Resumo:
Polycrystalline nano-grain-boundary multi-doping ZnO-based nonlinear varistors with higher concentration additives have been fabricated by sol-gel and standard solid-state reaction method, of which the best sample has a very high threshold voltage of E-b = 3300 V/mm. The effect of sintering processes, sintering temperature and sintering time, and that of additive concentration of Bi2O3 on E-b of the samples are systematically investigated. The results show that the great merit of sol-gel method is its high threshold voltage obtained by a lower sintering temperature than the solid-state reaction method. The present work also shows that five phases including solid-state sintering, rich Bi liquid phase formation and ZnO as well as other additive dissolution, ZnO grain growth, the secondary phase sufficient formation and evolution have been experienced at different sintering temperatures. The hole type defect and nonhomogeneity of the microstructure will lead to the decrease of threshold voltage, i.e., the grain size and the homogeneity of the material will be important factors and directly affect the characteristic of the varistor. The sintering characteristic and the influence of Bi2O3 content on the threshold voltage are also discussed. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
A new type of photovoltaic system with higher generation power density has been studied in detail. The feature of the proposed system is a V-shaped structure with two polycrystalline solar cells. Compared to solar cells in a conventional approach, the V-shaped structure enhances external quantum efficiency and leads to an increase of 24% in power conversion efficiency.
Resumo:
Using micro-photoluminescence technique, we observed a new photoluminescence peak about 0.348 eV above the bandgap of GaAs (E-0). By analyzing its optical characteristics, we assigned this peak to the nonequilibrium luminescence emission from the E-0 + Delta(0) bandgap in semi-insulated GaAs, which was further verified by Raman results. The observed polarization, excitation power dependence and temperature dependence of the photoluminescence spectra from the E-0 + Delta(0) energy level were very similar to those from the E-0 of GaAs. This mainly resulted from the common conduction band around Gamma(6) that was involved in the two optical transition processes, and indicated that the optical properties of bulk GaAs were mainly determined by the intrinsic properties of the conduction band. Our results demonstrated that the micro-photoluminescence technique is a powerful tool to investigate the high energy states above the fundamental bandgap in semiconductor materials.
Resumo:
We propose and demonstrate measurement of the frequency response of an electroabsorption (EA) modulator using an extended small-signal power measuring technique. In this technique, the modulator is driven by a microwave carrier amplitude modulated by a low-frequency signal, and the modulator frequency response is obtained without the need of a high-speed photodetector. Based upon the nonlinear characteristics of the EA modulator and the underlying principle of the present method, equations have been derived. A measurement scheme using a network analyzer and a low-speed photodetector has been proposed and constructed, and the experimental results confirm that our proposed method is as accurate as the swept-frequency measurement using a network analyzer directly.
Resumo:
Nonlinear optical properties of silicon nanocrystals (nc-Si) embedded in SiO2 films are investigated using time-resolved four-wave mixing technique with a femtosecond laser. the off-resonant third-order nonlinear susceptibility chi((3)) is observed to be 1.3 x 10(-10) esu at 800 nm. The relaxation time of the film is fast as short as 50 fs. The off-resonant nonlinearity is predominantly electronic in origin and enhanced due to quantum confinement.
Resumo:
Mode characteristics of a strongly confined square cavity suspended in air via a pedestal on the substrate are investigated by a three-dimensional finite-difference time-domain technique. The mode wavelengths and mode quality factors (Q factors) are calculated as the functions of the size of the pedestal and the slope angle 0 of the sidewalls of the square slab, respectively For the square slab with side length of 2 mu m, thickness of 0.2 mu m, and refractive index of 3.4, on a square pedestal with refractive index of 3.17, the Q factor of the whispering-gallery (WG)-like mode transverse-electric TE(3.5)o first increases with the side length b of the square pedestal and then quickly decreases as b > 0.4 mu m, but the Q factor of the WG-like mode TE(4.6)o drops down quickly as b > 0.2 mu m, owing to their different symmetries. The results indicate that the pedestal can also result in mode selection in the WG-like modes. In addition, the numerical results show that the Q factors decrease 50% as the slope angle of the sidewalls varies from 90 degrees to 80 degrees. The mode characteristics of WG-like modes in the square cavity with a rectangular pedestal are also discussed. The results show that the nonsquare pedestal largely degrades the WG-like modes. (c) 2006 Optical Society of America
Resumo:
The mode characteristics of a three-dimensional (3D) microdisk with a vertical refractive index distribution of n(2)/3.4/n(2) are investigated by the S-matrix method and 3D finite-difference time-domain (FDTD) technique. For the microdisk with a thickness of 0.2 mu m. and a radius of 1 mu m, the mode wavelengths and quality factors for the HE7,1 mode obtained by 3D FDTD simulation and the S-matrix method are in good agreement as n(2) increases from 1.0 to 2.6. But the Q factor obtained by the 3D FDTD rapidly decreases from 1.12 X 10(4) to 379 as n2 increases from 2.65 to 2.8 owing to the vertical radiation losses, which cannot be predicted by the proposed S-matrix method. The comparisons also show that quality factors obtained from the analytical solution of two-dimensional microdisks under the effective index approximation are five to seven times smaller than those of the 3D FDTD as n(2) = 1 and R = 1 mu m. (c) 2006 Optical Society of America.
Resumo:
Quality factor enhancement due to mode coupling is observed in a three-dimensional microdisk resonator. The microdisk, which is vertically sandwiched between air and a substrate, with a radius of 1 mu m, a thickness of 0.2 mu m, and a refractive index of 3.4, is considered in a finite-difference time-domain (FDTD) numerical simulation. The mode quality factor of the fundamental mode HE71 decreases with an increase of the refractive index of the substrate, n(sub), from 2.0 to 3.17. However, the mode quality factor of the first-order mode HE72 reaches a peak value at n(sub) = 2.7 because of the mode coupling between the fundamental and the first-order modes. The variation of mode field distributions due to the mode coupling is also observed. This mechanism may be used to realize high-quality-factor modes in microdisks with high-refractive-index substrates. (c) 2006 Optical Society of America.
Resumo:
The mode frequencies and quality factors (Q-factors) in two-dimensional (2-D) deformed square resonators are analyzed by finite-difference time-domain (FDTD) technique. The results show that the deformed square cavities with circular and cut corners have larger Q-factors than the perfect ones at certain conditions. For a square cavity with side length of 2 mu m and refractive index of 3.2, the mode Q-factor can increase 13 times as the perfect corners are replaced by a quarter of circle with radius of 0.3 pm. Furthermore the blue shift with the increasing deformations is found as a result of the reduction in effective resonator area. In square cavities with periodic roughness at sidewalls which maintains the symmetry of the square, the Q-factors of the whisperin gallery (WG)-like modes are still one order of magnitude larger that those of non-WG-like modes. However, the Q-tactors of these two types of modes are of the same order in the square cavity with random roughness. We also find that the rectangular and rhombic deformation largely reduce the Q-factors with the increasing offset and cause the splitting of the doubly degenerate modes due to the breaking of certain symmetry properties.
Resumo:
The mode frequency and the quality factor of nanowire cavities are calculated from the intensity spectrum obtained by the finite-difference time-domain (FDTD) technique and the Pade approximation. In a free-standing nanowire cavity with dielectric constant epsilon = 6.0 and a length of 5 mu m, quality factors of 130, 159, and 151 are obtained for the HE11 modes with a wavelength around 375 nm, at cavity radius of 60, 75, and 90 nm, respectively. The corresponding quality factors reduce to 78, 94, and 86 for a nanowire cavity standing on a sapphire substrate with a refractive index of 1.8. The mode quality factors are also calculated for the TE01 and TM01 modes, and the mode reflectivities are calculated from the mode quality factors.
Resumo:
Radio frequency magnetron sputtering/post-carbonized-reaction technique was adopted to prepare good-quality GaN films on Al2O3(0 0 0 1) substrates. The sputtered Ga2O3 film doped with carbon was used as the precursor for GaN growth. X-ray diffraction (XRD) pattern reveals that the film consists of hexagonal wurtzite GaN. X-ray photoelectron spectroscopy (XPS) shows that no oxygen can be detected. Electrical and room-temperature photoluminescence measurements show that good-quality polycrystalline GaN films were successfully grown on Al2O3(0 0 0 1) substrates. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
In this paper we propose a new method for measuring the thickness of the GaN epilayer, by using the ratio of the integrated intensity of the GaN epilayer X-ray diffraction peaks to that of the sapphire substrate ones. This ratio shows a linear dependence on the GaN epilayer thickness up to 2 mum. The new method is more accurate and convenient than those of using the relationship between the integrated intensity of GaN epilayer diffraction peaks and the GaN thickness. Besides, it can eliminate the absorption effect of the GaN epilayer.
Resumo:
Semiconducting gadolinium silicide GdxSi samples were prepared by mass-analyzed low-energy dual ion beam epitaxy technique. Auger electron spectroscopy depth profiles indicate that the gadolinium ions are implanted into the single-crystal silicon substrate and formed 20 nm thick GdxSi film. X-ray double-crystal diffraction measurement shows that there is no new phase formed. The XPS spectra show that one type of silicon peaks whose binding energy is between that of silicide and silicon dioxide, and the gadolinium peak of binding energy is between that of metal Gd and Gd2O3. All of these results indicate that an amorphous semiconductor is formed. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
We successfully used the metal mediated-wafer bonding technique in transferring the as-grown cubic GaN LED structure of Si substrate. The absorbing GaAs substrate was removed by using the chemical solutions of NH4OH : H2O2=1 : 10. SEM and PL results show that wafer bonding technique could transfer the cubic GaN epilayers uniformly to Si without affecting the physical and optical properties of epilayers. XRD result shows that there appeared new peaks related to AgGa2 and Ni4N diffraction, indicating that the metals used as adhesive and protective layers interacted with the p-GaN layer during the long annealing process. It is just the reaction that ensures the reliability of the integration of GaN with metal and minor contact resistance on the interface.
Resumo:
Semiconducting manganese silicide, Mn27Si47 and Mn15Si26, were obtained using mass-analyzed low energy dual ion beam epitaxy technique, Auger electron spectroscopy depth profiles showed that some of the Mn ions were deposited on single-crystal silicon substrate and formed a 37.5 nm thick Mn film, and the other Mn ions were successfully implanted into the Si substrate with the implantation depth of 618 nm. Some samples were annealed in the atmosphere of flowing N-2 at 840 degreesC. X-ray diffraction measurements showed that the annealing was beneficial to the formation of Mn27Si47 and Mn15Si26 (C) 2001 Published by Elsevier Science B.V.