810 resultados para ZNO NANOPARTICLES
Resumo:
Superconducting BSCCO samples made by melt-texturing process were prepared with the addition of calcium zirconate and calcium silicate nanoparticles. Bi:2212 melt-textured composites prepared with I wt.% of either addition showed different behavior for the critical current density as a function of the applied field, indicating that for each additional compound the improvement can be associated to different enhancement mechanisms, such as the creation of pinning centers and the increase on the connectivity of the grains. The estimated pinning forces indicated higher values for the calcium compound containing samples. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The phenomenon of electrical degradation in ZnO varistors was studied by application of high-intensity current pulses. A wave shape of 8 X 20-mu-s and rectangular waves of 1 and 2 ms were used. The degradation was estimated by reference electric-field variation and by Schottky voltage barrier deformation. The results showed that current pulses reduce both the height and the width of the barrier voltage. It was also observed that the donor density N(d) did not change but the surface states density N(s) decreased with degradation.
Resumo:
The effects of La2O3 on the properties of (Zn, Co, Ta) doped SnO2 varistors were investigated in this study. The samples with different La2O3 concentrations were sintered at 1400 degrees C for 2 h and their properties were characterized by XRD, SEM, I-V and impedance spectroscopy. The grain size was found to decrease from 13 pm to 9 gm with increasing La2O3 content. The addition of rare earth element leads to increase the nonlinear coefficient and the breakdown voltage. The enhancement was expected to arise from the possible segregation of lanthanide ion due to its larger ionic radius to the grain boundaries, thereby modifying its electrical characteristics. Furthermore, the dopants such as La may help in the adsorption of O' to O '' at the grain boundaries characteristics. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Undoped and indium-doped Zinc oxide (ZnO) solid films were deposited by the pyrosol process at 450 degrees C on glass substrates From solutions where In/Zn ratio was 2, 5, and 10 at.%. Electrical measurements performed at room temperature show that the addition of indium changes the resistance of the films. The resistivities of doped films are less than non-doped ZnO films by one to two orders of magnitude depending on the dopant concentration in the solution. Preferential orientation of the films with the c-axis perpendicular to the substrate was detected by X-ray diffraction and polarized extended X-ray absorption fine structures measurements at the Zn K edge. This orientation depends on the indium concentration in the starting solution. The most textured films were obtained for solutions where In/Zn ratio was 2 and 5 at.%. When In/Zn = 10 at.%, the films had a nearly random orientation of crystallites. Evidence of the incorporation of indium in the ZnO lattice was obtained from extended X-ray absorption fine structures at the In and Zn K edges. The structural analysis of the least resistive film (Zn/In = 5 at.%) shows that In substitutes Zn in the wurtzite structure. (C) 2000 Elsevier B.V. B.V. All rights reserved.
Resumo:
Structural and electrical properties of ZnO varistors were investigated as a function of spinel composition. Six varistor mixtures differing only in chemical composition of spinel, were prepared by mixing separately synthesized constituent phases (DSCP method). Compositions of constituent phases in sintered samples were investigated by changes of lattice parameters of the phases, as well as by EDS analysis of the constituent phases. It was found that compositions of ZnO, intergranular and spinel phases were partially changed during sintering due to redistribution of additives, that was controlled by starting spinel composition and its stability. Electrical characterization showed significant difference in electrical properties of investigated varistors: nonlinearity coefficients ranging from 22 to 55 and leakage currents differing by the order of magnitude. Activation energies of conduction were obtained from ac impedance spectroscopy measurements. Calculated values of activation energies were in the range 0.61-1.0 eV confirming difference in defect structure of ZnO grain boundaries in varistors containing different spinel phases. (C) 2001 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
The flat-panel-display's (FPD) market and demand for highly efficient and colored luminescent films have been growing quickly. In this work, thin films were obtained from Pechini's solution by dip-coating. The green films were thermally treated at 873 K in order to get ZnO:Eu 1 at% thin film. A Schott(R) glass plate hydrothermally treated was used as substrate. The films have a mosaic shaped feature that was observed by optical microscopy. That feature is a result of substrate thermal treatment. The film deposition decreases the substrate transmittance in the visible range. When the F-7(0) -->L-5(6) (392nm) Eu3+ transition is excited, it is possible to detect emission from D-5(0) --> F-7(J) (J = 1, 2, 3 and 4) transitions. The D-5(0) --> F-7(2) transition is also observed by using ZnO excitation wavelengths indicating energy transfer from ZnO to Eu3+ ion. (C) 2003 Elsevier B.V. (USA). All rights reserved.
Resumo:
Pt-modified RuO2 was prepared by a sol-gel procedure on titanium substrates in the form of thin films of similar to2-mum thickness. X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) analyses showed that these films actually consist of Pt nanoparticles dispersed in RuO2 and that neither metallic Ru nor Pt-Ru alloy are present on the surface. Electrodes with different Pt:Ru nominal compositions were prepared and their electrocatalytic activity for the oxidation of methanol was investigated by potential sweeps and chronoamperometry. The results obtained show an enhancement effect for methanol oxidation that can be interpreted as associated to the formation of hydrous oxides on the RuO2 surface.
Resumo:
The sintering of ZrO2. MgO . ZnO powder has been investigated by TMA (Thermal Mechanical Analyser) and its phases analysed by XRD (X-ray diffraction pattern). The data obtained from sintering was studied by the Bannister equation and its dominant sintering mechanism was calculated. It was observed that the ZnO addition in the ZrO2. MgO solid solution lead to increased zirconia stabilization, According to the vacancies model, the ZnO addition did not lead to zirconia phases stabilization (PSZ). An analysis of the rate control in the initial stage of the sintering (region I) showed a mechanism of volume diffusion type. In other regions (regions II and III), the grain growth did lead to the Bannister equation deviation, which was observed by SEM (Scanning Electron Microscopy). These results were different from those demonstrated by other authors who studied the ZrO2. Y2O3 solid solution and obtained a mechanism of grain boundary diffusion type. (C) 1999 Published by Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
Suspensions of undoped SnO2 nanoparticles and containing Eu3+ ions were prepared by a sol-gel procedure. Using the classical synthesis method ( precipitation), the particles tend to grow by a coarsening process in order to minimize the surface free energy. This effect can strongly be reduced by the addition of an amide and surfactant during the synthesis, which decreases the surface free energy of the colloidal particles. These additives promote the formation of powders composed of very small primary particles formed by a crystallite of 10 Angstrom, and exhibit good redispersion properties. The local and long order structures of the redispersible powder were studied by X-rays absorption spectroscopy at Sn L-I edge and X-rays diffraction, respectively. The structure of the colloidal aggregates in suspension was investigated by small angle X-rays scattering (SAXS). SAXS results indicate the sol are composed by a polidisperse system of hard spheres resulting of agglomeration of the primary particles and their size increasing by agglomeration for progressively higher Eu3+ content.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
The effects of the degradation process on the structural, microstructural and electrical properties of ZnO-based varistors were analyzed. Rietveld refinement showed that the BiO2-x phase is affected by the degradation process. Besides the changes in the spinel phase, the degradation process also affects the lattice microstrain in the ZnO phase. Scanning electron microscopy analysis showed electrode-melting failure, while wavelength dispersive X-ray spectroscopy qualitative analysis showed deficiency of oxygen species at the grain boundaries in the degraded samples. Atomic force microscopy using electrostatic mode force illustrated a decrease in the charge density at the grain boundaries of the degraded sample. Transmission electron microscopy showed submicrometric spinel grains embedded in a ZnO matrix, but their average grain size is smaller in the degraded sample than in the standard one. Long pulses appeared to be more harmful for the varistors' properties than short ones, causing higher leakage current values. The electrical characteristics of the degraded sample are partially restored after heat treatment in an oxygen-rich atmosphere. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Dense SnO2 ceramics were obtained by doping with ZnO concentrations varies from 0.5 to 5.0 mel. The obtained powder was isostaticaly pressed to 210MPa in cylindrical shape and sintered from ambient to 1.500 degrees C using constant heating rate of 10 degrees C/min. Densities above 97% were obtained depending on the ZnO doping concentration. A maximum density was reached with the addition of 2 mol%. It can be concluded from shrinkage data and the observed microstructure obtained by SEM that the solid solution limit for ZnO in SnO2 is about 1.0 mol%. Above this concentration the formation of a second ceramic phase is observed.
Resumo:
The surface properties of SnO2 nanoparticles were modified by grafting ionic (Tiron (R). (OH)(2)C6H2(SO3Na)(2)(H2O)-H-.) or non-ionic (Catechol (R). C6H4-1,2-(OH)(2)) capping Molecules during aqueous sol-gel processing to improve the redispersibility of powdered xerogel. The effect of the amount of grafted organic molecules on the redispersibility of powders in aqueous solution at several basic pH values was Studied. The nanostructural features of the colloidal suspensions were analyzed by small angle X-ray scattering (SAXS) measurements. Irrespective of the nature and amount of grafted molecules, complete redispersion was obtained in aqueous solution at pH = 13. The redispersion at pH = 11 results in a mixture of dispersed primary particles and aggregates. The proportion of well dispersed nanoparticles and aggregates (and their average size) can be tuned by the quantity of grafted ionic molecules.
Resumo:
Nanocrystallized boehmite gamma-AlOOH center dot nH(2)O had been synthesized by spray-drying (SD) of a solution of aluminium tri-sec-butoxide peptized by nitric acid. The sub-micronic spherical particles obtained had an average diameter of 500 nm and were built of 100 nm or less platelet-like sub-particles. The average crystallite size calculated from XRD was 1.6 nm following the b axis (i.e. one unit cell) and 3-4 nm perpendicular to b. As a result of the nanometric sizes of crystallites, there was a large surface free for water adsorption and it was found to be n = 1.18 +/- 0.24H(2)O per AlOOH. The SD spheres spontaneously dispersed in water at room temperature and formed stable-over months-suspensions with nanometre-size particles (25-85 nm). Luminescent europium-doped nanocrystallized boehmites AlOOH: Eu (Al0.98Eu0.02OOH center dot nH(2)O) were synthesized the same way by SD and demonstrated the same crystallization properties and morphologies as the undoped powders. It is inferred from the Eu3+ luminescence spectroscopy that partly hydrated europium species are immobilized on the boehmite nanocrystals where they are directly bonded to alpha(OH) groups of the AlOOH surface. The europium coordination is schematically written [Eu3+(OH)(alpha)(H2O)(7-alpha/2)]. The europium-doped boehmite from SD spontaneously dispersed in water: the luminescence spectroscopy proves that most of the Eu3+ ions were detached from the NPs during water dispersion. The AlOOH: Eu nanoparticles were modified by the amine acid asparagine (ASN). The modification aimed to render the NPs compatible for further bio-functionalization. After surface modification, the NPs easily dispersed in water; the luminescence spectra after dispersion prove that the Eu3+ ions were held at the boehmite surface.