DNA vaccines or proteins are capable of inducing specific immunity; however, the translation to the clinic has generally been problematic, primarily due to the reduced magnitude of immune response and poor pharmacokinetics. Herein we demonstrate a composite microsphere formulation, composed of mesoporous silica spheres (MPS) and poly(d,l-lactide-co-glycolide) (PLGA), enables the controlled delivery of a prime-boost vaccine via the encapsulation of plasmid DNA (pDNA) and protein in different compartments. Method with modified dual-concentric-feeding needles attached to a 40 kHz ultrasonic atomizer was studied. These needles focus the flow of two different solutions, which passed through the ultrasonic atomizer. The process synthesis parameters, which are important to the scale-up of composite microspheres, were also studied. These parameters include polymer concentration, feed flowrate, and volumetric ratio of polymer and pDNA-PEI/MPS-BSA. This fabrication technique produced composite microspheres with mean D[4,3] ranging from 6 to 34 μm, depending upon the microsphere preparation. The resultant physical morphology of composite microspheres was largely influenced by the volumetric ratio of pDNA-PEI/MPS-BSA to polymer, and this was due to the precipitation of MPS at the surface of the microspheres. The encapsulation efficiencies were predominantly in the range of 93-98% for pDNA and 46-68% for MPS. In the in vitro studies, the pDNA and protein showed different release kinetics in a 40 day time frame. The dual-concentric-feeding in ultrasonic atomization was shown to have excellent reproducibility. It was concluded that this fabrication technique is an effective method to prepare formulations containing a heterologous prime-boost vaccine in a single delivery system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Improved biopharmaceutical delivery may be achieved via the use of biodegradable microspheres as delivery vehicles. Biodegradable microspheres offer the advantages of maintaining sustained protein release over time whilst simultaneously protecting the biopharmaceutical from degradation. Particle samples produced by ultrasonic atomization were studied in order to determine a feed stock capable of producing protein loaded poly-ε-caprolactone (PCL) particles suitable for nasal delivery (i.e., less than 20 μm). A 40 kHz atomization system was used with a 6 mm full wave atomization probe. The effect of solids percent, feed flow rate, volumetric ratio of the polymer stock to the protein stock, and protein concentration in the protein stock on particle size characteristics were determined. It was shown that feed stocks containing 100 parts of 0.5 or 1.0% w/v PCL in acetone with one part 100 mg ml -1 BSA and 15 mg ml -1 PVA produced particles with a mass moment diameter (D[4,3]) of 13.17 μm and 9.10 μm, respectively in addition to displaying high protein encapsulation efficiencies of 93 and 95%, respectively. The biodegradable PCL particles were shown to be able to deliver encapsulated protein in vitro under physiological conditions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Simple and reliable formation of biodegradable nanoparticles formed from poly-ε-caprolactone was achieved using 1.645 MHz piston atomization of a source fluid of 0.5% w/v of the polymer dissolved in acetone; the particles were allowed to descend under gravity in air 8 cm into a 1 mM solution of sodium dodecyl sulfate. After centrifugation to remove surface agglomerations, a symmetric monodisperse distribution of particles φ 186 nm (SD=5.7, n=6) was obtained with a yield of 65.2%. © 2006 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Biopharmaceuticals have been shown to have low delivery and transformation efficiencies. To over come this, larger doses are administered in order to obtain the desired response which may lead to toxicity and drug resistance. This paper reports upon a continuous particle production method utilizing surface acoustic wave atomization to reliably produce micro and nanoparticles with physical characteristics to facilitate the cellular uptake of biopharmaceuticals. By producing particles of an optimal size for cellular uptake, the efficacy and specificity of drug loaded nanoparticles will be increased. Better delivery methods will result in dosage reduction (hence lower costs per dose), reduced toxicity, and reduced problems associated with multidrug resistance due to over dosing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Autogenous vein grafting is widely used in regular bypassing procedures. Due to its mismatch with the host artery in both mechanical property and geometry, the graft often over expands under high arterial blood pressure and forms a step-depth where eddy flow develops, thus causing restenosis, fibrous graft wall, etc. External stents, such as sheaths being used to cuff the graft, have been introduced to eliminate these mismatches and increase the patency. Although histological and immunochemical studies have shown some positive effects of the external stent, the mechanical mismatch under the protection of an external stent remains poorly analyzed. Methods: In this study, the jugular veins taken from hypercholesterolemic rabbits were transplanted into the carotid arteries, and non-woven polyglycolic acid (PGA) fabric was used to fabricate the external stents to study the effect of the biodegradable external stent. Eight weeks after the operation, the grafts were harvested to perform mechanical tests and histological examinations. An arc tangent function was suggested to describe the relationship between pressure and cross-sectional area to analyse the compliance of the graft. Results: The results from the mechanical tests indicated that grafts either with or without external stents displayed large compliance in the low-pressure range and were almost inextensible in the high-pressure range. This was very different from the behavior of the arteries or veins in vivo. The data from histological tests showed that, with external stents, collagen fibers were more compact, whilst those in the graft without protection were looser and thicker. No elastic fiber was found in either kind of grafts. Furthermore, grafts without protection were over-expanded which resulted in much bigger cross-sectional areas. Conclusion: The PGA external extent contributes little to the reduction of the mechanical mismatch between the graft and its host artery while remodeling develops. For the geometric mismatch, it reduces the cross-section area, therefore matching with the host artery much better. Although there are some positive effects, conclusively the PGA is not an ideal material for external stent.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, biodegradable blend of Poly (Ethylene-co-Vinyl Acetate) (EVA) and Ethyl Cellulose (EC) were prepared. Ethylene vinyl alcohol (EVOH) copolymer was used as an interfacial compatibilizer to enhance adhesion between EVA and EC. The melt blended compatibilized biocomposites were examined for mechanical and thermal properties as per the ASTM standards. It has been found that the EC has a reinforcing effect on EVA leading to enhanced tensile strength and also impart biodegradability. Thus, a high loading of 50% EC could be added without compromising Much on the mechanical properties. Analysis of the tensile data using predictive theories showed an enhanced interaction of the dispersed phase (EC) and the matrix (EVA). The compatibilizing effects of EVOH on these blends were confirmed by the significant improvement in the mechanical properties comparable with neat EVA as also observed by SEM microscopy. The TGA thermograms exhibits two-stage degradation and as EC content increases, the onset temperature for thermal degradation reduces. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 116: 1044-1056, 2010

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new family of castor oil based biodegradable polyesters was synthesized by catalyst free melt condensation reaction between two different diacids and castor oil with D-mannitol. The polymers synthesized were characterized by NMR spectroscopy, FF-IR and the thermal properties were analysed by DSC. The results of DSC show that the polymer is rubbery in physiological conditions. The contact angle measurement and hydration test results indicate that the surface of the polymer is hydrophilic. The mechanical properties, evaluated in the tensile mode, shows that the polymer has characteristics of a soft material. In vitro degradation of polymer in PBS solution carried out at physiological conditions indicates that the degradation goes to completion within 21 days and it was also found that the rate of degradation can be tuned by varying the curing conditions. (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three groups of poly(mannitol citric dicarboxylate) [p(MCD)] copolyesters were synthesized by catalyst-free melt condensation of mannitol with acids. The resulting copolyesters were designated as poly(mannitol citric succinate) [p(MCSu)], poly(mannitol citric adipate) [p(MCA)], poly(mannitol citric sebacate) [p(MCS)]. The polymers were characterized by FTIR, (1)H NMR, and DSC analysis. The synthesized p(MCD) polymers exhibit glass transition temperatures ranging from 16.5 to 58.58 degrees C. The mechanical, degradation properties, and the drug-releasing characteristics of these polymers were investigated. It was observed that the mechanical properties of the p(MCD) polymers cover a wide range with Young's modulus of the polymer varying from 12.25 to 660 MPa. Hydrolytic degradation of all polymers was investigated by incubating polymer discs in PBS and the hydrolytic degradation of p(MCD) polymers followed the order, p(MCSu) > p(MCA) > p(MCS). This was attributed to the number of -CH(2)(units in the dicarboxylic monomers. The release of model drug compounds from the p(MCD) polymer discs was also studied. POLYM. ENG. SCI., 51:2035-2043, 2011. (C) 2011 Society of Plastics Engineers

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Castor oil-based poly(mannitol-citric sebacate) was synthesized by simple, catalyst-free melt condensation process using monomers having potential to be metabolized in vivo. The polymer was characterized using various techniques and the tensile and hydration properties of the polymers were also determined. The biocompatibility of the polymer was tested using human foreskin fibroblasts cells. The in vitro degradation studies show that the time for complete degradation of the polymer was more than 21 days. The usage of castor oil polyester as a drug carrier was analysed by doping the polymer with 5-fluorouracil model drug and the release rate was studied by varying the percentage loading of drugs and the pH of the PBS solution medium. The cumulative drug-release profiles exhibited a biphasic release with an initial burst release and cumulative 100% release within 42 h. To understand the role of the polymer as a drug carrier in the release behaviour, drug-release studies were conducted with another drug, isoniazid. The release behaviour of isoniazid drug from the same polymer matrix followed an nth order kinetic model and 100% cumulative release was achieved after 12 days. The variation in the release behaviour for two model drugs from the same polymer matrix suggests a strong interaction between the polymer and the drug molecule.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new family of ricinoleic acid based polyesters was synthesized using catalyst free melt-condensation polymerization with sebacic acid, citric acid, mannitol and ricinoleic acid as precursors. The use of FT-IR and NMR characterisation techniques confirms the presence of ester linkages in the as-synthesized polymers. Depending on the precursor combination, their relative amount and the degree of curing, a broad range of elastic modulus (22-327 MPa) and tensile strength (0.7-12.7 MPa) can be obtained in the newly synthesized biopolymers. The polymers show rubbery behaviour at a physiological temperature (37 degrees C) and the contact angles of the synthesized polymers fall in the range of 42 degrees to 71 degrees, making them ideal substrates to study delivery of drugs through polymer scaffolds. The cytocompatibility assessment of the cured polymers confirmed good cell attachment and growth of smooth muscle cells (C2C12 myoblast cells). Importantly, oriented cell growth was observed after culturing myoblast cells for 3 days. The in vitro degradation in PBS indicates that the mild cured polymers follow a first order reaction kinetics and have degradation rate constants in the range of 0.009-0.038 h(-1), depending on the relative proportions of monomers. Overall, the results of our study indicate that the physical properties can be tailored by varying the composition of the monomers and curing conditions in the newly developed polyesters. Hence, they may be used as potential substrates for tissue engineering scaffolds and for localized drug delivery.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Biodegradable composites comprising of modified starch and modified nanoclay have been prepared. Starch has been modified by esterification and subsequently crosslinked. The thermal, mechanical, and biodegradation characteristics of the composites have been investigated. The compressive properties of the composites with the addition of nanoclay were twice that of crosslinked starch phthalate without addition of nanoclay. Predictive theories were used to analyze the obtained experimental results. SEM studies on fracture morphology indicated quasi-brittle fracture. Flexural properties showed considerable improvement due to nanoclay addition. The water uptake increased up to 6% nanoclay, beyond which the uptake decreased. Biodegradation studies showed an initial time lag prior to the onset of degradation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In order to suppress chronic inflammation while supporting cell proliferation, there has been a continuous surge toward development of polymers with the intention of delivering anti-inflammatory molecules in a sustained manner. In the above backdrop, we report the synthesis of a novel, stable, cross-linked polyester with salicylic acid (SA) incorporated in the polymeric backbone and propose a simple synthesis route by melt condensation. The as-synthesized polymer was hydrophobic with a glass transition temperature of 1 degrees C, which increases to 17 degrees C upon curing. The combination of NMR and FT-IR spectral techniques established the ester linkages in the as-synthesized SA-based polyester. The pH-dependent degradation rate and the rate of release of salicylic acid from the as-synthesized SA-based polymer were studied at physiological conditions in vitro. The polyester underwent surface erosion and exhibited linear degradation kinetics in which a change in degradation rate is observed after 4-10 days and 24% mass loss was recorded after 4 months at 37 degrees C and pH 7.4. The delivery of salicylic acid also showed a similar change in slopes, with a sustained release rate of 3.5% in 4 months. The cytocompatibility studies of these polyesters were carried out with C2C12 murine myoblast cells using techniques like MTT assay and flow cytometry. Our results strongly suggest that SA-based polyester supports cell proliferation for 3 days in culture and do not cause cell death (<7%), as quantified by propidium iodide (PI) stained cells. Hence, these polyesters can be used as implant materials for localized, sustained delivery of salicylic acid and have applications in adjuvant cancer therapy, chronic wound healing, and as an alternative to commercially available polymers like poly(lactic acid) and poly(glycolic acid) or their copolymers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mg and its alloys become natural biomaterials as the elemental Mg is found in the human body in abundance and their mechanical properties being akin to the natural bone as well as due to their inherent bioabsorbable/bioresorbable property. This paper discusses the development of new Mg alloys and their corrosion characteristics in detail. The latest advancements in coating of Mg alloys to control their degradation rate are also reviewed along with the future challenges that need to be addressed.