1000 resultados para Tucano, Bacia do (BA)


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dielectric properties of (Ba, Sr)TiO3 films were found to be remarkably sensitive to the postannealing treatment atmosphere. This study demonstrates that postannealing in an oxygen atmosphere increases the dielectric relaxation phenomenon and that postannealing in a nitrogen atmosphere produces a slight dielectric relaxation. Such dependence of the dielectric relaxation was related both to oxygen vacancies and to the presence of negatively charged oxygen, trapped at the grain boundary and/or at the electrode/dielectric film interface. (C) 2000 American Institute of Physics. [S0003-6951(00)00817-2].

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Photoluminescence (PL) properties at room temperature of disordered Ba0.50Sr0.50(Ti0.80Sn0.20)O-3 (BST:Sn) thin films were obtained by the polymeric precursor method. X-ray diffraction data and corresponding PL properties have been measured using the 488 nm line of an argon ion laser. The PL spectra of the film annealed at 350 degrees C for 21 h are stronger than those of the film annealed at 350 degrees C for 28 h, indicating a disorganized structure. The energy band gaps of the crystalline and amorphous BST:Sn thin films were 3.35 and 2.25 eV, respectively. The doped BST thin films also tend to a cubic structure, resulting from TiO6 deformations. (c) 2006 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

BaxSr1-xTiO3 (x = 0.6) (BST) thin films were successfully prepared on a Pt(111)/TiO2/SiO2/Si(100) substrate by spin coating, using the polymeric precursor method. BST films with a perovskite single phase were obtained after heat treatment at 700 degrees C. The multilayer BST thin films had a granular structure will a grain size of approximately 60 nm. A 480-nm-thick film was obtained by carrying out five cycles of the spin-coating/heating process. Scanning electron microscopy and atomic force microscopy analyses showed that the thin films had a smooth, dense, crack-free surface with low surface roughness (3.6 nm). At room temperature and at a frequency of 100 kHz, the dielectric constant and the dissipation factor were, respectively, 748 and 0.042. The high dielectric constant value was due to the high microstructural quality and chemical homogeneity of the thin films obtained by the polymeric precursor method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High-quality ABO(3)/LaNiO3 (A = Ph, Ca, Ba; B = Ti, Zr) hetero structures have been grown on LaAlO3 (1 0 0) substrate by the chemical solution deposition method and crystallized by a microwave oven technique. The structural, morphological and electric properties were characterized by means of X-ray diffraction (XRD), atomic force microscope (AFM), and dielectric and ferroelectric measurements. XRD patterns revealed single-phase polycrystalline and oriented thin films whose feature depends on the composition of the films. The AFM surface morphologies showed a smooth and crack-free surface with the average grain size ranging from 116 to 300 nm for both LaNiO3 electrode and the ferroelectric films. Dielectric measurements on these samples revealed dielectric constants as high as 1800 at frequency of 100 KHz. Such results showed that the combination of the chemical solution method with the microwave process provides a promising technique to grow high-quality thin films with good dielectric and ferroelectric properties. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Some Upper Permian conchostracans from the Rio do Rasto Formation (Parana Basin, South Brazil) have very characteristic recurved growth lines at the dorsal margin. All previously described specimens were classified as Palaeolimnadiopsis subalata (Reed) Raymond. However, a re-analysis of these fossils and of additional recently- collected specimens demonstrated that not all can be included in a single species, nor only in the Family Palaeolimnadiopseidae. According to their shape and the size of the umbo, they are classified into three species. The sub-elliptic carapaces with small anterior umbo are maintained in Palaeolimnadiopsis subalata (Reed, 1929) Raymond, 1946. The sub-circular carapaces with small sub-central umbo correspond to the new species Palaeolimnadiopsis riorastensis. The small size of the umbo is a character of the Family Palaeolimnadiopseidae. The small elliptic valves with large anterior umbo are assigned to the new species Falsisca brasiliensis of the Family Perilimnadiidae, which is characterized by large umbos. Palaeolimnadiopsis has a wide chronostratigraphic distribution, but Falsisca is restricted to the Upper Permian-Lower Triassic of Europe and Asia. This interval is in agreement with the probable Late Permian age of the respective strata of the Rio do Rasto formation. Falsisca was not previously recorded in Gondwana.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Intense and broad photoluminescence (PL) emission at room temperature was observed on structurally disordered Ba[Zr0.25Ti0.75]O-3 (BZT) powders synthesized by the polymeric precursor method. BZT powders were annealed at 573 K for different times and at 973 K for 2 h in oxygen atmosphere. The single-phase cubic perovskite structure of the powder annealed at 973 K for 2 It was identified by X-ray diffraction and Fourier transform Raman techniques. PL emission increased with the increase of annealing time, which reached its maximum value in the powder annealed at 573 K for 192 h. First principles quantum mechanical calculations based on density functional theory (B3LYP level) were employed to study the electronic structure of ordered and disordered models. The theoretical calculations and experimental measurements of Ultraviolet-visible absorption spectroscopy indicate that the presence of intermediary energy levels in the band gap is favorable for the intense and broad PL emission at room temperature in disordered BZT powders. The PL behavior is probably due the existence of a charge gradient on the disordered structure, denoted by means of a charge transfer process from [TiO5]-[ZrO6] or [TiO6]-[ZrO5] clusters to [TiO6]-[ZrO6] clusters. (C) 2008 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dielectric and Raman scattering experiments were performed on polycrystalline Pb(1-x)Ba(x)TiO(3) thin films (x=0.40 and 0.60) as a function of temperature. The dielectric study on single phase compositions revealed that a diffuse-type phase transition occurred upon transformation of the cubic paraelectric to the tetragonal ferroelectric phase in all thin films, which showed a broadening of the dielectric peak. Diffusivity was found to increase with increasing barium contents in the composition range under study. In addition, the temperature dependence of Raman scattering spectra was investigated through the ferroelectric phase transition. The temperature dependence of the phonon frequencies was used to characterize the phase transitions. Raman modes persisted above the tetragonal to cubic phase transition temperature, although all optical modes should be Raman inactive. The origin of these modes was interpreted as a breakdown of the local cubic symmetry by chemical disorder. The lack of a well-defined transition temperature and the presence of broadbands in some temperature intervals above the paraferroelectric phase transition temperature suggest a diffuse-type phase transition. (C) 2008 American Institute of Physics.