project did not outweigh the costs of up to $4200.00 per mile.
Resumo:
The report compares and contrasts the automated PASCO method of pavement evaluation to the manual procedures used by the Iowa Department of Transportation (DOT) to evaluate pavement condition. Iowa DOT's use of IJK and BPR roadmeters and manual crack and patch surveys are compared to PASCO's use of 35-mm photography, artificial lighting and hairline projection, tracking wheels and lasers to measure ride, cracking and patching, rut depths, and roughness. The Iowa DOT method provides a Present Serviceability Index (PSI) value and PASCO provides a Maintenance Control Index (MCI). Seven sections of Interstate Highway, county roads and city streets, and one shoulder section were tested with different speeds of data collection, surface types and textures, and stop and start conditions. High correlation of results between the two methods in the measurement of roughness (0.93 for the tracking wheel and 0.84 for the laser method) were recorded. Rut depth correlations of 0.61 and cracking of 0.32 are attributed to PASCO's more comprehensive measurement techniques. A cost analysis of the data provided by both systems indicates that PASCO is capable of providing a comparable result with improved accuracy at a cost of $125-$150 or less per two-lane mile depending on survey mileage. Improved data collection speed, accuracy, and reliability, and a visible record of pavement condition for comparable costs are available. The PASCO system's ability to provide the data required in the Highway Pavement Distress Identification Manual, the Pavement Condition Rating Guide, and the Strategic Highway Research Program Long Term Pavement Performance (LTPP) Studies, is also outlined in the report.
Resumo:
This report summarizes the analysis of transverse cracking in asphalt pavement by a five state study team from Iowa, Kansas, Nebraska, North Dakota, and Oklahoma. The study was initiated under the sponsorship of the Federal Highway Administration and four evaluation conferences were held during the course of the study. Each state conducted a crack inventory on their asphalt pavement. An effort was made to correlate this inventory with numerous factors that were considered to be pertinent to the cracking problem. One state did indicate that there was a correlation between transverse cracking severity and the subsurface geology. The other states were unable to identify any significant factors as being the primary contributors. The analysis of the problem was divided into, (1) mix design, (2) maintenance, and (3) 3R rehabilitation. Many potential factors to be considered were identified under each of these three study divisions. There were many conclusions as to good and bad practices. One major conclusions was that a more effective crack maintenance program with early sealing was essential. Some new practices were suggested as potentially more cost effective in design, construction and maintenance. The interchange of methods and procedures by individual states yielded benefits in that other states selected practices that would be an improvement to their program.
Resumo:
Major highway concrete pavements in Iowa have exhibited premature deterioration attributed to effects of ettringite formation, alkali-silica expansive reactions, and to frost attack, or some combination of them. These pavements were constructed in the mid- 1980s as non-reinforced, dual-lane, roads ranging in thickness between 200 mm and 300 mm, with skewed joints reinforced with dowels. Deterioration was initially recognized with a darkening of joint regions, which occurred for some pavements as soon as four years after construction. Pavement condition ranges from severe damage to none, and there appeared to be no unequivocal materials or processing variables correlated with failure. Based upon visual examinations, petrographic evaluation, and application of materials models, the deterioration of concrete highway pavements in Iowa appear related to a freeze-thaw failure of the coarse aggregate and the mortar. Crack patterns sub-parallel to the concrete surface transecting the mortar fraction and the coarse aggregate are indicative of freeze-thaw damage of both the mortar and aggregate. The entrained air void system was marginal to substandard, and filling of some of the finer-sized voids by ettringite appears to have further degraded the air void system. The formation of secondary ettringite within the entrained air voids probably reflects a relatively high degree of concrete saturation causing the smaller voids to be filled with pore solution when the concrete freezes. Alkali-silica reaction (ASR) affects some quartz and shale in the fine aggregate, but is not considered to be a significant cause of the deterioration. Delayed ettringite formation was not deemed likely as no evidence of a uniform paste expansion was observed. The lack of field-observed expansion is also evidence against the ASR and DEF modes of deterioration. The utilization of fly ash does not appear to have affected the deterioration as all pavements with or without fly ash exhibiting substantial damage also exhibit significant filling of the entrained air void system, and specimens containing fly ash from sound pavements do not have significant filling. The influence of the mixture design, mixing, and placing must be evaluated with respect to development of an adequate entrained air void system, concrete homogeneity, longterm drying shrinkage, and microcracking. A high-sand mix may have contributed to the difficult mixture characteristics noted upon placement and exacerbate concrete heterogeneity problems, difficulty in developing an adequate entrained air void system, poor consolidation potential, and increased drying shrinkage and cracking. Finally, the availability of moisture must also be considered, as the secondary precipitation of ettringite in entrained air voids indicates they were at least partially filled with pore solution at times. Water availability at the base of the slabs, in joints, and cracks may have provided a means for absorbing water to a point of critical saturation.
Resumo:
In conventional construction practices, a longitudinal joint is sawed in a PCC (Portland Cement Concrete) pavement to control concrete shrinkage cracking between two lanes of traffic. Sawing a joint in hardened concrete is an expensive and time consuming operation. The longitudinal joint is not a working joint (in comparison to a transverse joint) as it is typically tied with a tie bar at 30 inch spacing. The open joint reservoir, left by the saw blade, typically is filled or sealed with a durable crack sealant to keep incompressibles and water from getting into the joint reservoir. An experimental joint forming knife has been developed. It is installed under the paving machine to form the longitudinal joint in the wet concrete as a part of the paving process. Through this research method, forming a very narrow longitudinal joint during the paving process, two conventional paving operations can be eliminated. Joint forming eliminates the need of the joint sawing operation in the hard concrete, and as the joint that is formed does not leave a wide-open reservoir, but only a hairline crack, it does not need the joint filling or sealing operation. Therefore, the two conventional longitudinal joint sawing and sealing operations are both being eliminated by this innovation. A laboratory scale prototype joint forming knife was built and tested, initially forming joints in small concrete beams. The results were positive so the method was proposed for field testing. Initial field tests were done in the construction season of 2001, limited to one paving contractor. A number of modifications were made to the knife throughout the field tests. About 3000 feet of longitudinal joint was formed in 2001. Additional testing was done in the 2002 construction season, working with the same contractor. About 150,000 feet of longitudinal joint was formed in 2002. Evaluations of the formed joints were done to determine longitudinal joint hairline crack development rate and appearance. Additional tests will be done in the next construction season to improve or perfect the longitudinal joint forming technique.
Resumo:
Premature deterioration of Portland Cement Concrete (PCC) pavements led to investigations for causes of the concrete failures. Evidence of parallel longitudinal cracks in deteriorating pavements, with crack spacings similar to paver vibrator spacings, made it clear that the vibrators were related to the cause for deterioration. After a number of field trips observing paving operations and measuring vibrator frequencies, it soon became clear that the paver vibrators were, in many cases, not running in compliance with the Iowa DOT specification. The specified frequency was from 5000 to 8000 revolutions per minute (rpm). The pavers visited did not have a monitoring system to give a continuous frequency readout for any of it's vibrators. Occasionally, during a paving operation, frequency readings were taken on some vibrators with a hand held tachometer. However, that degree of monitoring was found to be far from providing the quality of information and control necessary to maintain compliance to the Iowa DOT specification. A paver vibrator monitoring system, which would operate continuously while paving and cover all vibrators, was determined to be essential. The output must be visible to the paver operator and inspector at all times.
Resumo:
Oxidation is the primary cause of long-term aging in asphalt pavements. As a pavement oxidizes, it stiffens and can eventually crack. The use of an antioxidant as a performance enhancer in an asphalt binder could delay aging, thus increasing the life of an asphalt pavement. Lignin is a highly available and well-studied antioxidant. A wet-mill ethanol plant produces several co-products, some of which contain lignin. The use of lignin from ethanol production could provide a benefit to asphalt pavements and also give more value to the co-products. The following research examined the effects of lignin on asphalt pavements. Three lignin-containing co-products were separately combined with four asphalt binders in varying amounts to determine the optimum amount of co-product that would provide the greatest benefit to the asphalt binders. The asphalt binder and co-product blends were evaluated according to Superpave specifications and performance graded on a continuous scale. The data indicated a stiffening effect on the binder caused by the addition of the co-products. The more a co-product was added, the more a binder stiffened. Binder stiffening benefited the high temperature properties and the low temperature binder properties were negatively affected. However, the low temperature stiffening effects were small and in many cases not significant. The co-products had an overall effect of widening the temperature range of the binders. This result suggests some antioxidant activity between the binder and the lignin. Testing with a fourth co-product with no lignin supported the idea that lignin acts as an antioxidant. The samples with no lignin aged significantly more than the samples with lignin. Infrared spectrometry also supported the idea that lignin acts as an antioxidant by observing decreases in some oxidative aging products.