993 resultados para Dental glass-ceramics


Relevância:

90.00% 90.00%

Publicador:

Resumo:

This paper presents a historical of the Biosilicate®, a bioactive glass-ceramic developed at the Vitreous Materials Laboratory of the Federal University of São Carlos, Brazil. After decades of study accomplished with bioactive glasses and glass-ceramics, Biosilicate® results from a natural evolution and has similar bioactivity index, but far superior mechanical properties than of all bioactive glasses. Biosilicate® is almost fully crystalline and also exhibits much higher bioactivity than all the currently commercially available bioactive glass-ceramics. Due to its special characteristics, Biosilicate® has been successfully tested for several medical and dental applications as we thoroughly discuss in this review paper.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Dental oxide ceramics have been inspired by their biocompability and mechanical properties which have made durable all-ceramic structures possible. Clinical longevity of the prosthetic structures is dependent on effective bonding with luting cements. As the initial shear bond strength values can be comparable with several materials and procedures, long-term durability is affected by ageing. Aims of the current study were: to measure the shear bond strength of resin composite-to-ceramics and to evaluate the longevity of the bond; to analyze factors affecting the bond, with special emphasis on: the form of silicatization of the ceramic surface; form of silanization; type of resin primer and the effect of the type of the resin composite luting cement; the effect of ageing in water was studied regarding its effect to the endurance of the bond. Ceramic substrates were alumina and yttrium stabilized zirconia. Ceramic conditioning methods included tribochemical silicatization and use of two silane couplings agents. A commercial silane primer was used as a control silane. Various combinations of conditioning methods, primers and resin cements were tested. Bond strengths were measured by shear bond strength method. The longevity of the bond was generally studied by thermocycling the materials in water. Additionally, in one of the studies thermal cycling was compared with long-term water storaging. Results were analysed statistically with ANOVA and Weibull analysis. Tribochemical treatment utilizing air pressure of 150 kPa resulted shear bond strengths of 11.2 MPa to 18.4 MPa and air pressure of 450 kPa 18.2 MPa to 30.5 MPa, respectively. Thermocycling of 8000 cycles or four years water storaging both decreased shear bond strength values to a range of 3.8 MPa to 7.2 MPa whereas initial situation varied from 16.8. Mpa to 23.0 MPa. The silane used in studies had no statistical significance. The use of primers without 10-MDP resulted spontaneous debonding during thermocycling or shear bond strengths below 5 MPa. As conclusion, the results showed superior long-term bonding with primers containing 10-MDP. Silicatization with silanizing showed improved initial shear bond strength values which considerably decreased with ageing in water. Thermal cycling and water storing for up to four years played the major role in reduction of bond strength, which could be due to thermal fatigue of the bonding interface and hydrolytic degradation of the silane coupled interface.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This study aimed at investigating in vitro osteogenesis on three fluorcanasite glass-ceramic compositions with different solubilities (K3, K5, and K8). Osteoblastic cells were obtained from human alveolar bone fragments and cultured under standard osteogenic condition until subconfluence. First passage cells were cultured on K3, K5, and K8 and on Bioglass (R) 45S5 (45S5-control). Cell adhesion was evaluated at 24 h. For proliferation and viability, cells were cultured for 1, 4, and 10 days. Total protein content and alkaline phosphatase (ALP) activity were measured at 7, 14, and 21 days. Cultures were stained with Alizarin red at 21 days, for detection of mineralized matrix. Data were compared by ANOVA followed by Duncan`s test. Cell adhesion, cell proliferation, viability, total protein content, and ALP activity were not affected by fluorcanasite glass-ceramic composition and solubility. Bone-like formation was similar on all fluorcanasite-glass ceramics and was reduced compared to 45S5. The changes in the chemical composition and consequently solubility of the fluorcanasite glass-ceramics tested here did not significantly alter the in vitro osteogenesis. Further modifications of the chemical composition of the fluorcanasite glass-ceramic would be required to improve bone response, making this biomaterial a good candidate to be employed as a bone substitute.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The preparation and characterization of transparent glass-ceramics in the composition of 30Li2O:5ZrO2:xBaO:(100-x) SiO2 with x = 0, 5, 10, 15, and 20 mol% are described. Glasses were melted in a platinum crucible at 1100°C for 2 h and then heat-treated at 900°C for 3 h. The characterizations were performed by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), Raman and infrared spectroscopy, and scanning electron microscopy (SEM). The experimental results indicate that there was a structural change in the glass-ceramics as the BaO concentration in the mixture increased. In the XRD patterns of samples without heat treatment, only the halo was observed. After heat treatment, the appearance of the materials was verified by X-ray diffraction peaks. The reorganization of the amorphous solid was confirmed by Raman and IR spectroscopy along with XPS and SEM, with a more homogeneous phase formation being observed.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Utilization of contemporary post and core systems has facilitated the aesthetic restoration of endodontically treated teeth. Light transmission and biocompatibility have been enhanced by the introduction of metal-free post systems. The periodontal and endodontic status, root length, and histological structure of the devitalized teeth must be considered in order to achieve successful restoration following endodontic treatment. This article presents various restorative criteria for the aesthetic placement and buildup of post and core materials, as well as the preservation of maximum coronal and root structure.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In this report we investigate the optical properties and energy-transfer upconversion luminescence of Ho3+- and Tb3+/Yb 3+-codoped PbGeO3-PbF2-CdF2 glass-ceramic under infrared excitation. In Ho3+/Yb 3+-codoped sample, green(545 nm), red(652 nm), and near-infrared(754 nm) upconversion luminescence corresponding to the 4S 2(5F4) → 5I8, 5F5 → 5I8, and 4S2(5F4) → 5I 7, respectively, was readly observed. Blue(490 nm) signals assigned to the 5F2,3 → 5I8 transition was also detected. In the Tb3+/Yb3+ system, bright UV-visible emission around 384, 415, 438, 473-490, 545, 587, and 623 nm, identified as due to the 5D3(5G6) → 7FJ(J=6,5,4) and 5D4→ 7FJ(J=6,5,4,3) transitions, was measured. The comparison of the upconversion process in glass ceramic and its glassy precursor revealed that the former samples present much higher upconversion efficiencies. The dependence of the upconversion emission upon pump power, and doping contents was also examined. The results indicate that successive energy-transfer between ytterbium and holmium ions and cooperative energy-transfer between ytterbium and terbium ions followed by excited-state absorption are the dominant upconversion excitation mechanisms herein involved. The viability of using the samples for three-dimensional solid-state color displays is also discussed.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Brazil is the world's largest producer of alcohol and sugar from sugarcane. Currently, sugarcane bagasse is burned in boilers to produce steam and electrical energy, producing a huge volume of ash. The major component of the ash is SiO 2, and among the minor components there are some mineralizing agents or fluxing. Published works have shown the potential of transforming silicate-based residues into glass-ceramic products of great utility. This work reports the research results of SCBA use to produce glass-ceramics with wollastonite, rankinite and gehlenite as the major phases. These silicates have important applications as building industry materials, principally wollastonite, due to their special properties: high resistance to weathering, zero water absorption, and hardness among others. The glasses (frits) were prepared mixing ash, calcium carbonate and sodium or potassium carbonates as flux agents, in different concentrations. X-ray fluorescence was used to determine the chemical composition of the glasses and their crystallization was assessed by using thermal analysis (DTA/DSC/TGA) and X-ray diffraction. The crystallization kinetics was evaluated using the Kissinger method, giving activation energies ranging from 200 to 600 kJ/mol. © 2011 Ceramic Society of Japan.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This paper reports on the sol-gel preparation and structural and optical characterization of new Er3+-doped SiO2-Nb 2O5 nanocomposite planar waveguides. Erbium-doped (100-x)SiO2-xNb2O5 waveguides were deposited on silica-on-silicon substrates and Si(1 0 0) by the dip-coating technique. The waveguides exhibited uniform refractive index distribution across the thickness, efficient light injection at 1538 nm, and low losses at 632 and 1538 nm. The band-gap values lied between 4.12 eV and 3.55 eV for W1-W5, respectively, showing an excellent transparency in the visible and near infrared region for the waveguides. Fourier Transform Infrared (FTIR) Spectroscopy analysis evidenced SiO2-Nb2O5 nanocomposite formation with controlled phase separation in the films. The HRTEM and XRD analyses revealed Nb2O5 orthorhombic T-phase nanocrystals dispersed in a silica-based host. Photoluminescence (PL) analysis showed a broad band emission at 1531 nm, assigned to the 4I13/2 → 4I15/2 transition of the Er3+ ions present in the nanocomposite, with a full-width at half medium of 48-68 nm, depending on the niobium content and annealing. Hence, these waveguides are excellent candidates for application in integrated optics, especially in EDWA and WDM devices. © 2012 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The evolution of ceramic systems currently allows the manufacture of prosthesis similar to the natural teeth, meeting the expectations of patients. However, when using vitreous ceramic the color of substrate is significant for the esthetic result, requiring planning aesthetic cores when involved reconstruction of endodontically treated teeth without coronal structure. Thus, the aim of this study to describe a case report of aesthetic rehabilitation in upper anterior teeths using vitreous ceramic system for the reconstruction of elements: 11, 12, 21 and 22 after endodontically treated. It was emphasized the removal of crowns and manufacture of custom cast post and core with ceramic in coronal portion, prioritizing the aesthetic result. Through the clinical results observed can be seen that the use of custom cast post and core with ceramic in association lithium disilicate glass ceramics provided a satisfactory aesthetic result.