830 resultados para Vanadium alloys
Resumo:
The thermal behavior of the Cu-10 mass%Al and Cu-10 mass% Al-4 mass%Ag alloys was studied using classical differential thermal analysis (DTA), optical microscopy (OM) and X-ray diffractometry (XRD). The DTA curves were obtained for annealed and quenched samples. The results indicated that the presence of silver introduces new thermal events, associated to the formation of a silver-rich phase, to the shift of the equilibrium concentration to higher A1 contents and to the decomposition of the silver-rich phase in the same temperature range of the beta(1) phase decomposition.
Resumo:
The effect of the addition of Cr and Nb on the microstructure and the electrochemical corrosion of the weldable, high-strength and stress corrosion cracking (SCC) resistant Al-5%Zn-1.67%Mg-0.23%Cu alloy (H) has been studied. Combined additions of the alloying elements, J (with Nb), L (with Cr) and O (with Cr and Nb) and different heat treatments, ST (cold-rolled), A (annealed), F (quenched), B (quenched and aged) and C (quenched in two steps and aged), to obtain different microstructures and hardness have been performed. To correlate the electrochemical corrosion with the microstructure of the specimens, corrosion potential (E(cor)) measurements in different chloride solutions were performed and optical microscopy, SEM, TEM and EDX were applied. In chloride solutions containing dissolved O-2 or H2O2, the present alloys were polarized up to the pitting attack. It was shown that the E(cor) measurements were very sensitive to the alloy composition and heat treatment, increasing in the order H < J < L < O < Al (for a given heat treatment) and F < A approximate to ST < B < C (for a given alloy). The MgZn2 precipitates of the annealed (A) and cold-rolled (ST) specimens were dissolved in chloride solutions containing oxidizing agents and pitting attack was shown to develop in the cavities where the precipitates were present. In the specimens B and C, the compositions of the precipitate free zones was found to be equal to that of the matrix solid solution and preferential intergranular attack was not evident, this being in agreement with their SCC resistance. The addition of Cr and Nb increased the pitting corrosion resistance. The effects of Cr and Nb were additive, that of Cr being predominant, either, in the E(cor) shift or in the increase in the pitting corrosion resistance.
Resumo:
Statement of problem. The success of metal-ceramic restorations is influenced by the compatibility between base metal alloys and porcelains. Although porcelain manufacturers recommend their own metal systems as the most compatible for fabricating metal-ceramic prostheses, a number of alloys have been used.Purpose. This study evaluated the shear bond strength between a porcelain system and 4 alternative alloys.Material and methods. Two Ni-Cr alloys: 4 ALL and Wiron 99, and 2 Co-Cr alloys: IPS d.SIGN 20 and Argeloy NP were selected for this study. The porcelain (IPS d.Sign porcelain system) portion of the cylindrical inetal-ceramic specimens was 4 mm thick and 4 mm high; the metal portion was machined to 4 x 4 mm, with a base that was 5 nun thick and 1 mm high. Forty-four specimens were prepared (n=11). Ten specimens from each group were subjected to a shear load oil a universal testing machine using a 1 min/min crosshead speed. One specimen from each group was observed with a scanning electron microscope. Stress at failure (MPa) was determined. The data were analyzed with a 1-way analysis of variance (alpha=.05).Results. The groups, all including IPS d.Sign porcelain, presented the following mean bond strengths (+/-SD) in MPa: 4 ALL, 54.0 +/- 20.0; Wiron, 63.0 +/- 13.5; IPS d.SIGN 20, 71.7 +/- 19.2; Argeloy NP, 55.2 +/- 13.5. No significant differences were found among the shear bond strength values for the metal-ceramic specimens tested.Conclusion. None of the base metal alloys studied demonstrated superior bond strength to the porcelain tested.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Supramolecular structures of polyaniline (PANI) and vanadium oxide (V2O5) have been assembled via the electrostatic layer-by-layer (LBL) technique. The films were characterized by vibrational analyses which indicated that the interactions between the two components lead to different properties in the films when compared to sol-gel films. of the neat compounds. In particular, using surface enhanced Raman scattering we were able to probe LBL film properties that depend on which material comprises the topmost layer.
Resumo:
The effect of consecutive cyclic polarization in de-aerated 0.5 M NaOH solutions on the surface microstructure of mechanically polished Cu-Al-Ag alloys of different compositions and heat treatments has been studied using optical microscopy, SEM and EDS. The current peaks of the cyclic polarization curves do not depend on the alloy composition in the composition range studied. The repetitive potential scans between H2 and O2 evolution in alkaline media lead to preferential dissolution of aluminium, the roughness and phase composition of the surface of the alloys changing significantly. The quasistationary I-E curves of the different Cu-Al-Ag alloys studied consist in the superposition of the quasistationary I-E curves of high-purity Cu and Ag, the EDS microanalysis showing that aluminium is not present on the surface of the alloy in these conditions.
Resumo:
The kinetics of eutectoid decomposition beta(1)' --> gamma(2) + (alpha + gamma(2)) in Cu-12.86 wt% Al and Cu-12.84 wt% Al-1.98 wt% Ag alloys was studied by hardness measurements, using the Johnson-Mehl-Avrami equation. The results indicate that the presence of silver seems to influence the nucleation rate and the activation energy of the reaction.
Resumo:
This work describes an analytical procedure for vanadium determination in human hair slurries by electrothermal AAS using longitudinal heating (LHGA) and transversal heating (THGA) graphite furnace atomizers. The samples were powdered using cryogenic grinding and the hair slurries containing 0.2% (m/v) were prepared in three different media for determination of vanadium: 0.14 mol L-1 HNO3, 0.1% (v/v) Triton X-100 and 0.1% (v/v) water soluble tertiary amines (CFA-C, pH 8). The limits of detection (LOD), limits of quantification (LOQ), and characteristic masses obtained were 0.28, 0.95 mu g L-1 and 35 pg (LHGA) and 0.34, 1.13 mu g L-1 and 78 pg (THGA), respectively. The accuracy of the analytical results obtained by the proposed procedure in both equipments was confirmed by a paired t-test at the 95% confidence level and compared with a conventional procedure based on acid digestion. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
In this work, zirconium titanate doped with 0. 1, 0.2, and 0.4 mole% of tin, chromium and vanadium was synthesized by the polymeric precursors method and characterized by thermal analysis (TG/DTA), X-ray diffraction (XRD), nitrogen adsorption and scanning electronic microscopy (SEM). The powder presented two mass losses attributed to the exit of water and to the pyrolysis of the organic material. The surface area reduction observed from 500 degrees C indicates the beginning of the sintering process. All the dopants led to changes in the lattice parameters and to the decrease of both crystallite size and particle size. (c) 2005 Elsevier B.V. All rights reserved.