The present investigation calculates the surface tension and adsorption functions of the Fe-S, Fe-N, and Fe-S-N melts at 1823 K using the modified form of Butler's equations and the derived values of the surface interaction parameters of the systems. The calculated values are found to be in good agreement with those of the experimental data of the systems. The present analysis indicates similar adsorption behavior of sulfur for the Fe-S and Fe-S-N systems at 1823 K. Although a linear adsorption behavior is observed in the Fe-N system, an inverse relationship in the adsorption behavior exists between sulur and nitrogen in the Fe-S-N system.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The utility of tetrathiomolybdate in a variety of organic transformations is presented in this account. The sulfur transfer ability of tetrathiomolybdate is exploited in the synthesis of organic disulfides under mild reaction conditions. The induced internal redox reactions associated with tetrathiomolybdate have been thoroughly exploited in developing various methodologies, which include the reduction of organic azides, synthesis of diselenides, cyclic imines, thioamides, and thiolactams. In addition, novel deprotection strategies using tetrathiomolybdate have been developed to cleave the propargyl and propargyloxy carbonyl (POC) protecting groups. Tetrathiomolybdate mediated tandem sulfur transfer-reduction-Michael reactions have been applied to the synthesis of sulfur containing bicyclic systems. Furthermore, the reactions in the solid state and the reactions in water medium assisted by tetrathiomolybdate have greatly simplified the synthesis of organic disulfides.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The design and synthesis of agents that can abstract zinc from their [CCXX] (C=cysteine; X=cysteine/histidine) boxes by thioldisulfide exchange-having as control, the redox parities of the core sulfur ligands of the reagent and the enzyme, has been illustrated, and their efficiency demonstrated by monitoring the inhibition of the transcription of calf thymus DNA by E. coli RNA polymerase, which harbors two zinc atoms in their [CCXX] boxes of which one is exchangeable. Maximum inhibition possible with removal of the exchangeable zinc was seen with redox-sulfanilamide-glutamate composite. In sharp contrast, normal chelating agents (EDTA, phenanthroline) even in a thousand fold excess showed only marginal inhibition, thus supporting an exchange mechanism for the metal removal. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Copper(II) complexes Cu(satp)(L)] (1-3) of a Schiff base thiolate (salicylidene-2-aminothiophenol, H(2)satP) and phenanthroline bases (L), viz. 1,10-phenanthroline (phen in 1), dipyrido3,2-d:2',3'-f]quinoxaline (dpq in 2) and dipyrido3,2-a:2',3'-c]phenazine (dppz in 3), were prepared, characterized and their anaerobic DNA photocleavage activity and hypoxic photocytotoxicity studied. The redox active complexes show the Cu(II)-Cu(I) couple near -0.5 V for 1 and near 0.0 V vs. SCE (saturated calomel electrode) for 2 and 3. The one-electron paramagnetic complexes (similar to 1.85 mu(B)) are avid DNA binders giving K(b) values within 1.0 x 10(5) - 8.0 x 10(5) M(-1). Thermal melting and viscosity data along with molecular docking calculations suggest DNA groove and/or partial intercalative binding of the complexes. The complexes show anaerobic DNA cleavage activity in red light under argon via type-I pathway, while DNA photocleavage in air proceeds via hydroxyl radical pathway. The DFT (density functional theory) calculations reveal a thyil radical pathway for the anaerobic DNA photocleavage activity and suggest the possibility of generation of a transient copper(I) species due to bond breakage between the copper and sulfur to generate the thyil radical. An oxidation of the copper(I) species is likely by oxygen in an aerobic medium or by the buffer medium in an anaerobic condition. Complex 3 exhibits significant photocytotoxicity in HeLa cells (IC(50) = 8.3(+/- 1.0) mu M) in visible light, while showing lower dark toxicity (IC(50) = 17.2(+/- 1.0) mu M). A significant reduction in the dark toxicity is observed under hypoxic cellular conditions (IC(50) = 30.0(+/- 1.0) mu M in dark), while retaining its photocytotoxicity (IC(50) = 8.0(+/- 1.0) mu M). (C) 2011 Elsevier Inc. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Ternary Schiff base copper(II) complex [CuL(phen)](ClO4), where HL is 2-(methylthio)ethylsalicylaldimine and phen is 1,10-phenanthroline, has been prepared and structurally characterized by X-ray crystallography. The complex shows a CuN3OS coordination in a square-pyramidal (4 + 1) geometry with the sulfur as an equatorial ligand. The complex is an avid binder to double-stranded DNA in the minor groove and exhibits both photonuclease and chemical nuclease activity. When exposed to UV light of 312 nm (96 W) or visible light of 532 nm (125 W) under aerobic conditions, the complex causes significant cleavage of supercoiled pUC19 DNA in the absence of any externally added reducing agent or H2O2.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel wet-chemical precipitation method is optimized for the synthesis of ZnS nanocrystals doped with Cu+ and halogen. The nanoparticles were stabilized by capping with polyvinyl pyrrolidone (PVP). XRD studies show the phase singularity of ZnS particles having zinc-blende (cubic) structure. TEM as well as XRD line broadening indicate that the average crystallite size of undoped samples is similar to2 nm. The effects of change in stoichiometry and doping with Cu+ and halogen on the photoluminescence properties of ZnS nanophosphors have been investigated. Sulfur vacancy (Vs) related emission with peak maximum at 434 nm has been dominant in undoped ZnS nanoparticles. Unlike in the case of microcrystalline ZnS phosphor, incorporation of halogens in nanoparticles did not result V-Zn related self-activated emission. However, emission characteristics of nanophosphors have been changed with Cu+ activation due to energy transfer from vacancy centers to dopant centers. The use of halogen as co-activator helps to increase the solubility of Cu+ ions in ZnS lattice and also enhances the donor-acceptor type emission efficiency. With increase in Cu+ doping, Cu-Blue centers (CuZn-Cui+), which were dominant at low Cu+ concentrations, has been transformed into Cu-Green (Cu-Zn(-)) centers and the later is found to be situated near the surface regions of nanoparticles. From these studies we have shown that, by controlling the defect chemistry and suitable doping, photoluminescence emission tunability over a wide wavelength range, i.e., from 434 to 514 nm, can be achieved in ZnS nanophosphors. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Substitutional self-assembly of thiol and selenol SAMs from a lying-down phase of butanedithiol (C4DT) (SAM) were investigated using thiols, disulfide, and diselenide molecules. The intent was to address the question if formation of a lying-down dithiol phase is an impediment to formation of standing-up dithiol phases as it has been assumed. It is demonstrated that this is not the case, and the C4DT SAM, where both the sulfur atoms are chemisorbed on gold, is removed and replaced in all cases. Differences in substitution kinetics are observed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Gold nanoparticles with average diameters in the range 2.515 nm, prepared at the organic/aqueous interface by using tetrakis( hydroxymethyl) phosphonium chloride (THPC) as reducing agent, exhibit ferromagnetism whereby the saturation magnetization M(S) increases with decreasing diameter and varies linearly with the fraction of surface atoms. The value of M(S) is higher when the particles are present as a film instead of as a sol. Capping with strongly interacting ligands such as alkane thiols results in a higher M(S) value, which varies with the strength of the metal-sulfur bond. Ferromagnetism is also found in Pt and Ag nanoparticles prepared as sols, and the M(S) values vary as Pt > Au > Ag. A careful study of the temperature variation of the magnetization of Au nanoparticles, along with certain other observations, suggests that small bare nanoparticles of noble metals could indeed possess ferromagnetism, albeit weak, which is accentuated in the presence of capping agents, specially alkane thiols which form strong metal-sulfur bonds.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In the present study, the synthesis and characterization of a series of N-methylimidazole-based thiourea and selenourea derivatives are described. The new compounds were also studied for their ability to inhibit peroxynitrite (PN)- and peroxidase-mediated nitration of protein tyrosine residues. It has been observed that the selenourea derivatives are more efficient than the thiourea-based compounds in the inhibition of protein nitration. The higher activity of selenoureas as compared to that of the corresponding thioureas can be ascribed to the zwitterionic nature of the selenourea moiety. Single crystal X-ray diffraction studies on some of the thiourea and selenourea derivatives reveal that the C S bonds in thioureas possess more of double bond character than the C=Se bonds in the corresponding selenoureas. Therefore, the selenium compounds can react with PN or hydrogen peroxide much faster than their sulfur analogues. The reactions of thiourea and selenourea derivatives with PN or hydrogen peroxide produce the corresponding sulfinic or seleninic acid derivatives, which upon elimination of sulfurous/selenous acids produce the corresponding N-methylimdazole derivatives.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Measurements on the solid electrolyte cell(Ar -b H2 ~ H2S/CaS + CaF2 ~- ( P t ) / / C a F 2 / / ( P t )-~- CaF2 ~ CaS/H2S ~- H2 ~- At) show that the emf of the cell is directly related through the Nernst equation to the difference in sulfur potentials established at the two Ar ~- H2 ~ H2S/electrode interfaces. The electrodes are designed to convert the sulfur potential gradient across the calcium fluoride electrolyte into an equivalent fluorine potential gradient with the aid of the reaction, CaF2(s) ~ 1~ S2(g)-e CaS(s) ~- F2(g). The response time of the probe varies from approximately 9 hr at 990~ to 2.5 hr at 1225~ The conversion of calcium sulfide and/or calcium fluoride into calcium oxide should not be a problem in anticipated commercial coal gasification systems. Suggestions are presented for improving the cell for such commercial applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The stability fields of various sulfide phases that form on Fe-Cr, Fe-Ni, Ni-Cr, and Fe-Cr-Ni alloys have been developed as a function of temperature and the partial pressure of sulfur. The calculated stability fields in the ternary A-B-S system are displayed on plots of log \textpS2 pS2 vs. the conjugate extensive variable (nA/nA–nB), which provides a better framework for following the sulfidation of Fe-Cr-Ni alloys at high temperatures. Experimental and estimated thermodynamic data were used in developing the sulfur potential diagrams. Current models and correlations were employed to estimate the unknown thermodynamic behavior of solid solutions of sulfides and to supplement the incomplete phase-diagram data of geophysical literature. These constructed stability field diagrams are in excellent agreement with the sulfide phases and compositions determined experimentally during the sulfidation of SAE 310 stainless steel. The sulfur potential plots appear to be very useful in predicting and correlating the sulfidation of commercial alloys.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A critical revi<:w of the possibilities of measuring the ~artlal pressure of sulfur using solid state galvanic cells )'n;;cd on AgI, C" , B-alumina, CaO-Zr02' Na2S04-I and doped ;:":;, ,,,Ilil "Iltl ,,11: auxiliary "jectrodes are presentlOu. SOIll..., df tllc!iL' sYHtcmH h,}vu inherent limltntlol1$ when <:xl'o" ...d to environments contilining both oxygen and sulfur. Electrode polarization due to electronic conduction in the solid electrolyte is a significant factor limiting the ;lC'e,"'acy of isotlwrm:l1 cell",. The electrochemical flux of{lit' !'\)ndlwl Ill}: Ion LhnHO',h tht' ('!('ctrojyt(~ C:Ul },(,! llIinlnliz(,{j pfUjJL!f cell. dL:~) i.t',11. Noni!:iot.herm~ll cells \.Jlth temperaLure compensated reference electrodes have a number of advantages over thC'ir isothermal counterparts.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Corrosion of SAE 310 stainless steel in H2-H2O-H2S gas mixtures was studied at a constant temperature of 1150 K. Reactive gas mixtures were chosen to yield a constant oxygen potential of approximately 6 × 10-13 Nm-2 and sulfur potentials ranging from 0.19 × 10-2 Nm-2 to 33 × 10-2 Nm-2. The kinetics of corrosion were determined using a thermobalance, and the scales were analyzed using metallography, scanning electron microscopy, and energy dispersive X-ray analysis. Two corrosion regimes, which were dependent on sulfur potential, were identified. At high sulfur potentials (P S 2 ± 2.7 × 10-2 Nm-2) the corrosion rates were high, the kinetics obeyed a linear rate equation, and the scales consisted mainly of sulfide phases similar to those observed from pure sulfidation. At low sulfur potentials (P S 2 ± 0.19 × 10-2 Nm-2) the corrosion rates were low, the kinetics obeyed a parabolic rate equation, and scales consisted mainly of oxide phases. Thermochemical diagrams for the Fe-Cr-S-O, Fe-Ni-S-O, Cr-Ni-S-O, and Si-Cr-S-O systems were constructed, and the experimental results are discussed in relation to these diagrams. Based on this comparison, reasonable corrosion mechanisms were developed. At high sulfur potentials, oxide and sulfide phases initially nucleate as separate islands. Overgrowth of the oxide by the sulfide occurs and an exchange reaction governs the corrosion process. Preoxidation at low oxygen potentials and 1150 K is beneficial in suppressing sulfidation at high sulfur potentials.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Mixed ionic and electronic conduction in Zr02-based solid electrolytes was studied.The effect of impurities and second-phase particles on the mixed conduction parameter, P,, was measured for different types of ZrOZ electrolytes. The performance of solid-state sensors incorporating ZrOZ electrolytes is sometimes limited by electronic conduction in ZrOZ, especially at temperatures >I800 K. Methods for eliminating or minimizing errors in measured emf due to electronically driven transport of oxygen anions are discussed. Examples include probes for monitoring oxygen content in liquid steel as well as the newly developed sulfur sensor based on a ZrOz(Ca0) + CaS electrolyte. The use of mixed conducting ZrOZ as a semipermeable membrane or chemically selective sieve for oxygen at high temperatures is discussed. Oxygen transport from liquid iron to CO + C& gas mixtures through a ZrOZ membrane driven by a chemical potential gradient, in the absence of electrical leads or imposed potentials, was experimentally observed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Ternary phase relations in the Co-Cr-S system at 1223 K were determined using microprobe analysis of quenched samples. The results are consistent with the data available on the binary systems. A complete solid solution exists between cobalt monosulfide and chromium monosulfide. The CoCr2S4 thiospinel is the only ternary compound formed. A sulfur potential diagram was constructed for the region involving equilibrium between alloy and monosulfide based on thermodynamic data on the Co-Cr, Co-S, and Cr-S binary systems and the ternary information obtained in this study. The sulfidation behavior of Co-Cr alloys reported in the literature is discussed in light of the sulfur potential diagram.