Resumo:
Effective surface passivation of lead sulfide (PbS) nanocrystals (NCs) in an aqueous colloidal solution has been achieved following treatment with CdS precursors. The resultant photoluminescent emission displays two distinct components, one originating from the absorption band edge and the other from above the absorption band edge. We show that both of these components are strongly polarized but display distinctly different behaviours. The polarization arising from the band edge shows little dependence on the excitation energy while the polarization of the above-band-edge component is strongly dependent on the excitation energy. In addition, time-resolved polarization spectroscopy reveals that the above-band-edge polarization is restricted to the first couple of nanoseconds, while the band edge polarization is nearly constant over hundreds of nanoseconds. We recognize an incompatibility between the two different polarization behaviours, which enables us to identify two distinct types of surface-passivated PbS NC.
Investigation of the role of cadmium sulfide in the surface passivation of lead sulfide quantum dots
Resumo:
Surface passivation of PbS nanocrystals (NC), resulting in strong photoluminescence, can be achieved by the introduction of CdS precursors. The role of CdS in the surface passivation of PbS NCs is uncertain, as the crystalline structure of CdS and PbS are different, which should impede effective epitaxial overgrowth. Absorption spectroscopy is used to show that the CdS precursors strongly interact with the PbS NC surface. Electron microscopy reveals that the introduction of CdS precursors results in an increased particle size, consistent with overcoating. However, we also find the process to be highly non-uniform. Nevertheless, evidence for epitaxial growth is found, suggesting that effective surface passivation may be possible.
Resumo:
We report absolute values for the radiative relaxation quantum yield of synthetic eumelanin as a function of excitation energy. These values were determined by correcting for pump beam attenuation and emission reabsorption in both eumelanin samples and fluorescein standards over a large range of concentrations. Our results confirm that eumelanins are capable of dissipating >99.9% of absorbed UV and visible radiation through nonradiative means. Furthermore, we have found that the radiative quantum yield of synthetic eumelanin is excitation energy dependent. This observation is supported by corrected emission spectra, which also show a clear dependence of both peak position and peak width on excitation energy. Our findings indicate that photoluminescence emission in eumelanins is derived from ensembles of small chemically distinct oligomeric units that can be selectively pumped. This hypothesis lends support to the theory that the basic structural unit of eumelanin is oligomeric rather than heteropolymeric.
Resumo:
Quasi-birth-and-death (QBD) processes with infinite “phase spaces” can exhibit unusual and interesting behavior. One of the simplest examples of such a process is the two-node tandem Jackson network, with the “phase” giving the state of the first queue and the “level” giving the state of the second queue. In this paper, we undertake an extensive analysis of the properties of this QBD. In particular, we investigate the spectral properties of Neuts’s R-matrix and show that the decay rate of the stationary distribution of the “level” process is not always equal to the convergence norm of R. In fact, we show that we can obtain any decay rate from a certain range by controlling only the transition structure at level zero, which is independent of R. We also consider the sequence of tandem queues that is constructed by restricting the waiting room of the first queue to some finite capacity, and then allowing this capacity to increase to infinity. We show that the decay rates for the finite truncations converge to a value, which is not necessarily the decay rate in the infinite waiting room case. Finally, we show that the probability that the process hits level n before level 0 given that it starts in level 1 decays at a rate which is not necessarily the same as the decay rate for the stationary distribution.
Resumo:
The molecular mechanism of how insects recognize intruding microorganisms and parasites and distinguish them from own body structures is not well known. We explored evolutionary adaptations in an insect parasitoid host interaction to identify components that interfere with the recognition of foreign objects and cellular encapsulation. Because some parasitoids provide protection for the developing wasp in the absence of an overt suppression of the insect host defense, we analyzed the surface of eggs and symbiotic viruses for protective properties. Here we report on the molecular cloning of a 32-kDa protein (Crp32) that is one of the major protective components. It is produced in the calyx cells of the female wasp ovaries and attached to the surface of the egg and other particles including polydnaviruses. The recombinant protein confers protection to coated objects in a cellular encapsulation assay suggesting that a layer of Crp32 may prevent cellular encapsulation reactions by a local inactivation of the host defense system.
Resumo:
The aim of this work is to develop 3-acyl prodrugs of the potent analgesic morphine-6-sulfate (M6S). These are expected to have higher potency and/or exhibit longer duration of analgesic action than the parent compound. M6S and the prodrugs were synthesized, then purified either by recrystallization or by semi-preparative HPLC and the structures confirmed by mass spectrometry, IR spectrophotometry and by detailed 1- and 2-D NMR studies. The lipophilicities of the compounds were assessed by a combination of shake-flask, group contribution and HPLC retention methods. The octanol-buffer partition coefficient could only be obtained directly for 3-heptanoylmorphine-6-sulfate, using the shake-flask method. The partition coefficients (P) for the remaining prodrugs were estimated from known methylene group contributions. A good linear relationship between log P and the HPLC log capacity factors was demonstrated. Hydrolysis of the 3-acetyl prodrug, as a representative of the group, was found to occur relatively slowly in buffers (pH range 6.15-8.01), with a small buffer catalysis contribution. The rates of enzymatic hydrolysis of the 3-acyl group in 10% rat blood and in 10% rat brain homogenate were investigated. The prodrugs followed apparent first order hydrolysis kinetics, with a significantly faster hydrolysis rate found in 10% rat brain homogenate than in 10% rat blood for all compounds. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
We review the description of noise in electronic circuits in terms of electron transport. The Poisson process is used as a unifying principle. In recent years, much attention has been given to current noise in light-emitting diodes and laser diodes. In these devices, random events associated with electron transport are correlated with photon emission times, thus modifying both the current statistics and the statistics of the emitted light. We give a review of experiments in this area with special emphasis on the ability of such devices to produce subshot-noise currents and light beams. Finally we consider the noise properties of a class of mesoscopic devices based on the quantum tunnelling of an electron into and out of a bound state. We present a simple quantum model of this process which confirms that the current noise in such a device should be subshot-noise.
Resumo:
Activated carbon as catalyst support was treated with HCl, HNO3, and HF and the effects of acid treatments on the properties of the activated carbon support were studied by N-2 adsorption, mass titration, temperature-programmed desorption (TPD), and X-ray photoelectron spectrometry (XPS). Ni catalysts supported on untreated and treated activated carbons were prepared, characterized and tested for the reforming reaction of methane with carbon dioxide. It is found that acid treatment significantly changed the surface chemical properties and pore structure of the activated carbon. The surface area and pore volume of the carbon supports are generally enhanced upon acid treatment due to the removal of impurities present in the carbon. The adsorption capacity of Ni2+ on the carbon supports is also increased, and the increase can be closely correlated with the surface acidity. The impregnation of nickel salts decreases the surface area and pore volume of carbon supports both in micropores and mesopores. Acid treatment results in a more homogeneous distribution of the nickel salt in carbon. When the impregnated carbons are heated in inert atmosphere, there exists a redox reaction between nickel oxide and the carbon. Catalytic activity tests for methane reforming with carbon dioxide show that the activity of nickel catalysts based on the acid-treated carbon supports is closely related with the surface characteristics of catalysts. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
Free-piston-driven expansion tubes are capable of generating flaw conditions over a wide range of enthalpies ranging from orbital up to superorbital velocities. Initial optical measurements aimed at investigating the flow in such a facility are presented. Emission studies were used to identify impurities in the how and to investigate spectral regions that are accessible by optical techniques. At moderate enthalpies, it was found that significant radiation resulted from metallic contaminants. At high enthalpies, the spectrum consisted of a number of atomic lines together with a broadband background component indicative of the presence of electrons. The presence of this radiation may limit the applicability of optical techniques that require spectral regions free from the influence of atomic transitions or background radiation. Emission spectroscopy (through Stark broadened hydrogen lines) and two-wavelength holographic interferometry were used to measure the electron number density behind a bow shock on a blunt body at conditions where significant ionization was observed. They yielded average concentrations of (3 +/- 1) x 10(17) cm(-3) from the emission measurements and (3.8 +/- 0.6) x 10(17) cm(-3) from the interferometry.
Resumo:
Instantaneous outbursts in underground coal mines have occurred in at least 16 countries, involving both methane (CH4) and carbon dioxide (CO2). The precise mechanisms of an instantaneous outburst are still unresolved but must consider the effects of stress, gas content and physico-mechanical properties of the coal. Other factors such as mining methods (e.g., development heading into the coal seam) and geological features (e.g., coal seam disruptions from faulting) can combine to exacerbate the problem. Prediction techniques continue to be unreliable and unexpected outburst incidents resulting in fatalities are a major concern for underground coal operations. Gas content thresholds of 9 m(3)/t for CH4 and 6 m(3)/t for CO2 are used in the Sydney Basin, to indicate outburst-prone conditions, but are reviewed on an individual mine basis and in mixed as situations. Data on the sorption behaviour of Bowen Basin coals from Australia have provided an explanation for the conflicting results obtained by coal face desorption indices used for outburst-proneness assessment. A key factor appears to be different desorption rates displayed by banded coals, which is supported by both laboratory and mine-site investigations. Dull coal bands with high fusinite and semifusinite contents tend to display rapid desorption from solid coal, for a given pressure drop. The opposite is true for bright coal bands with high vitrinite contents and dull coal bands with high inertodetrinite contents. Consequently, when face samples of dull, fusinite-or semifusinite-rich coal of small particle size are taken for desorption testing, much gas has already escaped and low readings result. The converse applies for samples taken from coal bands with high vitrinite and/or inertodetrinite contents. In terms of outburst potential, it is the bright, vitrinite-rich and the dull, inertodetrinite-rich sections of a coal seam that appear to be more outburst-prone. This is due to the ability of the solid coal to retain gas, even after pressure reduction, creating a gas content gradient across the coal face sufficient to initiate an outburst. Once the particle size of the coal is reduced, rapid gas desorption can then take place. (C) 1998 Elsevier Science.
Resumo:
The Hubble Deep Field South (HDF-S) Hubble Space Telescope (HST) observations are expected to begin in 1998 October. We present a composite spectrum of the QSO in the HDF-S held covering UV/optical/near-IR wavelengths, obtained by combining data from the Australian National University 2.3 m telescope with STIS on the HST.(1) This intermediate-resolution spectrum covers the range 1600-10000 Angstrom and allows us to derive some basic information on the intervening absorption systems which will be important in planning future higher resolution studies of this QSO. The QSO J2233 - 606 coordinates are alpha = 22(h)33(m)37(s).6, delta = -60 degrees 33'29 (J2000), the magnitude is B = 17.5, and its redshift is z(em) = 2.238, derived by simultaneously fitting several emission lines. The spectral index is alpha = -0.7 +/- 0.1, measured between the Ly alpha and Mg II emission lines. Many absorption systems are present, including systems with metal lines redward of the Ly alpha emission line at z(abs) 2.204, 1.942, 1.870, 1.787 and a few very strong Ly alpha features at z(abs) = 2.077, 1.928, without similarly strong metal lines. There is a conspicuous Lyman limit (LL) absorption system that is most likely associated with the z(abs) = 1.942 system with a neutral hydrogen column density of N-HI = (3.1 +/- 1.0) x 10(17) cm(-2). There is some evidence for the presence of a second LL absorber just to the blue of the conspicuous system at z = 1.870. We have employed a new technique, based on an analysis of the shape of the observed spectrum in the region of the LL absorption, to explore the properties of the gas. We tentatively conclude that this system might have suitable characteristics for measuring the deuterium-to-hydrogen (D/H) ratio.
Resumo:
We present models for the optical functions of 11 metals used as mirrors and contacts in optoelectronic and optical devices: noble metals (Ag, Au, Cu), aluminum, beryllium, and transition metals (Cr, Ni, Pd, Pt, Ti, W). We used two simple phenomenological models, the Lorentz-Drude (LD) and the Brendel-Bormann (BB), to interpret both the free-electron and the interband parts of the dielectric response of metals in a wide spectral range from 0.1 to 6 eV. Our results show that the BE model was needed to describe appropriately the interband absorption in noble metals, while for Al, Be, and the transition metals both models exhibit good agreement with the experimental data. A comparison with measurements on surface normal structures confirmed that the reflectance and the phase change on reflection from semiconductor-metal interfaces (including the case of metallic multilayers) can be accurately described by use of the proposed models for the optical functions of metallic films and the matrix method for multilayer calculations. (C) 1998 Optical Society of America.
Resumo:
Naturally occurring clays and pillared clays are used as supports of nickel catalysts for the methane reforming reaction with carbon dioxide to synthesis gas. The structural and textural characteristics of the supports and catalysts are systematically examined by N-2 adsorption/desorption and X-ray diffraction (XRD) techniques. It is found that the pore structures and surface properties of supports greatly affect the catalytic activities of the catalysts prepared. The catalysts supported on the mesoporous clays or pillared clays are obviously superior to those on microporous supports because the mesoporous supports are highly thermal stable compared to the microporous ones. It is found that introducing lanthanum to the supports can improve the catalyst basicity and thus enhance the catalytic activities of these catalysts. Deactivation of catalysts prepared and factors influencing their stability are also discussed. (C) 1998 Academic Press.