930 resultados para Rare earth compounds
Resumo:
The present work deals with the texture, mineralogy and geochemistry of bedload sediments of the main stream of the Chaliyar basin, a typical small drainage system of the tropics enjoying heavy rain fall and moderate climate, located essentially in the Northern Kerala and flowing over the crystalline rocks (and their laterized duricrust) of the South Indian granulite terrain. As the Chaliyar is the major river draining the Wynad Gold Fields and is known for its placer gold occurrences, the thesis gives special emphasize on understanding the nature and distribution of detrital gold in sediments of the basin, while attempting to infer the provenance characteristics and factors involved in the evolution of sediments in general. Minerologically the chaliyar basin sands are quartzose. The quartz and feldspar contents in the coarse sand fraction of the basin range from 64 to 86% and 2 to 16% respectively. The Q/F ration ranges from 4 to 38 with a slight decrease in the lower reaches. Other minerals present include, hornblende, pyroxene and heavy minerals like opaques, garnet, rutile, biotite, spene, silliminite, zircon, apatite and monazite some of which are seen as inclusions in quartz. The major element composition of Chaliyar bedload sediments in the main channel and the headwater tributaries is related to the mineralogical and textual characteristics of sediments.
Resumo:
Ceramic dielectric resonators in the BaO-RE2O3-TiO2 (RE=rare earth) system have been prepared by the conventional solid state ceramic route. The dielectric properties have been tailored by substitution of different rare earth oxides and by bismuth oxide addition. The dielectric constants increased with Bi addition whereas the Q decreased. The temperature coeffecient of the resonant frequency improved with bismuth addition.
Resumo:
Ceramic dielectric resonators in the BaO-RE2O3-TiO2 (RE = rare earth) system have been prepared by the conventional solid state ceramic route. The dielectric properties have been tailored by substitution of different rare earth oxides and by bismuth oxide addition. The dielectric constants increased with Bi addition whereas the 0 decreased. The temperature coefficient of the resonant frequency improved with bismuth addition
Resumo:
Dielectric ceramics based on solid solution phases of [RE1_x= REr]TiNb06, where REI_s = Nd, Pr, Sm and RE' = Dy, Gd and Y, were prepared by the conventional solid-state ceramic route for values of x. The ceramic samples are characterized by X-ray diffraction and microwave methods. Ceramics based on RE (Pr, Nd and Sm) belonging to aeschynite group shows positive value of Tf and those based on RE (Gd, Dy and Y) belonging to euxenite group show negative value of r f. The solid solution phases between the aeschynite and the euxenite group shows intermediate dielectric constant and r f values. The results indicate the possibility of tailoring the dielectric properties by varying the composition of the solid solution phases. The range of solid solubility of euxenite in aeschenite and aeschenite in euxenite are different for different rare earth ions
Resumo:
Microwave dielectric ceramics based on RETiTaO6 (RE = La, Cc, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Y, Er, Yb, Al, and In) were prepared using a conventional solid-state ceramic route. The structure and microstructure of the samples were analyzed using x-ray diffraction and scanning electron microscopy techniques. The sintered samples were characterized in the microwave frequency region. The ceramics based on Ce, Pr, Nd, Sm, Eu, Gd, Tb, and Dy, which crystallize in orthorhombic aeschynite structure, had a relatively high dielectric constant and positive T f while those based on Ho, Er, and Yb, with orthorhombic euxenite structure, had a low dielectric constant and negative Tf. The RETiTaO6 ceramics had a high-quality factor. The dielectric constant and unit cell volume of the ceramics increased with an increase in ionic radius of the rare-earth ions, but density decreased with it. The value of Tf increased with an increase in RE ionic radii, and a change in the sign of Tf occurred when the ionic radius was between 0.90 and 0.92 A. The results indicated that the boundary of the aeschynite to euxenite morphotropic phase change lay between DyTiTaO6 and HoTiTaO6. Low-loss ceramics like ErTiTaO6 (Er = 20.6, Qxf = 85,500), EuTiTaO6 (Er = 41.3, Qxf = 59,500), and YTiTaO6 (Er = 22.1, Q„xf = 51,400) are potential candidates for dielectric resonator applications
Resumo:
Microwave dielectric ceramics based on GdTiNb,-,.Ta,O6 and Sml _.,Y,TiTa06 have been prepared by conventional solid state method . The GdTiTaO6 and SmTiTaO6 have aeschenite structure with positive rr and GdTiNbO6 and YTiTaO6 have euxenite structure with negative rr. The rr of the ceramics has been tuned by preparing solid solution phases between the aeschynites and euxenites for a possible zero rr material . It is observed that GdTiNbt_YTa.,O6 undergoes a phase transition from aeschynite to euxenite when x=0.75 and in Sml-,YxTiTa06 for x= 0.73. The microwave dielectric properties change abruptly near the transition region . The rr value approaches zero near the phase transition region while the samples have poor sinterability and poor quality factor . The unloaded quality factor, dielectric constant and the sign of rr of the solid solution phases are found to depend on the average ionic radius of the rare earth ion in RE ,-5RE',TiTaO6. The boundary of the euxenite-aeschynite phase transition occurs at an average ( RE) ionic radius of 0.915 A in Sm,_, Y,.TiTaO6 solid solution phases
Resumo:
Rare earth metal ion exchanged (La3+, Ce3+, RE3+) KFAU-Y zeolites were prepared by simple ion-exchange methods and have been characterized using different physico-chemical techniques. In this paper a novel application of solid acid catalysts in the dehydration/ Beckmann rearrangement of aldoximes; benzaldoxime and 4-methoxybenzaldoxime is reported. Dehydration/Beckmann rearrangement reactions of benzaldoxime and 4-methoxybenzaldoxime is carried out in a continuous down flow reactor at 473K. 4-Methoxybenzaldoxime gave both Beckmann rearrangement product (4-methoxyphenylformamide) and dehydration product (4-methoxybenzonitrile) in high overall yields. The difference in behavior of the aldoximes is explained in terms of electronic effects. The production of benzonitrile was near quantitative under heterogeneous reaction conditions. The optimal protocol allows nitriles to be synthesized in good yields through the dehydration of aldoximes. Time on stream studies show a fast decline in the activity of the catalyst due to neutralization of acid sites by the basic reactant and product molecules.
Resumo:
The electron-donor properties of Sm2O3 activated at 300, 500, and 800°C are reported from studies on the adsorption of electron acceptors of various electron affinities (electron affinity values in eV are given in parentheses): 7,7,8,8-tetracyanoquino-dimethane (2.84), 2,3,5,6-tetrachloro-1,4-benzoquinone (2.40), p-dinitrobenzene (1.77), and m-dinitrobenzene (1.26) in acetonitrile and 1,4-dioxane. The extent of electron transfer during the adsorption was determined from magnetic measurements. The acid-base properties of Sm2O3 at different activation temperatures are reported using a set of Hammett indicators. Electron donor-acceptor interactions at interfaces are important in elucidating the adhesion forces.
Resumo:
Surface acidity/Basicity of mixed oxides of La and Zn activated at three different temperatures were determined. The data have been correlated with the catalytic activity for liquid phase reduction of cyclohexanone in isopropanol.
Resumo:
A series of rare-earth neodymia supported vanadium oxide catalysts with various V205 loadings ranging from 3 to 15 wt.% were prepared by the wet impregnation method using ammonium metavanadate as the vanadium precursor. The nature of vanadia species formed on the support surface is characterized hy a series of different physicochemical techniques like X-ray diffraction (XRD). Fourier transform infrared spectroscopy (FTIR). BET surface area, diffuse reflectance UV-vis spectroscopy (DR UV-vis), thermal analysis (TG-DTG/DTA) and SEM. The acidity of the prepared systems were verified by the stepwise temperature programmed desorprion of ammonia (NH3-TPD) and found that the total acidity gets increased with the percentage of vanadia loading. XRD and FT1R results shows the presence of surface dispersed vanadyl species at lower loadings and the formation of higher vanadate species as the percentage composition of vanadia is increased above 9 wt.%. The low surface area of the support. calcination temperature and the percentage of vanadia loading are found to influence the formation of higher vanadia species. The catalytic activity of the V205-Nd203 catalysts was probed in the liquid phase hydroxylation of phenol and the result show that the present catalysts are active at lower vanadia concentrations.
Resumo:
MAGNESIUM ALLOYS have strong potential for weight reduction in a wide range of technical applications because of their low density compared to other structural metallic materials. Therefore, an extensive growth of magnesium alloys usage in the automobile sector is expected in the coming years to enhance the fuel efficiency through mass reduction. The drawback associated with the use of commercially cheaper Mg-Al based alloys, such as AZ91, AM60 and AM50 are their inferior creep properties above 100ºC due to the presence of discontinuous Mg17A112 phases at the grain boundaries. Although rare earth-based magnesium alloys show better mechanical properties, it is not economically viable to use these alloys in auto industries. Recently, many new Mg-Al based alloy systems have been developed for high temperature applications, which do not contain the Mg17Al12 phase. It has been proved that the addition of a high percentage of zinc (which depends upon the percentage of Al) to binary Mg-Al alloys also ensures the complete removal of the Mg17Al12 phase and hence exhibits superior high temperature properties.ZA84 alloy is one such system, which has 8%Zn in it (Mg-8Zn-4Al-0.2Mn, all are in wt %) and shows superior creep resistance compared to AZ and AM series alloys. These alloys are mostly used in die casting industries. However, there are certain large and heavy components, made up of this alloy by sand castings that show lower mechanical properties because of their coarse microstructure. Moreover, further improvement in their high temperature behaviour through microstructural modification is also an essential task to make this alloy suitable for the replacement of high strength aluminium alloys used in automobile industry. Grain refinement is an effective way to improve the tensile behaviour of engineering alloys. In fact, grain refinement of Mg-Al based alloys is well documented in literature. However, there is no grain refiner commercially available in the market for Mg-Al alloys. It is also reported in the literature that the microstructure of AZ91 alloy is modified through the minor elemental additions such as Sb, Si, Sr, Ca, etc., which enhance its high temperature properties because of the formation of new stable intermetallics. The same strategy can be used with the ZA84 alloy system to improve its high temperature properties further without sacrificing the other properties. The primary objective of the present research work, “Studies on grain refinement and alloying additions on the microstructure and mechanical properties of Mg-8Zn-4Al alloy” is twofold: 1. To investigate the role of individual and combined additions of Sb and Ca on the microstructure and mechanical properties of ZA84 alloy. 2. To synthesis a novel Mg-1wt%Al4C3 master alloy for grain refinement of ZA84 alloy and investigate its effects on mechanical properties.