999 resultados para Amsterdam-3


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Theoretical molecular structures of the complexes cis-[PdCl2(tmen)] and cis-[Pd(N-3)(2)(tmen)] (tmen = N,N,N',N'-tetramethylethylenediamine) were investigated using B3LYP/DFT method. The calculated molecular parameters, bond distances and angles, revealed a square-planar geometry around the metallic center for both compounds with the azide being linear. The theoretical infrared spectra of C, symmetry (electronic state (1)A) of the compounds are in agreement with the experimental data. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Systematic studies in manganites of spinel structure have been undertaken. We report on the magnetic properties of two particular cases, in which one of the transition metals, Mg2+ is non-magnetic (NiMgxMn2-xO4) or presents a stable oxidation state, Cu2+ (CoxCuyMnzO4, x + y + z = 3). The magnetic behaviour is described with respect to varying contents of cobalt, copper or manganese. A ferrimagnetic transition is observed at 110-120 K, which depends on the cobalt content. Presence of copper increases the coercive field by a factor of ten with respect to the parent compound NiMn2O4. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The oldest fragment of continental crust recognized in South America occurs as an isolated Archean enclave in northeastem Brazil's Borborema Province, ca. 600 Ma Brasiliano-Pan African orogenic belt. This Archean fragment, the Sao Jose do Campestre massif, is surrounded by large tracts of 2.2-2.0 Ga Paleoproterozoic gneisses and is located more than 600-1500 km from the much larger assemblages of Archean rocks found in the Sao Fransciso and Amazonian cratons, located to the south and west, respectively. Geochronological studies of the Sao Jose do Campestre massif show that its oldest rocks contain zircons with U-Pb ages up to 3.5 Ga and Sm-Nd T-DM model ages of more than 3.7 Ga, indicating that they represent reworked crust. This older nucleus is flanked by both reworked and juvenile 3.25 and 3.18 Ga rocks which arc intruded by both 3.00 and 2.69 Ga plutonic bodies. The protracted evolution the Sao Jose do Campestre massif is consistent with that of a larger continental mass as opposed to a small crustal fragment that grew in isolation. As such, the Sao Jose do Campestre massif is interpreted as representing a detached piece of an evolved craton that became entrained with younger rocks during a subsequent Paleoproterozoic accretionary-orogenic event. This hypothesis is bolstered by the presence of Paleoproterozoic gneisses that envelop the Sao Jose do Campestre massif, as well as the existence of ca. 2.0 Ga metamorphic zircon and monazite within its rocks. The occurrence of several different Archean cratonic basement inliers within the greater Paleoproterozoic crustal framework of the Borborema Province suggests that cratonic slices spalled off one or more larger Archean masses prior to the ca. 2.2-2.0 Ga Paleoproterozoic orogenic collage. A important challenge is to link these older fragments to their parent cratons. Although results are not unique, the pattern of ages and isotopic signatures observed in the Sao Jose do Campestre massif is similar to that seen in parts of the Sao Francisco Craton, and it is possible that the Sao Jose do Campestre massif is a fragment of an Archean continental fragment formed during an episode of continental breakup prior to 2200 Ma. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The polymeric precursor method was employed in the preparation of PZT thin films on Pt(111)Ti/SiO2/Si(100) substrates. X-ray diffraction patterns revealed the polycrystalline nature of the PZT (53:47) thin films, which had a granular structure and a grain size of approximately 70 nm. A 350-nm thick film was obtained by running three cycles of the dip-coating/heating process. Atomic force microscopy (AFM) analyses showed the surface of these thin films to be smooth, dense and crack-free with low surface roughness (= 2.0 nm). The PZT (53:47) thin films annealed at 700 degreesC showed a well-saturated hysteresis loop. The C-V curves of perovskite thin film displayed normal ferroelectric behavior, while the remanent polarization (2P(r)) and coercive field (E-e) of the film deposited and measured at room temperature were 40 muC/cm(2) and 110 kV/cm, respectively. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Glassy films of 0.2[Sb(PO3)(3)]-0,8Sb(2)O(3) with 0.8 mum-thickness were deposited on quartz substrates by electron beam evaporation. A contraction in the film thickness (photoinduced decrease in volume) and photobleaching effect associated with a decrease of up to 25% in the index of refraction has been observed in the films after irradiation near the bandgap (3.89 eV), using the 350.7 nm (3.54 eV) Kr+ ion laser line with 2.5 W/cm(2) for 30 min. A loss of 30% in the phosphorus concentration was measured by wavelength dispersive X-ray microanalysis in the film after laser irradiation with 5.0 W/cm(2) for 1.0 h. These photoinduced changes in the samples are dependent on the power density and intensity profile of the laser beam. Using a Lloyd's mirror setup for continuous wave holography it was possible to record holographic gratings with period from 500 nm up to 20 mum and depth profile of similar to50 nm in the films after laser irradiation with 5.0 W/cm(2) for 1 h. Real-time diffraction efficiency measurements have shown that ultraviolet irradiation induces first a refractive index grating formation, and after this, the photocon traction effect takes place generating an irreversible relief grating. Diffraction efficiency up to 10% was achieved for the recorded gratings. 3D-refraction index measurements and atomic force microscopy images are presented. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Sodium phosphoniobate glasses with the composition (mol%) 75NaPO(3)-25Nb(2)O(5) and containing 2 mol% Yb3+ and x mol% Er3+ (0.01 <= x <= 2) were prepared using the conventional melting/casting process. Er3+ emission at 1.5 mu m and infrared-to-visible upconversion emission, upon excitation at 976 nm, are evaluated as a function of the Er3+ concentration. For the lowest Er3+ content, 1.5 mu m emission quantum efficiency was 90%. Increasing the Er3+ concentration up to 2 mol%, the emission quantum efficiency was observed to decrease to 37% due to concentration quenching. The green and red upconversion emission intensity ratio was studied as a function of Yb3+ co-doping and the Er3+-Er3+ energy transfer processes. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Luminescence data for Eu3+ and Gd3+ in fluoroindate glasses are compared to those of a fluorozirconate glass. Emission is observed from Eu3+ 5D(J) (J = 0, 1, 2 and 3) and Gd3+ P-6(7/2) excited-state levels and the results put in evidence Eu-Eu and Gd-Eu energy transfer processes. Vibronic bands related to a 320 cm-1 vibrational mode could be observed for Eu3+ luminescent transitions with DELTAJ = 0, 1 and 2 and also for the P-6(7/2) --> S-8(7/2) transition of Gd3+. Lanthanide ion site symmetry is closer to an inversion center in fluoroindate glasses than it is in fluorozirconate.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In situ solid state oxidation reaction for an alternative La1-xSrxMnO3 (x = 0, 0.1, 0.2 and 0.3) formation is reported. Samples have been obtained by using strontium peroxide, lanthanum and manganese (III) oxide reagents. Strontium peroxide has induced the oxidation of Mn+3 to Mn+4. Lanthanum strontium-doped manganite was obtained without secondary phase formation. La0.825Sr0.175MnO3 showed two structural transitions. The first from 88 to 373 K and the second at 1073 K. which are explained by Jahn-Teller effect at low temperature and cation displacement at high temperature. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Silica gel, chemically modified with 2,5-dimercapto-1,3,4-thiadiazole [=Si(CH2)(3)-NC2HNS3], abbreviated as SiB, was used to adsorb metal ions from ethanol by both batch and column techniques. Elution of Cu(II) was done with a solvent mixture of acetone and hydrochloric acid (9:1 v/v). Zn(II), Cd(II), Ni(II), Pb(II), Co(II) and Fe(III) were eluted with 0.5 mol l(-1) HC1 in ethanol solution. The modified silica was applied in the preconcentration of metal ions from commercial ethanol, normally used as engine fuel. The method is suitable for quantifying these metals at low mu g l(-1) levels.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Immunohistochemistry was used to analyze the rat brain distribution of thimet oligopeptidase and neurolysin. Both enzymes appear ubiquitously distributed within the entire rat brain. However, neuronal perikarya and processes stained for neurolysin, while intense nuclear labeling was only observed for thimet oligopeptidase. These data suggest that neurolysin and thimet oligopeptidase, endopeptidases sharing several functional and structural similarities, are present in distinctive intracellular compartments in neuronal cells. (C) 1999 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Linear low density polyethylene (LLDPE) with different branching contents were prepared from ethylene, without the addition of alpha-olefin comonomer, using a combination of catalyst precursors {Tp(Ms)}NiCl (1) (Tp(Ms) = hydridotris(3-mesitylpyrazol-1-yl)) and Cp2ZrCl2 (2) activated with MAO/TMA (1:1) in toluene at 0degreesC and by varying the nickel loading mole fraction (x(Ni)). The polymerization results showed that the turnover frequencies are strongly dependent on the x(Ni) varying from 6.6 x 10(3) to 32.1 x 10(3) mol[C2H4]/mol[Zr] h. The C-13 NMR spectra of the copolymers showed that the branch contents of the polymers increase as the x(Ni) increase in the medium promoting the production of polymers with a wide range of melting point (T-m) (C) 2004 Elsevier B.V. All rights reserved.