999 resultados para IRON FILMS


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work investigates the adsorption of Alizarin, Eriochrome Blue Black R and Fluorescein using chitosan, goethite and magnetite as adsorbents. For Alizarin, the best adsorbent is chitosan with a Langmuir parameter of 15.8 mmol dye/g adsorbent. For Eriochrome Blue Black R only 1.94 mmol dye/g chitosan is adsorbed. Langmuir parameters for the Alizarin adsorption on both iron oxides display one or two orders of magnitude lower than for chitosan and two orders of magnitude lower in the case of Eriochrome Blue Black R. Fluorescein does not adsorb in appreciable amounts on chitosan and it presents the lower affinity on the iron oxides.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Citric acid was used as a compatibilizer in the production of starch and PBAT films plasticized with glycerol and processed by blow extrusion. Films produced were characterized by WVP, mechanical properties, FT-IR-ATR and SEM. WPV ranged from 3.71 to 12.73×10-11 g m-1 s-1 Pa-1, while tensile strength and elongation at break ranged from 1.81 to 7.15 MPa and from 8.61 to 23.63%, respectively. Increasing the citric acid concentration improved WVP and slightly decreased film resistance and elongation. The films micrographs revealed a more homogeneous material with the addition of citric acid. However, the infrared spectra revealed little about cross-linking esterification reaction

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new sensitive and selective procedure for speciation of trace dissolved Fe(III) and Fe(II), using modified octadecyl silica membrane disks and determination by flame atomic absorption spectrometry was developed. A ML3 complex is formed between the ligand and Fe(III) responsible for extraction of metal ion on the disk. Various factors influencing the separation of iron were investigated and the optimized operation conditions were established. Under optimum conditions, an enrichment factor of 166 was obtained for Fe3+ ions. The calibration graph using the preconcentration system for Fe3+ was linear between 40.0 and 1000.0 μg L-1.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Titanium dioxide porous thin films on the Anatase phase were deposited onto glass slides by the sol-gel method assisted with polyethylene glycol (PEG). The dip-coated films were characterized using scanning electron microscopy (SEM), thermogravimetric analysis (TGA and DTG), UV-visible spectroscopy and X-ray diffraction (XRD). The photocatalytic activity of the films was determined by means of methyl-orange oxidation tests. The resultant PEG-modified films were crack-free and developed a porous structure after calcination at 500 °C. Photo-oxidation tests showed the dependency of catalytic activity of the films on the number of layers (thickness) and porosity, i.e. of the interfacial area.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Four new compounds with the general formula [Fe(phen)3][Zn(RSO2N=CS2)2], where phen = 1,10-phenanthroline, R = 4-FC6H4 (1), 4-ClC6H4 (2), 4-BrC6H4 (3) and 4-IC6H4 (4), respectively, were obtained by the reaction of the appropriate potassium N-R-sulfonyldithiocarbimate (RSO2N=CS2K2) and tris(1,10-phenanthroline)iron(II) sulfate, with zinc(II) acetate dihydrate in dimethylformamide. The elemental analyses and the IR data were consistent with the formation of the expected complexes salts. The ¹H and 13C NMR spectra showed the signals for the cationic iron(II) complex and dithiocarbimate moieties. The molar conductance data were consistent with the 1:1 cation:anion complexes in 1-4. The antifungal activities of the compounds were tested in vitro against Candida albicans, Candida tropicalis and Colletotrichum gloeosporioides.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study aims to prepare biodegradable films from cassava starch, poly (butylene adipate-co-terephthalate) (PBAT), and montmorillonite (MMT) using blow-extrusion process and analyze the effects of different types and concentrations of MMT on the microstructure, physicochemical, and mechanical properties of the resulting films. The films were produced by blending 30% of PBAT with glycerol (17.5%), starch (49.0-52.5%), and four different types of montmorillonite (Cloisite® Na+, 10A, 15A, and 30B) at two different concentrations (1.75% and 3.5%). All the films prepared in this study showed an increase in the basal spacing of MMT layers. In particular, the films with 10A and 30B showed the highest increase in intercalation basal spacing, suggesting the formation of intercalated composites. The addition of nanoclays decreased the elongation of films. The addition of Cloisite® 10A resulted in films with the lowest WVP values and the highest stability to water adsorption under different RH conditions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The viability of small-scale heavy-metal waste immobilization into iron phosphate glasses was investigated. Several waste forms containing different amounts of heavy-ion wastes were evaluated (5%, 10%, 15%, 20%, 26%, 33%, 40% and 50% by mass) and their X-ray diffraction patterns revealed that no crystallization occurred in glasses with waste concentrations up to 26%. The dissolution rates for all of the reported glass compositions (ca. 10-8 g cm-2 min-1) are similar to those reported for the materials most commonly used for waste vitrification. Iron phosphate glasses thus proved to be very useful for the immobilization of heavy-metal wastes, exhibiting good contention and chemical durability comparable to that of borosilicate glasses.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study investigated the reductive degradation of acetamiprid (5 mg L-1) in aqueous medium (at pH 2.0) induced by zero-valent iron (50 mg). The process was monitored using high-performance liquid chromatography (HPLC) to determine the degradation rate as a function of reaction time, and direct infusion electrospray ionization mass spectrometry (DI-ESI-MS) to search for (and potentially characterize) any possible byproducts formed during degradation. The results obtained via HPLC showed that after 60 min, the degradation of the substrate reached nearly 100% in an acidic medium, whereas the mineralization rate (as determined by total organic carbon measurements) was as low as 3%. Data obtained by DI-ESI-MS showed that byproducts were formed mainly by insertions of hydrogen atoms into the nitrile, imine, and pyridine ring moieties, in addition to the observation of chlorine substitution by hydrogen replacement (hydrodechlorination) reactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Silica gel chemically modified with 2-Aminotiazole groups, abbreviated as SiAT, was used for preconcentration of copper, zinc, nickel and iron from kerosene, normally used as a engine fuel for airplanes. Surface characteristics and surface area of the silica gel were obtained before and after chemical modification using FT-IR, Kjeldhal and surface area analysis (B.E.T.). The retention and recovery of the analyte elements were studied by applying batch and column techniques. The experimental parameters, such as shaking time in batch technique, flow rate and concentration of the eluent (HCl- 0.25-2.00 mol L-1) and the amount of silica, on retention and elution, have been investigated. Detection limits of the method for copper, iron, nickel and zinc are 0.77, 2.92, 1.73 and 0.097 mg L-1, respectively. The sorption-desorption of the studied metal ions made possible the development of a preconcentration method for metal ions at trace level in kerosene using flame AAS for their quantification.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of water molecules on the conductivity and electrochemical properties of vanadium pentoxide xerogel was studied in connection with changes of morphology upon thermal annealing at different temperatures. It was demonstrated that the conductivity was increased for the samples heated at 150ºC and 270ºC compared to the vanadium pentoxide xerogel. It was also verified a stabilization of electrochemical processes of the insertion and de-insertion of lithium ions the structure of thermally annealed vanadium pentoxide.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work aimed to find out the suitability of foam as medium in application of thin liquid films. This consists of research over phenomena related to foam physics and behaviour. Solutions and mixtures to be foamed, foaming agents, foam generation and application methods were evaluated. Over the evaluated solutions and mixtures coating paste and CMC did not foam well. Latex and PVA solutions were foamable and the best solution for foam use was starch. PVA and casein can be used as foaming agents, but the best results were achieved with sodium dodecyl sulphate (SDS). SDS works well with starch solutions producing fine and stable foam. Foaming was done with simple mixers where pressurized air was fed to the solution. The foaming works fine when enough shear force is used together with sufficient foaming agent concentration. Foam application with curtain, rod and cylinder methods with a gap between the application device and paper were not usable because of high coating amount. Coating amounts were smallest with the blade method which achieved 0.9 g/m2 starch layer. Although some strength decrease was expected because of the foaming agent, it dit not have significant effect. The targeted coating amount of 0.5 g/m2 was not achieved due to the limitations with the methods. More precise foam application methods are needed. Continuous foam generation and feed to the paper surface with controllable device such as application teeth could improve the results.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The possibility of using thiocyanate to determine iron(II) and/or iron(III) in water-acetone mixture has been re-examined as part of a systematic and comparative study involving metallic complexes of pseudohalide ligands. Some parameters that affect the complete oxidation of the ferrous cations, their subsequent complexation and the system stability have been studied to optimize the experimental conditions. Our results show the viability and potentiality of this simply methodology as an alternative analytical procedure to determine iron cations with high sensitivity, precision and accuracy. Studies on the calibration, stability, precision, and effect of various different ions have been carried out by using absorbance values measured at 480 nm. The analytical curve for the total iron determination obeys Beer's law (r = 0.9993), showing a higher sensitivity (molar absorptivity of 2.10x10(4) L cm-1 mol-1) when compared with other traditional systems (ligands) or even with the "similar" azide ion [1.53x10(4) L cm-1 mol-1, for iron-III/azide complexes, in 70% (v/v) tetrahydrofuran/water, at 396 nm]. Under such optimized experimental conditions, it is possible to determine iron in the concentration range from 0.5 to 2 ppm (15-65% T for older equipments, quartz cells of 1.00 cm). Analytical applications have been tested for some different materials (iron ores), also including pharmaceutical products for anemia, and results were compared with atomic absorption determinations. Very good agreement was obtained with these two different techniques, showing the potential of the present experimental conditions for the total iron spectrophotometric determinations (errors < 5%). The possibility of iron speciation was made evident by using another specific and auxiliary method for iron(II) or (III).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An amperometric sensor was constructed, by using humic acids to immobilize Fe3+ ions on a carbon paste electrode (CPE-HA-Fe), and used for ascorbic acid (H2A) determination. The cyclic voltammogram of the electrode showed electrochemical response due to the Fe3+/Fe2+ couple at E1/2=+0.78 V vs SCE, using 0.5 mol L-1 KCl and 0.2 mol L-1 acetate/0.020 mol L-1 phosphate buffer, at pH = 5.4, as supporting electrolyte. When H2A is added to the electrolyte solution it is observed an oxidation process. The oxidation current, obtained by chronoamperommetry at +0.87 V vs SCE, is proportional to the concentration, represented by the equation I(µA) = 7.6286 [H2A] (mmol L-1) + 1.9583, r = 0.9996, for concentrations between 0.0 and 1.4 mmol L-1. The electrode showed high stability and was used for H2A determination in a natural orange juice.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Copolymers of methyl methacrylate (MMA) and triethyleneglycol dimethacrylate (TEGDMA) obtained by photoinitiated polymerization using Fe(III) complexes were submitted to thermogravimetry (TGA) under dynamic air atmosphere and N2, and differential scanning calorimetric analysis (DSC). Thermal events were observed only between 90 - 110 ºC. Glass transitions were observed at ca. 100 ºC, followed by an exothermic peak at 170 ºC. The exothermic peak was assigned to a thermal curing process due to the presence of unreacted vinyl groups of the monomers. DSC revealed to be a useful tool to evaluate the curing completeness in this kind of material, using small amounts of sample in relatively short time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Direct leaching is an alternative to conventional roast-leach-electrowin (RLE) zinc production method. The basic reaction of direct leach method is the oxidation of sphalerite concentrate in acidic liquid by ferric iron. The reaction mechanism and kinetics, mass transfer and current modifications of zinc concentrate direct leaching process are considered. Particular attention is paid to the oxidation-reduction cycle of iron and its role in direct leaching of zinc concentrate, since it can be one of the limiting factors of the leaching process under certain conditions. The oxidation-reduction cycle of iron was experimentally studied with goal of gaining new knowledge for developing the direct leaching of zinc concentrate. In order to obtain this aim, ferrous iron oxidation experiments were carried out. Affect of such parameters as temperature, pressure, sulfuric acid concentration, ferrous iron and copper concentrations was studied. Based on the experimental results, mathematical model of the ferrous iron oxidation rate was developed. According to results obtained during the study, the reaction rate orders for ferrous iron concentration, oxygen concentration and copper concentration are 0.777, 0.652 and 0.0951 respectively. Values predicted by model were in good concordance with the experimental results. The reliability of estimated parameters was evaluated by MCMC analysis which showed good parameters reliability.