Solid-state compounds of general formula Ln(2)L(3)center dot nH(2)O, where L represents 1,4-bis(3-carboxy-3-oxo-prop-1-enyl)benzene and Ln = La, Ce, Pr, Nd, Sm, were synthesized. Complexometric titrations with EDTA, thermogravimetry (TG), differential thermal analysis (DTA), differential scanning calorimetry (DSC), X-ray powder diffractometry, elemental analysis and infrared spectroscopy have been employed to characterize and to study the thermal behavior of these compounds in dynamic air atmosphere. The results led to information about the composition, dehydration, crystallinity, and thermal decomposition of the synthesized compounds.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
The effect of thermal-shock cycles on the mechanical properties of fiber-metal laminates (FMLs) has been evaluated. FML plates were composed by two AA2024 Al sheets (1.6 mm thick) and one composite ply formed by two layers of unidirectional glass fiber epoxy prepreg and two layers of epoxy adhesive tape of glass fiber reinforced epoxy adhesive. The set was manufactured by hand layup and typical vacuum bag technique. The curing cycle was in autoclave at 125 +/- 5 degrees C for 90 min and an autoclave pressure of 400 kPa. FML coupons taken from the manufactured plate were submitted to temperature variations between -50 and +80 degrees C, with a fast transition between these temperatures. Tensile and interlaminar shear strength were evaluated on samples after 1000 and 2000 cycles, and compared to nonexposed samples. 2000 Cycles corresponds to typical C Check interval for commercial aircraft maintenance programs. It was observed that the thermal-shock cycles did not result in significant microstructural changes on the FML, particularly on the composite ply. Similarly, no appreciable effect on the mechanical properties of FML was observed by the thermal-shock cycles. (c) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Currently, high-strength materials, particularly AISI 4340 steel, are used in several landing gear components. Due to the high resistance to wear and corrosion required, the components are usually coating by hard chromium. This treatment produces waste, such as Cr+ 6 (hexavalent chromium), generally after applying the coating of hard chromium which is harmful to health and the environment. The process HVOF (High-velocity-oxygen-fuel) is considered a promising technique for deposition of hard chromium alternative coatings, for example, coatings based on tungsten carbide. This technique provides high hardness and good wear strength and more resistance to fatigue when compared to AISI 4340 hard chromium coated. To minimize loss fatigue due to the process of deposition, shot peening is used to obtain a compressive residual stress. The aim of this study was to analyze the effects of the tungsten carbide thermal spray coating applied by the HVOF, in comparison to the conventional hard chromium electroplating on the AISI 4340 high strength steel behavior in fatigue. Optical microscopy and scanning electron microscopy were used to observe crack origin sites, thickness and adhesion of the coating. (C) 2010 Published by Elsevier Ltd.
Resumo:
Borate glasses present an absorption coefficient very close to that of human tissue. This fact makes some borates ideal materials to develop medical and environmental dosimeters. Glass compositions with calcium tetraborate (CaB4O7) and calcium metaborate (CaB2O4), such as the xCaB(4)O(7) - (100-x)CaB2O4 System (0 <= x <= 100 wt%) were obtained by the traditional melting/quenching method. A phenomenon widely known as the 'boron anomaly' was observed in our thermal analysis measurements, as indicated by the increase of T, and the appearance of a maximum value in the composition with 40 wt% of CaB2O4. The Dy doped and Li co-doped 80CaB(4)O(7)-20CaB(2)O(4) (Wt%) glass samples were studied by the thermoluminescence technique. The addition of Dy improved the signal sensitivity in about three times with respect to the undoped glass sample. The addition of Li as a co-dopant in this glass caused a shift to a lower temperature of about 20 degrees C in the main glow peak. The structural analysis of the 80CaB(4)O(7)-20CaB(2)O(4) (wt%) undoped and doped samples were studied through infrared absorption. We have noted an increase in the coordination number of the boron atoms from 3 to 4, i.e., the conversion of the BO3 triangular structural units into BO4 tetrahedra. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).
Resumo:
In this work a biodegradable composite using the carnauba straw s powder as reinforcement on chitosan matrix polymeric were manufactured. Firstly, were carried out the chemistry characterization of the carnauba straw s powder before and after treatments with NaOH and hexane. Goering and Van Soest method (1970), flotation test, moisture absorption, FTIR, TG/DTG, DSC and SEM have also being carried out. Composites were developed with variations in granulometry and in powder concentrations. They were characterized by TG/DTG, SEM and mechanicals properties. The results of chemical composition showed that the carnauba straw s powder is composed of 41% of cellulose; 28,9% of hemicellulose and 14% of lignin.The flotation test have indicated that the chemical treatment with NaOH decreased the powder s hidrophilicity.The thermal analysis showed increased of thermal stability of material after treatments. The results of FTIR and SEM revealed the removal of soluble materials from the powder (hemicelluloses and lignin), the material became rougher and clean. The composites obtained showed that the mechanicals properties of the composites were decreased in respect at chitosan films, and the composites with the powder at 150 Mesh showed less variation in the modulus values. The speed test of 10 mm/min showed the better reproducibility of the results and is in agreement to the standard ASTM D638. The SEM analysis of fracture showed the low adhesion between the fiber/matrix. The increase of volume of powder in the composite caused a decrease in values of stress and strain for the samples with untreated powder and treated with hexane. The composite with 50% of the powder s treated in NaOH didn t have significant variation in the values of stress and strain as compared with the composites with 10% of the powder, showing that the increase in the volume of fiber didn t affect the stress and strain of the composite. Thereby, it is concluded that the manufacture of polymeric composites of chitosan using carnauba straw s powder can be done, without need for pre-treatment of reinforcement, become the couple of carnauba straw s powder-chitosan a good alternative for biodegradable composites
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
In the present work, tellurite 20Li(2)O-80TeO(2) glasses were prepared with identical nominal composition under different glass-forming histories to produce a stressed and stress-free samples. X-ray Diffraction (XRD) and Differential Scanning Calorimetry (DSC) techniques were used to study the effects of the glass-forming histories on the thermal and structural properties of these glasses. The gamma-TeO2 (metastable), alpha-TeO2 and alpha-Li2Te2O5 phases were identified during the controlled devitrification in these glasses. The mestastable character of the gamma-TeO2 phase was clearly observed in the glass under stress but this effect is not so clear in the stress-free glass. The gamma-TeO2 and alpha-TeO2 phases crystallizes during the initial stages of crystallization in both studied glasses while the alpha-Li2Te2O5 phase crystallize in the final stages of the crystallization. The activation energies and Avrami exponent were calculated for both studied glasses with different particle size leading to E-3 > E-2 > E-1 for stressed glass and E-3 > E-2 approximate to E-1 for stress-free glass, where E-1, E-2 and E-3 were associated to the gamma-TeO2, alpha-TeO2 and alpha-Li2Te2O5 phases, respectively. The observed distinct (n) over bar (1) < <(n)over bar>(2) < <(n)over bar>(3) in both glasses is an indicative that nucleation and growth takes place by more than one mechanism in the early stages of the crystallization. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)