978 resultados para INDIUM SULFIDES


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Bulk Ge15Te85−x In x (1 ≤ x ≤ 11) series of glasses have been found to exhibit a threshold switching behaviour for an input current of 2 mA. An initial decrease is seen in the switching voltages (V T) with the addition of indium, which is due to the higher metallicity of indium. An increase is seen in V T above 3 at.% of indium, which proceeds until 8 at.%, with a change in slope (lower to higher) seen around 7 at.%. Beyond x = 8, a reversal in trend is exhibited in the variation of V T, with a well-defined minimum around x = 9 at.%. Based on the composition dependence of V T, it is proposed that Ge15Te85−x In x glasses exhibit an extended rigidity percolation threshold. The composition, x = 3, at which the V T starts to increase and the composition, x = 7, at which a slope change is exhibited correspond to the onset and completion, respectively, of the extended stiffness transition. Thermal studies and photoconductivity measurements also support the idea of an extended rigidity percolation in Ge15Te85−x In x glasses. In addition, the minimum seen in V T at x = 9 is associated with the chemical threshold (CT) of this glassy system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present work, we report the growth of wurtzite InN epilayers on GaN/Si (1 1 1) substrate by plasma-assisted molecular beam epitaxy (PAMBE). The growth parameters such as indium flux, substrate temperature and RF power affect the crystallographic and morphological properties of InN layers, which were evaluated using high resolution X-ray diffraction (HRXRD) analysis and atomic force microscopy (AFM). It is found that excess indium (In) concentrations and surface roughness were increased with increase in In flux and growth temperature. The intensity of HRXRD (0 0 0 2) peak, corresponding to c-axis orientation has been increased and full width at half maxima (FWHM) has decreased with increase in RF power. It was found that highly c-axis oriented InN epilayers can be grown at 450 degrees C growth temperature, 450 W RF power and 1.30 x 10(-7) mbar In beam equivalent pressure (BEP). The energy gap of InN layers grown by optimizing growth conditions was determined by photoluminescence and optical absorption measurement. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Investigations were carried out on the ambient condition oxidation of self-assembled, fairly uniform indium nitride (InN) quantum dots (QDs) fabricated on p-Si substrates. Incorporation of oxygen in to the outer shell of the QDs was confirmed by the results of transmission electron microscopy (TEM), X-ray photoemission spectroscopy (XPS). As a consequence, a weak emission at high energy (similar to 1.03?eV) along with a free excitonic emission (0.8?eV) was observed in the photoluminescence spectrum. The present results confirm the incorporation of oxygen into the lattice of the outer shell of InN QDs, affecting their emission properties. (C) 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In-filled and Ge-doped Co4Sb12 skutterudites materials were synthesized by an induction melting process which was followed by annealing at 650 degrees C for 7 days. A structural, compositional, and morphological study was carried out by X-ray diffraction (XRD), electron probe micro analysis (EPMA), and scanning electron microscopy (SEM). The formation of a single skutterudite phase (delta-CoSb3) was confirmed by XRD and the composition of all the samples was verified by EPMA. The homogeneity and morphology of the samples was observed by potential Seebeck microprobe (PSM) and SEM, respectively. The PSM result confirmed the inhomogeneity of the samples. The temperature dependence of the Seebeck coefficient, electrical conductivity, and thermal conductivity were measured in the temperature range of 300-650 K. The samples of In0.16Co4Sb12-xGex (x = 0.05, 0.1, and 0.2) show a negative Seebeck coefficient confirming an n-type conductivity and the In0.16Co4Sb11.7Ge0.3 sample shows a positive Seebeck coefficient confirming a p-type conductivity. There was a change in the Seebeck coefficient from an n-type to a p-type at the doping concentration of x = 0.3 due to the excess Ge which increases in hole carrier concentration. Electrical conductivity decreases with an increase in Ge doping concentrations and with increases in temperature due to the bipolar effect. Thermal conductivity increases with an increase in carrier concentration and decreases when the temperature is increased. The highest ZT = 0.58 was achieved by In0.16Co4 Sb11.95Ge0.05 at 673K and In-filled and Ge-doped Co4Sb12 was not effective in improving the figure of merit. (C) 2012 American Institute of Physics. [doi: 10.1063/1.3677982]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ga and In co-doped ZnO (GIZO) thin films together with ZnO, In-doped ZnO (IZO), Ga-doped ZnO (GZO), and IZO/GZO multilayer for comparison, were grown on corning glass and boron doped Si substrates by PLD. The photoluminescence spectra of GIZO showed a strong white light emission and the current-voltage characteristics showed relatively lower turn-on voltage and larger forward current. The CIE coordinates for GIZO were observed to be (0.31, 0.33) with a correlated colour temperature of 6650 K, indicating a cool white light, and establishing a possibility of white light emitting diodes. (C) 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Photoresponse of n-type indium-doped ZnO and a p-type polymer (PEDOT:PSS) heterojunction devices are studied, juxtaposed with the photoluminescence of the In-ZnO samples. In addition to the expected photoresponse in the ultraviolet, the heterojunctions exhibit significant photoresponse to the visible (532 nm). However, neither the doped ZnO nor PEDOT: PSS individually show any photoresponse to visible light. The sub-bandgap photoresponse of the heterojunction originates from visible photon mediated e-h generation between the In-ZnO valence band and localized states lying within the band gap. Though increased doping of In-ZnO has limited effect on the photoluminescence, it significantly diminishes the photoresponse. The study indicates that optimally doped devices are promising for the detection of wavelengths in selected windows in the visible. (C) 2012 American Institute of Physics. http://dx.doi.org/10.1063/1.4704655]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A Pummerer rearrangement of 2,3-dideoxy-3-alkyl/arylsulfinyl-arabino-hexopyranosides is reported. Treatment of sulfinyl-arabino-hexopyranoside derivatives, obtained through oxidation of the corresponding thio-derivatives, with trifluoroacetic anhydride (TFAA)/pyridine led to a facile formation of 2,3-dideoxy-3-alkyl/arylthio-hex-2-enopyranosides. Upon conversion of sugar vinyl sulfides to vinyl sulfoxides, conjugate addition reactions were conducted with alkoxides, to afford 3-deoxy-3-alkyl/arylsulfinyl pyranosides, in the manno-configuration exclusively. Whereas the conjugate addition reaction did not proceed with ether protecting groups, ester protecting groups and free hydroxyl groups in the sugar vinyl sulfoxide permitted the reaction. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We show that the third order optical nonlinearity of 15-atom gold clusters is significantly enhanced when in contact with indium tin oxide (ITO) conducting film. Open and close aperture z-scan experiments together with non-degenerate pump-probe differential transmission experiments were done using 80 fs laser pulses centered at 395 nm and 790 nm on gold clusters encased inside cyclodextrin cavities. We show that two photon absorption coefficient is enhanced by an order of magnitude as compared to that when the clusters are on pristine glass plate. The enhancement for the nonlinear optical refraction coefficient is similar to 3 times. The photo-induced excited state absorption using pump-probe experiments at pump wavelength of 395 nm and probe at 790 nm also show an enhancement by an order of magnitude. These results attributed to the excited state energy transfer in the coupled gold cluster-ITO system are different from the enhancement seen so far in charge donor-acceptor complexes and nanoparticle-conjugate polymer composites.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The paper reports effect of small ternary addition of In on the microstructure, mechanical property and oxidation behaviour of a near eutectic suction cast Nb-19.1 at-%Si-1.5 at-%In alloy. The observed microstructure consists of a combination of two kinds of lamellar structure. They are metal-intermetallic combinations of Nb-ss-beta-Nb5Si3 and Nb-ss-alpha-Nb5Si3 respectively having 40-60 nm lamellar spacings. The alloy gives compressive strength of 3 GPa and engineering strain of similar to 3% at room temperature. The composite structure also exhibits a large improvement in oxidation resistance at high temperature (1000 degrees C).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Silicon nanowires were grown on Si substrates by electron beam evaporation (EBE) was demonstrated using Indium as an alternate catalyst to gold. We have studied the effect of substrate (growth) temperature, deposition time on the growth of nanowires. It was observed that a narrow temperature window from 300 degrees C to 400 degrees C for the nanowires growth. At growth temperature >= 400 degrees C suppression of nanowires growth was observed due to evaporation of catalyst particle. It is also observed that higher deposition times also leading to the absence of nanowire growth as well as uncatalyzed deposition on the nanowires side walls due to limited surface diffusion of ad atoms and catalyst evaporation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO films have been grown via a vapour phase transport (VPT) on soda lime glass (SLG) and indium-tin oxide (ITO) coated glass. ZnO film on ITO had traces of Zn and C which gives them a dark appearance while that appears yellowish-white on SLG. X-ray photoelectron spectroscopy studies confirm the traces of C in the form of C-O. The photoluminescence studies reveal a prominent green luminescence band for ZnO film on ITO. (C) 2013 Author(s).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Zinc Oxide (ZnO) and indium doped ZnO (IZO) thin films with different indium compositions were grown on p-type boron doped Si substrates by pulsed laser deposition (PLD). The effect of indium concentration on the structural, optical and electrical properties of the film was studied. XRD, XPS and Raman studies confirm the single phase formation and successful doping of In in to ZnO. We observed various photoluminescence emissions, ranging from UV to visible, with the incorporation of In into ZnO. Room temperature Current-Voltage (I-V) characteristics showed good p-n junction properties for n-type-undoped and In doped ZnO with p-type substrates. The turn on voltage was observed to be decreasing with increase in In composition.