886 resultados para Cyclic steam stimulation


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrical conductivity of a range of concrete mixes, with and without supplementary cementitious materials (SCM), is studied through multiple cycles of heating and cooling over the extended temperature range −30/+70 °C. When presented in an Arrhenius format, the experimental results display hysteresis effects at the low-temperature end of the thermal cycle and, in those concretes containing supplementary cementitious materials at higher water/binder ratios, hysteresis effects were evident over the entire temperature range becoming more discernible with increasing number of thermal cycles. The depression in both the freezing and thawing point could be clearly identified and was used to estimate pore-neck and pore-cavity radii. A simplified approach is presented to evaluate the volumetric ratio of frozen pore water in terms of conductivity measurements. The results also show that the conductivity and activation energy of the concrete specimens were related to the water/binder ratio, type of SCM, physical state of the pore water and the thermal cycling regime.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Highly reactive radicals play an important role in high-temperature gasification processes. However, the effect of radicals on gasification has not been systematically investigated. In the present study, the formation of carbon-radical precursors using atomic radicals such as OH, O, and H and molecules such as H2 and O2 was characterized, and the effect of the precursors on the adsorption step of steam char gasification was studied using quantum chemistry methods. The results revealed that the radicals can be chemisorbed exothermically on char active sites, and the following order of reactivity was observed: O > H2 > H > OH > O 2. Moreover, hydrogen bonds are formed between steam molecules and carbon-radical complexes. Steam molecule adsorption onto carbon-O and carbon-OH complexes is easier than adsorption onto clean carbon surfaces. Alternatively, adsorption on carbon-O2, carbon-H2, and carbon-H complexes is at the same level with that of clean carbon surfaces; thus, OH and O radicals accelerate the physical adsorption of steam onto the char surface, H radical and O2 and H2 molecules do not have a significant effect on adsorption. © 2010 American Chemical Society.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A systematic theoretical study on the adsorption of steam and its thermal decomposition products on carbon both zigzag and armchair surface was performed to provide molecular-level understanding of the reaction activity of all these reactants in biomass steam gasification process. All the calculations were carried out using density functional theory (DFT) at the B3LYP/6-31+g(d,p) level. The structures of carbonaceous surfaces, all reactants and surface complexes were optimized and characterized. Based on the value of adsorption heat been obtained from the calculation, the activity of all reactants can be ordered as: O > O2 >H2 >H >OH >H2O for both zigzag and armchair surface, and the adsorption style is physisorption to water molecule and chemisorption to the other dissociated components.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper investigates the mechanism of nanoscale fatigue of functionally graded TiN/TiNi films using nano-impact and multiple-loading-cycle nanoindentation tests. The functionally graded films were deposited on silicon substrate, in which TiNi films maintain shape memory and pseudo elastic behavior, while a modified TiN surface layer provides tribological and anti-corrosion properties. Nanomechanical tests were performed to comprehend the localized film performance and failure modes of the functionally graded film using NanoTestTM equipped with Berkovich and conical indenter between 100 μN to 500 mN loads. The loading mechanism and load history are critical to define film failure modes (i.e. backward depth deviation) including the shape memory effect of the functionally graded layer. The results are sensitive to the applied load, loading type (e.g. semi-static, dynamic) and probe geometry. Based on indentation force-depth profiles, depth-time data and post-test surface observations of films, it is concluded that the shape of the nanoindenter is critical in inducing the localized indentation stress and film failure, including shape recovery at the lower load range. Elastic-plastic finite element (FE) simulation during nanoindentation loading indicated that the location of subsurface maximum stress near the interface influences the backward depth deviation type of film failure. A standalone, molecular dynamics simulation was performed with the help of a long range potential energy function to simulate the tensile test of TiN nanowire with two different aspect ratios to investigate the theory of its failure mechanism.