596 resultados para miniscleral contact lens
Resumo:
This paper reports an experimental investigation of low Weber number water drops impacting onto solid surfaces exhibiting anisotropic wetting. The wetting anisotropy is created by patterning the solid surfaces with unidirectional parallel grooves. Temporal measurements of impacting drop parameters such as drop base contact diameter, apparent contact angle of drop, and drop height at the center are obtained from high-speed video recordings of drop impacts. The study shows that the impact of low Weber number water drops on the grooved surface exhibits beating phenomenon in the temporal variations of the dynamic contact angle anisotropy and drop height at the center of the impacting drop. It is observed that the beating phenomenon of impacting drop parameters is caused by the frequency difference between the dynamic contact angle oscillations of impacting drop liquid oriented perpendicular and parallel to the direction of grooves on the grooved surface. The primary trigger for the phenomenon is the existence of non-axisymmetric drop flow on the grooved surface featuring pinned and free motions of drop liquid in the directions perpendicular and parallel to the grooves, respectively. The beat frequency is almost independent of the impact drop Weber number. Further experimental measurements with solid surfaces of different groove textures show that the grooved surface with larger wetting anisotropy may be expected to show a dominant beating phenomenon. The phenomenon is gradually damped out with time and is fully unrecognizable at higher drop impact Weber numbers. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Soot particles are generated in a flame caused by burning ethylene gas. The particles are collected thermophoretically at different locations of the flame. The particles are used to lubricate a steel/steel ball on flat reciprocating sliding contact, as a dry solid lubricant and also as suspended in hexadecane. Reciprocating contact is shown to establish a protective and low friction tribo-film. The friction correlates with the level of graphitic order of the soot, which is highest in the soot extracted from the mid-flame region and is low in the soot extracted from the flame root and flame tip regions. Micro-Raman spectroscopy of the tribo-film shows that the a priori graphitic order, the molecular carbon content of the soot and the graphitization of the film as brought about by tribology distinguish between the frictions of soot extracted from different regions of the flame, and differentiate the friction associated with dry tribology from that recorded under lubricated tribology.
Resumo:
We report the effect of surface treatments on the dynamic conductance curves (G=dI/dV‐V) of Au‐Bi2Sr2CaCu2O8+δ (single crystal) point contact junctions of variable junction conductances (100 mS≳G≳100 μS). We find that if the crystal surface is cleaved freshly just prior to making contacts, all irreproducible sharp multiple features often observed in tunneling data of Bi(2212) oxide superconductors disappear. If the cleaved crystal surfaces are left under ambient conditions for a few days and the tunneling experiments are repeated, these multiple features reappear. We also find that if the current in the junction is made to pass predominantly through the bulk (and not along the surface), gap features are sharper. The observed conductance curves are fitted to a modified model [G. E. Blonder et al., Phys. Rev. B 25, 4515 (1982)] and estimated gap values are Δ≂28 to 30 meV corresponding to the ratio 2Δ/kBTc ≂ 7.5 with lifetime broadening Γ/Δ≂0.2. We conclude that the sharp multiple features observed in Bi(2212) tunneling curves has no intrinsic origin in the bulk and they arise from the surface only.
Resumo:
In order to understand the influence of ductile metal interlayer on the overall deformation behavior of metal/nitride multilayer, different configurations of metal and nitride layers were deposited and tested under indentation loading. To provide insight into the trends in deformation with multilayer spacings, an FEM model with elastic-perfect plastic metal layers alternate with an elastic nitride on top of an elastic-plastic substrate. The strong strain mismatch between the metal and nitride layers significantly alters the stress field under contact loading leading to micro-cracking in the nitride, large tensile stresses immediately below the contact, and a transition from columnar sliding in thin metal films to a more uniform bending and microcracking in thicker coatings.
Resumo:
Anisotropy plays important roles in various biological phenomena such as adhesion of geckos and grasshoppers enabled by the attachment pods having hierarchical structures like thin longitudinal setae connected with threads mimicked by anisotropic films. We study the contact instability of a transversely isotropic thin elastic film when it comes in contact proximity of another surface. In the present study we investigate the contact stability of a thin incompressible transversely isotropic film by performing linear stability analysis. Based on the linear stability analysis, we show that an approaching contactor renders the film unstable. The critical wavelength of the instability is a function of the total film thickness and the ratio of the Young's modulus in the longitudinal direction and the shear modulus in the plane containing the longitudinal axis. We also analyze the stability of a thin gradient film that is elastically inhomogeneous across its thickness. Compared to a homogeneous elastic film, it becomes unstable with a longer wavelength when the film becomes softer in going from the surface to the substrate.
Resumo:
This study presents unambiguous experimental evidence in support of the highly debated ``halogen bond donor'' character of organic fluorine. Two examples of intermolecular Cl center dot center dot center dot F contacts, with F-atom as halogen bond acceptor and donor, have been analyzed by in situ cryocrystallography and theoretical charge density studies.
Resumo:
In order to resolve some missing micromechanistic details regarding contact deformation in nitride multilayer coatings we report here observations from cross-sectional transmission electron microscopy and focused ion beam studies of the Vickers indentations on TiN/TiAlN multilayer films of various total thicknesses as well as bilayer periods. The study of damage induced by contact deformation in a nitride multilayer coating is complemented by stress calculated using an analytical model. Kinked boundaries of sliding columns give rise to cracks which propagate at an angle to the indentation axis under a combination of compressive and shear stresses. It is seen that multilayers provide more distributed columnar sliding, thereby reducing the stress intensity factor for shear cracking, while interfacial dislocations provide a stress relief mechanism by enabling lateral movement of material. (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
We employ nanoindentation coupled with electrical contact resistance measurements for simultaneous characterization of the electrical and mechanical behaviors of a cellular assembly of carbon nanotubes (CNTs). Experimental results reveal two different responses that correspond to relatively dense and porous regions of the cellular structure. Distinct nonlinear electron transport characteristics are observed, which mainly originate from diffusive conductance in the CNT structure. In the denser region, differential conductance shows asymmetric minima at lower bias, implying that conductivity mainly results from bulk tunneling. However, the porous regions show insignificant differential conduction as opposed to the denser region.