In this work, spinels with the general formula Zn2-xCoxTiO4 were synthesized by the polymeric precursor method and thermally treated at 1,000 A degrees C. The powder precursors were characterized by TG/DTA. A decrease in the DTA peak temperature with the amount of zinc was observed. After the thermal treatment, the characterizations were performed by XRD, IR, colorimetry and UV/VIS spectroscopy. The XRD patterns of all the samples showed the presence of the spinel phase. Infrared spectroscopy showed the presence of ester complexes for Zn2TiO4 after thermal treatment at 500 A degrees C, which disappeared after cobalt addition, indicating that organic material elimination was favored.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

PANI films were deposited on glass substrates by in-situ polymerization and characterized by UV-VIS spectroscopy and atomic force microscopy. A method is developed to accurately analyze ellipsometric data obtained for transparent glass substrates before and after modification with absorbing polymer films. Surface modification was made with an overlayer such as polyaniline ( PANI), which exhibits different optical properties by varying its oxidation state. First, the issue of using transparent substrates for ellipsometry studies was examined and then, spectroscopic ellipsometry was used to characterize absorbing overlayers on transparent glasses. The same methodologies of data analysis can be also applied to other absorbing films on transparent substrates, and deposited by different techniques.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Thin films of chemically synthesized polyaniline and poly(o-methoxyaniline) were exposed to ionizing X-ray radiation and characterized by radiation induced conductivity measurements, ultraviolet-visible spectroscopy, electron paramagnetic resonance, electrical conductivity and solubility measurements. Samples irradiated in vacuum or dry Oxygen atmosphere did not have their electronic spectra changed. However, under humid atmosphere the energy of the excitonic transition was decreased and accompanied by a great conductivity increase. The results indicate that doping of polyaniline can be induced by X-ray radiation which might be of great interest for applications on lithography and microelectronics.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The pyH[trans-RuCl4(py)2](1) and pyH[trans-RuCl4(CO)(py)](2) complexes were synthesized and found to crystallize in space group P21/n, Z = 4 with a = 8.080(7), b = 22.503(7), c = 10.125(6) Å, β = 93.19(6)° for (1) and a = 7.821(1), b = 10.337(3), c = 19.763(3) Å, β = 93.07(1)° for (2). The structures were solved by Patterson and difference Fourier techniques and refined to R = 0.062 for (1) and R = 0.038 for (2). In both cases the Ru(III) ion is octahedrally coordinated to four co-planar chlorine atoms, the nitrogen of the pyridine rings or carbon from the carbon monoxide. Another protonated pyridine group, which forms the counter-cation completes the crystal structures. The UV-Vis absorption spectra show three bands: (1) 360 (ε = 1180 M-1 cm-1), 441 (ε = 3200 M-1 cm-1) and 532 nm (ε = 400 M-1 cm-1); (2) 315(ε = 1150 M-1 cm-1), 442 (ε = 3170 M-1 cm-1) and 530 nm (ε = 390 M-1 cm-1). The two higher energy bands were associated with ligand-to-metal charge transfer transitions and a third band at lower energy was assigned to a d-d transition. Low temperature EPR data confirmed the presence of the paramagnetically active Ru(III) and it is consistent with axial symmetry of the complexes. The position of the stretching CO band in complex (2) is discussed in terms of metal-CO backbonding.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The purpose of this work is to study the preparation and spectroscopic behavior of the europium diphenylphosphinate complex -Eu(DPP)3. Elemental and thermogravimetric analysis, powder X-ray diffractometry, and infrared spectroscopy were applied to characterize the formula of the final product and the sixfold coordination of the Eu3+ ion. Excitation and emission spectra have been recorded at liquid nitrogen and room temperatures. The 5D0→7F2 transition intensity decreases when T decreases in comparison to the 5D0→7F1 transition intensity. Molecular mechanic calculations were developed in order to obtain the spatial coordinates of the Eu3+ and ligand ions. The simple overlap model was used to calculate the total splitting of the 5D0→7F1 transition, 5D0→7F0/5D 0→7F2 ntensity ratio and the intensity parameters, Ωλ (λ=2 and 4). Good agreements between theoretical predictions and experimental results have been obtained with g=2/3 as the effective charge and α=0.8×10-24 cm3 as the isotropic polarizability of the oxygen. © 1998 Elsevier Science S.A.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Room-temperature photoluminescence (PL) was observed in undoped and 2 mol% Cr-, Al- and Y-doped amorphous SrTiO3 thin films. Doping increased the PL, and in the case of Cr significantly reduced the associated PL wavelength. The optical bandgaps, calculated by means of UV-vis absorption spectra, increased with crystallinity and decreased with the doping level. It was considered that yttrium and aluminum substituted Sr2+, whereas chromium replaced Ti4+. It is believed that luminescence centers are oxygen-deficient BO6 complexes, or the same centers with some other defects, such as oxygen or strontium vacancies, or BO6 complexes with some other defects placed in their neighborhood. The character of excitation and the competition for negatively charged non-bridging oxygen (NBO) among numerous types of BO6 defect complexes in doped SrTiO3 results in various broadband luminescence peak positions. The results herein reported are an indicative that amorphous titanates are sensitive to doping, which is important for the control of the electro-optic properties of these materials. The probable incorporation of Cr into the Ti site suggests that the existence of a double network former can lead to materials displaying a more intense photoluminescence.