957 resultados para LIGHT EMITTING DIODES
Resumo:
Two new star-burst compounds based on 1,3,5-triazine core and carbazole end-capped phenylene ethynylene arms (1a and 1b) were synthesized and characterized. Their photophysical properties were investigated systematically via spectroscopic and theoretical methods. Both compounds exhibit strong 1π–π⁎ transitions in the UV region and intense 1π–π⁎/intramolecular charge transfer (1ICT) absorption bands in the UV–vis region. Introducing the carbazole end-capped phenylene ethynylene arm on the 1,3,5-triazine core causes a slight bathochromic shift and enhanced molar extinction coefficient of the 1π–π⁎/1ICT transition band. Both compounds are emissive in solution at room temperature and 77 K, which exhibit pronounced positive solvatochromic effect. The emitting state could be ascribed to 1ICT state in more polar solvent, and 1π–π⁎ state in low-polarity solvent. The high emission quantum yields (Φem=0.90~1.0) of 1a and 1b (in hexane and toluene) make them potential candidates as efficient light-emitting materials. The spectroscopic studies and theoretical calculations indicate that the photophysical properties of these compounds can be tuned by the carbazole end-capped phenylene ethynylene arm, which would also be useful for rational design of photofunctional materials.
Resumo:
A high contrast ratio between windows and surrounding walls may lead to office workers visual discomfort that could negatively affect their satisfaction and productivity. Consequently, occupants may try to adapt their working environment by closing blinds and/ or turning on the lights to enhance indoor visual comfort, which can reduce predicted energy savings. The hypothesis of this study is that reducing luminance contrast ratio on the window wall will improve window appearance which potentially will reduce visual discomfort and decrease workers interventions. Thus, this PhD research proposes a simple strategy to diminish the luminance contrast on the window wall by increasing the luminance of the areas surrounding the windows using supplementary light emitting diode (LED) systems. To test the hypothesis, this investigation will involve three experiments in different office layouts with various window types and orientations in Brisbane, Australia. It will assess user preferences for different luminance patterns in windowed offices featuring flexible, lowpower LED lighting installations that allows multiple lighting design options on the window wall. Detailed luminance and illuminance measures will be used to match quantitative lighting design assessment to user preferences.
Resumo:
The light emitted by flat panel displays (FPD) can be generated in many different ways, such as for example alternating current thin film electroluminescence (ACTFEL), liquid crystal display (LCD), light emitting diode (LED), or plasma display panel (PDP) technologies. In this work, the focus was on ACTFEL devices and the goal was to develop new thin film processes for light emitting materials in ACTFEL devices. The films were deposited with the atomic layer deposition (ALD) method, which has been utilized in the manufacturing of ACTFEL displays since the mid-1980s. The ALD method is based on surface-controlled self-terminated reactions and a maximum of one layer of the desired material can be prepared during one deposition cycle. Therefore, the film thickness can be controlled simply by adjusting the number of deposition cycles. In addition, both large areas and deep trench structures can be covered uniformly. During this work, new ALD processes were developed for the following thin film materials: BaS, CuxS, MnS, PbS, SrS, SrSe, SrTe, SrS1-xSex, ZnS, and ZnS1-xSex. In addition, several ACTFEL devices were prepared where the light emitting material was BaS, SrS, SrS1-xSex, ZnS, or ZnS1-xSex thin film that was doped with Ce, Cu, Eu, Mn, or Pb. The sulfoselenide films were made by substituting the elemental selenium for sulfur on the substrate surface during film deposition. In this way, it was possible to replace a maximum of 90% of the sulfur with selenium, and the XRD analyses indicated that the films were solid solutions. The polycrystalline BaS, SrS, and ZnS thin films were deposited at 180-400, 120-460, and 280-500 °C, respectively, and the processes had a wide temperature range where the growth rate of the films was independent of the deposition temperature. The electroluminescence studies showed that the doped sulfoselenide films resulted in low emission intensity. However, the emission intensities and emission colors of the doped SrS, BaS, and ZnS films were comparable with those found in earlier studies. It was also shown that the electro-optical properties of the different ZnS:Mn devices were different as a consequence of different ZnS:Mn processes. Finally, it was concluded that because the higher deposition temperature seemed to result in a higher emission intensity, the thermal stability of the reactants has a significant role when the light emitting materials of ACTFEL devices are deposited with the ALD method.
Resumo:
Photoluminescence (PL), electroluminescence (EL) and photoconductivity (PC) of poly[(2,5-dimethoxy-p-phenylene) vinylene] (DMPPV) of varying conjugation length were studied. Thin film devices of the DMPPV with different conjugation lengths, as the active medium, were prepared. The PL emission spectra revealed the radiative decay of the singlet excitons with peak values corresponding to energies below the absorption onset. The PL. emission spectra of the copolymer films also revealed vibronic features, which get well resolved upon cooling to 80K, The devices exhibit light emitting diode (LED) behavior; the I-V curves and EL spectra are compared in these DMPPV samples having different conjugation lengths. The PC studies reveal subtle features, which can be attributed to the optically generated excitations in the system.
Resumo:
Inorganic and organic semiconductor devices are generally viewed as distinct and separate technologies. Herein we report a hybrid inorganic-organic light-emitting device employing the use of an air stable polymer, Poly (9,9-dioctylfluorene-alt-benzothiadiazole) as a p-type layer to create a heterojunction, avoiding the use of p-type GaN, which is difficult to grow, being prone to the complex and expensive fabrication techniques that characterises it. I-V characteristics of the GaN-polymer heterojunction fabricated by us exhibits excellent rectification. The luminescence onset voltage is typically about 8-10 V. The device emits yellowish white electroluminescence with CIE coordinates (0.42, 0.44). (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The use of reduced graphene oxide (RGO) and graphene nanoribbons (GNRs) as infrared photodetectors is explored, based on recent results dealing with solar cells, light-emitting devices, photodetectors, and ultrafast lasers. IR detection is demonstrated by both RGO and GNRs (see image) in terms of the time-resolved photocurrent and photoresponse. The responsivity of the detectors and their functioning are presented.
Resumo:
Novel amphiphilic poly(meta-phenylene)s were prepared by an oxidative coupling approach. These polymers were synthesized to shed light on their solution properties with special emphasis on aggregation and folding behavior. The polymers were characterized by NMR spectroscopy and molecular weights were determined by Gel Permeation Chromatography using Universal calibration. Literature studies revealed that the backbone of these PMPs can be helical moreover, the light emitting properties of this conjugated polymer can be used as a handle to study the possible aggregation or self-assembling behavior. In this report we show the synthesis, characterization and preliminary aggregation properties that points out that one of the synthesized PMP behave as a polysoap.
Resumo:
Solar cells on thin conformable substrates require conventional plastics such asPS and PMMA that provide better mechanical and environmental stability with cost reduction. We can also tune charge transfer between PPV derivatives and fullerene derivatives via morphology control of the plastics in the solar cells. Our group has conducted morphology evolution studies in nano- and microscale light emitting domains in poly (2-methoxy, 5-(2'-ethyl-hexyloxy)-p-phenylenevinylene) (MEH-PPV) and poly (methyl methacrylate) (PMMA) blends. Our current research has been focused on tricomponent-photoactive solar cells which comprise MEH-PPV, PMMA, and [6,6]-phenyl C61-butyric acid methyl ester (PCBM, Figure 1) in the photoactive layer. Morphology control of the photoactive materials and fine tuning of photovoltaic properties for the solar cells are our primary interest. Similar work has been done by the Sariciftci research group. Additionally, a study on inter- and intramolecular photoinduced charge transfer using MEH-PPV derivatives that have different conjugation lengths (Figure 1, n=1 and 0.85) has been performed.
Resumo:
Red light emitting cubic Y1.95Eu0.05O3 nanophosphors have been synthesized by a low temperature solution combustion method using ethylene diamine tetra acetic acid (EDTA) as fuel. The systematic studies on the effect of calcination temperature on its structural, photoluminescence (PL), and thermoluminescence (TL) properties were reported. The crystallinity of the samples increases, and the strain is reduced with increasing calcination temperature. SEM micrographs reveal that samples lose their porous nature with an increase in calcination temperature. PL spectra show that the intensity of the red emission (611 nm) is highly dependent on the calcination temperature and is found to be 10 times higher when compared to as-formed samples. The optical band gap (E-g) was found to reduce with an increase of calcination temperature due to reduction of surface defects. The thermoluminescence (TL) intensity was found to be much enhanced in the 1000 degrees C calcined sample. The increase of PL and TL intensity with calcination temperature is attributed to the decrease of the nonradiative recombination probability, which occurs through the elimination of quenching defects. The trap parameters (E, b, s) were estimated from Chen's glow peak shape method and are discussed in detail for their possible usage in dosimetry.
Resumo:
In the current communication, we report the synthesis, spectroscopic, crystal structure, DFT and photophysical studies of a new nicotinonitrile derivative, viz. 2-methoxy-6-(4-methoxy-phenyl)-4-p-tolyl-nicotinonitrile (2) as a potential blue light emitting material. The compound 2 was synthesized in good yield via a simple route. The acquired spectral and elemental analysis data were in consistent with the chemical structure of 2. The single crystal study further confirms its three dimensional structure, molecular shape, and nature of short contacts. Its DFT calculations reveal that compound 2 possesses a non-planar structure and its theoretical IR spectral data are found to be in accordance with experimental values. In addition, its UV visible and fluorescence spectral measurements prove that the compound exhibits good absorption and fluorescence properties. Also, it shows positive solvatochromic effect when the solvent polarity was varied from non-polar to polar. (c) 2014 Elsevier B.V. All rights reserved.
Resumo:
CaTiO3:Sm3+ (1-11 mol%) nanophosphors were successfully synthesized by a low temperature solution combustion method LCS]. The structural and morphological properties of the phosphors were studied by using Powder X-ray diffractometer (PXRD), Fourier transform infrared (FTIR), X-ray photo electron spectroscopy (XPS), scanning electron microscope (SEM) and transmission electron microscopy (TEM). TEM studies indicate that the size of the phosphor is similar to 20-35 nm. Photoluminescence (PL) properties of Sm3+ (1-11 mol%) doped CaTiO3 for NUV excitation (407 nm) was studied in order to investigate the possibility of its use in White light emitting diode (WLED) applications. The emission spectra consists of intra 4f transitions of Sm3+, such as (4)G(5/2) -> H-6(5/2) (561 nm), (4)G(5/2) -> H-6(7/2) (601-611 nm), (4)G(5/2) -> H-6(9/2) (648 nm) and (4)G(5/2) -> H-6(11/2) (703 nm) respectively. Further, the emission at 601-611 nm show strong orange-red emission and can be applied to the orange-red emission of phosphor for the application for near ultra violet (NUV) excitation. Thermoluminescence (TL) of the samples irradiated with gamma source in the dose range 100-500 Gy was recorded at a heating rate of 5 degrees C s(-1). Two well resolved glow peaks at 164 degrees C and 214 degrees C along with shouldered peak at 186 degrees C were recorded. TL intensity increases up to 300 Gy and thereafter, it decreases with further increase of dose. The kinetic parameters namely activation energy (E), frequency factor (s) and order of kinetics were estimated and results were discussed in detail. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
We have synthesized a series of 4'-aryl substituted 2,2':6',2 `'-terpyridine (terpy) derivatives, namely 4'-(4-methylphenyl)-2,2':6',2 `'-terpyridine (C-1), 4'-(2-furyl)-2,2':6'2 `'-terpyridine (C-2), and 4'-(3,4,5-trimethoxyphenyl)-2,2':6',2 `'-terpyridine (C-3). The synthesized terpy compounds were characterized by elemental analyses, FTIR, NMR (H-1 and C-13), and ESI-Mass spectrometry. Photophysical, electrochemical and thermal properties of terpy compounds were systematically studied. Maximum excitation band was observed between 240 and 330 nm using UV-visible spectra, and maximum emission peaks from PL spectra were observed at 385, 405 and 440 nm for C-1, C-2 and C-3 respectively. Fluorescence lifetime (tau) of the fluorophores was found to be 035 and 1.55 ns at the excitation wavelength of 406 nm for C-1 and C-2 respectively, and tau value for C-3 was found to be 0.29 ns at the excitation wavelength of 468 nm. We noticed that the calculated values of HOMO energy levels were increased from 5.96 (C-1) to 6.08 (C-3) eV, which confirms that C-3 derivative is more electrons donating in nature. The calculated electrochemical band gaps were 2.95, 2.82 and 3.02 eV for C-1, C-2 and C-3 respectively. These blue fluorescent emitter derivatives can be used as an electron transport and electroluminescent material to design the blue fluorescent organic light emitting diode (OLED) applications. (C) 2015 Elsevier B.V: All rights reserved.
Resumo:
Diffuse optical tomography (DOT) using near-infrared light is a promising tool for non-invasive imaging of deep tissue. This technique is capable of quantitative reconstruction of absorption (mu(a)) and scattering coefficient (mu(s)) inhomogeneities in the tissue. The rationale for reconstructing the optical property map is that the absorption coefficient variation provides diagnostic information about metabolic and disease states of the tissue. The aim of DOT is to reconstruct the internal tissue cross section with good spatial resolution and contrast from noisy measurements non-invasively. We develop a region-of-interest scanning system based on DOT principles. Modulated light is injected into the phantom/tissue through one of the four light emitting diode sources. The light traversing through the tissue gets partially absorbed and scattered multiple times. The intensity and phase of the exiting light are measured using a set of photodetectors. The light transport through a tissue is diffusive in nature and is modeled using radiative transfer equation. However, a simplified model based on diffusion equation (DE) can be used if the system satisfies following conditions: (a) the optical parameter of the inhomogeneity is close to the optical property of the background, and (b) mu(s) of the medium is much greater than mu(a) (mu(s) >> mu(a)). The light transport through a highly scattering tissue satisfies both of these conditions. A discrete version of DE based on finite element method is used for solving the inverse problem. The depth of probing light inside the tissue depends on the wavelength of light, absorption, and scattering coefficients of the medium and the separation between the source and detector locations. Extensive simulation studies have been carried out and the results are validated using two sets of experimental measurements. The utility of the system can be further improved by using multiple wavelength light sources. In such a scheme, the spectroscopic variation of absorption coefficient in the tissue can be used to arrive at the oxygenation changes in the tissue. (C) 2016 AIP Publishing LLC.
Resumo:
White-light emitting Dy3+ doped layered BiOCl phosphors were synthesized by the solid state route and their structure was confirmed by the Rietveld refinement method. On substitution of Dy3+ ion to Bi3+-site in BiOCl, the photoluminescence spectra exhibit blue (F-4(9/2) -> H-6(15/2)), yellow (F-4(9/2) -> H-6(13/2)) and red (F-4(9/2) -> H-6(11/2)) emissions which function together to generate white light. It was found that the emission intensity increases up to 9 mol% of Dy3+ and then quenched due to dipole-dipole interaction. Judd-Ofelt theory and radiative properties suggest that the present phosphors have a long lifetime, high quantum efficiency, excellent color purity and better stimulated emission cross-section compared to reported Dy3+ doped compounds. The obtained color chromaticity results are close to the National Television System Committee standard and clearly establish the bright prospects of these phosphors in white luminescence. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
White-light emitting Dy3+ doped layered BiOCl phosphors were synthesized by the solid state route and their structure was confirmed by the Rietveld refinement method. On substitution of Dy3+ ion to Bi3+-site in BiOCl, the photoluminescence spectra exhibit blue (F-4(9/2) -> H-6(15/2)), yellow (F-4(9/2) -> H-6(13/2)) and red (F-4(9/2) -> H-6(11/2)) emissions which function together to generate white light. It was found that the emission intensity increases up to 9 mol% of Dy3+ and then quenched due to dipole-dipole interaction. Judd-Ofelt theory and radiative properties suggest that the present phosphors have a long lifetime, high quantum efficiency, excellent color purity and better stimulated emission cross-section compared to reported Dy3+ doped compounds. The obtained color chromaticity results are close to the National Television System Committee standard and clearly establish the bright prospects of these phosphors in white luminescence. (C) 2015 Elsevier Ltd. All rights reserved.