It is generally accepted that growth of eutectic silicon in aluminium-silicon alloys occurs by a twin plane re-entrant edge (TPRE) mechanism. It has been proposed that modification of eutectic silicon by trace additions occurs due to a massive increase in the twin density caused by atomic effects at the growth interface. In this study, eutectic microstructures and silicon twin densities in samples modified by elemental additions of barium (Ba), calcium (Ca), yttrium (Y) and ytterbium (Yb) (elements chosen due to a near-ideal atomic radii for twinning) in an A356.0 alloy have been determined by optical microscopy, thermal analysis, X-ray diffractometry (XRD) and transmission electron microscopy (TEM). Addition of barium or calcium caused the silicon structure to transform to a fine fibrous morphology, while the addition of yttrium or ytterbium resulted in a refined plate-like eutectic structure. Twin densities in all modified samples are higher than in unmodified alloys, and there are no significant differences between fine fibrous modification (by Ba and Ca) and refined plate-like modification (by Y and Yb). The twin density in all modified samples is less than expected based on the predictions by the impurity induced twining model. Based on these results it is difficult to explain the modification with Ba, Ca, Y and Yb by altered twin densities alone.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of addition of maltodextrin on drying kinetics of drops containing fructose, glucose, sucrose and citric acid individually and in mixtures was studied experimentally using single drop drying experiments and numerically by solving appropriate mass and heat transfer equations. The numerical predictions agreed with the experimental moisture and temperature histories within 5-6% average relative (absolute) errors and average differences of +/- 1degreesC, respectively. The stickiness of these drops was determined using the glass transition temperature (T-g) of the drops' surface layer as an indicator. The experimental stickiness histories followed the model predictions with reasonable accuracy. A safe drying (non-sticky) regime in a spray drying environment has been proposed, and used to estimate the optimum amount of addition of maltodextrin for successful spray drying of 120 micron diameter droplets of fruit juices. (C) 2003 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To study the phase relations in the Bi-2212 and Yb2O3 system, Bi2Sr2Ca1-xYbxCu2Oy thick films are prepared by partial melt processing via an intermediate reaction between Bi-2212 and Yb2O3. When Bi-2212 and Yb2O3 are partially melted and then slowly cooled, solid solutions of Bi2Sr2Ca1-xYbxCu2Oy form by reactions between liquid and solid phases which contain Yb. Following these reactions, Ca is partially replaced in Bi-2212 matrix and participates in the formation of secondary phases, such as Bi-free, (Ca, Sr)O-x and CaO. Variation of the Bi-2212-Yb2O3 ratios and processing parameters changes the balance between the phases and leads to different Yb:Ca ratios in the Bi-2212 matrix of processed thick films. When the partial melting process is optimized for each sample to minimize the growth of secondary phases, x = 0.42-0.46 for the samples prepared at pO(2) = 0.01 atm, x = 0.24-0.29 for the samples prepared at pO(2) = 0.21 atm, x = 0.18-0.23 for the samples prepared at pO(2) = 0.99 atm are obtained regardless to the starting compositions. It is found that superconducting properties of Bi2Sr2Ca1-xYbxCu2Oy thick films strongly depend on the processing conditions, because the conditions result in different Yb content in the Bi-2212 matrix and the volume fraction of the secondary phases. The highest T-c(0) of 77, 90 and 91 K were obtained for the samples processed at 0.01, 0.21 and 0.99 atm of O-2, respectively.