This paper aims to describe the synthesis of the semi-crystalline and crystalline powder of lanthanum doped with zirconium titanate (65/35), LZT through Pechini method. The analysis done by Raman demonstrated that semi-crystalline phase at 550 degrees C and crystalline phase after 600 degrees C were formed. The XRD pattern shows the ZrTiO4 phase formation demonstrating that La substitutions into the lattice take place. The calcined powder at different temperatures shows a semi-crystalline phase presenting photoluminescence effect when processed at low temperatures. From 300 to 400 degrees C a broadband is observed at 563 nm and 568 nm, respectively. Defects creation such as: Zr3+ center dot Vo(center dot center dot) and Ti3+ - V-O(center dot center dot), Zr and Ti replaced by La with vacancy formation, impurities and imperfections contributed to the photoluminescence effect. However, the main emission is due to a reverse Ti4+ -> O2- or/and Zr4+ -> O2- transition that occur within a regular titanate or zirconate eight-fold coordination [BO8-delta], B = Zr4+, Ti4+. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

During a study of the LaF3-ZrF4 system, both La3Zr4F25 and alpha-LaZr3F15 compounds have been evidenced. Their crystal structures have been determined from single-crystal X-ray diffraction data. La3Zr4F25 crystallises in the cubic system with a= 12.384 Angstrom and I (4) over bar 3d space group (no. 220). Its crystal structure is built up of (ZrF6)(2-) octahedra and (LaF8)(5-) dodecahedra sharing corners. The low temperature form, alpha, of LaZr3F15 is orthorhombic (space group Pmmn, no. 59) with a = 15.721 Angstrom, b = 16.299 Angstrom, c= 8.438 Angstrom. Its structure is built of corner-sharing tricaped trigonal prisms surrounding the La3+ ions and both octahedra and monocapped trigonal prisms encompassing the Zr4+ ions. This structure is characterised by dynamically disordered (ZrF6)(2-) complex anions.The Eu3+ luminescence properties of these phases have been investigated and are discussed in relationship with their crystal structures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Upconversion fluorescence emission of Er3+/Yb3+-doped Bi2O3-Na2O-Nb2O5-GeO2 heavy metal glass samples excited at 1.06 mu m is experimentally investigated. The results reveal the existence of intense emission bands centered around 520, 545, and 655 nm. The germano-niobate based host glass presents high transparency in the region of 400-2700 nm, the capability of incorporating high dopant concentrations, high melting temperature, and large resistance to atmospheric moisture. The observed intensity of the green fluorescence emission, suggested that the niobium based host glass material plays an important role in the efficiency of the upconversion process. Emission lines centered at 425, 483, 503, 608, and 628 nm were also observed. (C) 1997 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The polymeric precursor method was used to synthesize lead zirconate titanate powder (PZT). The crystalline powder was then amorphized by a high-energy ball milling process during 120h. A strong photoluminescence emission was observed at room temperature for the amorphized PZT powder. The powders were characterized by XRD and the percentage of amorphous phase was calculated through Rietveld refinement. The microstructure for both phases was investigated by TEM. The optical gap was calculated through the Wood and Tauc method using the UV-Vis. data. Quantum mechanical calculations were carried out to give an interpretation of the photoluminescence in terms of electronic structure. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The IRSL and TL responses of three different feldspar crystals have been analysed. TL measurements were taken in the ultraviolet UV (290-370 nm) and the visible VIS (340-610 nm) regions of the spectrum. For the UV region and for a natural sample, peaks were observed at 283, 287 and 310 degrees C for grey, white and pink crystals, respectively. For samples irradiated after prior preheating, it was noted that TL peaks occurred at about 200 degrees C for all the samples; irradiation with high doses above 500 Gy induced the formation of one additional peak at 170 degrees C. The VIS region results were similar to those for the UV. ESR experiments have been developed to verify the influence of radiation and heat treatments on the centres and preliminary results showed great variation in the intensities of [TiO(4)](-), Al-O(-)-Al and Fe(3+) centres. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Erbium-activated silica-based planar waveguides were prepared by three different technological routes: RF-sputtering, sol-gel and ion exchange. Various parameters of preparation were varied in order to optimize the waveguides for operation in the NIR region. Particular attention was devoted to the minimization of the losses and the increase of the luminescence efficiency of the metastable I-4(13/2) state of the Er3+ ion. Waveguide properties were determined by m-line spectroscopy and loss measurements. Waveguide Raman and luminescence spectroscopy were used to obtain information about the structure of the prepared films and about the dynamical processes related to the luminescence of the Er3+ ions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The deactivation of the two lowest excited states of Ho3+ was investigated in Ho3+ singly doped and Ho3+, Pr3+-codoped fluoride (ZBLAN) glasses. We establish that 0.1-0.3 mol % Pr3+ can efficiently deactivate the first excited (I-5(7)) state of Ho3+ while causing a small reduction of similar to 40% of the initial population of the second excited (I-5(6)) state. The net effect introduced by the Pr3+ ion deactivation of the Ho3+ ion is the fast recovery of the ground state of Ho3+. The Burshstein model parameters relevant to the Ho3+-> Pr3+ energy transfer processes were determined using a least squares fit to the measured luminescence decay. The energy transfer upconversion and cross relaxation parameters for 1948, 1151, and 532 nm excitations of singly Ho3+-doped ZBLAN were determined. Using the energy transfer rate parameters we determine from the measured luminescence, a rate equation model for 650 nm excitation of Ho3+-doped and Ho3+, Pr3+-doped ZBLAN glasses was developed. The rate equations were solved numerically and the population inversion between the I-5(6) and the I-5(7) excited states of Ho3+ was calculated to examine the beneficial effects on the gain associated with Pr3+ codoping. (c) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hybrid Eu3+-doped silica-poliethyleneoxide (PEO) nanocomposites with covalent bonds between the inorganic (siloxane) and organic (PEO) phases have been obtained by sol-gel process. These materials are transparent, flexible and present high Eu3+ luminescence output. Their luminescence properties, local environment around europium ions and structure have been investigated as a function of europium content. EXAFS measurements indicate that the increase in Eu-doping induces a decrease in Eu3+ coordination number. An increase in symmetry degree around the metal ion is also observed for increasing Eu3+ concentration, while non radiative decay paths from the D-5(0) excited state become more important. SAXS results suggest the preferential interaction of europium ions with ether-type oxygens of the polymer chains. However, the existence of interactions between the cations and the carbonyl groups from urea bridges located at the siloxane-PEO interface can not be excluded.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent, flexible, and luminescent EU3+-doped siloxane-poly(ethylene glycol) (PEG) nanocomposites have been obtained by the sol-gel process. The inorganic (siloxane) and organic PEG phases are usually linked by weak bonds (hydrogen bonds or van der Waals forces), and small-angle X-ray scattering (SAXS) measurements suggest that the structure of these materials consists of fractal siloxane aggregates embedded in the PEG matrix. For low Eu3+ contents, n = 300 and n = 80, the aggregates are small and isolated and their fractal dimensions are 2.1 and 1.7, respectively. These values are close to those expected for gelation mechanisms consisting of reaction-limited cluster-cluster aggregation (RLCCA) and diffusion-limited cluster-cluster aggregation (DLCCA). For high Eu3+ content, SAYS results are consistent with a two-level structure: a primary level of siloxane aggregates and a second level, much larger, formed by the coalescence of the primary ones. The observed increase in the glass transition temperature for increasing Eu3+ content is consistent with the structural model derived from SAXS measurements. Extended X-ray absorption fine structure (EXAFS) and luminescence spectroscopy measurements indicate that under the experimental conditions utilized here Eu3+ ions do not strongly interact with the polymeric phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work reports on the study about the luminescence behavior of Eu3+-O2- associates in Sr2SiO4 doped with Eu3+, or simultaneously doped with Eu3+ and Zn2+ ions, where the Zn2+ doping ion acts as a charge compensating agent. Both Sr2SiO4:Eu3+ and Sr2SiO4:Eu3+,Zn2+ emission spectra show two types D-5(0)-->F-7(0) type transitions, one type related to Eu3+ in the Sr2+ Site, at 577 and 580 nm and the other one related to Eu3+-O2- associates, at 574 nm. Excitation spectra present two CT bands at 275 and 324 nm related to each emission center, respectively. Comparing the relative intensities between the emission spectra, the 0-->0 transition at 574 nm assigned to Eu3+-O2- associates in the Sr2SiO4:Eu3+ emission spectrum is much more intense than the same transition in the Sr2SiO4:Eu3+,Zn2+ emission spectrum. Moreover, in the Sr2SiO4:Eu3+ excitation spectrum, the intensity ratio between the CT band related to the Eu3+-O2- emission center and Eu3+ F-7-->L-5(6) transition is also larger than in the Sr2SiO4:Eu3+,Zn2+ one. Therefore, the presence of Zn2+ species provides an extra charge compensating mechanism, which decreases the formation of Eu3+-O2- associates. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Germanate glasses are of interest for optoelectronic applications because they combine high mechanical strength, high chemical durability and temperature stability with a large transmission window (400 to 4500 nm) and high refractive index (2.0). GeO2-PbO-Bi2O3 glasses doped with Y-b(3+) were fabricated by melting powders in a crucible and then pouring them in a brass mold. Energy Dispersive Spectroscopy showed that the glass composition has a high spatial uniformity and that the Yb concentration in the solid sample is proportional to the Yb concentration in the melt, what was confirmed by absorption measurements. Intense blue emission at 507 nm was observed, corresponding to half of the wavelength of the near infrared region (NIR) emission; besides, a decay lifetime of 0.25 ms was measured and this corresponds to half of the decay lifetime in the infrared region; these are very strong indications of the presence of blue cooperative luminescence. Larger targets have been produced to be sputtered, resulting in thin films for three dimensional (3D) display and waveguide applications. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

70SiO(2)-30HfO(2) mol% planar waveguides, doped with Er3+ with concentrations ranging from 0.3 to 2 mol% were prepared by sol-gel route, using dip-coating deposition on vitreous-SiO2 substrates. Infrared-to-visible upconversion emission, upon excitation at 980 nm, has been observed for all the samples. The upconversion results in green, red and blue emissions. The investigation of the upconversion dynamic as a function of the Er3+ concentration and excitation power, show that processes such as excited state absorption and energy transfer upconversion are effective. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Amorphous and crystalline powder of PLT phase was synthesized by using the Pechini method. Infrared (FTIR) analysis of the polymeric resin shows intense bands of organic materials from 250 to 1620 cm(-1). X-ray diffraction (XRD) and Raman spectra of calcined powder at different temperatures show amorphous phase at 450 degrees C/3 h, semi-crystalline phase at 550 degrees C/3 h and a crystalline phase at 800 degrees C/3 h. Luminescence effect was observed in amorphous powder calcined from 300 to 350 degrees/3 h with broad absorption peaks in 579 nm at 300 degrees C/3 h and 603 rum at 350 degrees C/3 h, respectively. The photoluminescence effect is attributed to emissions of Ti -> 0 directly from the oxygen 2p orbital (valence band) to the titanate 3d orbital (conduction bands). (c) 2004 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this work is to report on the luminescence properties of BaZnSiO4 activated by Eu3+ and Mn2+ ions. Doped and undoped powder samples were prepared by solid-state reaction starting from oxides and carbonates or Ba2SiO4:Eu3+ and Zn2SiO4:Mn2+ precursors. X-ray diffraction powder data, IR vibrational, and UV-vis luminescence spectroscopies were carried out. Results showed that doped and undoped samples from both types of precursors have the same structure and crystallize with a superstructure of hexagonal kalsilite. Vibrational spectroscopy has confirmed the formation of a silicate group, which outlines differences between products and silicate precursors. The observed luminescence assigned to Eu3+ and Mn2+ transitions covered most parts of the visible spectrum, an important requirement for phosphors in fluorescent low-pressure mercury vapor lamps.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of binary diphenylphosphinates with Eu3+ and Gd3+ were prepared. The compounds have the general formula Gd1-xEux(DPP)(3), where x ranges from 0 to 1. The spectroscopic measurements show interesting behavior. The intensity of the D-5(0) --> F-7(2) transitions decreases relative to D-5(0) --> F-7(1) With an increase in europium dispersion. Inside the temporal domain, the same decrease is observed with increasing delay after excitation. The lifetimes are also affected, which can be seen in the x = 1 compound, where the decay is a first-order process and lifetime values are 4.81 ms. In the binary compound, as an effect of dispersion, the lifetime of the D-5(0) level measured at the D-5(0) --> F-7(1) transition increases with europium dispersion, and the average along the series is 6.25 ms. The decay measured at the D-5(0) --> F-7(2) transitions reveals a second-order process with lifetimes ranging from 1.90 to 6.00 ms. (C) 2001 Elsevier B.V. B.V. All rights reserved.