This study proposes to synthesize (1-x)PMN-xPT powders, where 0.10 < x < 0.45, using the T-modified columbite route. This methodology consists in the preparation of the MNT columbite precursor via the polymeric precursor method, followed by the solid state reaction with PbO to get the PMN-PT powders. It was verified that from 15 mol% of Ti, the MNT presents the coexistence of two main phases with different crystal symmetry: Rutile and Columbite. However, the synthesis of (1-x)PMN-xPT powders is not affected by this event. A detailed study of structural effects in MNT and PMN-PT powders as function of Ti content was made using the Rietveld method. It was also demonstrated that powders possess high chemical and microstructural homogeneity.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ceramic samples of SrBi2(Nb1-xTax)O-9 (0 less than or equal to x less than or equal to 1) were prepared by the solid state reaction method in order to investigate their structural and electrical features as well as obtain useful information to improve the properties of SrBi2(Nb1-xTax)O-9 as a thin film. The X-ray diffraction patterns and the scanning electronic microscopy photomicrographs show no secondary phases but the formation of a solid-state solution for all the composition. The ac conductivity of the samples, measured at 25 degreesC and 100 kHz frequency, decreases with the increase of Ta content. Such results were explained by intrinsic conductivity of pure components.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ferroelectric layefed-perovskite BaBi2Ta2O9 (BBT) has been prepared successfully by solid-state reaction. The influence of pressure and temperature/time annealing regime on the BBT phase formation was analyzed. The powders were characterized by thermal analysis and Xray diffraction and the sintered pellets by scanning electron microscopy. The crystalline BBT phase, free of secondary phases was obtained at 950 degreesC for 2 h. For an applied field strength of 380 kV/cm, a remnant polarization of 7.6 muC/cm(2) and an electric coercive field of 45.7 kV/cm were obtained. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Substitutions of Ti and Cu in ZrO2.MgO (Z), cause transformation from monoclinic (m) to cubic (c) and tetragonal (t). According to the vacancy model and solid Solution formation models, neither CuO nor TiO2 cause zirconia stabilization, which derives front other phenomena. Data analysis by TMA using the CRH (constant rate of heating) method shows a solid state reaction of ZrO2.MgO.TiO2 (Z.TiO2) demonstrating a dominant mechanism of volume diffusion (n = 1). However, the sintering of ZrO2.MgO.CuO (Z.CuO) shows a viscous flow mechanism (n = 0), a similar phenomena to that of by sintering of glass. Transformations, such as: CuO to Cu2O at 1000 degreesC, ZrO2 (m) to ZrO2 (t) at 1100 degreesC and Cu2O (s) to Cu2O (l) at 1230 degreesC cause successive rearrangements of microstructure inside of region I (sintering process) and lead to interpretation errors when the Bannister equation is used. (C) 2003 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this study, the effect of bismuth content on the crystal structure, morphology and electric properties of barium-bismuth-tantalate (BBT) ceramics was explored with the aid of X-ray diffraction (XRD), scanning electron microcopy (SEM), dielectric properties and ferroelectric hysteresis loops. BaBi2Ta2O9 (BBT) ceramics have been successfully prepared by the solid-state reaction. The BBT phase was crystallized at 900 degreesC for 2 h. The excess of bismuth controls the grain size, affecting the density of the material. Measurements of dieletric constant and dieletric losses confirm that the material is a ferroeletric with a Curie temperature around 77 degreesC. The dieletric constant measured at room temperature was 400, with a dielectric loss of 0.03. Both the phase-transition behaviour and ferroelectric properties, such as spontaneous polarization (P-s), showed a dependence on Bi content. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper reports on time-resolved emission and excitation spectra measurement studies of Gd2SiO5:Ce3+ in powder or pellet samples, from spherical particles, in order to assign the Ce3+ ion transitions into two different symmetry sites. Samples were obtained from solid-state reaction of the spherical particles oxides, SiO2 and Gd2O3:Ce3+. From time-resolved spectroscopy measurements Ce3+ ion transitions occupying the two different gadolinium crystallographic sites in Gd2SiO5 were separated and assigned. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

SnO2-based varistors doped with 0.5% cobalt, 0.5% zinc and various tantalum amounts were prepared by the solid-state route. Experimental evidence shows that small quantities of Ta2O5 improve the nonlinear properties of the samples significantly. It was found that samples doped with 0.05 mol% Ta2O5 exhibit the highest density (98.5%), the lowest electric breakdown field (E-b = 1050 V/cm) and the highest coefficient of nonlinearity (alpha = 11.5). The effect of Ta2O5 dopant could be explained by the substitution of Ta5+ by Sn4+. (C) 2004 Elsevier Ltd and Techna S.r.l. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report experiments of electron spin resonance (ESR) of Cu2+ in polycrystalline samples of CaCu3Ti4O12 post-annealed in different atmospheres. After being synthesized by solid state reaction, pellets of CaCu3Ti4O12 were annealed for 24 h at 1000 degrees C under air, Ar or O-2. Our temperature dependent ESR data revealed for all samples nearly temperature independent g value (2.15(1)) and linewidth for T > T-N approximate to 25 K. However, the values of ESR linewidth are strongly affected by the oxygen content in the sample. For instance, argon post-annealed samples show a much larger linewidth than the O-2 or air post-annealed samples. We attribute this broadening to an increase of the dipolar homogeneous broadening of the Cu2+ ESR lines due to the presence of oxygen vacancies which induce an S=1/2 spin inside the TiO6 octahedra. Correlation between a systematic dependence of the ESR linewidth on the oxygen content and the high dielectric constant of these materials is addressed. Also, ESR, magnetic susceptibility, and specific heat data for a single crystal of CaCu3Ti4O12 and for polycrystals of CdCu3Ti4O12 are reported.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Recently, mechanochemical synthesis was widely used in preparation of perovskite type of materials, such as BaTiO3, PbTiO3, PZT, etc. In this work, the possibility of mechanochemical synthesis of CaTiO3 from different precursors, such as CaCO3 or CaO and TiO2 was investigated. Intensive milling of mixture of CaO and TiO2, under optimal milling conditions, resulted in synthesis of single phase CaTiO3. It was also found that intensive milling of powder mixture containing CaCO3 and TiO2 only activate the powders for the sintering process; hence the CaTiO3 could be obtained at lower temperatures of sintering. To complete reaction of CaTiO3 formation during milling it is necessary to reduce CO2 partial pressure, i.e. it is necessary to change the atmosphere inside the vials during milling. In this work, an explanation for difference in milling behavior of different precursors was proposed and discussed. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polycrystalline materials of SnO(2) doped with ZnO, WO(3), CoO, Nb(2)O(5), and MoO(3). were synthesized by solid state reaction. X-ray powder diffraction data were collected with Cu K(alpha) radiation from a Rigaku-Rint 2000 rotating anode source. The structural and profile parameters were refined by the Rietveld method using GSAS [2]. The obtained residual parameters are R(wp) = 11,93% and R(Bragg) = 4,19%. The refined profile parameters indicate no anisotropic crystallite microstrain. The refinement results and Fourier differences calculations indicate that the dopants do not occupy interstitial sites in the crystal structure of SnO(2).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The magnetorefractive effect (MRE) has been used for the first time to study the magnetotransport properties of La1-xSrxMnO3 perovskite materials. A direct correlation between the MRE and colossal magnetoresistance was observed. Samples with x = 0-0.3 prepared using the homogeneous coprecipitation and the solid state reaction methods were studied, covering the range of insulating to metallic behaviour. The M RE probed both the magnetically induced modification of the scattering of Drude-like electrons and the magnetic dependence of a stretching vibration mode. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

PTCR barium titanate has been prepared following two different powder preparation techniques: the solid-state reaction route and co-precipitation route for the comparison of results. The co-precipitation route produces better PTCR characteristics with low room temperature resistivity and better reproducibility of prepared samples. The effects of different concentrations of additives like donors, acceptors and excess titanium have been optimized to get good quality PTCR samples. (C) 2002 Elsevier B.V. B.V. All rights reserved.