Preparação de óxidos mistos de níquel e zinco nanoparticulados a partir de combustíveis alternativos
Resumo:
The field of "Materials Chemistry" has been developing in recent years and there has been a great increase of interest in the synthesis and chemical and physical properties of new inorganic solids. New routes of synthesis and synthesis modified has been developed with the aim not only to optimize the processes in laboratory scale, but also on an industrial scale, and make them acceptable by current environmental legislation. The phenomenology of current solid state chemistry properties coupled with the high temperature superconductivity, ferromagnetism, porosity molecular and colors are evidence affected by the synthesis method, which in turn can influence the technological application of these materials. From this understanding, mixed oxides of nickel and zinc nanoparticulate were synthesized by microwave-assisted combustion route using three specific types of organic fuels employing the weight ratios 1:1/2 and 1:1 of cation metallic/fuel, in order to investigate the influence of such proportions to obtain the solids. The new fuels were chosen to replace, for example, urea or glycine that are the fuels most commonly preferred in this kind of synthesis. The powders without heat treatment were studied by Thermogravimetric analysis (TGA), X-Ray Diffraction (XRD) and then calcined at 900°C. After heat treatment, the samples were characterized by analysis of X Ray Diffraction (XRD) and Scanning Electron Microscopy (SEM). The modified synthesis route porposed was effective for obtaining powders. Both the alternative fuels chosen as the different weight ratios employed, influenced in the morphology and obtaining oxides
Resumo:
Generally, cellulose ethers improves mortar properties such as water retention, workability and setting time, along with adherence to the substrate. However, a major disadvantage of the addition of cellulose ethers in mortars is the delay in hydration of the cement. In this paper a cellulose phosphate (Cp) was synthesized water soluble and has been evaluated the effect of their incorporation into mortar based on Portland cement. Cellulose phosphate obtained was characterized by spectrophotometry Fourier transform infrared (FTIR), X-ray diffraction (XRD), elemental analysis and scanning electron microscopy (SEM). Mortar compositions were formulated with varying phosphorus content in cellulose and cellulose phosphate concentrations, when used in partial or total replacement of the commercial additive based hydroxyethyl methyl cellulose (HEMC). The mortars formulated with additives were prepared and characterized by: testing in the fresh state (consistency index, water retention, bulk density and air content incorporated) and in the hardened state (absorption by capillarity, density, flexural and compression strength). In mixtures the proportion of sand:cement of 1:5 (v / v) and factor a / c = 1.31 and water were held constant. Overall, the results showed that the celluloses phosphates employed in mortars added acted significantly when partially substituting the commercial additive. With regard to consistency index, water retention and bulk density in the fresh state and absorption by capillarity and bulk density apparent in the hardened state, showed no appreciable differences as compared to the commercial additive. The incorporated air content in the fresh state reduced markedly, but did not affect other properties. The mortars with cellulose phosphate, partially replacing the commercial additive showed an improvement of the properties of flexural strength and compressive strength
Resumo:
The use of raw materials from renewable sources for production of materials has been the subject of several studies and researches, because of its potential to substitute petrochemical-based materials. The addition of natural fibers to polymers represents an alternative in the partial or total replacement of glass fibers in composites. In this work, carnauba leaf fibers were used in the production of biodegradable composites with polyhydroxybutyrate (PHB) matrix. To improve the interfacial properties fiber / matrix were studied four chemical treatments to the fibers..The effect of the different chemical treatments on the morphological, physical, chemical and mechanical properties of the fibers and composites were investigated by scanning electron microscopy (SEM), infrared spectroscopy, X-ray diffraction, tensile and flexural tests, dynamic mechanical analysis (DMA), thermogravimetry (TGA) and diferential scanning calorimetry (DSC). The results of tensile tests indicated an increase in tensile strength of the composites after the chemical treatment of the fibers, with best results for the hydrogen peroxide treated fibers, even though the tensile strength of fibers was slightly reduced. This suggests a better interaction fiber/matrix which was also observed by SEM fractographs. The glass transition temperature (Tg) was reduced for all composites compared to the pure polymer which can be attributed to the absorption of solvents, moisture and other low molecular weight molecules by the fibers
Resumo:
Over recent years the structural ceramics industry in Brazil has found a very favorable market for growth. However, difficulties related to productivity and product quality are partially inhibiting this possible growth. An alternative for trying to solve these problems and, thus, provide the pottery industry the feasibility of full development, is the substitution of firewood used in the burning process by natural gas. In order to contribute to this process of technological innovation, this paper studies the effect of co-use of ceramic phyllite and kaolin waste on the properties of a clay matrix, verifying the possible benefits that these raw materials can give to the final product, as well as the possibility of such materials to reduce the heat load necessary to obtain products with equal or superior quality. The study was divided into two steps: characterization of materials and study of formulations. Two clays, a phyllite and a residue of kaolin were characterized by the following techniques: laser granulometry, plasticity index by Atterberg limits, X-ray fluorescence, X-ray diffraction, mineralogical composition by Rietveld, thermogravimetric and differential thermal analysis. To study the formulations, specifically for evaluation of technological properties of the parts, was performed an experimental model that combined planning involving a mixture of three components (standard mass x phyllite x kaolin waste) and a 23 factorial design with central point associated with thermal processing parameters. The experiment was performed with restricted strip-plot randomization. In total, 13 compositional points were investigated within the following constraints: phyllite ≤ 20% by weight, kaolin waste ≤ 40% by weight, and standard mass ≥ 60% by weight. The thermal parameters were used at the following levels: 750 and 950 °C to the firing temperature, 5 and 15 °C/min at the heating rate, 15 and 45min to the baseline. The results showed that the introduction of phyllite and/or kaolin waste in ceramic body produced a number of benefits in properties of the final product, such as: decreased absorption of water, apparent porosity and linear retraction at burn; besides the increase in apparent specific mass and mechanical properties of parts. The best results were obtained in the compositional points where the sum of the levels of kaolin waste and phyllite was maximal (40% by weight), as well as conditions which were used in firing temperatures of 950 °C. Regarding the prospect of savings in heat energy required to form the desired microstructure, the phyllite and the residue of kaolin, for having small particle sizes and constitutions mineralogical phases with the presence of fluxes, contributed to the optimization of the firing cycle.
Resumo:
The gradual replacement of conventional materials by the ones called composite materials is becoming a concern about the response of these composites against adverse environmental conditions, such as ultraviolet radiation, high temperature and moist. Also the search for new composite using natural fibers or a blend of it with synthetic fibers as reinforcement has been studied. In this sense, this research begins with a thorough study of microstructural characterization of licuri fiber, as a proposal of alternative reinforcement to polymeric composites. Thus, a study about the development of two composite laminates was done. The first one, involving only the fiber of licuri and the second comprising a hybrid composite based of fiber glass E and the fiber of licuri, in order to know the performance of the fiber when of fiber across the hybridization process. The laminates were made in the form of plates using the tereftálica ortho-polyester resin as matrix. The composite laminate made only by licuri fiber had two reinforcing fabric layers of unidirectional licuri and the hybrid composite had two reinforcing layers of unidirectional licuri fabric and three layers of fiber short glass-E mat. Finally, both laminates was exposed to aging acceleration in order to study the influence of environmental degradation involving the mechanical properties and fracture characteristics thereof. Regarding the mechanical properties of composites, these were determined through uniaxial tensile tests, uniaxial compression and three bending points for both laminates in original state, and uniaxial tensile tests and three bending points after accelerated aging. As regards the study of structural degradation due to aging of the laminates, it was carried out based on microscopic analysis and microstructure, as well as measuring weight loss. The characteristics of the fracture was performed by macroscopic and microscopic (optical and SEM) analysis. In general, the laminated composites based on fiber licuri showed some advantages in their responses to environmental aging. These advantages are observed in the behavior related to stiffness as well as the microstructural degradation and photo-oxidation processes. However, the structural integrity of this laminate was more affected in case the action of uniaxial tensile loads, where it was noted a lower rate of withholding his last resistance property
Resumo:
The coatings mortars are essential elements of building structures because they execute an important role in protecting walls and are particularly exposed to aggressive action responsible for its degradation over time. The importance of wall coverings has been the subject of discussion and analysis in the conservation and rehabilitation of old buildings. Are sometimes removed and replaced with inappropriate solutions of constructive point of view or architecture. The most commonly used coatings on walls of old buildings is based on traditional hydraulic lime mortars. The present study aims at the formulation of new lime- based mortars and aerial fine aggregate, in order to contribute to a better field of conservation and restoration mortar coating of old buildings. Residue was used for polishing porcelain as fine aggregate, replacing the aggregate (sand), in percentages 05-30% by mass. We conducted a thorough evaluation of the mortar properties in fresh and hardened state by comparing the performance of the same with a reference mortar. The residue used was characterized as the density, bulk density, and particle size laser, scanning electron microscopy, X-ray diffraction and X-ray fluorescence. Formulations were produced 7, 6 with residue and one commonly used formulation, which served as a reference. In the formulations of lime mortars air (hydrated lime powder CH-I) has been adopted a stroke volume (1:3) with constant binder, was varied and the water / binder and aggregate and waste. For evaluation of mortars fresh, proceeded to consistency analysis, specific gravity, water retention and air content embedded. In the hardened state assays were performed in specific gravity, water retention, modulus of elasticity, tensile strength in bending, compressive strength, water absorption by capillary action, adhesion, tensile strength, resistance to shrinkage and salts by of crystallization trials with resources chloride solution, nitrate and sulfate all sodium in prismatic at 90 days of age, in addition to the micro structural analysis of mortars. Based on the results we can see that the mortar formulated with 10% content of waste and the reference free retraction feature more stable closer to neutrality. The composition of 10% was obtained better performance against the action of the salt crystallization. The mortar with 15% residue obtained better density, lower air content embedded and high capacity for water retention developing good workability. The replacement of 20% of waste generates a satisfactory utilization of resistance to compression, flexion and traction grip the base. And, finally, it can be seen that the mortar with 10, 15 and 20% residual show, in principle, good suitability as coatings, thus enabling a final result consistent with durability, workability and aesthetics developing therefore a material with better performance to repair or replace existing mortars in old buildings
Resumo:
Nowadays, in the plastic industry are used mills that accomplish the recycling of residues generated in the production of its components. These mills contain cut sheets that suffer accelerated wear, once they are submitted constantly to the tribologic efforts, decreasing its useful life. To reduce this problem, it s used noble steels or takes place superficial treatments. The ionic nitriding process presents some limitations related to the uniformity of the layer in pieces with complex geometry, committing its application in pieces as knives, head offices, engagements, etc. However, the new technique of nitriding in cathodic cage eliminates some problems, as the restrictions rings, inherent to the conventional ionic nitriding. In present work, was studied the use viabilization of steels less noble, as SAE 1020, SAE 4320 and SAE 4340, nitreded by two different techniques, to substitute the AISI 01 steels, usually used in the cut knifes fabrication, seeking to reduce the costs and at the sane time to increase the useful life of these knifes. The steel most viable was the SAE 4340, nitrided in cathodic cage, because it presented uniformity in thickness and in the hardness of the layer, besides of increased 58% in the average its useful life
Resumo:
This research was motivated by the requirement of asbestos s replacement in building systems and the need to generate jobs and income in the country side of the state of Bahia, Brazil. The project aimed at using fibers from licuri leaves (syagrus coronata), an abundant palm in the region, to produce composites appropriate for the sustainable production of cement fibre reinforced products in small plants. The composites were produced in laboratory using Portland cement CP-II-F32, sand, water, licuri palm fiber contents of 1.0, 1.5 and 2.0% by weight of binder (two different fiber length) and metakaolin. The latter was chosen as an additional binder for its efficiency to reduce the alkalinity of cementitious matrixes therefore preventing the degradation of vegetable fibers. The characterization of the composite components was carried out by sieving and laser particle size analyses, thermal analysis, fluorescence and X-ray diffraction. The composites performance was evaluated by 3- point-bending tests, compressive strength, ultrasound module of elasticity, free and restrained shrinkage, water capillarity absorption and apparent specific gravity. It has been found that the addition of fibers increased the time to onset of cracking over 200.00% and a 25% reduction in cracks opening in the restrained shrinkage test. The capillary absorption reduced about 25% when compared to fiber-free composites. It was also observed with regard to flexural strength, compressive strength and specific gravity, that the addiction of fibers did not affect the composite performance presenting similar results for compounds with and without fibers. In general it can be stated that the reinforced composite fibers of palm licuri presents physical and mechanical characteristics which enable them to be used in the intended proposals of this research
Resumo:
Universidade Federal do Rio Grande do Norte
Resumo:
Researches have shown that the introduction of rubber in concrete improves the features of its deformability, as well as contributes to environmental disposal of waste generated in the tire retreading process. Furthermore, there is a high availability of limestone within RN and CE country. Ignorance about this stone, does not allow its wide use as aggregate, leaving, this abundant supply idle. A composite of limestone gravel, with proportions of tire rubber waste which could be used as concrete would be an alternative to concrete for low applications. Therefore, this research aims to evaluate the characteristics of concrete containing limestone gravel and proportions of little aggregate replacement (sand) by tire rubber waste. To this goal, the material components of the concrete were characterized, concrete specimens with limestone gravel were made, from the dash 1.0: 2.5: 3.5, varying the water/cement ratio, and inserting a commercial plasticizer, without a proportion of residue, known as reference. From this, concrete with and without the presence of the additive in the same proportions were chosen, as well as these with the use of granite gravel, for being the most used. Selected the references, to these, replacements of little aggregate (sand) were added replaced by rubber waste from the tire retreading process, treated with 1M NaOH in proportions from 5.0 to 20.0 % by mass, cured and exposed to the semiarid environment. The results indicate the possibility of using limestone gravel in the concrete composition with workability correction using plasticizer. There was a decrease in the mechanical properties of the concrete with increments of waste rubber, but there is an improvement in toughness and deformability of the composite, which makes it interesting for the construction of non-structural concrete floors, as well as, the rubber waste delayed the hardening process, continuing to gain resistance after 28 days
Resumo:
In the present work it was developed originals alternatives of enveronmentally safe and economically viable destination of thermoset plastic residue from a button factory, which at presnte stores such residue tempor and in a way that is inconvenient to the atmosphere, a waiting safe solutions. As the residue is not recycleab and its burning leberates strongly aggressive gases, safe alternatives were researched. Inicially, ghe residue in incineration was performed in cement ovens with precise control ofe emission of gases, but it was proved inviable due to its low calorific power, as well as the liberation of free lead in the ashes. An original and feasible option was the residue confinemente in soil-ciment blocks, lohich resulted in blocks highly resistant to simple compression with structural block, and also a significant increase in thermal resistence. Was got up other options of original and important composites as: making of blocks for pré-moulded flagstone, internal coating of walls with plaster being obtained good texture results, replenish of ceramic blocks and blocks with cement, also implying in increase of thermal resistance. Besides these original and scientific contributions, the it was technologically contribution of defreadation with suggestions of the material using torch of thermal plasm; for this was projected, built, characterized and tested a torch to it shapes it being obtained exciting results for the development of this technology come back for ending destruction from all the types of inconvenient garbage to the atmosphere
Resumo:
Steam injection is the most used thermal recovery method of oil nowadays because of the high degree of development of the technique that allows high recovery factors. However, injection of superheated steam into the reservoir affects the entire structure of the well, including the cemented layer that presents a retrogression of compressive strength and increases the permeability due to formation of more crystalline and denser phases at temperatures above 110 °C. These changes result in failures in the cement that favor the entrance of formation fluids into the annulus space resulting in unsafe operations and restrictions in the economic life of the well. But the strength retrogression can be prevented by partial replacement of cement by silica-based materials that reduce the CaO/SiO2 ratio of cement slurries changing the trajectory of the reactions, converting those deleterious phases in phases with satisfactory mechanical strength and permeability. The aim of this study was to evaluate the behavior of a ceramic waste material rich in silica in partial and total substitution of a mineral additive used to fight the strength retrogression of cement slurries subjected to high temperatures. The evaluation was made by compression, X-ray diffraction (XRD) and thermogravimetry (TG/DTG). The samples were submitted to a cycle of low temperature (38 °C) for 28 days and a cycle of low temperature followed by exposure to 280 ºC and 1000 psi by 3 days. The results showed that slurries with additions of up to 30% of the waste material are not enough to prevent the strength retrogression, while slurries with additions of the waste material combined with silica flour in various proportions produced hydrated products of low Ca/Si ratios that maintained the compressive strength at satisfactory levels
Resumo:
The preparation of cement slurries for offshore well cementing involves mixing all solid components to be added to the mixing water on the platform. The aim of this work was to study the formulation of pre-prepared dry mixtures, or grouts, for offshore oilwell cementing. The addition of mineral fillers in the strength of lightweight grouts applied for depths down to 400 m under water depths of 500 m was investigated. Lightweight materials and fine aggregates were selected. For the choice of starting materials, a study of the pozzolanic activity of low-cost fillers such as porcelain tile residue, microsilica and diatomaceous earth was carried out by X-ray diffraction and mechanical strength tests. Hardened grouts containing porcelain tile residue and microsilica depicted high strength at early ages. Based on such preliminary investigation, a study of the mechanical strength of grouts with density 1.74 g/cm3 (14.5 lb/gal) cured initially at 27 °C was performed using cement, microsilica, porcelain tile residue and an anti-foaming agent. The results showed that the mixture containing 7% of porcelain tile residue and 7% of microsilica was the one with the highest compressive strength after curing for 24 hours. This composition was chosen to be studied and adapted for offshore conditions based on testes performed at 4 °C. The grout containing cement, 7% of porcelain tile residue, 7% of active silica and admixtures (CaCl2), anti-foaming and dispersant resulted satisfactory rheology and mechanical strength after curing for 24 hours of curing
Resumo:
Actually in the oil industry biotechnological approaches represent a challenge. In that, attention to metal structures affected by electrochemical corrosive processes, as well as by the interference of microorganisms (biocorrosion) which affect the kinetics of the environment / metal interface. Regarding to economical and environmental impacts reduction let to the use of natural products as an alternative to toxic synthetic inhibitors. This study aims the employment of green chemistry by evaluating the stem bark extracts (EHC, hydroalcoholic extract) and leaves (ECF, chloroform extract) of plant species Croton cajucara Benth as a corrosion inhibitor. In addition the effectiveness of corrosion inhibition of bioactive trans-clerodane dehydrocrotonin (DCTN) isolated from the stem bark of this Croton was also evaluated. For this purpose, carbon steel AISI 1020 was immersed in saline media (3,5 % NaCl) in the presence and absence of a microorganism recovered from a pipeline oil sample. Corrosion inhibition efficiency and its mechanisms were investigated by linear sweep voltammetry and electrochemical impedance. Culture-dependent and molecular biology techniques were used to characterize and identify bacterial species present in oil samples. The tested natural products EHC, ECF and DCTN (DMSO as solvent) in abiotic environment presented respectively, corrosion inhibition efficiencies of 57.6% (500 ppm), 86.1% (500 ppm) and 54.5% (62.5 ppm). Adsorption phenomena showed that EHC best fit Frumkin isotherm and ECF to Temkin isotherm. EHC extract (250 ppm) dissolved in a polar microemulsion system (MES-EHC) showed significant maximum inhibition efficiency (93.8%) fitting Langmuir isotherm. In the presence of the isolated Pseudomonas sp, EHC and ECF were able to form eco-compatible organic films with anti-corrosive properties
Resumo:
Foram analisados os dados de desempenho ponderal de bubalinos Murrah do Sistema de Produção de Leite da Universidade Estadual Paulista, Faculdade de Medicina Veterinária e Zootecnia, campus de Botucatu. Os pesos foram corrigidos às diversas idades-padrão e o modelo incluiu os efeitos de sexo (S), mês (M) e ano (A) de nascimento, classe de idade da búfala ao parto (C) e as interações S x M, S x A, S x C e M x A. As médias ajustadas e respectivos erros-padrão estimados para as características estudadas foram: Peso ao Nascer (PN): 37,71 ± 8,25kg; Peso aos 120 dias (P120): 102,08 ± 16,27kg; Peso aos 240 dias (P240): 169,84 ± 22,83kg; Peso aos 365 dias (P365): 250,59 ± 25,12kg; Peso aos 550 dias (P550): 326,13 ± 39,27kg e Peso aos 730 dias (P730): 389,80 ± 31,26kg. O efeito de sexo (S) foi significativo somente para PN e P365, sendo que machos tenderam a nascer mais pesados que fêmeas. O mês de nascimento (M) exerceu efeito sobre o PN, P120 e P730 sendo que animais nascidos em maio foram os mais pesados ao nascer, enquanto os nascidos em janeiro e maio, foram os mais pesados aos 120 e 730 dias, respectivamente. O efeito de ano de foi significativo sobre o PN, P120, P240 e P730. Os filhos de búfalas das classes de idade 1 (3 anos ou menos) e da classe 6 (10,11 e 12 anos) foram os mais leves e mais pesados ao nascer, respectivamente. O fato de a classe de idade da búfala não exercer efeito sobre os P365, P550 e P730 sugere que, em rebanhos comerciais possa ser feita a substituição de búfalas não gestantes por novilhas prenhes, apesar de esta prática reduzir a média de idade do rebanho de cria. Bubalinos da raça Murrah oriundos de rebanhos leiteiros podem ser utilizados para a produção de carne.