891 resultados para rubber to rubber bonding
Resumo:
Because a greater research effort has been directed to analyzing the adhesive effectiveness of self etch primers to dentin, the aim of this study was to evaluate, by microtensile testing, the bond strength to enamel of a composite resin combined with a conventional adhesive system or with a self-etching primer adhesive, used according to its original prescription or used with previous acid etching. Thirty bovine teeth were divided into 3 groups with 10 teeth each (n= 10). In one of the groups, a self-etching primer (Clearfil SE Bond - Kuraray) was applied in accordance with the manufacturer's instructions and, in the other, it was applied after previous acid etching. In the third group, a conventional adhesive system (Scotchbond Multipurpose Plus - 3M-ESPE) was applied in accordance with the manufacturer's instructions. The results obtained by analysis of variance revealed significant differences between the adhesive systems (F = 22.31). The self-etching primer (Clearfil SE Bond) presented lower enamel bond strength values than the conventional adhesive system (Scotchbond Multipurpose Plus) (m = 39.70 ± 7.07 MPa) both when used according to the original prescription (m = 27.81 ± 2.64 MPa) and with previous acid etching (m = 25.08 ± 4.92 MPa).
Resumo:
The purpose of this study was to evaluate the influence of intrapulpal pressure simulation on the bonding effectiveness of etch & rinse and self-etch adhesives to dentin. Eighty sound human molars were distributed into eight groups, according to the permeability level of each sample, measured by an apparatus to assess hydraulic conductance (Lp). Thus, a similar mean permeability was achieved in each group. Three etch & rinse adhesives (Prime & Bond NT - PB, Single Bond -SB, and Excite - EX) and one self-etch system (Clearfil SE Bond - SE) were employed, varying the presence or absence of an intrapulpal pressure (IPP) simulation of 15 cmH2O. After adhesive and restorative procedures were carried out, the samples were stored in distilled water for 24 hours at 37°C, and taken for tensile bond strength (TBS) testing. Fracture analysis was performed using a light microscope at 40 X magnification. The data, obtained in MPa, were then submitted to the Kruskal-Wallis test ( a = 0.05). The results revealed that the TBS of SB and EX was significantly reduced under IPP simulation, differing from the TBS of PB and SE. Moreover, SE obtained the highest bond strength values in the presence of IPP. It could be concluded that IPP simulation can influence the bond strength of certain adhesive systems to dentin and should be considered when in vitro studies are conducted.
Resumo:
Neste trabalho estudou-se o desempenho mecânico e térmico de compostos de borracha natural (Hevea brasiliensis) de 4 diferentes clones (GT 1, IAN 873, PB 235 e RRIM 600) cultivados no Estado de São Paulo, assim como de uma mistura destes clones e de uma borracha comercial, GEB-1. Estas borrachas foram formuladas e vulcanizadas com tempos de 5, 7 e 9 minutos. A caracterização foi realizada por calorimetria exploratória diferencial, termogravimetria, ensaios de resistência à tração, análise dinâmico-mecânica, medidas de dureza Shore A, microscopia eletrônica de varredura e espectroscopia na região do infravermelho. Os resultados permitiram concluir que o tempo de vulcanização e o tipo de clone não influenciaram na temperatura de transição vítrea (Tg) dos compostos. Os valores de Tg obtidos por DMA foram de cerca de -62 °C, e os resultados ensaios de dureza apresentaram valores próximos de 60 para todos os compostos estudados. Os ensaios de resistência à tração mostraram que o melhor desempenho mecânico foi obtido pelo clone RRIM 600. De acordo com os resultados obtidos neste trabalho, todos os clones atingiram as propriedades reportadas na literatura, podendo ser utilizados, em princípio, nas indústrias de artefatos de borracha separadamente ou na forma de mistura.
Resumo:
Background: Structural myocardial abnormalities have been extensively documented in hypothyroidism. Experimental studies in animal models have also shown involvement of thyroid hormones in gene expression of myocardial collagen. This study was planned to investigate the ability of ultrasonic tissue characterization, as evaluated by integrated backscatter (IBS), to early identify myocardial involvement in thyroid dysfunction. Patients and Methods: We studied 15 patients with hyperthyroidism (HYPER), 8 patients with hypothyroidism (HYPO), 14 patients with subclinical hypothyroidism (SCH) and 19 normal (N) subjects, who had normal LV systolic function. After treatment, 10 HYPER, 6 HYPO, and 8 SCH patients were reevaluated. IBS images were obtained and analyzed in parasternal short axis (papillary muscle level) view, at left ventricular (LV) posterior wall. The following IBS variables were analyzed: 1) the corrected coefficient (CC) of IBS, obtained by dividing IBS intensity by IBS intensity measured in a rubber phantom, using the same equipment adjustments, at the same depth; 2) cardiac cyclic variation (CV) of IBS - peak-to-peak difference between maximal and minimal values of IBS during cardiac cycle; 3) cardiac cyclic variation index (CVI) of IBS - percentual relationship between the cyclic variation (CV) and the mean value of IBS intensity. Results: CC of IBS was significantly larger (p < 0.05) in HYPER (1.57 +/- 0.6) and HYPO (1.53 +/- 0.3) as compared to SCH (1.32 +/- 0.3) or N (1.15 +/- 0.27). The CV (dB) (HYPO: 7.5 +/- 2.4; SCH: 8.2 +/- 3.1; HYPER: 8.2 +/- 2.0) and the CVI (HYPO: 35.6 +/- 19.7%; SCH: 34.7 +/- 17.5%; HYPER: 37.8 +/- 11.6%) were not significantly different in patients with thyroid dysfunction as compared to N (7.0 +/- 2.0 and 44.5 +/- 15.1%). Conclusions: CC of IBS was able to differentiate cardiac involvement in patients with overt HYPO and HYPER who had normal LV systolic function. These early myocardial structural abnormalities were partially reversed by drug therapy in HYPER group. On the other hand, although mean IBS intensity tended to be slightly larger in patients with SCH as compared to N, this difference was not statistical significant.
Resumo:
Background: The use of laser irradiation for dental surface treatment may increase tooth-composite bond strength. Its use on bleached teeth may decrease the waiting time between bleaching and restorative procedures. Objective: This study aimed to evaluate the bond strength between a composite resin and bovine enamel bleached with 35% hydrogen peroxide and etched with Er:YAG laser. Materials and Methods: Thirty bovine teeth were randomly divided into six groups (n = 5): G1, unbleached and restored 24 h after storage in artificial saliva, etching with 35% phosphoric acid (PA) (control); G2, unbleached and restored 24 h after storage in artificial saliva, etching with Er:YAG laser and 35% PA; G3, bleached and restored immediately afterward, etching with 35% PA; G4, bleached and restored 24 h after bleaching, etching with 35% PA; G5, bleached and restored immediately afterward, etching with Er:YAG and 35% PA laser; G6, bleached and restored 24 h after bleaching, etching with Er:YAG laser and 35% PA. Bond strength was quantitatively evaluated by microtensile test (1.0 mm/min). Data were submitted to statistical analysis using ANOVA and Tukey tests (alpha - 0.05). Results: Bond strength values (MPa) were G1, 26.17 +/- 4.44; G2, 28.87 +/- 3.94; G3, 17.25 +/- 4.58; G4, 21.93 +/- 5.02; G5, 16.69 +/- 2.31; and G6, 29.06 +/- 8.31. There was no statistically significant difference among groups G1, G2, and G6 (p - 0.119), which presented higher bond strength than group G4, followed by groups G3 and G5. Conclusion: Er:YAG irradiation of bleached surfaces may favor bonding procedures when performed 24 h after bleaching.
Resumo:
Objective: This in vitro study evaluated the influence of the surface pretreatment of a feldspathic ceramic on the shear bond strength of two different resin cements. Background Data: Although several conventional surface treatments have been used on feldspathic ceramic, few studies have investigated the effects of an alternative surface treatment, the association of aluminum oxide sandblasting with Nd:YAG and Er:YAG lasers. Methods: Sixty samples made of a feldspathic ceramic were divided into three groups (n = 20) and treated with (1) controlled-air abrasion with Al(2)O(3) + 10% hydrofluoric acid (HF), (2) Al(2)O(3) + Er:YAG laser, and (3) Al(2)O(3) + Nd:YAG laser. Afterward, silane (Dentsply) was applied on each treated surface. Each of the three main groups was divided into two subgroups (n = 10), where a different resin cement was employed for each subgroup. It was built a cylinder with resin cement (RelyX Arc) in subgroup (A) and with self-adhesive cement (RelyX U100) in subgroup (B). After 24 h at 37 degrees C, the prepared specimens were submitted to shear bond strength test and stereoscopic evaluation to determine the type of failure. Results: Bond strength mean values were not statistically significant for the surface treatment methods or resin cements. Conclusion: The null surface treatment proposed with aluminum oxide sandblasting associated with the Er:YAG or Nd:YAG laser and using cementation with self-adhesive cement can be an alternative bonding technique for feldspathic ceramic, since it was as effective as the conventional treatment with aluminum oxide sandblasting and hydrofluoric acid using the conventional resin cement.
Resumo:
SETTING: Thirty-six priority cities in Sao Paulo State, Brazil, with a high incidence of tuberculosis (TB) cases, deaths and treatment default. OBJECTIVE: To identify the perspectives of city TB control coordinators regarding the most important components of adherence strategies adopted by health care teams to ensure patient adherence in 36 priority cities in the State of Sao Paulo, Brazil. DESIGN: Qualitative research with semi-structured interviews conducted with the coordinators of the National TB Control Programme involved in the management of TB treatment services in the public sector. RESULTS: The main issues thought to influence adherence to directly observed treatment (DOT) by coordinators include incentives and benefits delivered to patients, patient-health care worker bonding and comprehensive care, the encouragement given by others to follow treatment (family, neighbours and health professionals), and help provided by health professionals for patients to recover their self-esteem. CONCLUSION: The main aspects mentioned by city TB control coordinators regarding patient adherence to treatment and to DOT in Sao Paulo are improvements in communications, relationships based on trust, a humane approach and including the patients in the decision-making process concerning their health.
Resumo:
Urban solid residues are constituted of food remaining, grass leaves, fruit peelings, paper, cardboard, rubber, plastic, etc. The organic fraction formed represents about 50% during the decomposition yields biogas and leachate, which are sources of pollution. Residue samples were collected from the landfill in different and cells from several ages and the corresponding leachate, both after treatments, were submitted to thermal analysis. Kinetic parameters were determined using Flynn-Wall-Ozawa method. The linear relation between the two kinetic parameters (ln A and E) was verified for organic residue urban`s samples, but not for leachate`s sample. The occurred difference can be attributed to the constituents present in leachate.
Resumo:
The high velocity oxygen fuel (HVOF) thermal spray process produces highly wear and/or corrosion resistant coatings. Tungsten carbide with a metallic binder is often used for this purpose. In this work, tungsten carbide coatings containing cobalt or nickel binder were produced by HVOF and characterised by optical and electron microscopy, hardness and a dry sand/rubber wheel abrasion test. The HVOF process produced dense coatings with low porosity levels and high hardness. The wear resistance of the specimens, which were surface treated, increased as the roughness percentage decreased. Tungsten carbide nickel based coating yielded the best wear resistance in the as sprayed condition. However, the wear rate and wear of the two coatings converged to the same values as the number of revolutions increased. Wear behaviour in the ground condition was similar, although the tungsten carbide cobalt based coating yielded better performance with increasing distance travelled during the wear test.
Resumo:
This paper presents an analytical method for analyzing trusses with severe geometrically nonlinear behavior. The main objective is to find analytical solutions for trusses with different axial forces in the bars. The methodology is based on truss kinematics, elastic constitutive laws and equilibrium of nodal forces. The proposed formulation can be applied to hyper elastic materials, such as rubber and elastic foams. A Von Mises truss with two bars made by different materials is analyzed to show the accuracy of this methodology.
Resumo:
The effects of different tempering temperatures (300-600 degrees C) on abrasive wear resistance of mottled cast iron were studied. Abrasive wear tests were carried out using the rubber-wheel test on quartz sand and the pin test on Al(2)O(3) abrasive cloths. The retained austenite content of the matrix was determined by X-ray diffraction. The wear surface of the specimens was examined by scanning electron microscopy for identifying the wear micromechanism. Bulk hardness and matrix hardness before and after the tests were measured. The results showed that in the two-body (pin-on-disc test) system, the main wear mechanism was microcutting and high matrix hardening was presented. The wear rates presented higher correlation with the retained austenite than with the bulk and matrix hardness. In the three-body system (sand-rubber wheel), the wear surfaces presented indentations due to abrasive rolling. The wear rates had better correlation with both the bulk and matrix hardness (before and after the wear test) than with the retained austenite content. There are two groups of results, high and low wear rates corresponding to each tribosystem, two-body abrasive wear and three-body abrasive wear, respectively. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Coatings based on NiCrAlC intermetallic based alloy were applied on AISI 316L stainless steel substrates using a high velocity oxygen fuel torch. The influence of the spray parameters on friction and abrasive wear resistance were investigated using an instrumented rubber wheel abrasion test, able to measure the friction forces. The corrosion behaviour of the coatings were studied with electrochemical techniques and compared with the corrosion resistance of the substrate material. Specimens prepared using lower O(2)/C(3)H(8) ratios showed smaller porosity values. The abrasion wear rate of the NiCrAlC coatings was much smaller than that described in the literature for bulk as cast materials with similar composition and one order of magnitude higher than bulk cast and heat treated (aged) NiCrAlC alloy. All coatings showed higher corrosion resistance than the AISI 316L substrate in HCl (5%) aqueous solution at 40 degrees C.
Resumo:
Poly(3-hydroxybutyrate) (PHB) is a very promising biopolymer. In order to improve its processability and decrease its brittleness, PHB/elastomer blends can be prepared. In the work reported, the effect of the addition of a rubbery phase, i.e. ethylene - propylene-diene terpolymer (EPDM) or poly(vinyl butyral) (PVB), on the properties of PHB was studied. The effects of rubber type and of changing the PHB/elastomer blend processing method on the crystallinity and physical properties of the blends were also investigated. For blends based on PHB, the main role of EPDM is its nucleating effect evidenced by a decrease of crystallization temperature and an increase of crystallinity with increasing EPDM content regardless of the processing route. While EPDM has a weak effect on PHB glass transition temperature, PVB induces a marked decrease of this temperature thank to its plasticizer that swells the PHB amorphous phase. A promising solution to improve the mechanical properties of PHB seems to be the melt-processing of PHB with both plasticizer and EPDM. In fact, the plasticizer is more efficient than the elastomer in decreasing the PHB glass transition temperature and, because of the nucleating effect of EPDM, the decrease of the PHB modulus due to the plasticizer can be counterbalanced. (C) 2010 Society of Chemical Industry
Resumo:
Polyurethane composites reinforced with curaua fiber at 5, 10 and 20% mass/mass proportions were prepared by using the conventional melt-mixing method. The influence of curaua fibers on the thermal behavior and polymer cohesiveness in polyurethane matrix was evaluated by dynamic mechanical thermal analysis (DMTA) and by differential scanning calorimetry (DSC). This specific interaction between the fibers and the hard segment domain was influenced by the behavior of the storage modulus E` and the loss modulus EaEuro(3) curves. The polyurethane PU80 is much stiffer and resistant than the other composites at low temperatures up to 70A degrees C. All samples were thermoplastic and presented a rubbery plateau over a wide temperature range above the glass transition temperature and a thermoplastic flow around 170A degrees C.
Resumo:
The radiolysis of nitrile rubbers with different acrylonitrile/butadiene composition and the homopolymers, poly(butadiene) (PBD) and poly(acrylonitrile) (PAN) has been investigated and compared with the photolysis of the same polymers. A significantly different mechanism of degradation was found for the two types of radiation. The results obtained by ESR, FTIR and measurements of soluble fractions of irradiated samples, indicated that the acrylonitrile units of the nitrile rubbers are more sensitive units to gamma-radiation, with the effects of irradiation increasing with the acrylonitrile content. The reactions observed were consumption of double bonds, crosslinking, and cyclization with the formation of conjugated double bonds. No chain-scission reactions were detected. In contrast to gamma-irradiation, the effects of photolysis were centred at the butadiene units, and increases in the acrylonitrile content resulted in a proportional decrease in the sensitivity of the copolymers. Crosslinking and chain scission were identified as the main effects of photolysis of NBR rubbers. (C) 1999 Society of Chemical Industry.