926 resultados para Propylene Glycol
Resumo:
The syntheses of several dialkyl complexes based on rare-earth metal were described. Three beta-diimine compounds with varying N-aryl substituents (HL1 = (2-CH3O(C6H4))N=C(CH3)CH=C(CH3)NH(2-CH3O(C6H4)), HL2 = (2,4,6-(CH3)(3) (C6H2))N=C(CH3)CH=C(CH3)NH(2,4,6-(CH3)(3)(C6H2)), HL3 = PhN=C(CH3)CH(CH3) NHPh) were treated with Ln(CH2SiMe3)(3)(THF)(2) to give dialkyl complexes L(1)Ln (CH2SiMe3)(2) (Ln = Y (1a), Lu (1b), Sc (1c)), L(2)Ln(CH2SiMe3)(2)(THF) (Ln = Y (2a), Lu (2b)), and (LLu)-Lu-3(CH2SiMe3)(2)(THF) (3). All these complexes were applied to the copolymerization of cyclohexene oxide (CHO) and carbon dioxide as single-component catalysts.
Resumo:
The morphology of a H-shaped block copolymer (poly(ethylene glycol) backbone and polystyrene branches (PS)(2)PEG(PS)(2)) in a thin film has been investigated. A peculiar square lamella that has a phase-separated microdomain at its surface is obtained after spin coating. The experimental temperature plays a critical role in the lamellar formation. The copolymer first self-assembles into square lamellar micelles with an incomplete crystalline core due to the crystallizability of PEG.
Resumo:
The formation of ring-shaped structures in an H-shaped block copolymer [a poly(ethylene glycol) backbone with polystyrene branches, i.e., (PS)(2)PEG(PS)(2)] thin film was investigated when it was annealed in saturated PEG-selective acetonitrile vapor. Our results clearly indicate that ring formation is determined by the initial morphology of the spin-coated film, the solvent vapor selectivity and the environmental temperature of the solvent-annealing process. Only the films with the initial core-shell cylindrical structure in strongly PEG-selective acetonitrile vapor could form the ring-shaped structures.
Resumo:
A new biodegradable amphiphilic block copolymer, poly(ethylene glycol)-b-poly(L-factide-co-9-phenyl-2,4,8, 10-tetraoxaspiro[5,5]undecan-3-one) [PEG-b-P(LA-co-PTO)], was successfully prepared by ring-opening polymerization (ROP) Of L-lactide (LA) and functionalized carbonate monomer 9-phenyl-2,4,8,10-tetraozaspiro[5,5]undecan-3-one (PTO) in the presence of monohydroxyl poly(ethylene glycol) as macroinitiator using Sn(Oct)(2) as catalyst. NMR, FT-IR, and GPC studies confirmed the copolymer structure.
Resumo:
This report describes a facile route to prepare the vesicles and large compound micelles (LCMs) from a series of poly(epsilon-benzyloxycarbonyl L-lysine)-block-poly[diethylene glycol bis(3-amino propyl) ether]-block-poly(epsilon-benzyloxycarbonyl L-lySine) (PZLL-DGBE-PZLL) in their water solution, depending on molecular weight of the polypeptides. A pyrene probe is used to demonstrate the aggregate formation of PZLL-DGBE-PZLL in solution, and also to measure their critical micelle concentration as a function of molecular weight of the polymer.
Resumo:
The amphiphilic PEG1 500-b-EM AP-b-PEG1 500 (EM PAP) triblock copolymer of poly(ethylene glycol) (PEG) and emeraldine aniline-pentamer (EM AP) in its concentrated solution can self-assemble into a special shape like "sandglass", as observed by transmission electron microscopy (TEM), field emission scanning electron microscopy (ESEM) and atomic force microscopy (AFM). This "sandglass"- shaped assembly is composed of several "rods" aggregated in the middle, with every "rod" being about 8 VLrn in length and 300 nm in diameter.
Resumo:
The release behavior of a water-soluble small molecule drug from the drug-loaded nanofibers prepared by emulsion-electrospinning was investigated. Doxorubicin hydrochloride (Dox), a water-soluble anticancer agent, was used as the model drug. The laser scanning confocal microscopic images indicated that the drug was well incorporated into amphiphilic poly(ethylene glycol)-poly(L-lactic acid) (PEG-PLA) diblock copolymer nanofibers, forming "core-sheath" structured drug-loaded nanofibers.
Resumo:
Amphiphilic biodegradable star-shaped polymer was conveniently prepared by the Sn(Oct)(2)-catalyzed ring opening polymerization of c-caprolactone (CL) with hyperbranched poly(ester amide) (PEA) as a macroinitiator. Various monomer/initiator ratios were employed to vary the length of the PCL arms. H-1 NMR and FTIR characterizations showed the successful synthesis of star polymer with high initiation efficiency. SEC analysis using triple detectors, RI, light scattering, and viscosity confirmed the controlled manner of polymerization and the star architecture.
Resumo:
Branched polystyrenes with abundant pendant vinyl functional groups were prepared via radical polymerization of an asymmetric divinyl monomer, which possesses a higher reactive styryl and a lower reactive butenyl. Employing a fast reversible addition fragmentation chain transfer (RAFT) equilibrium, the concentration of active propagation chains remained at a low value and thus crosslinking did not occur until a high level of monomer conversion. The combination of a higher reaction temperature (120 degrees C) and RAFT agent cumyl dithiobenzoate was demonstrated to be optimal for providing both a more highly branched architecture and a higher polymer yield.
Resumo:
A series of novel titanium(IV) complexes combining a phosphine oxide-bridged bisphenolato ligand TiCl2{2,2'-O=P-R-3 (4-R-2-6-R-1-C6H2O)(2)}(THF) (6a: R-1 = tBu, R-2 - H, R-3 Ph; 6b: R-1 - Ph, R-2 = H, R-3 = Ph; 6c: R-1 = R-2 = tBu, R-3 = Ph; 6d: R-1 = R-2 cumyl, R-3 = Ph; 6e: R-1 = tBu, R-2 = H, R-3 = PhF5) were prepared by the reaction of corresponding bisphenolato ligands with TiCl4 in THF. X-ray analysis reveals that complex 6a adopts distorted octahedral geometry around the titanium center. These catalysts were performed for ethylene polymerization in the presence of modified methyaluminoxane (MMAO).
Resumo:
Vanadium(III) complexes bearing salicylaldiminato ligands (2a-k) [RN=CH(Ar0)]VCl2(THF)2 (Ar C61714, R = Ph, 2a; p-CF3Ph, 2b; p-CH3Ph, 2c; 2,6-Me2Ph, 2d; 2,6-iPr2Ph, 2e; cyclohexyl, 2f; Ar = C6H3tBu(2), R = Ph, 2g; 2,6-iPr2Ph, 2h; Ar = C6H2tBU2(2,4), R = Ph, 2i; 2,6-iPr2Ph, 2j; Ar = C6H2Br2, R = Ph, 2k) were prepared from VC13(THF)3 by treating with 1.0 equiv of (RN=CH)ArOH in tetrahydrofuran (THF) in the presence of excess triethylamine (TEA).
Resumo:
A series of new titanium complexes with two asymmetric bidentate beta-enaminoketonato (N,O) ligands (4b-t), [RN=CCF3)CHC(t-BU)O](2)TiCl2 (4b, R = -C6H4F(o); 4c, R = -C6H4F(m);4d, R = -C6H4F(p); 4e, R = - C6H3F2(2,3); 4f, R = -C6H3F2(2,4); 4g, R = -C6H3F2(2,5); 4h, R = -C6H3F2(2,6); 4i, R = -C6H3F2(3,4); 4j, R = -C6H3F2(3,5); 4k, R = -C6H2F3(2,3,4); 4l, R = -C6H2F3(3,4,5); 4m, R = -C6H4CF3(o); 4n, R =-C6H4CF3(m); 4o, R = -C6H4CF3(p); 4p, R = -C6H4Cl(p); 4q, R = -C6H4I(p); 4r, R = -C6H4NO2(P); 4s, R = -CH2C6H5; 4t, R = -C6H11), have been synthesized and characterized.
Resumo:
Chloro( 5,10,15,20-tetraphenyl-porphyrinato)-aluminum/tetraethylammonium bromide ( Et4NBr) in combination with bulky Lewis acid was used for the copolymerization of CO2 and cyclohexene oxide ( CHO). Bulky Lewis acid having substituents at the ortho positions of the phenolate ligands, like methylaluminum bis(2,6-di-tert-butyl-4-methylphenolate), significantly shortened the induction period and raised the catalytic activity, the corresponding turnover frequency reached 44.9 h(-1) in 9 h, which was 23.8% higher than that from ( TPP)AlCl/Et4NBr binary catalyst. The resulting polycarbonate has carbonate linkage over 93% with number average molecular weight of ( 4.5-6.5) x 10(3) and polydispersity index below 1.10.
Resumo:
The multiphase morphology of high impact polypropylene (hiPP), which is a reactor blend of polypropylene (PP) with ethylene-propylene copolymer, was investigated by transmission electron microscopy, selected area electron diffraction, atomic force microscopy, and field-emission scanning electron microscopy techniques in conjunction with an analysis of the hiPP composition and chain structure based on solvent fractionation, C-13-NMR, and differential scanning calorimetry measurements.
Resumo:
In this study, binodal curves and tie line data of [Amim]Cl + salt (K3PO4, K2HPO4, K2CO3) + water aqueous biphasic systems (ABS) were measured and correlated satisfactorily with the Merchuk equation and Othmer-Tobias and Bancroft equations, respectively. [Amim]Cl could be recovered from aqueous solutions using the ABS, and the recovery efficiency could reach 96.80%. The recovery efficiency was influenced by the concentrations of the salts and their Homeister series: K3PO4 > K2HPO4 > K2CO3. Our method provides a new and effective route for the recovery of hydrophilic IL using [Amim]Cl + salt + water ABS from aqueous solutions.