The structure of laser glasses in the system (B(2)O(3))(0.6){(Al(2)O(3))(0.4-x)(Y(2)O(3))(x)} (0.1 <= x <= 0.25) has been investigated by means of (11)B, (27)Al, and (89)Y solid state NMR as well as Y-3d core-level X-ray photoelectron spectroscopy, (11)B magic-angle spinning (MAS) NMR spectra reveal that the majority of the boron atoms are three-coordinated, and a slight increase of four-coordinated boron content with increasing x can be noticed. (27)Al MAS NMR spectra show that the alumina species are present in the coordination states four, five and six. All of them are in intimate contact with both the three- and the four-coordinate boron species and vice versa, as indicated by (11)B/(27)Al rotational echo double resonance (REDOR) data. These results are consistent with the formation of a homogeneous, nonsegregated glass structure. For the first time, (89)Y solid state NMR has been used to probe the local environment of Y(3+) ions in a glass-forming system. The intrinsic sensitivity problem associated with (89)Y NMR has been overcome by combining the benefits of paramagnetic doping with those of signal accumulation via Carr-Purcell spin echo trains. Both the (89)Y chemical shifts and the Y-3d core level binding energies are found to be rather sensitive to the yttrium bonding state and reveal that the bonding properties of the yttrium atoms in these glasses are similar to those found in the model compounds YBO(3) and YAl(3)(BO(3))(4), Based on charge balance considerations as well as (11)B NMR line shape analyses, the dominant borate species are concluded to be meta- and pyroborate anions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

As amostras de esmectita do estado do Pará, Amazônia, Brasil foram caracterizadas utilizando XRD, 27Al MAS NMR, FTIR e análise textural por curvas isotérmicas de adsorção-dessorção de nitrogênio. Na produção das argilas pilarizadas foi usado como íon intercalante, o Al13 (o íon de keggin), obtido pela reação das soluções AlCl36H2O/NaOH, com razão molar OH/Al=2. Foram adotadas as proporções (Al/Argila): 5, 10, 20 e 25 meq/g de argila, com intercalação em 25 ºC, durante as 3 h e calcinada a 450 ºC (temperatura adequada da calcinação). O resultado mostrou que o processo de pilarização aumentou o espaçamento basal da argila natural de 14,02 para 18,84 Å e a área superficial de 44,30 para 198,03 m2/g (Al/Argila=25meq/g de argila, pH=4). O material preparado com relação Al/Argila=25meq/g de argila mostrou a incorporação máxima de Al. A estabilidade térmica da argila natural foi melhorada pelo procedimento de pilarização.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

High precision elastic and inelastic angular distributions have been measured for the O-16 + Al-27 system at a beam energy of 100 MeV. The data analysis confirms a rainbow formation as already predicted by parameter-free Coupled Channel calculations. It also helps to reveal the crucial role of inelastic couplings in the rainbow formation for heavier systems even at energies far above the Coulomb barrier. This feature, well known in atomic/molecular scattering, is experimentally studied for the first time in Nuclear Physics. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The effect of several desilication experimental parameters (base concentration, temperature and time) on the characteristics of MOR zeolite was studied. The samples were characterized by X-ray diffraction, Al-27 and Si-29 MAS-NMR, chemical analysis, and FTIR (framework vibration region). The textural characterization was made by N-2 adsorption and the acidity was evaluated by pyridine adsorption followed by FTIR and by the catalytic model reaction of n-heptane cracking. The alkaline treatments promoted the Si extraction from the zeolite framework, without considerable loss of crystallinity and, as it was envisaged, an important increase of the mesoporous structure was attained. A linear correlation between the number of framework Si per unit cell. N-Si and the asymmetric stretching wavenumber, nu(i), was observed. The acidity characterization shows that the desilicated samples exhibit practically the same acid properties than the parent HMOR zeolite. The optimum desilication conditions were those used to obtain sample M/0.2/85/2, i.e., sample treated with 0.2 M NaOH solution at 85 degrees C for 2 h.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Bifunctional Pt-HMOR catalysts were prepared by incipient wetness impregnation of various desilicated MOR obtained by alkaline treatment using NaOH concentrations ranging from 0.1 to 0.5 M. The zeolite structural changes upon modification were investigated by several techniques including powder X-ray diffraction,Al-27 and Si-29 MAS-NMR spectroscopy, N-2 adsorption, pyridine adsorption followed by infrared spectroscopy and the catalytic model reaction of m-xylene transformation. For low alkaline concentration the zeolite acidity is preserved, along with a slight increase of the volume correspondent to the larger micropores due to the removal of extra-framework debris already existent at the parent zeolite. At higher NaOH concentrations there is a significant loss of crystalinity and acidity as well as the formation of mesoporosity. The characterization of the metal function shows similar patterns for Pt-HMOR and Pt-M/0.1 samples, with Pt particles located mainly inside the inner porosity. In contrast, large Pt particles become visible at the intercrystalline mesoporosity of MOR crystals developed during the desilication treatments at severe alkaline conditions. The catalytic results obtained for n-hexane hydroisomerization showed an improved selectivity for dibranched over monobranched isomers for Pt-M/0.1 sample, likely due to the preservation of the support acidity and the slight enlargement of the micropores. This work is a new example in which the mesoporous development does not improve the catalytic efficiency of the zeolites, whereas mild alkaline desilication might be considered as an effective solution to produce customized catalysts with enhanced performance for a given application. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Desilication and a combination of alkaline followed by acid treatment were applied to MCM-22 zeolite using two different base concentrations. The samples were characterised by powder X-ray diffraction, Al-27 and Si-29 MAS-NMR spectroscopy, SEM, TEM and low temperature N-2 adsorption. The acidity of the samples was study through pyridine adsorption followed by FTIR spectroscopy and by the analyses of the hydroxyl region. The catalytic behaviour, anticipated by the effect of post-synthesis treatments on the acidity and space available inside the two internal pore systems was evaluated by using the model reaction of m-xylene transformation. The generation of mesoporosity was achieved upon alkaline treatment with 0.05 M NaOH solution and practically no additional gain was obtained when the more concentrate solution, 0.1 M, was used. Instead, Al extraction takes place along with Si, as shown by Si-29 and Al-27 MAS-NMR data, followed by Al deposition as extraframework species. Samples submitted to alkaline plus acid treatments present distinct behaviour. When the lowest NaOH solution was used no relevant effect was observed on the textural characteristics. Additionally, when the acid treatment was performed on an already fragilized MCM-22 structure, due to previous desilication with 0.1 M NaOH solution, the extraction of Al from both internal pore systems promotes their interconnection, evolving from a 2-D to a 3-D porous structure. This transformation has a marked effect in the catalytic behaviour, allowing an increase of m-xylene conversion as a consequence of an easier and faster molecular traffic in the 3-D structure. On the other hand, the continuous deposition of extraframework Al species inside the pores leads to a shape selective effect that privileges the formation of the more valuable isomer p-xylene.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Since long ago cellulosic lyotropic liquid crystals were thought as potential materials to produce fibers competitive with spidersilk or Kevlar, yet the processing of high modulus materials from cellulose-based precursors was hampered by their complex rheological behavior. In this work, by using the Rheo-NMR technique, which combines deuterium NMR with rheology, we investigate the high shear rate regimes that may be of interest to the industrial processing of these materials. Whereas the low shear rate regimes were already investigated by this technique in different works [1-4], the high shear rates range is still lacking a detailed study. This work focuses on the orientational order in the system both under shear and subsequent relaxation process arising after shear cessation through the analysis of deuterium spectra from the deuterated solvent water. At the analyzed shear rates the cholesteric order is suppressed and a flow-aligned nematic is observed which for the higher shear rates develops after certain time periodic perturbations that transiently annihilate the order in the system. During relaxation the flow aligned nematic starts losing order due to the onset of the cholesteric helices leading to a period of very low order where cholesteric helices with different orientations are forming from the aligned nematic, followed in the final stage by an increase in order at long relaxation times corresponding to the development of aligned cholesteric domains. This study sheds light on the complex rheological behavior of chiral nematic cellulose-based systems and opens ways to improve its processing. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Reseña del congreso WePreserve 2009 que tuvo lugar los pasados 23 al 27 de marzo en Barcelona, organizadopor la Facultad de Biblioteconomía y Documentación de la Universitat de Barcelona, con la colaboración del Institut d'Estudis Catalans, la Biblioteca de Catalunya y el Consorci de Biblioteques de Barcelona. El seminario 2009 WePreserve se celebra anualmente desde el año 2007 y participan todas las figuras de referencia europeas en materia de investigación en sistemas y metodologías que garantizan la preservación digital de los documentos: Digital Preservation Europe (DPE), Preservation and Long-term Access Through Networked Services (Planets), Cultural Artistic and Scientific Knowledge for Preservation, Access and Retrieval (CASPAR), y Network of expertise in Digital long-term preservation (nestor).

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Molybdenum(II) complexes [MOX(CO)(2)(eta(3)-allyl)(CH3CN)(2)] (X = Cl or Br) were encapsulated in an aluminium-pillared natural clay or a porous clay heterostructure and allowed to react with bidentate diimine ligands. All the materials obtained were characterised by several solid-state techniques. Powder XRD, and Al-27 and Si-29 MAS NMR were used to investigate the integrity of the pillared clay during the modification treatments. C-13 CP MAS NMR, FTIR, elemental analyses and low-temperature nitrogen adsorption showed that the immobilisation of the precursor complexes was successful as well as the in situ ligand-substitution reaction. The new complex [MoBr(CO)(2)(eta(3)-allyl)(2-aminodipyridyl)] was characterised by single-crystal X-ray diffraction and spectroscopic techniques, and NMR studies were used to investigate its fluxional behaviour in solution. The prepared materials are active for the oxidation of cis-cyclooctene using tert-butyl hydroperoxide as oxidant, though the activity of the isolated complexes is higher. ((c) Wiley-VCH Verlag GmbH & Co. KGaA, 69451 Weinheim, Germany, 2008).

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Rhodamine 6G (RH6G) laser dye-doped AlPO(4) xerogel and glass were prepared via a simple sol-gel route by one-step process and two-step process, respectively. The aggregating behavior of dyes in xerogel and glass was studied by excitation and emission spectra. The results indicated the dye aggregates become significantly weak in AlPO(4) glass than in xerogel, which might be attributed to the enhanced interactions between dye and AlPO(4) network as well as the nano-scale separation of dye by the mesoporous structure of AlPO(4) glass. The (27)Al MAS NMR of AlPO(4) glass confirms the interaction of RH6G with AlPO(4) glass network. Incorporation of RH6G into AlPO(4) glass converts Al(4) to Al(6) units, resulting in the increase of Al(6) concentration with the doped RH6G concentration. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In this paper 4.5SiO(2)-3Al(2)O(3-x)Nb(2)O(5)-2CaO powders have been synthesized using a chemical process the Polymeric Precursor Method. The process of glass formation has been investigated by XRD and DTA, the results confirm that the prepared powders are glasses. Experimental data show that amount of Nb2O5 had a considerable effect on the T-g values. The structures of glasses prepared. have been determined by Si-29 and Al-27 MAS NMR and the results indicated that the network is formed by SiO4 and AlO4 tetrahedral linked and probably Si-O-Nb bonds are present in the vitreous network. (C) 2005 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Glass ionomer cements (GICs) are currently used for various dental applications such as luting cements or as restorative materials. The calcium fluoro-alumino-silicate system is the basis for degradable glasses used to obtain the GICs. The purpose of the present paper is to add niobium to conventional glass system because according to previous papers niobium addition improves the chemical resistance and the mechanical properties of glasses. Therefore, the GICs prepared from these glasses would result in cements with higher chemical and mechanical resistance. The niobium fluoride powders were prepared using the sol-gel process and were characterized by X-ray diffraction, differential thermal analysis (DTA) and Al-27 and Si-29 MAS NMR. The results obtained by XRD showed that the powders prepared by this method are glass-ceramic. In the DTA curve was detected the presence of T-g and T-c temperatures. The analysis of MAS NMR spectra indicated that the framework of the powders is formed by SiO4 and AlO4 linked tetrahedra which are essential structures to yield the cements. Thus, we concluded that niobium fluoride silicate powders can be used in the preparation of GICs. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Glass ionomer cements (GICs) are glass and polymer composite materials. These materials currently find use in the dental field. The purpose of this work is to obtain systems based on composition 4.5SiO(2)-3Al(2)O(3)-XNb2O5-2CaO to be used in Dentistry. The systems were prepared by chemical route at 700 degrees C. The results obtained by XRD and DTA showed that all systems prepared are glasses. The structures of the obtained glasses were compared to commercial material using Al-27 and Si-29 MAS NMR. The analysis of MAS NMR spectra indicated that the systems developed and commercial material are formed by SiO4 and AlO4 linked tetrahedra. The properties of glass ionomer cements based on the glasses prepared with several niobium contents were studied. Setting and working times of the cement pastes, microhardness and diametral tensile strength were evaluated for the experimental GICs and commercial luting cements. It was concluded that setting time of the cement pastes increased with increasing niobium content of the glasses (X). The properties to the GICs such as setting time and microhardness were influenced by niobium content. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This study answers several pending questions about alumina-catalyzed epoxidation with aqueous 70 wt% H2O2. To evaluate the effect of the water-to-aluminum tri-sec-butoxide molar ratio, this was systematically changed from 1 to 24. The xerogels were calcined at 450 degrees C and gave different gamma-Al2O3's with distinct textural and acidic properties. A combination of Al-27 MAS NMR and TPD-NH3 results of calcined aluminas allowed us to assign the type la. Al-OH sites as the catalytic sites for epoxidation. The type Ib Al-OH sites have no function in catalytic epoxidation, because ethyl acetate poisons these sites. The strong acid sites of types IIa, IIb, and III Al-OH groups are responsible for the undesired H2O2 decomposition and decreased oxidant selectivity. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Glass ionomer cements (GICs) are largely employed in Dentistry for several applications, such as luting cements for the attachment of crowns, bridges, and orthodontic brackets as well as restorative materials. The development of new glass systems is very important in Dentistry to improve of the mechanical properties and chemical stability. The aim of this study is the preparation of two glass systems containing niobium in their compositions for use as GICs. Glass systems based on the composition SiO2,Al2O3-Nb2O5-CaO were prepared by chemical route at 700degreesC. The XRD and DTA results confirmed that the prepared materials are glasses. The structures of the obtained glasses were compared to commercial material using FTIR, Al-27 and Si-29 MAS-NMR. The analysis of FTIR and MAS-NMR spectra indicated that the systems developed and commercial material are formed by SiO4 and AlO4 linked tetrahedra. These structures are essential to get the set time control and to have cements. These results encourage further applications of the experimental glasses in the formation of GICs. (C) 2004 Elsevier B.V. All rights reserved.