976 resultados para Conductivity, electrical
Resumo:
Bulk Ge7Se93-xSbx (21 <= x <= 32) glasses are prepared by melt quenching method and electrical switching studies have been undertaken on these samples to elucidate the type of switching and the composition and thickness dependence of switching voltages. On the basis of the compressibility and atomic radii, it has been previously observed that Se-based glasses exhibit memory switching behavior. However, the present results indicate that Ge7Se93-xSbx glasses exhibit threshold type electrical switching with high switching voltages. Further, these samples are found to show fluctuations in the current-voltage (I-V) characteristics. The observed threshold behavior of Ge7Se93-xSbx glasses has been understood on the basis of larger atomic radii and lesser compressibilities of Sb and Ge. Further. the high switching voltages and fluctuations in the I-V characteristics of Ge-Se-Sb samples can be attributed to the high resistance of the samples and the difference in thermal conductivities of different structural units constituting the local structure of these glasses. The switching voltages of Ge7Se93-xSbx glasses have been found to decrease with the increase in the Sb concentration. The observed composition dependence of switching voltages has been understood on the basis of higher metallicity of the Sb additive and also in the light of the Chemically Ordered Network (CON) model. Further, the thickness dependence of switching voltages has been studied to reassert the mechanism of switching.
Resumo:
Two new donor-acceptor type liquid crystalline semiconductors based on benzothiazole have been synthesized. Their structural, photophysical and electronic properties were investigated using X-ray diffraction, atomic force microscopy, cyclic voltammetry, UV-Vis, photoluminescence, and Raman spectroscopy. The liquid crystalline behaviour of the molecules was thoroughly examined by differential scanning calorimetry (DSC) and optical polarizing microscope. The DSC and thermogravimetric analysis (TGA) show that these materials posses excellent thermal stability and have decomposition temperatures in excess of 300 degrees C. Beyond 160 degrees C both molecules show a smectic A liquid crystalline phase that exists till about 240 degrees C. Field-effect transistors were fabricated by vacuum evaporating the semiconductor layer using standard bottom gate/top contact geometry. The devices exhibit p-channel behaviour with hole mobilities of 10(-2) cm(2)/Vs. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
A reduced 3D continuum model of dynamic piezoelectricity in a thin-film surface-bonded to the substrate/host is presented in this article. While employing large area flexible thin piezoelectric films for novel applications in device/diagnostics, the feasibility of the proposed model in sensing the surface and/or sub-surface defects is demonstrated through simulations - which involve metallic beams with cracks and composite beam with delaminations of various sizes. We have introduced a set of electrical measures to capture the severity of the damage in the existing structures. Characteristics of these electrical measures in terms of the potential difference and its spatial gradients are illustrated in the time domain. Sensitivity studies of the proposed measures in terms of the defected areas and their region of occurence relative to the sensing film are reported. The simulations' results for electrical measures for damaged hosts/substrates are compared with those due to undamaged hosts/substrates, which show monotonicity with high degree of sensitivity to variations in the damage parameters.
Resumo:
A novel sintering additive based on LiNO3 was used to overcome the drawbacks of poor sinterability and low grain boundary conductivity in BaZr0.8Y0.2O3-δ (BZY20) protonic conductors. The Li-additive totally evaporated during the sintering process at 1600°C for 6 h, which led to highly dense BZY20 pellets (96.5% of the theoretical value). The proton conductivity values of BZY20 with Li sintering-aid were significantly larger than the values reported for BZY sintered with other metal oxides, due to the fast proton transport in the "clean" grain boundaries and grain interior. The total conductivity of BZY20-Li in wet Ar was 4.45 × 10-3 S cm-1 at 600°C. Based on the improved sinterability, anode-supported fuel cells with 25 μm-thick BZY20-Li electrolyte membranes were fabricated by a co-firing technique. The peak power density obtained at 700°C for a BZY-Ni/BZY20-Li/La0.6Sr0.4Co0.2Fe 0.8O3-δ (LSCF)-BZY cell was 53 mW cm-2, which is significantly larger than the values reported for fuel cells using electrolytes made of BZY sintered with the addition of ZnO and CuO, confirming the advantage of using Li as a sintering aid.
Resumo:
In3+ was used as dopant for BaZrO3 proton conductor and 30 at%-doped BaZrO3 samples (BaZr0.7In 0.3O3-δ, BZI) were prepared as electrolyte materials for proton-conducting solid oxide fuel cells (SOFCs). The BZI material showed a much improved sinteractivity compared with the conventional Y-doped BaZrO 3. The BZI pellets reached almost full density after sintering at 1600 °C for 10 h, whereas the Y-doped BaZrO3 samples still remained porous under the same sintering conditions. The conductivity measurements indicated that BZI pellets showed smaller bulk but improved grain boundary proton conductivity, when compared with Y-doped BaZrO3 samples. A total proton conductivity of 1.7 × 10-3 S cm -1 was obtained for the BZI sample at 700 °C in wet 10% H 2 atmosphere. The BZI electrolyte material also showed adequate chemical stability against CO2 and H2O, which is promising for application in fuel cells.
Resumo:
Because of its high electrical conductivity and good diffusion barrier properties ruthenium dioxide (RuO2) is a good electrode material for use with ferroelectric lead zirconate-titanate (PZT) solid solutions. Under certain conditions, RuO2 can react with PZT to form lead ruthenate (Pb2Ru2O6.5) during processing at elevated temperatures resulting in lead depletion from PZT. The standard Gibbs energies of formation of RuO2 and Pb2Ru2O6.5 and activities of components of the PZT solid solution have been determined recently. Using this data along with older thermodynamic information on PbZrO3 and PbTiO3, the stability domain of Pb2Ru2O6.5 is computed as a function of PZT composition, temperature and oxygen partial pressure in the gas phase. The results show PbZrO3-rich compositions are more prone to react with RuO2 at all temperatures. Increasing temperature and decreasing oxygen partial pressure suppress the reaction. Graphically displayed are the reaction zones as a function of oxygen partial pressure and PZT composition at temperatures 973, 1173 and 1373 K.
Resumo:
Electrical Switching Studies on bulk Ge10Se90-xTlx ( 15 <= x <= 34) glasses have been undertaken to examine the type of switching, composition and thickness dependence of switching voltages. Unlike Ge-Se-Tl thin films which exhibit memory switching, the bulk Ge10Se90-xTlx glasses are found to exhibit threshold type switching with fluctuations seen in their current-voltage (I-V) characteristics. Further, it is observed that the switching voltages (V-T) of Ge10Se90-xTlx glasses decrease with the increase in the Tl concentration. An effort has been made to understand the observed composition dependence on the basis of nature of bonding of Tl atoms and a decrease in the chemical disorder with composition. In addition. the network connectivity and metallicity factors also contribute for the observed decrease in the switching voltages of Ge10Se90-xTlx glasses with Tl addition. It is also interesting to note that the composition dependence of switching voltages of Ge10Se90-xTlx glasses exhibit a small Cusp around the composition x = 22. which is understood on the basis of a thermally reversing window in this system in the composition range 22 <= x <= 30. The thickness dependence of switching voltages has been found to provide an insight about the type of switching mechanism involved in these samples. (C) 2009 Elsevier B.V. All rights reserved
Resumo:
There exist many investigations of ionic transport in a variety of glasses. These studies exhibit strong correlation between ionic conductivity and activation energy: Typically, it is found that higher conductivity is associated with lower activation energies and vice versa. Although there are explanations for this at a phenomenological level, there is no consistent physical picture to explain the correlation between conductivity and activation energy. We have carried out molecular dynamics simulation as a function of the size of the impurity atom or diffusant (both neutral and charged) in a host amorphous matrix. We find that there is a maximum in self-diffusivity as a function of the size of the impurity atom suggesting that there is an appropriate size for which the diffusivity is maximum. The activation energy is found to be the lowest for this size of the impurity. A similar maximum has been previously found in other condensed phases, such as confined fluids and dense liquids, and has its origin in the levitation effect. The implications of this result for understanding ionic conductivity in glasses are discussed. Our results suggest that there is a relation between microscopic structure of the amorphous solid, diffusivity or conductivity, and activation energy. The nature of this relationship is discussed in terms of the levitation parameter showing that diffusivity is maximum when the size of the neck or doorway radius is comparable with the size of the diffusant. Our computational results here are in excellent agreement with independent experimental results of Nascimento et al. [Braz. J. Phys. 35, 626 (2005)] that structural features of the glass are important in determining the ionic conductivity.
Resumo:
Bulk Ge15Te85-xInx (1 <= x <= 11) series of glasses have been found to exhibit a threshold switching behaviour for an input current of 2 mA. An initial decrease is seen in the switching voltages (V-T) with the addition of indium, which is due to the higher metallicity of indium. An increase is seen in V-T above 3 at.% of indium, which proceeds until 8 at.%, with a change in slope (lower to higher) seen around 7 at.%. Beyond x = 8, a reversal in trend is exhibited in the variation of V-T, with a well-defined minimum around x = 9 at.%. Based on the composition dependence of V-T, it is proposed that Ge15Te85-xInx glasses exhibit an extended rigidity percolation threshold. The composition, x = 3, at which the V-T starts to increase and the composition, x = 7, at which a slope change is exhibited correspond to the onset and completion, respectively, of the extended stiffness transition. Thermal studies and photoconductivity e85-xInx glasses. In addition, the minimum seen in V-T at x = 9 is associated with the chemical threshold (CT) of this glassy system.
Resumo:
Bulk Ge15Te83Si2 glass has been found to exhibit memory-type switching for 1 mA current with a threshold electric field of 7.3 kV/cm. The electrical set and reset processes have been achieved with triangular and rectangular pulses, respectively, of 1 mA amplitude. In situ Raman scattering studies indicate that the degree of disorder in Ge15Te83Si2 glass is reduced from off to set state. The local structure of the sample under reset condition is similar to that in the off state. The Raman results are consistent with the switching results which indicate that the Ge15Te83Si2 glass can be set and reset easily. (C) 2007 American Institute of Physics.
Resumo:
The lead based ferroelectric PbZr0.53Ti0.47O3 (PZT), (Pb0.90La0.10)TiO3 (PLT10) and (Pb0.80La0.20)TiO3 (PLT20) thin films, prepared by pulsed laser ablation technique, were studied for their response to the 70 MeV oxygen ion irradiation. The dielectric analysis, capacitance-voltage (C- V) and DC leakage current measurements were performed before and after the irradiation to high-energy oxygen ions. The irradiation produced considerable changes in the dielectric, C-V, leakage characteristics and induced some amount of amorphization. The PZT films showed partial recrystallization after a thermal annealing at 400 degrees C for 10 min. The phase transition temperature [T-c] of PLT20 increased from 115 degrees C to 120 degrees C. The DC conductivity measurements showed a shift in the onset of non-linear conduction region. The current density decreased by two orders of magnitude after irradiation. After annealing the irradiated films at a temperature of 400 degrees C for 10 min, the films partially regained the dielectric and electrical properties. The results are discussed in terms of the irradiation-induced amorphization, the pinning of the ferroelectric domains by trapped charges and the thermal annealing of the defects generated during the irradiation. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
In1-xMnxSb films have been grown with different Mn doping concentrations (x = 0.0085, 0.018, 0.029 and 0.04) beyond the equilibrium 14 solubility limit by liquid phase epitaxy. We have studied temperature dependent resistivity, the Hall effect, magnetoresistance and magnetization for all compositions. Saturation in magnetization observed even at room temperature suggests the existence of ferromagnetic clusters in the film which has been verified by scanning electron microscopy studies. The anomalous Hall coefficient is found to be negative. Remnant field present on the surface of the clusters seems to affect the anomalous Hall effect at very low fields (below 350 Gauss). In the zero field resistivity, a variable-range hopping conduction mechanism dominates below 3.5 K for all samples above which activated behavior is predominant. The temperature dependence of the magnetization measurement shows a magnetic ordering below 10 K which is consistent with electrical measurements. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Investigations on the electrical switching behavior and thermal studies using Alternating Differential Scanning Calorimetry have been undertaken on bulk, melt-quenched Ge22Te78-,Is (3 <= x <= 10) chalcohalide glasses. All the glasses studied have been found to exhibit memory-type electrical switching. The threshold voltages of Ge22Te78-I-x(x) glasses have been found to increase with the addition of iodine and the composition dependence of threshold voltages of Ge22Te78-xIx glasses exhibits a cusp at 5 at.% of iodine. Also, the variation with composition of the glass transition temperature (Tg) of Ge22Te78-I-x(x) glasses, exhibits a broad hump around this composition. Based on the present results, the composition x = 5 has been identified as the inverse rigidity percolation threshold at which Ge22Te78-I-x(x) glassy system exhibits a change from a stressed rigid amorphous solid to a flexible polymeric glass. Further, a sharp minimum is seen in the composition dependence of non-reversing enthalpy (Delta H-nr) of Ge22Te78-I-x(x) glasses at x = 5, which is suggestive of a thermally reversing window at this composition. (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
The variation of resistivity in an amorphous As30Te70-xSix system of glasses with high pressure has been studied for pressures up to 8 GPa. It is found that the electrical resistivity and the conduction activation energy decrease continuously with increase in pressure, and samples become metallic in the pressure range 1.0-2.0 GPa. Temperature variation studies carried out at a pressure of 0.92 GPa show that the activation energies lie in the range 0.16-0.18eV. Studies on the composition/average co-ordination number (r) dependence of normalized electrical resistivity at different pressures indicate that rigidity percolation is extended, the onset of the intermediate phase is around (r) = 2.44, and completion at (r) = 2.56, respectively, while the chemical threshold is at (r) = 2.67. These results compare favorably with those obtained from electrical switching and differential scanning calorimetric studies.
Resumo:
Electrical switching and differential scanning calorimetric studies are undertaken on bulk As20Te80-xGax glasses, to elucidate the network topological thresholds. It is found that these glasses exhibit a single glass transition (T-g) and two crystallization reactions (T-cl & T-c2) upon heating. It is also found that there is only a marginal change in T-g with the addition of up to about 10% of Ga; around this composition an increase is seen in 7, which culminates in a local maximum around x = 15. The decrease exhibited in T, beyond this composition, leads to a local minimum at x = 17.5. Further, the As20Te80-xGax glasses are found to exhibit memory type electrical switching. The switching voltages (VT) increase with the increase in gallium content and a local maximum is seen in V-tau around x = 15. VT is found to decrease with x thereafter, exhibiting a local minimum around x = 17.5. The composition dependence of T-cl is found to be very similar to that of V-T of As20Te80-xGax glasses. Based on the present results, it is proposed that the composition x = 15 and x = 17.5 correspond to the rigidity percolation and chemical thresholds, respectively, of As20Te80-xGax glasses. (c) 2007 Elsevier B.V. All rights reserved.