926 resultados para powder ceramic
Resumo:
In this study, the physicochemical characteristics of calcium phosphate based bioactive ceramics of different compositions and blends presenting similar micro/nanoporosity and micrometer scale surface texture were characterized and evaluated in an in vivo model. Prior to the animal experiment, the porosity, surface area, particle size distribution, phase quantification, and dissolution of the materials tested were evaluated. The bone regenerative properties of the materials were evaluated using a rabbit calvaria model. After 2, 4, and 8 weeks, the animals were sacrificed and all samples were subjected to histologic observation and histomorphometric analysis. The material characterization showed that all materials tested presented variation in particle size, porosity and composition with different degrees of HA/TCP/lower stoichiometry phase ratios. Histologically, the calvarial defects presented temporal bone filling suggesting that all material groups were biocompatible and osteoconductive. Among the different materials tested, there were significant differences found in the amount of bone formation as a function of time. At 8 weeks, the micro/nanoporous material presenting similar to 55,TCP:45%,HA composition ratio presented higher amounts of new bone regeneration relative to other blends and a decrease in the amount of soft tissue infiltration. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Dense SnO2-based ceramics (relative density >95%) have been obtained by natural sintering at a moderate temperature (less than or equal to 1300 degrees C) with the help of a small amount of manganese, Further thermal treatments above 1500 degrees C result in grain growth and transport of manganese toward the sample surface. If the ceramic is embedded inside alumina powder, the diffusion of Mn out of the sample and into alumina during such heat treatments leads to a manganese-free body (<40 ppm) which is translucent. The transmission in the visible region depends on sample thickness; 61% was achieved for a 0.05 mm thick sample.
Resumo:
Purpose: This study aimed to investigate the influence of ceramic thickness and shade on the Knoop hardness and dynamic elastic modulus of a dual-cured resin cement.Materials and Methods: Six ceramic shades (Bleaching, A1, A2, A3, A3.5, B3) and two ceramic thicknesses (1 mm, 3 mm) were evaluated. Disk specimens (diameter: 7 mm; thickness: 2 mm) of the resin cement were light cured under a ceramic block. Light-cured specimens without the ceramic block at distances of 1 and 3mm were also produced. The Knoop hardness number (KHN), density, and dynamic Young's moduli were determined. Statistical analysis was conducted using ANOVA and a Tukey B rank order test (p = 0.05).Results: The bleaching 1-mm-thick group exhibited significantly higher dynamic Young's modulus. Lower dynamic Young's moduli were observed for the 3-mm-thick ceramic groups compared to bleaching 3-mm-thick group, and no difference was found among the other 3-mm groups. For the KHN, when A3.5 3-mm-thick was used, the KHN was significantly lower than bleaching and A1 1-mm-thick ceramic; however, no difference was exhibited between the thicknesses of the same shade.Conclusions: The dual-cured resin cement studied irradiated through the 1-mm-thick ceramic with the lightest shade (bleaching ceramic) exhibited a better elastic modulus, and there was no effect in KHN of the resin cement when light cured under different ceramic shades and thicknesses (1 and 3 mm), except when the A3.5 3-mm-thick ceramic was used.Clinical Significance: Variolink II irradiated through ceramic with the lowest chroma exhibited the highest elastic modulus; therefore, the light activation method might not be the same for all clinical situations.
Resumo:
The fracture of porcelain structures have been related in either natural dentition or implant-supported restorations. Techniques using a composite resin or indirect methods can be used. This article presents a porcelain fracture on implant-supported metal-ceramic restoration. IPS Empress e.max laminate veneer restoration was used to repair the fracture. With this technique, it was possible to restore aesthetics and function, combined with low cost and patient satisfaction.
Resumo:
Purpose: To evaluate the survival rate, success rate, load to fracture, and finite element analysis (FEA) of maxillary central incisors and canines restored using ceramic veneers and varying preparation designs.Methods and Materials: Thirty human maxillary central incisors and 30 canines were allocated to the following four groups (n=15) based on the preparation design and type of tooth: Gr1 = central incisor with a conservative preparation; Gr2 = central incisor with a conventional preparation with palatal chamfer; Gr3 = canine with a conservative preparation; Gr4 = canine with a conventional preparation with palatal chamfer. Ceramic veneers (lithium disilicate) were fabricated and adhesively cemented (Variolink Veneer). The specimens were subjected to 4 x 106 mechanical cycles and evaluated at every 500,000 cycles to detect failures. Specimens that survived were subjected to a load to fracture test. Bidimensional models were modeled (Rhinoceros 4.0) and evaluated (MSC.Patrans 2005r2 and MSC.Marc 2005r2) on the basis of their maximum principal stress (MPS) values. Survival rate values were analyzed using the Kaplan-Meier test (alpha = 0.05) and load to fracture values were analyzed using the Student t-test (alpha = 0.05).Results: All groups showed 100% survival rates. The Student t-test did not show any difference between the groups for load to fracture. FEA showed higher MPS values in the specimens restored using veneers with conventional preparation design with palatal chamfer.Conclusion: Preparation design did not affect the fracture load of canines and central incisors, but the veneers with conventional preparation design with palatal chamfer exhibited a tendency to generate higher MPS values.
Resumo:
The search for new methods of manufacture of glass-ceramics with controlled porosity and permeability is interesting of the industrial and commercial point of view, and a challenge of great complexity. Porous glass-ceramics produced by sintering and crystallization of glasses can find applications, for example, as filters, materials with bactericidal properties, bio-implants, as catalytic and enzymes supports, among others. An alternative and low cost method of ceramic manufacture reaching different levels of porosity, for diverse purposes, is the conformation assisted by addition of starch, known as consolidation with starch. The objective of this project is to study the process of conformation with starch for making porous glass-ceramics from a commercial glass in the system Na2O-CaO-SiO2, whose kinetics of sintering by viscous flow and surface crystallization are known. The method of conformation with starches is innovative for glass-ceramics and its development opens the way for obtaining a new class of materials. We found a possible route for the production of porous compacts of glass particles, from the powder preparation to the removal of starch. It was observed that a glass powder obtained by dry milling in a ball mill with alumina balls for 24 h, afterwards mixed with water in an eccentric ball mill for 2 h, without the addition of a deflocculant, and subsequently mixed with starch also in an eccentric ball mill for 5 min resulted in slurries stable against sedimentation
Resumo:
This work presents a proposal to create a Polo Ceramic Craft in the town of Indiana - SP, through the potter’s organization in a cooperative that will coordinate activities to add value to ceramic pieces. To achieve this, two things are essential: improving the ceramic body and improve the properties of the ceramic material. For the first action it’s necessary to create a Central Mass Production of Ceramics, to provide raw materials and homogeneous composition that results in differentiated ceramic after burning process (sintering). To this end, we propose the incorporation of additives (which act as fluxes) to the clay material. These additives can be mineral such as feldspar and nefelinas or leavings, such as glass powder obtained from disposable containers. For the second action is necessary to acquire an oven, electric or gas, it reaches higher temperatures (around 1200 ° C). The presence of the additive and burning at higher temperatures will enable better production of sintered ceramic material with less porosity and water absorption and higher mechanical strength, and pieces vitrified and glazed, allowing them to assign a higher value. For the production of these materials (thinner walls) requires a smaller volume of clayey raw materials. Besides benefiting the ceramic pieces, the proposed changes reduce the environmental impact caused by burning wood, since it will be replaced by natural gas (or electricity), and even will reduce the disposal of glass containers in the environment by recycling and incorporating this material in the clay. From a social standpoint, the cooperative is crucial to the viability of the proposed project, to coordinate activities and commercial production, which will result in better wages and profits for companies and consequently for the city and its population
Resumo:
The ceramic pigments are colored inorganic substances that during the process of dispersion in the ceramic glazes and subsequent calcination, are stable against physical and chemical attack. Therefore, they are crystalline compounds applied in the ceramic industry for coloring vitreous base. In this study, the Pechini method was used for obtaining the pigment CuCr2O4 with heat treatment at the temperatures of 800, 900 and 1000 ° C. The powder pigments were characterized on their structural, morphological and colorimetric aspects. The thermal analysis conducted on an amorphous precursor in a TG / DTA indicates the weight loss in the entire temperature range investigated, with characteristic exothermic peak of the elimination of the organic composition of the precursor around 300°C. The development of the crystalline phases were investigated by XRD, using a diffractometer with Cu Ka radiation and graphite monochromator, where it was observed the presence of crystalline phases corresponding to Cr2O3 and CuCr2O4.The measurements of the specific surface area of the powders pigments were carried out in an equipment Micromeritcs, model ASAP 2000, using N2 as gas of adsorption/desorption. The colorimetric measurements of the pigments were made in a colorimeter Gretac Macbeth Color-eye spectrophotometer 2180 / 2180UV in CIELAB standards. Based on the obtained results, it can be verified the thermal stability of the powder pigments of green coloration, which enables it as an alternative to the materials currently used in the manufacture of ceramic tiles.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Low crystalline PZT powder samples were successfully synthesized using polymeric precursor method and slow decomposition steps. The polymeric resin precursor was thermal treated in a muffle type oven varying the temperature from 250 °C to 700 °C and the time from 3 to 24 hours in order to investigate the order/disorder mechanism toward the amorphous powders. Powder samples with low crystalline phases were obtained at lower temperatures and long time of thermal treatment, demonstrating a kinetic dependence for organic removal and a thermodynamic barrier for crystallization processes. Through XRD and FTIR spectroscopy characterizations the long time thermal treated samples showed to be composed of the solid solution of metal oxides in absent of organic matter, originating broad XRD peaks profiles and no carbonaceous bands in FTIR spectra. A Photoluminescence characterization showed that the peak emission is higher for disordered and homogeneous phases, which only can be reached through the long time of thermal treatment.
Resumo:
The photon statistics of the random laser emission of a Rhodamine B doped di-ureasil hybrid powder is investigated to evaluate its degree of coherence above threshold. Although the random laser emission is a weighted average of spatially uncorrelated radiation emitted at different positions in the sample, a spatial coherence control was achieved due to an improved detection configuration based on spatial filtering. By using this experimental approach, which also allows for fine mode discrimination and timeresolved analysis of uncoupled modes from mode competition, an area not larger than the expected coherence size of the random laser is probed. Once the spectral and temporal behavior of nonoverlapping modes is characterized, an assessment of the photon-number probability distribution and the resulting second-order correlation coefficient as a function of time delay and wavelength was performed. The outcome of our single photon counting measurements revealed a high degree of temporal coherence at the time of maximum pump intensity and at wavelengths around the Rhodamine B gain maximum.
Resumo:
The aim of the present study was to evaluate the efficacy of peroxidase immobilized on corncob powder for the discoloration of dye. Peroxidase was extracted from soybean seed coat, followed by amination of the surface of the tertiary structure. The aminated peroxidase was immobilized on highly activated corncob powder and employed for the discoloration of bromophenol blue. Amination was performed with 10 or 50 mmol.L-1 carbodiimide and 1 mol.L-1 ethylenediamine. The amount of protein in the extract was 0.235 ± 0.011 mg.mL-1 and specific peroxidase activity was 86.06 ± 1.52 µmol min-1 . mg-1, using 1 mmol.L-1 ABTS as substrate. Ten mmol.L-1 and 50 mmol.L-1 aminated peroxidase retained 88 and 100% of the initial activity. Following covalent immobilization on a corncob powder-glyoxyl support, 10 and 50 mmol.L-1 aminated peroxidase retained 74 and 86% of activity, respectively. Derivatives were used for the discoloration of 0.02 mmol.L-1 bromophenol blue solution. After 30 min, 93 and 89% discoloration was achieved with the 10 mmol.L-1 and 50 mmol.L-1 derivatives, respectively. Moreover, these derivatives retained 60% of the catalytic properties when used three times. Peroxidase extracted from soybean seed coat immobilized on a low-cost corncob powder support exhibited improved thermal stability.
Resumo:
To evaluate the effect of grinding and airborne-particle abrasion on the biaxial flexural strength (BFS) and phase transformation of a Y-TZP ceramic, and examine whether sintering the veneering porcelain renders the previous heat treatment recommended by the manufacturer unnecessary. Materials and Methods: Lava zirconia specimens (N = 108) were obtained with the following dimensions: 14.0 mm diameter × 1.3 mm thickness (n = 36) and 14.0 mm × 1.6 mm (n = 72). The thicker specimens were ground with diamond burs under irrigation and received (heat-treated groups) or not (non-heat-treated groups) a heat treatment (1000°C for 30 min) prior to the four firing cycles applied to simulate the sintering of the veneering porcelain. All specimens were air abraded as follows (n = 12): 1) 30-μm silica-modified Al2O3 particles (Rocatec Soft); 2) 110-μm silica-modified Al2O3 particles (Rocatec Plus); and 3) 120-μm Al2O3 particles, followed by Rocatec Plus. Three specimens of each group were analyzed by x-ray diffraction (XRD) to assess the monoclinic phase content (%). The BFS test was performed in a mechanical testing machine (Instron 8874). Data (MPa) were analyzed by two-way ANOVA (grinding × airborne-particle abrasion and heat treatment × airborne-particle abrasion) and Tukey's post-hoc test (α = 0.05). The strength reliability was analyzed using the Weibull distribution. Results: Grinding significantly decreased the BFS of the non-heat-treated groups (p < 0.01). Within the ground groups, the previous heat treatment did not influence the BFS (p > 0.05). Air abrasion only influenced the BFS of the ground/heat-treated groups (p < 0.01). For the non-heat-treated groups, the grinding did not decrease the Weibull modulus (m), but it did decrease the characteristic strength (σ0). For Rocatec Soft and 120-μm Al2O3 particles + Rocatec Plus, the heat-treated groups presented lower m and higher σ0 than the ground/non-heat-treated groups. The independent variables did not seem to influence phase transformation. Air-abraded surfaces presented higher monoclinic zirconia content than the as-sintered and ground surfaces, which exhibited similar content. Conclusion: Even under irrigation, grinding compromised the Y-TZP ceramic strength. The sintering of the veneering porcelain rendered the previous heat treatment recommended by the manufacturer unnecessary. Airborneparticle abrasion influenced the strength of heat-treated zirconia.