971 resultados para Steel Fatigue


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Collective damage of short fatigue cracks was analyzed in the light of equilibrium of crack numerical density. With the estimation of crack growth rate and crack nucleation rate, the solution of the equilibrium equation was studied to reveal the distinct feature of saturation distribution for crack numerical density. The critical time that characterized the transition of short and long-crack regimes was estimated, in which the influences of grain size and grain-boundary obstacle effect were investigated. Furthermore, the total number of cracks and the first order of damage moment were discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Stochastic characteristics prevail in the process of short fatigue crack progression. This paper presents a method taking into account the balance of crack number density to describe the stochastic behaviour of short crack collective evolution. The results from the simulation illustrate the stochastic development of short cracks. The experiments on two types of steels show the random distribution for collective short cracks with the number of cracks and the maximum crack length as a function of different locations on specimen surface. The experiments also give the variation of total number of short cracks with fatigue cycles. The test results are consistent with numerical simulations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

应用有限元方法对层流等离子体射流不锈钢表面重熔工艺中的瞬态热物理现象进行了数值模拟研究.针对不同加热距离,确定了材料熔化和凝固过程中的瞬态温度场、温度梯度和凝固率的时间和空间分布特征.通过引入等效温度面积密度概念,研究了不锈钢重熔热处理的适合条件.结果表明,9~13mm的范围是较为适宜的加热距离,该结果与试验观察基本符合.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

在四辊冷轧试验机和Gleeble-1500试验机上进行了热轧微碳钢板的冷轧和退火试验。用D/max-RC衍射仪测量了试样的,/”层织构,并用Roe软件进行了ODF分析。研究表明,所研究的热轧微碳深冲板压下率约为75%,退火升温速度为20-40℃/h时,试样为{111}织构特征;压下率较大(80%)时,退火织构为较弱的{111}组分。无论{111}织构还是非{111}织构都是在形核阶段开始形成,在晶粒长大优先长大,受到定向形核和选择生长双重机制的作用。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Electron beam surface remelting has been carried out on AISI D2 cold-worked die steel. The microstructure and hardening behavior of the electron beam surface remelted AISI D2 cold-worked die steel have been studied by means of optical microscopy and Vickers hardness testing. It was found that AISI D2 steel can be successfully surface hardened by electron beam surface remelting. This surface hardening effect can be attributed to microstructural refinement following electron beam surface remelting. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The feasibility of the fabrication of coatings for elevated-temperature structural applications by laser cladding MoSi2 powder on steel was investigated. A dense and crack-free fine coating, well-bonded with the substrate has been obtained by this technique. This coating consists of FeMoSi, Fe2Si and a small amount of Mo5Si3 due to dilution of the substrate in the coating. The microstruelure of the coating is characterized of typical fine dendrites. The dendrites are composed of FeMoSi primary phase, and the interdendritic areas are two eutectic phases of FeMoSi and Fe2Si. The hardness of the coating reaches 845 Hv(0.5), 3.7 times larger than that of the steel substrate (180Hv(0.5)).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A laser-discrete quenched steel (LDQS) substrate/as-deposited chromium (top high-contraction (HC) and underlying low-contraction (LC) chromium) system was investigated by dissolving coatings in order to reveal the mechanism that the service life of the coated parts is largely improved using the hybrid technique of laser pre-quenching plus chromium post-depositing. It was found that the surface characteristics of the substrate, LC and HC chromium layer can be simultaneously revealed owing to the dissolution edge effect of chromium coatings. Moreover, the periodical gradient morphologies of the LDQS substrate are clearly shown: the surfaces of laser transformation-hardened regions are rather smooth; a lot of fine micro-holes exist in the transition zones; there are many micro-dimples in the original substrate. Furthermore, the novel method of dissolving coatings with sharp interfaces may be used to reveal the structural features of a substrate/coating system, explore the effect of the substrate on the initial microstructure and morphologies of coatings, and check the quality of the coated-parts.