948 resultados para 091207 Metals and Alloy Materials
Resumo:
Kikuchi diffraction was used to accurately determine the orientation relationship (OR) between Mg17Al12 precipitates and matrix in an AZ91D alloy. For both continuous and discontinuous precipitations, the Burgers OR and the Potter OR were equally observed. The lattice parameter of Mg17Al12 associated with the former is bigger than that of the latter. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
Resumo:
The aim of this article is to demonstrate that the apparent controversy between the infinitesimal deformation (ID) approach and the phenomenological theory of martensitic transformations (PTMTs) in predicting the crystallographic characteristics of a martensitic transformation is entirely based on unjustified approximations associated with the way in which the ID calculations are performed. When applied correctly, the ID approach is shown to be absolutely identical to the PTMT. Nevertheless, there may be some advantages in using the ID approach. In particular, it is somewhat simpler than the PTMT; it is based on a physical concept that is easier to understand and, most important, it may provide a tool for investigating some of the features of martensitic transformations that have eluded explanation via the PTMT.
Resumo:
The flow stress in tensile and compressive deformation has been determined in cast Mg, for a wide range of grain sizes between 36 mum and 1.5 mm. The grain size was varied by alloying Mg with small amounts of Zr. It was found that the 0.2% offset flow stress, sigma(y) (MPa), varies with the grain size, d (m), as sigma(y) = 17.7 + 0.25 d(-1/2) in tension, while sigma(y) = -2.3 + 0.39 d(-1/2) in compression. Possible reasons for the difference between tension and compression are discussed.
Resumo:
The corrosion behaviour of die cast magnesium alloy AZ91D aged at 160degreesC was investigated. The corrosion rate of the alloy decreases with ageing time in the initial stages and then increases again at ageing times greater than 45 h. The dependence of the corrosion rate on ageing time can be related to the changes in microstructure and local composition during ageing. Precipitation of the beta phase (Mg17Al12) occurs exclusively along the grain boundaries during ageing. The beta phase acts as a barrier, resulting in a decreasing corrosion rate in the initial stages of ageing. In the later stages, the decreasing aluminium content of alpha grains makes the alpha matrix more active, causing an increase in the corrosion rate. Electrochemical testing results also confirm the combined effects of the changes in alpha and beta phases on the corrosion resistance of the aged die cast AZ91D alloy. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Selective laser sintering has been used to fabricate an aluminium alloy powder preform which is subsequently debound and infiltrated with a second aluminium alloy. This represents a new rapid manufacturing system for aluminium that can be used to fabricate large, intricate parts. The base powder is an alloy such as AA6061. The infiltrant is a binary or higher-order eutectic based on either Al-Cu or At-Si. To ensure that infiltration occurs without loss of dimensional precision, it is important that a rigid skeleton forms prior to infiltration. This can be achieved by the partial transformation of the aluminium to aluminium nitride. In order for this to occur throughout the component, magnesium powder must be added to the alumina support powder which surrounds the part in the furnace. The magnesium scavenges the oxygen and thereby creates a microclimate in which aluminium nitride can form. The replacement of the ionocovalent Al2O3 with the covalent AlN on the surface of the aluminium powders also facilitates wetting and thus spontaneous and complete infiltration. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The effect of iron on the grain refinement of high-purity Mg-3%Al and Mg-91%Al alloys has been investigated using anhydrous FeCl3 as an iron additive at 750degreesC in carbon-free aluminium titanite crucibles. It was shown that grain refinement was readily achievable for both alloys. Fe- and Al-rich intermetallic particles were observed in many magnesium grains. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
A trace of beryllium can lead to dramatic grain coarsening in Mg-Al alloys at normal cooling rates. It is, however, unclear whether this effect applies to aluminium-free magnesium alloys or not. This work shows that a trace of beryllium also causes considerable grain coarsening in Mg-Zn, Mg-Ca, Mg-Ce and Mg-Nd alloys and hinders grain refinement of magnesium alloys by zirconium as well. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Banded defects are often found in high-pressure die castings. These bands can contain segregation, porosity, and/or tears, and changing casting conditions and alloy are known to change the position and make-up of the bands. Due to the complex, dynamic nature of the high-pressure die-casting (HPDC) process, it is very difficult to study the effect of individual parameters on band formation. In the work presented here, bands of segregation similar to those found in cold-chamber HPDC aluminum alloys were found in laboratory gravity die castings. Samples were cast with a range of fraction solids from 0 to 0.3 and the effect of die temperature and external solid fraction on segregation bands was investigated. The results are considered with reference to the theological properties of the filling semisolid metal and a formation mechanism for bands is proposed by considering flow past a solidifying immobile wall layer.
Resumo:
The effect of increasing levels of silicon on the microstructure and creep properties of high-pressure die-cast Mg-Al-Si (AS) alloys has been investigated. The morphology of the Mg2Si phase in die-cast AS alloys was found to be a function of the silicon content. The Mg2Si particles in castings with up to 1.14 wt pct Si have a Chinese script morphology. For AS21 alloys with silicon contents greater than 1.4 wt pet Si (greater than the alpha-Mg2Si binary eutectic point), some Mg2Si particles have a coarse blocky shape. Increasing the silicon content above the eutectic level results in an increase in the number of coarse faceted Mg2Si particles in the microstructure. Creep rates at 100 hours were found to decrease with increasing silicon content in AS-type alloys. The decrease in creep rate was most dramatic for silicon contents up to 1.1 wt pct. Further additions of silicon of up to 2.64 wt pct also resulted in significant decreases in creep rate.
Resumo:
The tensile deformation behavior of a range of supersaturated Mg-Al solid solutions and an as-cast magnesium alloy AM60 has been studied. The Mg-Al alloys were tested at room temperature while the alloy AM60 was tested in the temperature range 293-573 K. The differences in the deformation behavior of the alloys is discussed in terms of hardening and softening processes. In order to identify which processes were active, the stress dependence of the strain-hardening coefficient was assessed using Lukac and Balik's model of hardening and softening. The analysis indicates that hardening involves solid solution hardening and interaction with forest dislocations and non-dislocation obstacles such as second phase particles. Cross slip is not a significant recovery process in the temperature range 293-423 K. At temperatures between 473 and 523 K the analysis suggests that softening is controlled by cross slip and climb of dislocations. At temperatures above 523 K softening seems to be controlled by dynamic recrystallisation. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
In this work, the different adsorption properties of H and alkali metal atoms on the basal plane of graphite are studied and compared using a density functional method on the same model chemistry level. The results show that H prefers the on-top site while alkali metals favor the middle hollow site of graphite basal plane due to the unique electronic structures of H, alkali metals, and graphite. H has a higher electronegativity than carbon, preferring to form a covalent bond with C atoms, whereas alkaline metals have lower electronegativity, tending to adsorb on the highest electrostatic potential sites. During adsorption, there are more charges transferred from alkali metal to graphite than from H to graphite.
Resumo:
An aluminum-alloyed coating was applied onto the surface of magnesium alloy AZ91D. The coating formed in aluminium powder at 420 degrees C is rich in the beta (Mg17Al12) phase. Polarisation curve, AC impedance, salt immersion and salt spray were carried out to investigate the corrosion behaviour and assess the corrosion performance of the coated magnesium alloy. It was found that a coated AZ91D specimen was much more corrosion resistant and harder than an uncoated one. The improved corrosion resistance was mainly ascribed to the high volume fraction of beta phase in the coating. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
The thickness, chemical composition and microstructure of anodised coatings formed on magnesium alloy AZ91D at various anodising current densities were measured. It was found that all these parameters could be affected by anodising current density, and hence the coatings formed at different anodising current densities had different corrosion resistances. This suggests that the corrosion performance of an anodised coating could be improved if a properly designed current waveform is used for anodising. In addition, based on the experimental results, some physical, chemical and electrochemical reactions involved in the anodising process were proposed to explain the anodising behaviour in this paper. (c) 2005 Elsevier Ltd. All rights reserved.