Resumo:
La0.15Sr0.85Ga0.3Fe0.7O3-delta (LSGFO) and La0.15Sr0.85Co0.3Fe0.7O3-delta (LSCFO) mixed oxygen-ion and electron conducting oxides were synthesized by using a combined EDTA and citrate complexing method, and the corresponding dense membranes were fabricated. The properties of the oxide powders and membranes were characterized with combined SEM, XRD, H-2-TPR, O-2-TPD techniques, mechanical strength and oxygen permeation measurement. The results showed that LSGFO had much higher thermochemical stability than LSCFO due to the higher valence stability of Ga3+. After the temperature-programmed reduction by 5% H-2 in Ar from 20 degreesC to 1020 degreesC, the basic perovskite structure of LSGFO was successfully preserved. LSGFO also favors the oxygen vacancy formation better than LSCFO. Oxygen permeation measurement demonstrated that LSGFO had higher oxygen permeation flux than LSCFO, but they had similar activation energy for oxygen transportation, with a value of 110 and 117 kJ . mol(-1), respectively The difference in oxygen permeation fluxes was correlated with the difference in oxygen vacancy concentrations for the two materials.
Resumo:
A mixed-conducting perovskite-type Ba0.5Sr0.5Co0.8Fe0.2O3-delta (BSCFO) ceramic membrane reactor with high oxygen permeability was applied for the activation of methane. The membrane reactor has intrinsic catalytic activities for methane conversion to ethane and ethylene. C-2 selectivity up to 40-70% was achieved, albeit that conversion rate were low, typically 0.5-3.5% at 800-900 degreesC with a 50% helium diluted methane inlet stream at a flow rate of 34 ml/min. Large amount of unreacted molecular oxygen was detected in the eluted gas and the oxygen permeation flux improved only slightly compared with that under non-reactive air/He experiments. The partial oxidation of methane to syngas in a BSCFO membrane reactor was also performed by packing LiLaNiO/gamma -Al2O3 with 10% Ni loading as the catalyst. At the initial stage, oxygen permeation flux, methane conversion and CO selectivity were closely related with the state of the catalyst. Less than 21 h was needed for the oxygen permeation flux to reach its steady state. 98.5% CH4 conversion, 93.0% CO selectivity and 10.45 ml/cm(2) min oxygen permeation flux were achieved under steady state at 850 degreesC. Methane conversion and oxygen permeation flux increased with increasing temperature, No fracture of the membrane reactor was observed during syngas production. However, H-2-TPR investigation demonstrated that the BSCFO was unstable under reducing atmosphere, yet the material was found to have excellent phase reversibility. A membrane reactor made from BSCFO was successfully operated for the POM reaction at 875 degreesC for more than 500h without failure, with a stable oxygen permeation flux of about 11.5 ml/cm(2) min. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
A novel zirconium-based membrane material of BaCo0.4Fe0.4Zr0.2O3-6 with cubic perovskite structure was synthesized for the first time through a method of citric and EDTA acid combined complexes. The structural stability was characterized by XRD, O-2-TPD and H-2-TPR techniques respectively. The high oxygen permeation flux of 0.873 mL/cm(2) min at 950 degreesC was obtained under He/Air gradient. Meanwhile, the single activation energy for oxygen permeation and the long-term steady operation of 200 h at 800 degreesC were achieved.
Resumo:
We report the experimental results of an unstable ring resonator with 90-deg beam rotation for a kilowatt class chemical oxygen iodine laser (COIL). The distributions of near-field phase and far-field intensity were measured. A beam quality of 1.6 was achieved when the COIL average output power was approximately 5 kW. (C) 1999 Optical Society of America.
Resumo:
Oxygen spillover and back spillover on Pt/TiO2 catalysts have been studied by a potential dynamic sweep method. The characteristics of I-V profiles of Pt/TiO2 electrodes in the three potential sweep regions are different from those of Pt and TiO2 electrodes. The catalytic role of Pt/TiO2 in oxygen spillover and back spillover is identified. It decreases, and the electrochemical oxygen adsorption (or desorption) increases with elevating temperature of hydrogen post-treatment of Pt/TiO2; to a certain extent (hydrogen post-treatment of Pt/TiO2 at 700 degrees C), the control step of oxygen electrode process (anodic oxidation or cathodic reduction) changes from oxygen diffusion to electrochemical oxygen adsorption or desorption, respectively. Increasing the amount of Pt supported on TiO2 enhances the processes of oxygen spillover and back spillover. (C) 1999 Elsevier Science B.V. All rights reserved.
Kinetic Study of the formation of oxygen vacancy on lanthanum manganite electrodes 锰酸镧电极上氧空位形成动力学的研究
Resumo:
The coadsorption of NO and O-2 on Ag(110) surface has been studied by X-ray photoelectron spectroscopy (XPS), ultraviolet photoelectron spectroscopy (UPS) and in situ Raman spectroscopy. The existence of oxygen enhances the adsorption of NO by forming the NOx species, that is, NO2 and NO3, and the NO in turn as a promotor facilitates the cleavage of the dioxygen bond, forming the surface atomic oxygen species having the same spectral characteristics as those produced using oxygen at high pressure. The oxygen species generated by the interaction is composed of two parts. One is produced directly by the decomposition of surface NO-O-2 complex at ca 625 K, which raised an O 1s feature at 530.5 eV and is absent at ca 800 K, while the another with an O 1s binding energy of 529.2 eV emerges at higher temperatures and shows similar properties as the reported gamma-state oxygen which bound tightly on restructured silver surface. The exposure to NO and O-2 causes noticeable changes in the morphology of the Ag(110) surface and the flat terraces superseded by small (ca 0.1 mu m) pits, and particles with typical diameters of a few micrometres were formed at elevated temperatures. (C) 1999 Elsevier Science B.V. All rights reserved.
Resumo:
Oxygen adsorption and desorption on a Pd(100) surface with a mesoscopic defect were studied by photoemission electron microscopy (PEEM). The defect surface, with an area of approximately 200 x 60 mu m(2), behaved differently from the perfect Pd(100) surface towards the adsorption of oxygen. When saturated, both surface oxygen and subsurface oxygen coexisted on the defect surface, whereas only surface oxygen was present on the Pd(100) surface. Upon heating, subsurface oxygen diffused back to the surface and desorbed with surface oxygen at the same time. The difference in oxygen adsorption ability between the defect surface and the perfect Pd(100) surface can be attributed to different structures of these two surfaces. (C) 1999 Elsevier Science B.V. All rights reserved.