Nowadays environmental pollution can be identified as a major problem in developed and developing countries. This is the result of several factors, such as inappropriate use of natural resources, inficiente legislation and not ecological awareness. Moreover, many other procedures as incorrect use of chemicals still contributed to the worsening of the problem. In this work, we develop a working with the environmental ideals, aiming to contribute to the decomposition of organic material through decomposition of rhodamine in TiO2 thin films on a silicon substrate. The degradation performance was monitored with the aid of techniques such as atomic force microscopy, transmission electron microscopy, field emission gun scanning electron microscopy, Fourier transform spectroscopy, thermal and photocatalytic analyses
Resumo:
The objective of the present work was to evaluate surface of experimental alloy Ti-7.5Mo after hydrothermal treatment. Ingots were obtained in arc melting furnace under an argon atmosphere and then homogenized under vacuum at 1100ºC for 86.4 ks to eliminate chemical segregation and after cold worked discs were cutting and grinding. For surface treatment, samples were immersed in a container with NaOH aqueous solution 5M, autoclaved, washed with distilled water. Followed, samples were heat treated and they were soaking in 5xSBF to form an apatite layer on the surface. Surfaces were investigated by, scanning electron microscopy, X-Rays powder diffraction, atomic force microscopy and contact angle, in order to evaluate the wettability of the alloy surface. The results were compared with our previous studies using the group of chemical surface treatments and results shows better condition is 120 minutes in the autoclave
Resumo:
In this work, plasma immersion ion implantation (PIII) treatments of carbon fibers (CFs) were performed in order to induce modifications of chemical and physical properties of the CF surface aimed to improve the performance of thermoplastic composite. The samples to be treated were immersed in nitrogen or air glow discharge plasma and pulsed at −3.0 kV for 2.0, 5.0, 10.0, and 15.0 min. After PIII processing, the specimens were characterized by atomic force microscopy (AFM), scanning electron microscopy, Raman spectroscopy, and X-ray photoelectron spectroscopy (XPS). After CFs treatments, the CF/Polypropylene (PP) composites were produced by hot pressing method. Surface morphology of as-received CFs exhibited some scratches aligned along the fibers due to the fiber manufacturing process. After both treatments, these features became deeper, and also, a number of small particles nonuniformly distributed on the fiber surface can be observed. These particles are product of CF surface sputtering during the PIII treatment, which removes the epoxy layer that covers as-received samples. AFM analyses of CF samples treated with nitrogen depicted a large increase of the surface roughness (Rrms value approximately six times higher than that of the untreated sample). The increase of the roughness was also observed for samples treated by air PIII. Raman spectra of all samples presented the characteristic D- and G-bands at approximately 1355 and 1582 cm−1, respectively. Analysis of the surface chemical composition provided by the XPS showed that nitrogen and oxygen were incorporated onto the surface. The polar radicals formed on the surface lead to increasing of the CF surface energy. Both the modification of surface roughness and the surface oxidation contributed for the enhancement of CF adhesion to the polymeric matrix. These features were confirmed ... (Complete abstract click electronic access below)
Resumo:
Pós-graduação em Engenharia Mecânica - FEG
Resumo:
The influence of both thermal treatment and laser irradiation on the structural and optical properties of films in the Sb 2 O 3 –Sb 2 S 3 system was investigated. The films were prepared by RF-sputtering using glass compositions as raw materials. Irreversible photodarkening effect was observed after exposure the films to a 458nm solid state laser. It is shown, for the first time, the use of holographic technique to measure “in situ”, simultaneously and independently, the phase and amplitude modulations in glassy films. The films were also photo-crystallized and analysed “in situ” using a laser coupled to a micro-Raman equipment. Results showed that Sb 2 S 3 crystalline phase was obtained after irradiation. The effect of thermal annealing on the structure of the films was carried out. Different from the result obtained by irradiation, thermal annealing induces the crystallization of the Sb 2 O 3 phase. Photo and thermal induced effects on films were studied using UV–Vis and Raman spectroscopy, atomic force microscopy (AFM), thermal analysis (DSC), X-ray diffraction, scanning electron microscopy (MEV) and energy-dispersive X-ray spectroscopy (EDX).
Resumo:
Pós-graduação em Odontologia Restauradora - ICT
Resumo:
Pós-graduação em Química - IQ
Resumo:
To evaluate changes in microhardness, roughness and surface morphology of dental enamel and composite resin after different tooth bleaching techniques. Material and Methods: Dental fragments from bovine incisors with composite resin restorations were submitted to different bleaching protocols: G1 – daily 8 hours application of a 10% carbamide peroxide (CP) gel during 21 days; G2: 3 applications of 15 minutes of a 38% hydrogen peroxide (H2O2) gel; G3: 38% H2O2 gel associated to irradiation with LED (470nm) during 6 minutes. The Knoop micro hardness of enamel and composite resin were evaluated at 1, 7, 14 and 21 days for G1, and after 1, 2 and 3 sessions for G2 and G3. The roughness and superficial morphology (atomic force microscopy) were evaluated before and at the end of the bleaching treatment. The data were analyzed by Mann-Whitney and Wilcoxon tests (=5%). Results: Significant reduction on enamel hardness was observed after 2 and 3 sessions for G2 and G3. For composite, the reduction occurred after 21 days for G1, and after 3 sessions for G2 and G3 (p<0.05). Significant reduction on roughness and superficial morphology were observed only for enamel of G1 group (p<0.05). Conclusion: The 10% CP gel promoted only superficial alterations on dental enamel, while the 38% H2O2 gel promoted mineral reduction of this dental tissue. All the bleaching protocols promoted reduction on hardness of composite resin.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Pós-graduação em Engenharia Mecânica - FEG
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Engenharia e Ciência de Alimentos - IBILCE
Resumo:
Purpose: To analyze whether immersion in sodium fluoride (NaF) solutions and/or common acidic beverages (test solutions) would affect the surface roughness or topography of lithium disilicate ceramic. Methods: 220 ceramic discs were divided into four groups, each of which was subdivided into five subgroups (n = 11). Control group discs were immersed in one of four test beverages for 4 hours daily or in artificial saliva for 21 days. Discs in the experimental groups were continuously immersed in 0.05% NaF, 0.2% NaF, or 1.23% acidulated phosphate fluoride (APF) gel for 12, 73, and 48 hours, respectively, followed by immersion in one of the four test beverages or artificial saliva. Vickers microhardness, surface roughness, scanning electron microscopy (SEM) associated with energy dispersive spectroscopy, and atomic force microscopy (AFM) assessments were made. Data were analyzed by nested analysis of variance (ANOVA) and Tukey's test (alpha = 0.05). Results: Immersion in the test solutions diminished the microhardness and increased the surface roughness of the discs. The test beverages promoted a significant reduction in the Vickers microhardness in the 0.05% and 0.2% NaF groups. The highest surface roughness results were observed in the 0.2% NaF and 1.23% APF groups, with similar findings by SEM and AFM. Acidic beverages affected the surface topography of lithium disilicate ceramic. Fluoride treatments may render the ceramic surface more susceptible to the chelating effect of acidic solutions.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)