983 resultados para spectrophotometry UV-VIS


Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this work is to report on the luminescence properties of BaZnSiO4 activated by Eu3+ and Mn2+ ions. Doped and undoped powder samples were prepared by solid-state reaction starting from oxides and carbonates or Ba2SiO4:Eu3+ and Zn2SiO4:Mn2+ precursors. X-ray diffraction powder data, IR vibrational, and UV-vis luminescence spectroscopies were carried out. Results showed that doped and undoped samples from both types of precursors have the same structure and crystallize with a superstructure of hexagonal kalsilite. Vibrational spectroscopy has confirmed the formation of a silicate group, which outlines differences between products and silicate precursors. The observed luminescence assigned to Eu3+ and Mn2+ transitions covered most parts of the visible spectrum, an important requirement for phosphors in fluorescent low-pressure mercury vapor lamps.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

In this work particles of ZnO of size range 33-56 Angstrom were prepared by a sol-gel method. The effect of reaction time on the particle size of ZnO or ZnO:Ce was investigated by transmission electron microscopy measurements, UV-vis absorption and luminescence spectroscopy. A linear increase of the mean particle size is observed as a function of reaction time. The cerium-doped particles are bigger than the pure ZnO ones obtained at the same reaction time. A shift to lower energy at the maximum of the bands is observed in all absorption, emission and excitation spectra as a function of particle growth. From the absorption spectra the optical energy gap values (Eg) for these particles were determined. In the quantum size regime, Eg was found to decrease with particle growth.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

NiWO4 and ZnWO4 were synthesized by the polymeric precursor method at low temperatures with zinc or nickel carbonate as secondary phase. The materials were characterized by thermal analysis (TG/DTA), infrared spectroscopy, UV-Vis spectroscopy and X-ray diffraction. NiWO4 was crystalline after calcination at 350 A degrees C/12 h while ZnWO4 only crystallized after calcination at 400 A degrees C for 2 h. Thermal decomposition of the powder precursor of NiWO4 heat treated for 12 h had one exothermic transition, while the precursor heat treated for 24 h had one more step between 600 and 800 A degrees C with a small mass gain. Powder precursor of ZnWO4 presented three exothermic transitions, with peak temperatures and mass losses higher than NiWO4 has indicating that nickel made carbon elimination easier.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Alkaline earth stannates have recently become important materials in ceramic technology due to its application as humidity sensor. In this work, alkaline earth stannates doped with Fe3+ were synthesized by the polymeric precursor method, with calcination at 300 A degrees C/7 h and between 400 and 1100 A degrees C/4 h. The powder precursors were characterized by TG/DTA after partial elimination of carbon. Characterization after the second calcination step was done by X-ray diffraction, infrared spectroscopy, and UV-vis spectroscopy. Results confirmed the formation of the SrSnO3:Fe with orthorhombic perovskite structure, besides SrCO3 as secondary phase. Crystallization occurred at 600 A degrees C, being much lower than the crystallization temperature of perovskites synthesized by solid state reaction. The analysis of TG curves indicated that the phase crystallization was preceded by two thermal decomposition steps. Carbonate elimination occurred at two different temperatures, around 800 A degrees C and above 1000 A degrees C.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Vitreous samples containing high concentrations of WO3 (above 40% M) have been used as a target to prepare thin films. Such films were deposited using the electron beam evaporation method onto soda-lime glass substrates. These films were characterized by X-ray diffraction (XRD), perfilometry, X-ray energy dispersion spectroscopy (EDS), M-Lines and UV-vis absorption spectroscopy. In this work, experimental parameters were established to obtain stable thin films showing a chemical composition close to the glass precursor composition and with a high concentration of WO3. These amorphous thin films of about 4 mu m in thickness exhibit a deep blue coloration but they can be bleached by thermal treatment near the glass transition temperature. Such bleached films show several guided modes in the visible region and have a high refractive index. Controlled crystallization was realized and thus it was possible to obtain WO3 microcrystals in the amorphous phase. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)