982 resultados para applied physics
Resumo:
Oxides RNiO(3) (R - rare-earth, R not equal La) exhibit a metal-insulator (MI) transition at a temperature T(MI) and an antiferromagnetic (AF) transition at T(N). Specific heat (C(P)) and anelastic spectroscopy measurements were performed in samples of Nd(1-x)Eu(x)NiO(3), 0 <= x <= 0.35. For x - 0, a peak in C(P) is observed upon cooling and warming at essentially the same temperature T(MI) - T(N) similar to 195 K, although the cooling peak is much smaller. For x >= 0.25, differences between the cooling and warming curves are negligible, and two well defined peaks are clearly observed: one at lower temperatures that define T(N), and the other one at T(MI). An external magnetic field of 9 T had no significant effect on these results. The elastic compliance (s) and the reciprocal of the mechanical quality factor (Q(-1)) of NdNiO(3), measured upon warming, showed a very sharp peak at essentially the same temperature obtained from C(P), and no peak is observed upon cooling. The elastic modulus hardens below T(MI) much more sharply upon warming, while the cooling and warming curves are reproducible above T(MI). Conversely, for the sample with x - 0.35, s and Q(-1) curves are very similar upon warming and cooling. The results presented here give credence to the proposition that the MI phase transition changes from first to second order with increasing Eu doping. (C) 2011 American Institute of Physics. [doi: 10.1063/1.3549615]
Resumo:
The effect of weak dipolar interactions (DIs) between Ni nanoparticles (NPs) in samples with different Ni concentrations was investigated by performing a detailed characterization of their structural and magnetic properties. From the determination of several physical parameters of Ni NP assemblies, it was found that the ac and dc magnetic susceptibility measurements are valuable for identifying the DIs between NPs while hysteresis loops measurements showed to be very insensitive, provided that the strength of the DI field is much smaller than the maximum coercive field. Therefore, the sensitivity of the observed static and dynamical magnetic properties to the effect of weak DI depends on the measurement protocols used. (C) 2011 American Institute of Physics. [doi:10.1063/1.3556767]
Resumo:
We show, using ab initio density functional theory calculations, that Mn dimers adsorbed on graphene nanoribbons (Mn(2)/GNRs) present a magnetic bistability, as does the isolated Mn dimer. Our total energy results indicate that Mn dimers lying along the edge sites of zigzag GNRs represent the most likely configuration. We find that similar to the isolated Mn(2) molecule, the antiferromagnetic coupling represents the ground state for Mn(2)/GNR, and the spin density configuration of the GNR does not play an important role on the net magnetic moment of Mn(2), which makes GNRs an ideal substrate for adsorption of these molecules. The ground state and the excited state configuration of the Mn dimer, viz., low-spin (LS) and high-spin (HS), are maintained in the face of changes in the spin density configuration of the substrate. Here we find that the Mn(2)/GNR systems exhibit a LS <-> HS binary behavior, which can be considered as a useful property in the development of nanomemories based upon metallic clusters. (C) 2011 American Institute of Physics. [doi:10.1063/1.3553849]
Resumo:
The energy barrier distribution E(b) of five samples with different concentrations x of Ni nanoparticles using scaling plots from ac magnetic susceptibility data has been determined. The scaling of the imaginary part of the susceptibility chi""(v, T) versus T ln (iota t/tau(0)) remains valid for all samples, which display Ni nanoparticles with similar shape and size. The mean value < E(b)> increases appreciably with increasing x, or more appropriately with increasing dipolar interactions between Ni nanoparticles. We argue that such an increase in < E(b)> constitutes a powerful tool for quality control in magnetic recording media technology where the dipolar interaction plays an important role. (c) 2011 American Institute of Physics. [doi: 10.1063/1.3533911]
Resumo:
Bulk Zn(1-x)Co(x)O samples were synthesized via standard solid-state reaction route with different Co molar concentrations up to 21%. A detailed microstructural analysis was carried out to investigate alternative sources of ferromagnetism, such as secondary phases and nanocrystals embedded in the bulk material. Conjugating different techniques we confirmed the Zn replacement by Co ions in the wurtzite ZnO structure, which retains, however, a high crystalline quality. No segregated secondary phases neither Co-rich nanocrystals were detected. Superconducting quantum interference device magnetometry demonstrates a paramagnetic Curie-Weiss behavior with antiferromagnetic interactions. We discuss the observed room temperature paramagnetism of our samples considering the current models for the magnetic properties of diluted magnetic semiconductors. (C) 2010 American Institute of Physics. [doi: 10.1063/1.3459885]
Resumo:
The thermodynamic properties of the magnetic semiconductors GaMnAs and GaCrAs are studied under biaxial strain. The calculations are based on the projector augmented wave method combined with the generalized quasichemical approach to treat the disorder and composition effects. Considering the influence of biaxial strain, we find a tendency to the suppression of binodal decomposition mainly for GaMnAs under compressive strain. For a substrate with a lattice constant 5% smaller than the one of GaAs, for GaMnAs, the solubility limit increases up to 40%. Thus, the strain can be a useful tool for tailoring magnetic semiconductors to the formation or not of embedded nanoclusters. (C) 2010 American Institute of Physics. [doi:10.1063/1.3448025]
Resumo:
Magnetic nanoparticles (NP) of magnetite (Fe(3)O(4)) coated with oleic acid (OA) and dodecanoic acid (DA) were synthesized and investigated through transmission electron microscopy (TEM), magnetization M, and ac magnetic susceptibility measurements. The OA coated samples were produced with different magnetic concentrations (78%, 76%, and 65%) and the DA sample with 63% of Fe(3)O(4). Images from TEM indicate that the NP have a nearly spherical geometry and mean diameter similar to 5.5 nm. Magnetization measurements, performed in zero-field cooled (ZFC) and field cooled processes under different external magnetic fields H, exhibited a maximum at a given temperature T(B) in the ZFC curves, which depends on the NP coating (OA or DA), magnetite concentration, and H. The temperature T(B) decreases monotonically with increasing H and, for a given H, the increase in the magnetite concentration results in an increase in T(B). The observed behavior is related to the dipolar interaction between NP, which seems to be an important mechanism in all samples studied. This is supported by the results of the ac magnetic susceptibility chi(ac) measurements, where the temperature in which chi' peaks for different frequencies follows the Vogel-Fulcher model, a feature commonly found in systems with dipolar interactions. Curves of H versus T(B)/T(B) (H=0) for samples with different coatings and magnetite concentrations collapse into a universal curve, indicating that the qualitative magnetic behavior of the samples may be described by the NP themselves, instead of the coating or the strength of the dipolar interaction. Below T(B), M versus H curves show a coercive field (H(C)) that increases monotonically with decreasing temperature. The saturation magnetization (M(S)) follows the Bloch's law and values of M(S) at room temperature as high as 78 emu/g were estimated, a result corresponding to similar to 80% of the bulk value. The overlap of M/M(S) versus H/T curves for a given sample and the low H(C) at high temperatures suggest superparamagnetic behavior in all samples studied. The overlap of M/M(S) versus H curves at constant temperature for different samples indicates that the NP magnetization behavior is preserved, independently of the coating and magnetite concentration. (C) 2010 American Institute of Physics. [doi: 10.1063/1.3311611]
Resumo:
We have performed a systematic study of the magnetic properties of a series of ferrimagnetic nanoparticles of Mg(x)Fe(3-x)O(4) (0.8 <= x <= 1.5) prepared by the combustion reaction method. The magnetization data can be well fitted by Bloch's law with T(3/2). Bloch's constant B determined from the fitting procedure was found to increase with Mg content x from similar to 3.09 X 10(-5) K(-3/2) for x = 0.8 to 6.27 X 10(-5) K(-3/2) for x=1.5. The exchange integral J(AB) and the spin-wave stiffness constant D of Mg(x)Fe(3-x)O(4) nanoparticles were also determined as similar to 0.842 and 0.574 meV and 296 and 202 meV angstrom(2) for specimens with x=0.8 and 1.5, respectively. These results are discussed in terms of cation redistribution among A and B sites on these nanostructured spinel ferrites. (C) 2010 American Institute of Physics. [doi: 10.1063/1.3359709]
Resumo:
Magnetization and Mossbauer spectroscopy measurements are performed at low temperature under high field, on nanoparticles with a nickel ferrite core and a maghemite shell. These nanoparticles present finite size and surface effects, together with exchange anisotropy. High field magnetization brings the evidences of a monodomain ordered core and surface spins freezing in disorder at low temperature. Mossbauer spectra at 4.2 K present an extra contribution from the disordered surface which is field dependent. Field and size dependences of this latter show a progressive spin alignment along the ferrite core which is size dependent. The weak surface pinning condition of the nanoparticles confirms that the spin disorder is localized in the external shell. The underfield decrease in the mean canting angle in the superficial shell is then directly related to the unidirectional exchange anisotropy through the interface between the ordered core and the disordered shell. The obtained anisotropy field H(Ea) scales as the inverse of the nanoparticle diameter, validating its interfacial origin. The associated anisotropy constant K(Ea) equals 2.5 x 10(-4) J/m(2). (C) 2009 American Institute qf Physics. [doi: 10.1063/1.3245326]
Resumo:
A phonon structure in the photoluminescence of EuTe was discovered, with a well-defined zero-phonon emission line (ZPL). The ZPL redshifts linearly with the intensity of applied magnetic field, indicating spin relaxation of the photoexcited electron, and saturates at a lower magnetic field than the optical absorption bandgap, which is attributed to formation of magnetic polarons. From the difference in these saturation fields, the zero-field polaron binding energy and radius are estimated to be 43 meV and 3.2 (in units of the EuTe lattice parameter), respectively. (C) 2011 American Institute of Physics. [doi:10.1063/1.3634030]
Resumo:
The addition of transition metals to III-V semiconductors radically changes their electronic, magnetic, and structural properties. We show by ab initio calculations that in contrast to the conventional semiconductor alloys, the lattice parameter in magnetic semiconductor alloys, including those with diluted concentration, strongly deviates from Vegard's law. We find a direct correlation between the magnetic moment and the anion-transition metal bond lengths and derive a simple and general formula that determines the lattice parameter of a particular magnetic semiconductor by considering both the composition and magnetic moment. This dependence can explain some experimentally observed anomalies and stimulate other kind of investigations.
Resumo:
We report accurate magnetization measurements on the spin-gap compound NiCl(2)-4SC (NH(2))(2) around the low portion of the magnetic induced phase ordering. The critical density of the magnetization at the phase boundary is analyzed in terms of a Bose-Einstein condensation (BEC) of bosonic particles, and the boson interaction strength is obtained as upsilon(0)=0.61 meV. The detailed analysis of the magnetization data across the transition leads to the conclusion for the preservation of the U(1) symmetry, as required for BEC. (c) 2009 American Institute of Physics. [DOI: 10.1063/1.3055265]
Resumo:
In this work we use resonant x-ray diffraction combined with polarization analysis of the diffracted beam to study the magnetic ordering in EuTe/PbTe multilayers. The presence of satellites at the (1/2 1/2 1/2) magnetic reflection of a 50 /repetition EuTe/PbTe superlattice demonstrated the existence of magnetic correlations among the alternated EuTe layers. The behavior of the satellites intensity as T increases toward the Neel temperature T(N) indicates that these correlations persist nearly up to T(N) and suggests the preferential decrease of the magnetic order parameter of external monolayers of each EuTe layer within the superlattice. (C) 2008 American Institute of Physics.
Resumo:
The electron spin precession about an external magnetic field was studied by Faraday rotation on an inhomogeneous ensemble of singly charged, self-assembled (In,Ga)As/GaAs quantum dots. From the data the dependence of electron g-factor on optical transition energy was derived. A comparison with literature reports shows that the electron g-factors are quite similar for quantum dots with very different geometrical parameters, and their change with transition energy is almost identical. (C) 2011 American Institute of Physics. [doi:10.1063/1.3588413]
Resumo:
The dynamics and mechanism of migration of a vacancy point defect in a two-dimensional (2D) colloidal crystal are studied using numerical simulations. We find that the migration of a vacancy is always realized by topology switching between its different configurations. From the temperature dependence of the topology switch frequencies, we obtain the activation energies for possible topology transitions associated with the vacancy diffusion in the 2D crystal. (C) 2011 American Institute of Physics. [doi:10.1063/1.3615287]