Ultasonic spray pyrolysis (SP) has been investigated for the production of the barium strontium titanate (BST) powders from the polymeric precursors. The processing parameters, such as flux of aerosol and temperature profile inside the furnace, were optimized to obtain single phase BST. The powders were characterized by the methods of X-ray diffraction analysis, SEM, EDS and TEM. The obtained powders were submicronic, consisting of spherical, polycrystalline particles, with internal nanocrystalline structure. Crystallite size of 10 nut, calculated using Rietveld refinement, is in a good agreement with results of HRTEM. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), with x ranging from 0 to 0.75 was grown on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution and spin-coating method. The dielectric constant of highly doped bismuth titanate was equal to 148 while dielectric losses remained low (tan delta = 0.0018), and the films showed well-saturated polarization-electric field curves (2P(r) = 40.6 muC/cm(2) and V-c = 0.99 V). The leakage current densities improve for the lanthanum-doped system. For five-layered BLT films with x = 0.75, a charge storage density of 35 fC/mum(2) and a thickness of 320 nm were found. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Vanadium modified barium zirconium titanate ceramics Ba(Zr(0.10)Ti(0.90))O(3):2V (BZT:2V) were prepared from the mixed oxide method. According to X-ray diffraction analysis, addition of vanadium leads to ceramics free of secondary phases. Electrical characteristics reveal a dielectric permittivity at around 15,000 with low dielectric loss with a remnant polarization (P(r))of 8 mu C/cm(2) at 2 kV/cm. From the obtained results, we assume that vanadium substitution in the BZT lattice affects dielectric characteristics due to the electron-relaxation-mode in which carriers (polarons, protons, and so on) are coupled with existing dielectric modes. (C) 2009 Published by Elsevier B.V.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Um método de correção de interferência espectral e de transporte é proposto, e foi aplicado para minimizar interferências por moléculas de PO produzidas em chama ar-acetileno e de transporte causada pela variação da concentração de ácido fosfórico. Átomos de Pb e moléculas de PO absorvem a 217,0005 nm, então Atotal217,0005 nm = A Pb217,0005 nm + A PO217,0005 nm. Monitorando o comprimento de onda alternativo de PO em 217,0458 nm, é possível calcular a contribuição relativa de PO na absorbância total a 217,0005 nm: A Pb217,0005 nm = Atotal217,0005 nm - A PO217,0005 nm = Atotal217,0005 nm - k (A PO217,0458 nm). O fator de correção k é a razão entre os coeficientes angulares de duas curvas analíticas para P obtidas a 217,0005 e 217,0458 nm (k = b217,0005 nm/b217,0458 nm). Fixando-se a taxa de aspiração da amostra em 5,0 ml min-1, e integrando-se a absorbância no comprimento de onda a 3 pixels, curvas analíticas para Pb (0,1 - 1,0 mg L-1) foram obtidas com coeficientes de correlação típicos > 0,9990. As correlações lineares entre absorbância e concentração de P nos comprimentos de onda 217,0005 e 217,0458 foram > 0,998. O limite de detecção de Pb foi 10 µg L-1. O método de correção proposto forneceu desvios padrão relativos (n=12) de 2,0 a 6,0%, ligeiramente menores que os obtidos sem correção (1,4-4,3%). As recuperações de Pb adicionado às amostras de ácido fosfórico variaram de 97,5 a 100% (com correção pelo método proposto) e de 105 a 230% (sem correção).
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Crystalline lead-pyrophosphate precursor was prepared in aqueous solution from lead nitrate and phosphoric acid and characterized by X-ray diffraction, thermogravimetry and Raman scattering. This crystalline lead-phosphate was then used to prepare glass samples in the binary system Pb(2)P(2)O(7)-WO(3). Dependence of WO(3) content on thermal, structural and optical properties were investigated by thermal analysis (DSC), Raman spectroscopy, UV-visible and near-infrared absorption and M-Line technique to access refractive index values. Incorporation of WO(3) in the lead-pyrophosphate matrix enhances the glass transition temperature and thermal stability against devitrification, favors formation of P-O-W bonds and WO(6) clusters. In addition, optical properties are strongly modified with a redshift of the optical bandgap with WO(3) incorporation as well as an increase of the refractive index from 1.89 to 2.05 in the visible. (C) 2011 Elsevier B.V. All rights reserved.