895 resultados para gel electrolyte
Evolution of the viscoelastic properties of SnO2 colloidal suspensions during the sol-gel transition
Resumo:
This paper describes the effect of the concentration of electrolyte and pH on the kinetics of aggregation and gelation processes of SnO2 colloidal suspensions. Creep, creep-recovery, and oscillatory rheological experiments have been done in situ during aggregation and gelation. A phenomenological description of the structure of the colloidal system is given from the time evolution of rheological parameters. The dependence of the equilibrium steady-state shear compliance on the terminal region of clusters or aggregates seems to be a way to determine the beginning of interconnection of aggregates and the gel point. We propose that at this point the equilibrium steady-state compliance is a minimum. The steady-state viscosity determined from creep experiment can be fit with a power law with the extent of the transformation, giving critical exponent s = 0.7 ± 0.1. The value of the critical exponent Δ = 0.78 ± 0.05 was determined from oscillatory experiment. These results indicate that gelation of SnO2 colloidal suspension exhibits the typical scale expected from the scalar percolation theory. © 2000 Elsevier Science B.V. All rights reserved.
Resumo:
A solid state system having the configuration WO 3/Ormolyte/CeO2-TiO2 has been assembled. Syntheses routes for tungsten oxide WO3, and cerium-titanium CeO 2-TiO2 oxide sols, were developed. A novel solid electrolyte - Ormolyte is reported, which were obtained by the sol-gel process, they have a chemical stability due to the covalent bonds between the inorganic and organic phase, and were prepared with different [O]/[L] ratios, being the best for [O]/[L]=15. The variation of transmittance of the electrochromic device using the ormolyte [O]/[L]=15 was 35% (colored state) and 77% (bleached state).
Resumo:
Gellan-based polymer electrolytes (PEs), doped with lithium iodide (LiI), were prepared and their electrical properties were characterized. The samples are thermally stable up to 234 degrees C and exhibit ionic conductivity of 3.8 x 10(-4) S/cm at room temperature for the sample doped with 40 wt% of LiI. Addition of 10 wt% of glycerol promotes an increase of the ionic conductivity to 1.5 x 10(-3) S/cm, which remains stable up to 100 degrees C. The activation energies of 2.4 to 12.4 kJ/mol were derived from the Arrhenius model. The repeated ionic conductivity measurements as a function of temperature show that these membranes can be reversibly used between the room temperature and 100 degrees C.
Resumo:
A 10 mol%Sc2O3, 1 mol%CeO2 stabilized-ZrO2 (SSZ) powder was successfully prepared using the sol-gel method. Subsequent SSZ electrolyte pellets were prepared by tape casting technique and sintered at 1400 °C, 1450 °C, 1500 °C, 1550 °C and 1600 °C. These were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and electrochemical impedance spectroscopy (EIS). SSZ showed a pure cubic phase after sintering, the grain size of SSZ increased with the increase of sintering temperature. The SSZ sintered at 1550 °C showed the highest ion conductivity. The maximum power densities of Ni-SSZ/SSZ/La0.8Sr0.2MnO3-δ (LSM)-SSZ single cells sintered at 1550 °C were 0.18, 0.36, 0.51 and 0.72 W cm-2 at 650, 700, 750 and 800 °C, respectively. The polarization resistance (Rp) of the single cell attained 0.201 Ω cm2 at 800 °C.
Nafion-mesoporous silica composite electrolyte: properties and direct ethanol fuel cells performance