Resumo:
Very intense visible green photoluminescence (PL) was observed at room temperature in structurally ordered-disordered BaZrO3 powders. Ab initio calculations, ultraviolet-visible absorption spectroscopy, electron paramagnetic resonance, and PL were performed. Theoretical and experimental results showed that local defects in the cubic structure caused by [ZrO5 center dot V-O(z)] complex clusters, where V-O(z) = V-O(x), V-O(center dot), and V-O(center dot center dot), play an important role in the formation of hole-electron pairs, giving rise to a charge gradient in the structure which is responsible for PL emission. (c) 2008 American Institute of Physics.
Resumo:
intense photoluminescence in the visible region was observed at room temperature in standard soda-lime-silica glass powder, mechanically milled in a high-energy attrition mill. The emission band maximum shows an interesting dependence on the exciting wavelength, suggesting the possibility to tune the PL emission. These findings indicate that the photoluminescence may be directly related to unsatisfied chemical bonds correlated with the high surface area. The Raman scattering and ultraviolet-visible optical reflectance measurements corroborate this assertion. Transmission electron microscopy measurements indicate that samples milled more than 10 h present the formation of nanocrystallites with about 10-20 nm. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
This study aimed to verify the prevalence of lip and perioral lesions in worker who were under sunshine on the beaches of Natal/RN and to investigate possible associations of these with sociodemographic, occupational and general health variables. For this, 362 individuals who had one of the urban beaches (Ponta Negra / Environment / Redinha) in the city of Natal/RN as a working environment in the study. We excluded people under 18 years old. Data collection was done through epidemiological analysis and extra-oral validated questionnaire with questions that characterize socioeconomic and demographic factors, occupational exposure and general health. The male subjects (72.6%) were the majority in the sample. The people who worked directly exposed to high peaks of ultraviolet radiation, as well as informal workers predominated. Considering the total sample of individuals, ephelides in the perioral region (33.7%) and labial region (24.0%), solar lentigo perioral (15.2%) and actinic cheilitis (13.8%) stood out as the most prevalent lesions. Indoor workers and those who had a habit occurrence of injuries by 19% and 21% respectively higher when compared to outdoor workers and people without habits. The variable use of cap / hat was associated with the presence of cold sores (Qui2 = 1,328, p = 0,058). On the threshold of significance, the type of work was also associated with lesions in lip occurrence (p = 0,042). Men showed a lower incidence of perioral lesions when compared to female workers (PR=0,716, p valor = 0,002). The present study showed high prevalence of lip and perioral lesions. The premalignant lesions were the most identified, both as in lip skin. It is important therefore to be encouraged to adopt protective measures against excessive sun exposure, fairly and consistently
Resumo:
Lip squamous cell carcinoma (SCC) may develop from a premalignant condition, actinic cheilitis (AC) in 95% of the cases. Both premalignant and neoplastic lip diseases are caused mainly by chronic exposure to the ultraviolet component of solar radiation, especially UVB. This exposure causes disruption of the cell cycle and damage to DNA repair systems, like mismatch repair, altering proteins repair as hMLH1 and hMSH2. This research aimed to investigate the immunohistochemical expression of hMLH1 and hMSH2 proteins in lower lip SCCs and ACs, providing additional information about carcinogenesis of the lower lip. The sample consisted 40 cases of ACs and 40 cases of lower lip SCCs. Histological sections of 3 μm were submitted to immunoperoxidase method, for immunohistochemical analysis of lesions were counted in 1000 cells (positive and negative), data were evaluated both in absolute numbers and percentage of immunostained cells, the latter by assigning scores. Associations of the variables and comparative analysis of biomarker expression were performed by Fisher s exact and Pearson s chi-square, "t" student, one-way ANOVA, Mann- Whitney e Kruskal-Wallis tests. The level of significance was 5%. It was found that, in lower lip SCC, the mean of the proteins was higher in female patients (hMLH1= 369,80 + 223,98; hMHS2 = 534,80 + 343,62), less than 50 years old (hMLH1 = 285,50 + 190,65; hMHS2 = 540,00 + 274,79) and classified as low-grade malignancy (hMLH1 = 264,59 + 179,21; hMHS2 = 519,32 + 302,58), in these data only to sex, for hMLH1 protein, was statistically significant (p=0.034). Comparing the different lesions, we observed that for both hMLH1 and hMSH2 protein, the average of positive epithelial cells decreased as the lesion was graded at later stages. The ACs classified without dysplasia or mild dysplasia had the highest average of immunostained cells (hMLH1 = 721.23 + 88.116; hMHS2 = 781.50 + 156.93). The ACs classified as moderate or severe dysplasia had intermediate values (hMLH1 = 532,86 + 197,72; hMHS2 = 611,14 + 172,48) and SSCs of the lower lip had the lowest averages (hMLH1 = 255,03 + 199,47; hMHS2 = 518,38 + 265,68). There was a statistically significant difference between groups (p<0.001). In conclusion, our data support the hypothesis that changes in immunoexpression of these proteins is related to the process of carcinogenesis of the lower lip
Resumo:
Polymer films, deposited from acetylene and argon plasma mixtures, were bombarded with 150 keV He+ ions, varying the fluence, Phi, from 10(18) to 10(21) ions/m(2). Molecular structure and optical gap of the samples were investigated by infrared and ultraviolet-visible spectroscopies, respectively. Two-point probe was employed to determine the electrical resistivity while hardness was measured by nanoindentation technique. It was verified modification of the molecular structure and composition of the films. There was loss of H and increment in the concentration of unsaturated carbon bonds with Phi. Optical gap and electrical resistivity decreased while hardness increased with Phi. Interpretation of these results is proposed in terms of chain crosslinking and unsaturation. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
This paper deals with the study of optical, structural and biocompatible properties of PEO-like plasma polymerized films resulting from RF excited diethylene glycol dimethyl ether (CH3O(CH2CH2O)(2)CH3 diglyme) glow discharges. The study was carried out using visible-ultraviolet and FTIR spectroscopies and contact angle measurements. FTIR spectra of plasma polymerized diglyme showed a stronger presence of ethylene glycol groups in film structure for lower RF power levels. The contact angle measurements for water revealed an increasing from 30degrees to 62,5degrees when the RF power was varied from 2 to 45 W, indicating the decreasing of the hydrophilic character of diglyme films with the increasing of RF power. This trend is in agreement with FTIR results. The data from visible-ultraviolet reflectance and transmittance spectra revealed alterations on optical properties of plasma polymerized diglyme films. The film's optical gap varied from 3.8 to 3 eV for RF power running from 5 to 45 W.
Resumo:
Benzene plasma polymer films were bombarded with Ar ions by plasma immersion ion implantation. The treatments were performed using argon pressure of 3 Pa and 70 W of applied power. The substrate holder was polarized with high voltage negative pulses (25 kV, 3 Hz). Exposure time to the immersion plasma, t, was varied from 0 to 9000 s. Optical gap and chemical composition of the samples were determined by ultraviolet-visible and Rutherford backscattering spectroscopies, respectively. Film wettability was investigated by the contact angle between a water drop and the film surface. Nanoindentation technique was employed in the hardness measurements. It was observed growth in carbon and oxygen concentrations while there was decrease in the concentration of H atoms with increasing t. Furthermore, film hardness and wettability increased and the optical gap decreased with t. Interpretation of these results is proposed in terms of the chain crosslinking and unsaturation. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Diamond-like carbon (DLC) films were grown from radiofrequency plasmas of acetylene-argon mixtures, at different excitation powers, P. The effects of this parameter on the plasma potential, electron density, electron temperature, and plasma activity were investigated using a Langmuir probe. The mean electron temperature increased from about 0.5 to about 7.0 eV while the mean electron density decreased from about 1.2x10(9) to about 0.2x10(9) cm(-3) as P was increased from 25 to 150 W. Both the plasma potential and the plasma activity were found to increase with increasing P. Through actinometric optical emission spectrometry, the relative concentrations of CH, [CH], and H, [H], in the discharge were mapped as a function of the applied power. A rise in [H] and a fall in [CH] with increasing P were observed and are discussed in relation to the plasma characteristics and the subimplantation model. The optical properties of the films were calculated from ultraviolet-visible spectroscopic data; the surface resistivity was measured by the two-point probe method. The optical gap, E(G), and the surface resistivity, rho(s), fall with increasing P. E(G) and rho(s) are in the ranges of about 2.0-1.3 eV and 10(14)-10(16) Omega/square, respectively. The plasma power also influences the film self-bias, V(b), via a linear dependence, and the effect of V(b) on ion bombardment during growth is addressed together with variation in the relative densities of sp(2) and sp(3) bonds in the films as determined by Raman spectroscopy.
Resumo:
In this work, it was used a plasma system composed of a cylindrical stainless steel reactor, a radio-frequency (13.56MHz) power source fixed at either 25 W or 70 W, a power source with a negative bias of 10kV and a 100Hz pulse. The system worked at an operational pressure of 80mTorr which consisted of varying concentrations of the monomer HMDSN and gaseous nitrogen in ratios: HMDSN (mTorr)/nitrogen (mTorr) from 70/10 to 20/60 in terms of operational pressure. The structural characterization of the films was done by FTIR spectroscopy. Absorptions were observed between 3500 cm(-1) to 3200 cm(-1), 3000 cm(-1) to 2900 cm(-1), 2500 cm(-1) to 2000 cm(-1), 1500 cm(-1) to 700 cm(-1), corresponding, respectively, to OH radicals, C-H stretching bonds in CH2 and CH3 molecules, C-N bonds, and finally, strain C-H bonds, Si-CH3 and Si-N groups, for both the 70 W and the 25 W. The contact angle for water was approximately 100 degrees and the surface energy is near 25mJ/m(2) which represents a hydrophobic surface, measured by goniometric method. The aging of the film was also analyzed by measuring the contact angle over a period of time. The stabilization was observed after 4 weeks. The refractive index of these materials presents values from 1.73 to 1.65 measured by ultraviolet-visible technique.
Resumo:
This paper describes the effect of nitrogen Plasma Immersion Ion Implantation (PIII) on chemical structure, refraction index and surface hardness of plasma-polymerized hexamethyldisilazane (PPHMDSN) thin films. Firstly, polymeric films were deposited at 13.56 MHz radiofrequency (RF) Plasma Enhanced Chemical Vapour Deposition (PECVD) and then, were treated by nitrogen PIII from 15 to 60 min. Fourier Transformed Infrared (FTIR) spectroscopy was employed to analyse the molecular structure of the samples, and it revealed that vibrations modes at 3350 cm(-1), 2960 cm(-1), 1650 cm(-1), 1250 cm(-1) and 1050 cm(-1) were altered by nitrogen PIII. Visible-ultraviolet (vis-UV) spectroscopy was used to evaluate film refractive index and the results showed a slight increase from 1.6 to 1.8 following the implantation time. Nanoindentation revealed a surface hardness rise from 0.5 to 2.3 GPa as PIII treatment time increased. These results indicate nitrogen PIII is very promising in improving optical and mechanical properties of PPHMDSN films.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fiber reinforced epoxy composites are used in a wide variety of applications in the aerospace field. These materials have high specific moduli, high specific strength and their properties can be tailored to application requirements. In order to screening optimum materials behavior, the effects of external environments on the mechanical properties during usage must be clearly understood. The environmental action, such as high moisture concentration, high temperatures, corrosive fluids or ultraviolet radiation (UV), can affect the performance of advanced composites during service. These factors can limit the applications of composites by deteriorating the mechanical properties over a period of time. Properties determination is attributed to the chemical and/or physical damages caused in the polymer matrix, loss of adhesion of fiber/resin interface, and/or reduction of fiber strength and stiffness. The dynamic elastic properties are important characteristics of glass fiber reinforced composites (GRFC). They control the damping behavior of composite structures and are also an ideal tool for monitoring the development of GFRC's mechanical properties during their processing or service. One of the most used tests is the vibration damping. In this work, the measurement consisted of recording the vibration decay of a rectangular plate excited by a controlled mechanism to identify the elastic and damping properties of the material under test. The frequency amplitude were measured by accelerometers and calculated by using a digital method. The present studies have been performed to explore relations between the dynamic mechanical properties, damping test and the influence of high moisture concentration of glass fiber reinforced composites (plain weave). The results show that the E' decreased with the increase in the exposed time for glass fiber/epoxy composites specimens exposed at 80 degrees C and 90% RH. The E' values found were: 26.7, 26.7, 25.4, 24.7 and 24.7 GPa for 0, 15, 30, 45 and 60 days of exposure, respectively. (c) 2005 Springer Science + Business Media, Inc.
Resumo:
The influences of hygrothermal conditioning on mechanical properties of a fiber/metal laminate (FML) have been investigated by tensile and compression tests. The environmental action, such as high moisture concentration, high temperatures, corrosive fluids or ultraviolet radiation (UV), can affect the performance of advanced composites during service. In the present work, the results show that for the glass fiber/epoxy composites tensile and compression values decrease after hygrothermal conditioning. However, no changes on mechanical properties (tensile and compression strength) are observed for the Glare laminate, regardless the hygrothermal conditioning. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
The break of polymer chemical bonds may occur due to penetration of sun short wavelengths. In sanitary landfills for instance, ultraviolet radiation affects uncovered materials and can be dangerous during the installation of the liner and before the placement of the waste. Only the ultraviolet part of the light is harmful to the geosynthetic materials, moreover, each material is sensitive to a particular wavelength. This article evaluates the effects of UV degradation and condensation in black HDPE (1.0 and 1.5 mm) and white HDPE (textured - 1.0 mm) geomembrane that were tested in laboratory during 6 months. The tests were performed using a weatherometer assembled at EESC-USP in accordance to ASTM G154. The results have shown variations in punction and tear resistance after each period of exposure.
Resumo:
The thermoluminescence (TL) response of Dy and Li doped 20CaB(4)O(7)-80CaB(2)O(4) (Wt%) glass-ceramic irradiated with ultraviolet (UV) radiation was studied. In order to act as TL activator ions, the Dy and Li ions were included in the matrix during the melting process to increase its TL efficiency. A single crystalline CaB2O4 phase was present in the glass-ceramic as determined by X-ray diffraction (XRD). The glass-ceramic 20CaB(4)O(7)-80CaB(2)O(4):Dy,Li wt% (named 20CBO7:Dy,Li) is a newly prepared TL material. Its thermoluminescent dosimetric characteristics have shown a linear response under UV radiation exposure and a good TL signal reproducibility, thus proving to be a promising material for using as an ultraviolet radiation dosimeter. (C) 2007 Elsevier B.V. All rights reserved.