977 resultados para solvent free


Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the shape evolution of free gold agglomerates with different morphologies that transform to ellipsoidal and then to spherical shapes during the heating cycle. The shape transformation is associated with a structural transition from polycrystalline to single crystalline. The structural transition temperature is shown to be dependent on the final size of the particles and not on the initial morphologies of the agglomerates. It is also shown that the transition occurs well below the melting temperature which is in contrast with the melt-freeze process reported in the literature.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Surfactant-intercalated layered double-hydroxide solid Mg-Al LDH-dodecyl sulfate (DDS) undergoes rapid and facile delamination to its ultimate constituent, single sheets of nanometer thickness and micrometer size, in a nonpolar solvent such as toluene to form stable dispersions. The delaminated nanosheets are electrically neutral because the surfactant chains remain tethered to the inorganic layer even on exfoliation. With increasing volume fraction of the solid, the dispersion transforms from a free-flowing sol to a solidlike gel. Here we have investigated the sol-gel transition in dispersions of the hydrophobically modified Mg-Al LDH-DDS in toluene by rheology, SAXS, and (1)H NMR measurements. The rheo-SAXS measurements show that the sharp rise in the viscosity of the dispersion during gel formation is a consequence of a tactoidal microstructure formed by the stacking of the nanosheets with an intersheet separation of 3.92 nm. The origin and nature of the attractive forces that lead to the formation of the tactoidal structure were obtained from 1D and 2D (1)H NMR measurements that provided direct evidence of the association of the toluene solvent molecules with the terminal methyl of the tethered DDS surfactant chains. Gel formation is a consequence of the attractive dispersive interactions of toluene molecules with the tails of DDS chains anchored to opposing Mg-Al LDH sheets. The toluene solvent molecules function as molecular ``glue'' holding the nanosheets within the tactoidal microstructure together. Our study shows how rheology, SAXS, and NMR measurements complement each other to provide a molecular-level description of the sol-gel transition in dispersions of a hydrophobically modified layered double hydroxide.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A cross-linked polymer ``gel'' electrolyte obtained from free radical polymerization of a vinyl monomer (acrylonitrile; AN) in a room temperature ionic liquid electrolyte (N,N-methyl butyl pyrrolidinium-bis (trifluoromethanesulphonyl)imide-lithium bis(trifluoromethanesulphonyl) imide;LiTFSI-[Py(1,4)-TFSI]) for application in high rate capability rechargeable lithium-ion batteries is discussed here. This is a novel alternative compared to the often employed approach of using a molecular liquid as the medium for performing the polymerization reaction. The polymer ``gel'' electrolytes (AN:Py(1,4)-TFSI = 0.16-0.18, w/w) showed remarkable compliable mechanical strength and higher thermal stability compared to LiTFSI-[Py(1,4)-TFSI]. Despite two orders increase in magnitude of viscosity of polymer ``gels'', the room temperature ionic conductivity of the ``gels'' (1.1 x 10(-3)-1.7 x 10(-3) Omega(-1) cm(-1)) were nearly identical to that of the ionic liquid (1.8 x 10(-3) Omega(-1) cm(-1)). The present ``gel'' electrolytes did not exhibit any ageing effects on ionic conductivity similar to the conventional polymer gel electrolytes (e.g. high molecular weight polymer + salt + high dielectric constant molecular solvent). The disorder (ionic liquid) to a relative order (cross-linked polymer electrolyte) transformation does not at all influence the concentration of conducting species. The polymer framework is still able to provide efficient pathways for fast ion transport. Unlike the ionic liquid which is impossible to assemble without a conventional separator in a cell, the polymer ``gel'' electrolyte could be conveniently assembled without a separator in a Li vertical bar lithium iron phosphate (LiFePO(4)) cell. Compared to the ionic liquid, the ``gel'' electrolyte showed exceptional cyclability and rate capability (current density: 35-760 mA g(-1) with LiFePO(4) electronically wired with carbon (amorphous or multiwalled nanotube [MWCNT]).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Single chain fragment variables (ScFvs) have been extensively employed in studying the protein-protein interactions. ScFvs derived from phage display libraries have an additional advantage of being generated against a native antigen, circumventing loss of information on conformational epitopes. In the present study, an attempt has been made to elucidate human chorionic gonadotropin (hCG)-luteinizing hormone (LH) receptor interactions by using a neutral and two inhibitory ScFvs against hCG. The objective was to dock a computationally derived model of these ScFvs onto the crystal structure of hCG and understand the differential roles of the mapped epitopes in hCG-LH receptor interactions. An anti-hCG ScFv, whose epitope was mapped previously using biochemical tools, served as the positive control for assessing the quality of docking analysis. To evaluate the role of specific side chains at the hCG-ScFv interface, binding free energy as well as residue interaction energies of complexes in solution were calculated using molecular mechanics Poisson-Boltzmann/surface area method after performing the molecular dynamic simulations on the selected hCG-ScFv models and validated using biochemical and SPR analysis. The robustness of these calculations was demonstrated by comparing the theoretically determined binding energies with the experimentally obtained kinetic parameters for hCG-ScFv complexes. Superimposition of hCG-ScFv model onto a model of hCG complexed with the 51-266 residues of LH receptor revealed importance of the residues previously thought to be unimportant for hormone binding and response. This analysis provides an alternate tool for understanding the structure-function analysis of ligand-receptor interactions. Proteins 2011;79:3108-3122. (C) 2011 Wiley-Liss, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thin foils of Cu, Au and Cu + Au alloys embedded in indium sesquioxide were equilibrated with controlled streams of CO-CO2 mixtures. The equilibrium concentrations of indium in the foils were determined by neutron activation analysis. The corresponding chemical potentials of indium were calculated from the standard free energies of formation of carbon monoxide, carbon dioxide, and indium oxide. It was found that the size difference between the solute and the solvent does not make significant contributions to the solute—solute interaction energy in the α-phase. The chemical potential of indium at one at.% concentration is 8.6 Kcals more negative in gold than in copper at 900°K. The variation of this chemical potential with alloy composition in Cu + Au system was in good agreement with Alcock and Richardson's quasichemical equation. The agreement is strengthened by the accurate knowledge of the co-ordination number in these substitutional solid solutions from X-ray diffraction studies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thin foils of copper, silver and gold were equilibrated with tetragonal GeO2 under controlled View the MathML source gas streams at 1000 K. The equilibrium concentration of germanium in the foils was determined by the X-ray fluorescence technique. The standard free energy of formation of tetragonal GeO2 was measured by a solid oxide galvanic cell. The chemical potential of germanium calculated from the experimental data and the free energies of formation of carbon monoxide and carbon dioxide was found to decrease in the sequence Ag + Ge > Au + Ge > Cu + Ge. The more negative value for the chemical potential of germanium in solid copper, compared to that in solid gold, cannot be explained in terms of the strain energy factor, electro-negativity differences or the vaporization energies of the solvent, and suggests that the d band and its hybridization with s electrons are an important factor in determining the absolute values for the chemical potential in dilute solutions. However, the variation of the chemical potential with solute concentration can be correlated to the concentration of s and p electrons in the outer shell.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The chemical potentials of tin in its α-solid solutions with Cu, Au and Cu + Au alloys have been measured using a gas-solid equilibration technique. The variation of the excess chemical potential of tin with its composition in the alloy is related to the solute-solute repulsive interaction, while the excess chemical potential at infinite dilution of the solute is a measure of solvent-solute interaction energies. It is shown that solute-solute interaction is primarily determined by the concentration of (s + p) electrons in the conduction band, although the interaction energies are smaller than those predicted by either the rigid band model or calculation based on Friedel oscillations in the potential function. Finally, the variation of the solvent-solute interaction with solvent composition in the ternary system can be accounted for in terms of a quasi-chemical treatment which takes into account the clustering of the solvent atoms around the solute.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The standard free energies of formation of zinc aluminate and chromite were determined by measuring the oxygen potential over a solid CuZn alloy, containing 10 at.−% Zn, in equilibrium with ZnO, ZnAl2O4+Al2O3(χ) and ZnCr2O4+Cr2O3, in the temperature range 700–900°C. The oxygen potential was monitored by means of a solid oxide galvanic cell in which a Y2O3 ThO2 pellet was sandwiched between a CaOZrO2 crucible and tube. The temperature dependence of the free energies of formation of the interoxidic compounds can be represented by the equations, The heat of formation of the spinels calculated from the measurements by the “Second Law method” is found to be in good agreement with calorimetrically determined values. Using an empirical correlation for the entropy of formation of cubic spinel phases from oxides with rock-salt and corundum structures and the measured high temperature cation distribution in ZnAl2O4, the entropy of transformation of ZnO from wurtzite to rock-salt structure is evaluated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The standard Gibbs free energy of formation of magnesium and cadmiumchromites have been determined by potentiometric measurements on reversiblesolid-state electrochemical cells [dformula (Au-5%Cd, , Au-5%Cd; Pt, + , CaO-ZrO[sub 2], + ,Pt; CdO, , CdCr[sub 2]O[sub 4] + Cr[sub 2]O[sub 3])] in the temperature range 500°–730°C, and [dformula Pt, Cr + Cr[sub 2]O[sub 3]/Y[sub 2]O[sub 3]-ThO[sub 2]/Cr + MgCr[sub 2]O[sub 4] + MgO, Pt] in the temperature range 800°–1200°C. The temperature dependence of the freeenergies of formation of the ternary compounds can be represented by theequations [dformula CdO(r.s.) + Cr[sub 2]O[sub 3](cor) --> CdCr[sub 2]O[sub 4](sp)] [dformula Delta G[sup 0] = - 42,260 + 7.53T ([plus-minus]400) J] and [dformula MgO(r.s.) + Cr[sub 2]O[sub 3](cor) --> MgCr[sub 2]O[sub 4](sp)] [dformula Delta G[sup 0] = - 45,200 + 5.36T ([plus-minus]400) J] The entropies of formation of these spinels are discussed in terms of cationdisorder and extent of reduction of Cr3+ ions to Cr2+ ions. Thermodynamicdata on the chromates of cadmium and magnesium are derived by combiningthe results obtained in this study with information available in the literatureon high temperature, high pressure phase equilibria in the systems CdO-Cr2O3-O2 and MgO-Cr2O3-O2.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

he thermodynamic properties of the spinel Mg2SnO4 have been determined by emf measurements on the solid oxide galvanic cell,View the MathML source in the temperature range 600 to 1000°C. The Gibbs' free energy of formation of Mg2SnO4 from the component oxides can be expressed as View the MathML source,View the MathML source These values are in good agreement with the information obtained by Jackson et al. [Earth Planet. Sci. Lett.24, 203 (1974)] on the high pressure decomposition of magnesium stannate into component oxides at different temperatures. The thermodynamic data suggest that the spinel phase is entropy stabilized, and would be unstable below 207 (±25)°C at atmospheric pressure. Based on the information obtained in this study and trends in the stability of aluminate and chromite spinels, it can be deduced that the stannates of nickel and copper(II) are unstable.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Emf measurements on the galvanic cell Pt, Ta, In + In,O, / Tho,-Y,03 / Cu + C+O, Pt were used to obtain the standard free energy of formation of 1%03fr om 600 to 900°C. Differential thermal analysis was used to detect the decomposition of In2(S0,), under controlled SO2 + O2 + Ar mixtures in thqtemperature range 640-8wC. X-ray diffraction analysis indicated that the decomposition product was 1%03 without an oxywlphate intermediate. The following equations were obtained for the variation of the standard free-energy change(Jlmole) with temperature:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sortases are cell-membrane-anchored cysteine transpeptidases that are essential for the assembly and anchoring of cell-surface adhesins in Gram-positive bacteria. Thus, they play critical roles in virulence, infection and colonization by pathogens. Sortases have been classified into four types based on their primary sequence and the target-protein motifs that they recognize. All Gram-positive bacteria express a class A housekeeping sortase (SrtA). Sortase A from Streptococcus pneumoniae (NP_358691) has been crystallized in two crystal forms. Diamond-shaped crystals of Delta N(59)SrtA diffracted to 4.0 angstrom resolution and belonged to a tetragonal system with unit-cell parameters a = b = 122.8, c = 86.5 angstrom, alpha = beta = gamma = 90 degrees, while rod-shaped crystals of Delta N(81)SrtA diffracted to 2.91 angstrom resolution and belonged to the monoclinic space group P2(1) with unit-cell parameters a = 66.8, b = 103.47, c = 74.79 angstrom, alpha = gamma = 90, beta = 115.65 degrees. The Matthews coefficient (V(M) = 2.77 angstrom(3) Da(-1)) with similar to 56% solvent content suggested the presence of four molecules in the asymmetric unit for Delta N(81)SrtA. Also, a multi-copy search using a monomer as a probe in the molecular-replacement method resulted in the successful location of four sortase molecules in the asymmetric unit, with statistics R = 41.61, R(free) = 46.44, correlation coefficient (CC) = 64.31, CC(free) = 57.67.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The standard Gibbs' free energies of formation of compounds of type Cu2L%05 (Ln = Tb,Dy,Er,Yb) were measured using the solid state cell in the temperature range of 970 to 1323 K For formation of Cu2L?O5 compounds from their binary component oxides according to the reaction 2 CUO (s) + L%03 (s) -, Cu,,L%05 (s),the Gibbs' free energy changes can be represented by the following equations:AGO = 13 080 - 13.70 'I" (+80) J mol-' (Ln = Tb)AGq = 11 480 - 13.51 T (260) J mol-I (Ln = Dy)AGO = 10 750 - 13.99 T (260) J mol-I (Ln = Er)AGO = 9 920 - 13.90 T (260) J mol-' (Ln = Yb) Since formation of the compounds is endothermic, the compounds become thermodynamically unstable with respect to their component oxides below 955 K for Cu2Tb205, 850 K for Cu2Dy205, 768 K for Cu2Er205 and 714 K for Cu2Yb2OS When the oxygen partial pressure over Cu2L%05 is lowered, they decompose according to the scheme, 2 CU,L%O, (s) -r 2 L%03 (s) +2 cu20 (s) + 02(g)The equilibrium chemical potentials of oxygen corresponding to the dissociation reactions are computed from the emf data and auxiliary information on Cu20 and CuO. The computed decomposition temperatures at an oxygen partial pressure of 5.0 x ld Pa are compared with those obtained directly from combined thermogravimetric (TGA) and differential thermal analyses (DTA).The free energy, enthalpy and entropy of formation of Cu2Ln205 compounds show systematic variation with the ionic radius of the trivalent lanthanide ion. The trends obtained in this study are compared with information available in the literature. The staZbility of Cu2Ln205 compounds increases with the decrease in ionic radii of the ~ n ion~. +

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Temperature dependence of the energy gap and free carrier absorption in a high-quality InAs0.05Sb0.95 single crystal was studied between 90 K and 430 K through the absorption spectra. At this alloy concentration, the room-temperature energy gap was measured to be 0.15 eV. Varshni- and the Bose–Einstein-type fit parameters were obtained from the measured temperature dependence of the energy gap, and the latter gave the zero-temperature gap to be 0.214 eV. It was found that although Weider’s empirical formula for the dependence of the energy gap on temperature and the alloy concentration agrees with the value of the gap at room temperature, it is inaccurate in describing its temperature dependence. From the free carrier absorption measurements, the phonon limited cross section of 7.35×10−16 cm2 at 15 μm was deduced at room temperature.